KR960023292A - High Elongation Low Shrinkage Polyester Fiber and Manufacturing Method Thereof - Google Patents

High Elongation Low Shrinkage Polyester Fiber and Manufacturing Method Thereof Download PDF

Info

Publication number
KR960023292A
KR960023292A KR1019940037633A KR19940037633A KR960023292A KR 960023292 A KR960023292 A KR 960023292A KR 1019940037633 A KR1019940037633 A KR 1019940037633A KR 19940037633 A KR19940037633 A KR 19940037633A KR 960023292 A KR960023292 A KR 960023292A
Authority
KR
South Korea
Prior art keywords
polyester fiber
high elongation
low shrinkage
manufacturing
shrinkage polyester
Prior art date
Application number
KR1019940037633A
Other languages
Korean (ko)
Other versions
KR100193940B1 (en
Inventor
박충환
Original Assignee
이웅열
주식회사 코오롱
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이웅열, 주식회사 코오롱 filed Critical 이웅열
Priority to KR1019940037633A priority Critical patent/KR100193940B1/en
Publication of KR960023292A publication Critical patent/KR960023292A/en
Application granted granted Critical
Publication of KR100193940B1 publication Critical patent/KR100193940B1/en

Abstract

본 발명은 직물의 내구성 및 후가공시 형태 안정성을 향상시키기 위하여 사용하는 고신율 저수축 폴리에스테르 섬유 및 그 제조방법에 관한 것으로, 담섬유 섬도가 7∼15데니어이며 다음 특성을 동시에 만족함을 특징으로 하는 것이다.The present invention relates to a high-elongation low-shrink polyester fiber used to improve the durability of the fabric and form stability during post-processing and a method of manufacturing the same, characterized in that the bile fiber fineness is 7 to 15 denier and simultaneously satisfies the following characteristics: will be.

고유점도 : 0.85 이상, 절단신도 : 25% 이상, 190℃×15분 처리후의 건열수축율 : 5% 이하, 강도지수 : 35 이상.Intrinsic viscosity: 0.85 or more, Elongation at break: 25% or more, dry heat shrinkage after treatment at 190 ° C for 15 minutes: 5% or less, strength index: 35 or more.

Description

고신율 저수축 폴리에스테르 섬유 및 그의 제조방법High Elongation Low Shrinkage Polyester Fiber and Manufacturing Method Thereof

본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.

Claims (2)

단섬유 섬도가 7∼15데니어이며 다음 특성을 동시에 만족함을 특징으로 하는 고신율 저수축 폴리에스테르 섬유.A high elongation low shrinkage polyester fiber characterized by short fiber fineness of 7 to 15 deniers and simultaneously satisfying the following characteristics. 고유점도 : 0.85 이상, 절단신도 : 25% 이상, 190℃×15분 처리후의 건열수축율 : 5% 이하, 강도지수 : 35 이상.Intrinsic viscosity: 0.85 or more, Elongation at break: 25% or more, dry heat shrinkage after treatment at 190 ° C for 15 minutes: 5% or less, strength index: 35 or more. 고유점도가 0.85 이상인 폴리에스테르 폴리머를 400∼1,000/min으로 방사하고 연이어 5.0∼6.5 연신배율로 220∼250℃에서 연신하여 단섬도가 7∼15데니어로 하고 10∼15%로 이완, 열처리한 후 권취함을 특징으로 하는 고신율 저수축 폴리에스테르 섬유의 제조방법.After spinning the polyester polymer having an intrinsic viscosity of 0.85 or more at 400 to 1,000 / min and subsequently stretching at 220 to 250 ° C. at 5.0 to 6.5 draw ratio, the single fineness is 7 to 15 denier, and is relaxed and heat treated to 10 to 15%. A method for producing a high elongation low shrinkage polyester fiber characterized by winding. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019940037633A 1994-12-28 1994-12-28 Manufacturing method of high elongation low shrink polyester fiber KR100193940B1 (en)