KR20160147429A - The complexing agent for the solid fuel - Google Patents
The complexing agent for the solid fuel Download PDFInfo
- Publication number
- KR20160147429A KR20160147429A KR1020150084164A KR20150084164A KR20160147429A KR 20160147429 A KR20160147429 A KR 20160147429A KR 1020150084164 A KR1020150084164 A KR 1020150084164A KR 20150084164 A KR20150084164 A KR 20150084164A KR 20160147429 A KR20160147429 A KR 20160147429A
- Authority
- KR
- South Korea
- Prior art keywords
- paraffin
- solid fuel
- easy
- fiber board
- complexing agent
- Prior art date
Abstract
The present invention relates to a complexing agent for a solid fuel, which comprises a paraffin wax in a solid state in a vessel and heating the liquid phase to paraffin by heating at 45 ° C to 65 ° C. And a paraffin melting step of immersing the paraffin in phase change liquid paraffin for 10 minutes to a size of 60 mm x 90 mm x 15 mm to allow the paraffin to penetrate through the pores of the fiber board And a fibrous panel drying step of taking out the fibrous sheet impregnated with the paraffin between the pores through the fiber board immersion step and then drying at room temperature for at least one day to complete the complexing agent.
Therefore, the solid fuel such as firewood, charcoal, various coal, etc. can be quickly and safely ignited, and since the user does not need to ignite the solid fuel for a long time at a close distance, It is a very useful invention that is easy to manufacture and easy to manufacture, cheap in production cost, easy to use, lightweight and small in volume, easy to store and move.
Description
The present invention relates to a complexing agent for solid fuel, and more particularly, to a complexing agent for solid fuel capable of rapidly and safely igniting solid fuel such as wood, including charcoal, coal and firewood, in a camping field.
Generally, camping grounds use fuel such as gas or briquettes, but charcoal grilling that can enjoy the flavor of charcoal fire is popularly popular because fumes from charcoal fire permeate into meat.
Solid fuels such as firewood, charcoal, briquette, coal, and coke are not easily ignited because they have a higher ignition point than liquid or gaseous fuels. However, since they are burnt for a long time after being ignited and are cheap, they are used as fuels in greenhouses, It is widely used.
These solid fuels must be supplied with a sufficient amount of heat until they are ignited. Since such solid fuels are usually exposed to the outdoor or stored in a moist place, the fuel itself contains a lot of moisture and takes considerable time to be ignited. There is a considerable inconvenience in igniting the solid fuel because the harmful gas harmful to the human body is generated and released during the ignition and the heat should be supplied again when the supply of heat is stopped before the solid fuel is ignited, Thermal energy is lost as it is.
Meanwhile, in order to ignite the solid fuel such as firewood and various coal including the above-mentioned charcoal, it is a primitive method of spraying petroleum with firewood or spraying gas directly to the solid fuel using a torch In this case, the ignition is slow, the smell is bad, the smoke is not only serious but also has a dangerous disadvantage.
In addition, conventionally, since there is no suitable complexing agent for igniting solid fuel, it is troublesome to ignite by injecting a large amount of harmonized wood or paper box, resulting in dust, soot, and the like.
Therefore, it is required to develop a solid fuel complexing agent which can continuously supply heat until the solid fuel is stably ignited without igniting the solid fuel directly when igniting the solid fuel, and does not need to ignite the solid fuel for a long time. .
Therefore, it is a first object of the present invention to solve and solve the above-mentioned problems, and it is an object of the present invention to provide a fuel cell system capable of quickly and safely igniting a solid fuel and preventing a solid fuel from igniting when the solid fuel is ignited The second is to provide a complexing agent for solid fuel which is advantageous not to be exposed to various harmful gases. Secondly, it is easy to manufacture and low in production cost, easy to use, light and small in volume, And it is an object of the present invention to provide a complexing agent for a solid fuel which is easy to be stored for a long period of time even when wetted with water and easy to ignite.
In order to achieve the above object, the present invention provides a method for producing a paraffin wax (Paraffin wax) in which a paraffin wax in a solid state is placed in a vessel and the phase is changed to liquid paraffin by heating at 45 to 65 ° C. Dipping a medium density fiberboard (MDF) having a size of 60 mm x 90 mm x 15 mm into a phase-change liquid paraffin through the paraffin melting step for 10 minutes to infiltrate paraffin between the pores of the fiber board, And a fiber board drying step of taking out the fiber board in which the paraffin has permeated between the pores through the fiber board immersion step, and drying the fiber board at room temperature for one day or more to complete the complex agent.
According to the construction of the present invention as described above, solid fuel such as firewood, charcoal, various coal, etc. can be quickly and safely ignited, and the user does not need to ignite the solid fuel for a long time at a close distance. There is an advantage that the user is not exposed to various harmful gases generated.
In addition, it is a very useful invention that is easy to manufacture, easy to manufacture, low in production cost, easy to use, light and small in volume, easy to store and transport, easy to store for a long period of time even in wet water, and easy to ignite.
1 is a block diagram showing a method for producing a complexing agent for a solid fuel according to an embodiment of the present invention
Hereinafter, embodiments according to the present invention will be described with reference to the accompanying drawings.
FIG. 1 is a block diagram showing a method for producing a complexing agent for a solid fuel according to an embodiment of the present invention. Referring to FIG. 1, a method for producing a complexing agent for a solid fuel according to an embodiment of the present invention includes a paraffin melting step It consists of fiber board immersion stage and fiberboard drying stage.
The paraffin melting step is a step of putting a paraffin wax in a solid state in a vessel and changing the phase to liquid paraffin by heating at 45 ° C to 65 ° C.
Particularly, when the paraffin wax has a melting point of 45 ° C to 65 ° C and is heated to a temperature of less than 45 ° C, the paraffin wax is not melted.
The paraffin wax is not only a paraffin wax but also a candle made of beeswax.
After the melting step of the paraffin, a medium density fiberboard (MDF) having a size of 60 mm × 90 mm × 15 mm was immersed in a liquid phase paraffin which was phase-changed from a solid to a liquid through a paraffin melting step for 10 minutes, A fiberboard immersion step is carried out to allow paraffin to penetrate between the pores.
The medium-density fiberboard is commonly used as a MDF, and a low-density fiberboard (LDF) or a compressed paper can be used instead of the medium-density fiberboard. In general, all wood has a disadvantage that it is difficult to use due to the difficulty of permeation of paraffin because of a small gap between the fiber boards at high density.
In addition, the medium-density fiberboard has a width of 60 mm, a length of 90 mm, and a thickness of 15 mm, but it may be 50 to 70 mm long, 70 to 100 mm long, and 10 to 20 mm thick depending on the type and properties of the solid fuel .
However, in general, when a medium-density fiberboard having a size of 60 mm × 90 mm × 15 mm is used, the burning time required to fire coal and coal types and firewood is enough.
After the fiber board immersion step, the fibrous sheet impregnated with the paraffin through the pores is taken out of the container through the fiber board immersion step, and the fibrous panel is dried at room temperature for 1 day or more, and the fibrous sheet is dried to complete the complex agent for solid fuel.
Since the complexing agent for solid fuel thus produced can quickly and safely ignite the solid fuel and the user does not need to ignite the solid fuel at a close distance for a long time, It is easy to manufacture, easy to manufacture, easy to manufacture, cheap and easy to use, light and small in volume, easy to store and transport, easy to store for a long time even when wet, and easy to ignite Very useful invention to be.
Claims (3)
Dipping a medium density fiberboard (MDF) having a size of 60 mm x 90 mm x 15 mm into phase change liquid paraffin through the paraffin melting step for 10 minutes so that paraffin penetrates between pores of the fiber board;
And a fiber board drying step of taking out the fiber board in which the paraffin has penetrated between the pores through the fiber board immersion step and then drying the fiber board at room temperature for 1 day or longer to complete the complex agent.
Wherein the medium density fibrous sheet is a low density fibrous sheet (LDF)