KR20080076890A - The manufacturing method of the fishing rod - Google Patents

The manufacturing method of the fishing rod Download PDF

Info

Publication number
KR20080076890A
KR20080076890A KR1020080074935A KR20080074935A KR20080076890A KR 20080076890 A KR20080076890 A KR 20080076890A KR 1020080074935 A KR1020080074935 A KR 1020080074935A KR 20080074935 A KR20080074935 A KR 20080074935A KR 20080076890 A KR20080076890 A KR 20080076890A
Authority
KR
South Korea
Prior art keywords
fishing rod
mold
manufacturing
long groove
yarn
Prior art date
Application number
KR1020080074935A
Other languages
Korean (ko)
Other versions
KR101008826B1 (en
Inventor
반용오
Original Assignee
주식회사 강원산업
반용오
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 강원산업, 반용오 filed Critical 주식회사 강원산업
Priority to KR1020080074935A priority Critical patent/KR101008826B1/en
Publication of KR20080076890A publication Critical patent/KR20080076890A/en
Application granted granted Critical
Publication of KR101008826B1 publication Critical patent/KR101008826B1/en

Abstract

A manufacturing method of a fishing rod is provided to prevent the fishing rod from getting curved as time lapses by attaching a reinforcing yarn inside the surface of a fishing rod. A manufacturing method of a fishing rod includes: a mold manufacturing step of manufacturing a mold by forming a long groove(12) in a longitudinal direction to insert and attach a reinforcing yarn(13) to the mold(11); a molding step of attaching a reinforcing yarn to the long groove, attaching and winding a textile(14) consisting of anyone of a glass fiber and a carbon fiber, whose upper surfaces are impregnated with resin, on the mold and heating it up to 120 deg.C to mold; and a painting step of separating the molded fishing rod body(10) from the mold and painting and grinding the surface thereof.

Description

낚싯대의 제조방법 { The manufacturing method of the fishing rod }The manufacturing method of the fishing rod}

본 발명은 낚싯대의 제조방법에 관한 것으로, 더욱 상세하게 설명하면, 낚싯대 금형에 길이방향으로 장홈을 형성하여 상기 장홈에 탄성과 강도가 우수한 보강사를 부착하여 성형함으로써 탄성 및 강도는 물론 낚싯대의 휘어짐을 방지하는 낚싯대의 제조방법에 관한 것이다. The present invention relates to a method of manufacturing a fishing rod, in more detail, by forming a long groove in the rod mold in the longitudinal direction by attaching a reinforcing yarn excellent in elasticity and strength to the long groove, the elastic and strength as well as the bending of the fishing rod It relates to a method of manufacturing a fishing rod to prevent.

일반적으로 낚싯대라 함은 낚싯줄을 매어 물고기를 잡을 때, 쓰는 가늘고 긴 대를 말하는 것으로, 종래에는 대나무 낚싯대를 주로 사용하였으나, 근래에 들어서는 수지가 함침된 유리섬유 또는 카본섬유 등의 원단으로 제작된 낚싯대가 주목을 받고 있다. In general, a fishing rod refers to a thin and long rod that is used when catching a fish by tying a fishing line. In the past, a bamboo fishing rod is mainly used. However, in recent years, a fishing rod made of fabric such as glass fiber or carbon fiber impregnated with resin Is getting attention.

상기와 같은 낚싯대는 단지 물고기를 낚는 도구를 뛰어넘어 소장가치 또한 대단히 높아서 낚싯대 표면의 외관이나 강도 등의 부분도 대단히 중요시되는바, 종래 낚싯대의 제조방법을 살펴보면, 금형에 맞추어 재단된 원단을 낚싯대 본체 제조 용 금형에 맞추어 접착후 롤링시키고 롤링된 원단표면에 보강사인 보론사 또는 케블라사 중 어느 하나를 'X'자 또는 나선형으로 감아 부착시키고, 상면에 성형용 고온 테이프를 조밀한 간격으로 감은 후, 이를 120℃의 성형로에서 2~3시간을 가열 성형시키면 롤링된 원단이 성형되면서 원단에 함유된 열가소성수지는 팽창되어져 원단과 함께 성형되고 잔여량의 수지액은 고온 테이프의 틈 사이로 유출되어지면서 성형이 이루어진다. Such a fishing rod is more than just a fish-fishing tool, the collection value is also very high, so the appearance and strength of the surface of the fishing rod is also very important. After bonding to the mold for manufacturing, roll and roll any one of reinforcement boron yarn or Kevlar yarn on the rolled fabric surface by 'X' or spirally wound and wind the high temperature tape for molding on the upper surface at a tight interval. When this is heated for 2 ~ 3 hours in the forming furnace at 120 ℃, the rolled fabric is molded and the thermoplastic resin contained in the fabric is expanded and molded together with the fabric, and the remaining amount of resin liquid flows out between the gaps of the high temperature tape. Is done.

이와 같이 성형된 낚싯대 본체를 금형과 분리시킨 후, 낚싯대 표면의 고온 테이프를 풀어내고 도장작업을 위한 연마공정과 낚싯대 외관의 무늬장식을 위한 도장공정을 통하여 낚싯대가 가공되어진다. After separating the fishing rod body formed in this way from the mold, the fishing rod is processed through a high temperature tape on the surface of the fishing rod, a polishing process for painting and a painting process for decoration of the appearance of the fishing rod.

상기와 같은 방법으로 제조된 종래의 낚싯대 본체를 도 1을 통해 살펴보면, 낚싯대 본체(10) 표면 외부에 보강사(13)가 감겨져 있어 탄성 및 강도가 향상되는 효과는 있으나, 시간이 지날수록 낚싯대 본체가 길이방향으로 휘어지는 문제점을 해결하지 못하였다.Looking at the conventional fishing rod body manufactured by the above method through Figure 1, the reinforcement yarn 13 is wound around the surface of the fishing rod body 10, the elasticity and strength is improved, but the rod body as time passes Did not solve the problem of bending in the longitudinal direction.

또한 낚싯대 본체 표면 외부에 보강사(13)가 감겨져 있기 때문에 도장공정과 연마공정시 표면의 보강사때문에 작업이 어렵고 작업 시간이 오래 걸리는 등의 또 다른 문제점을 내포하고 있다.In addition, since the reinforcing yarn 13 is wound on the outer surface of the fishing rod main body, the reinforcing yarn of the surface during the coating process and the polishing process has another problem such as difficulty in working and long working time.

이에 본 발명은 상기와 같은 문제점을 감안하여 발명한 것으로, Therefore, the present invention was invented in view of the above problems,

본 발명은 크게 세 단계의 공정으로 이루어지는 바, 테이퍼진 금속 환봉 형태로 구성된 금형에 상기 금형의 표면 길이 방향으로 보강사가 삽입될 수 있도록 장홈을 형성하여 제작하는 금형제조공정과; 상기 장홈에 보강사를 부착한 뒤 상면에 원단을 부착 권취하여 낚싯대 본체를 성형하는 성형공정과; 상기 성형된 낚싯대 본체의 표면을 도장 및 연마하는 도장공정으로 이루어지는 대략적인 구성을 갖는다. The present invention includes a mold manufacturing process for forming a long groove so that a reinforcement thread can be inserted into a mold formed in a tapered metal round bar shape in the longitudinal direction of the surface of the mold. A molding process of forming a fishing rod body by attaching a reinforcing yarn to the long groove and then attaching and winding a fabric to an upper surface thereof; It has a rough structure which consists of a coating process which coats and polishes the surface of the said molded rod main body.

상기와 같이 구성된 본 발명은, 일반적으로 낚싯대 본체의 표면 외부에 보강사를 'X'자 또는 나선형으로 감아 부착하는 제조방법과 달리, 보강사가 낚싯대의 표면 내부에 길이 방향으로 일정하게 부착되어 있어, 상기 부착된 보강사로 인해 낚시대 본체가 시간이 경과함에 따라 조금씩 휘어지는 현상을 방지하는 한편, 길이 방향으로 결합된 보강사로 인해 낚싯대의 길이방향 탄성력이 향상될 수 있으며, 보강사가 낚싯대 본체의 내부에 부착됨으로써 성형된 낚싯대 표면이 매끄러워 표면 도장 및 연마공정 작업이 종래보다 수월해지고, 외관 또한 간결하고 미려해지는 효 과가 있다. In the present invention configured as described above, in general, unlike the manufacturing method of winding the reinforcement yarn on the outside of the surface of the fishing rod body in a 'X' shape or spirally, the reinforcement yarn is constantly fixed in the longitudinal direction inside the surface of the fishing rod, Due to the attached reinforcement yarn to prevent the fishing rod body slightly bends over time, while the longitudinal reinforcement of the fishing rod due to the reinforcement coupled in the longitudinal direction can be improved, the reinforcement is attached to the inside of the fishing rod body The molded rod surface is smooth, which makes the surface painting and polishing process easier than before, and the appearance is simple and beautiful.

본 발명은 낚싯대의 제조방법에 관한 것으로, 더욱 상세하게 설명하면, 보강사를 삽입할 수 있는 장홈이 형성된 금형을 이용하여 낚싯대 본체의 내부면에 보강사를 결합시킴으로써 장시간 사용 시의 낚싯대의 휨현상을 방지하고 길이방향의 탄성력을 향상시킬 수 있도록 한 낚싯대의 제조방법에 관한 것이다.The present invention relates to a method of manufacturing a fishing rod, and in more detail, by using a mold having a long groove into which a reinforcement thread can be inserted, the reinforcement yarn is bonded to the inner surface of the fishing rod body to prevent bending of the fishing rod during long time use. The present invention relates to a method for manufacturing a fishing rod, which can prevent and improve elasticity in a longitudinal direction.

이하 본 발명의 실시 예를 예시도면을 통해 살펴보면 다음과 같다. An embodiment of the present invention will be described below with reference to the accompanying drawings.

도 2는 본 발명 낚싯대 제조방법을 보여주는 사시도이며, 도 3은 본 발명의 낚싯대를 도시한 단면도이고, 도 4는 본 발명 낚싯대의 제조공정을 나타낸 공정도로, 도시한 바와 같이 본 발명은 크게 세 단계의 공정으로 제조되는 바, 금형제조공정(S1)과 성형공정(S2), 도장공정(S3)을 통해 낚싯대의 제작을 완료한다. Figure 2 is a perspective view showing a fishing rod manufacturing method of the present invention, Figure 3 is a cross-sectional view showing a fishing rod of the present invention, Figure 4 is a process diagram showing a manufacturing process of the fishing rod of the present invention, as shown in the present invention is largely three steps Bar is manufactured by the process of, the manufacturing process of the fishing rod is completed through the mold manufacturing process (S1), the molding process (S2), the coating process (S3).

우선, 제 1공정은 원단을 접착 후 권취할 수 있는 금형(11)을 제작하는 금형제조공정(S1) 단계로서, 테이퍼진 금속 환봉 형태로 구성되되, 길이방향으로는 보강사(13)가 삽입될 수 있도록 반원형상의 장홈(12)이 형성되어 있는 것이 특징이다.First, the first process is a mold manufacturing process (S1) step of manufacturing a mold 11 that can be wound up after the fabric is bonded, consisting of a tapered metal round bar form, the reinforcement yarn 13 is inserted in the longitudinal direction It is characterized in that the semicircular long groove 12 is formed to be.

상기 보강사(13)는 보론사 또는 케블라사 중 어느 하나를 사용하면 되고, 상기 금형(11)에 형성되어 있는 장홈(12)의 개수는 도 2에 도시된 바와 같이 장홈(12)의 개수가 상,하,좌,우 4개로 표현이 되어 있으나, 이는 일 예로 설명한 것 뿐이고, 금형(11)의 규격에 따라 3 내지 7개 이상으로 구성될 수 있으며, 이러한 구성은 발명이 속하는 기술분야에서 통상의 지식을 가진 자라면 누구든지 용이하게 변형실시가 가능한 것은 물론이고, 그와 같은 변형실시는 본 발명의 권리범위 내에 속하는 것이 자명한 사실이라 할 것이다.The reinforcing yarn 13 may be any one of boron yarn or kevlar yarn, and the number of the long grooves 12 formed in the mold 11 is the number of the long grooves 12 as shown in FIG. 2. Up, down, left, and right four are represented, but this is only described as an example, it may be composed of three to seven or more according to the standard of the mold 11, this configuration is usually in the art to which the invention belongs. Anyone skilled in the art can easily make modifications, and such modifications are obviously within the scope of the present invention.

그 후 행해지는 제 2공정은, 상기 금형제조공정(S1)이 완료된 후 소재를 성형하는 성형공정(S2)단계로, 이를 더욱 상세하게 살펴보면, 금형제조공정(S1)에서 제작된 금형(11)을 바탕으로 우선 금형(11)에 형성되어 있는 장홈(12)에 보강사(13)를 삽입한 뒤, 금형의 외면에 원단(14)을 접착 권취하고, 권취된 원단 표면에 성형용 고온 테이프를 조밀한 간격으로 감은 후 이를 120℃의 성형로에서 2 내지 3시간 가열시킨다. After that, the second step is a molding step (S2) of molding a material after the mold manufacturing step (S1) is completed. Looking at this in more detail, the mold (11) manufactured in the mold manufacturing step (S1) First, the reinforcing yarn 13 is inserted into the long groove 12 formed in the mold 11, and then the fabric 14 is adhesively wound on the outer surface of the mold, and the high temperature tape for molding is applied to the wound fabric surface. After winding at dense intervals, it is heated in a forming furnace at 120 ° C. for 2-3 hours.

상기 성형공정(S2)에서 사용되는 원단(14)은 수지가 함침된 유리섬유 또는 카본섬유 등을 사용한다. The fabric 14 used in the molding process S2 uses glass fiber or carbon fiber impregnated with resin.

상기에서 원단(14)이 가열되면 원단에 함유된 열가소성수지는 팽창되어져 원단과 함께 낚싯대 본체를 형성하게 되고 잔여량의 수지액은 성형용 고온 테이프의 틈 사이로 유출되어지면서 성형이 이루어진다.When the fabric 14 is heated, the thermoplastic resin contained in the fabric is expanded to form a fishing rod body together with the fabric, and the remaining amount of the resin liquid flows out between the gaps of the high-temperature tape for molding.

상기의 낚싯대의 성형공정은 일반적으로 사용되는 낚싯대의 성형방법이다.The forming process of the fishing rod is a forming method of a fishing rod which is generally used.

상기 금형의 장홈(12)에 부착되어져 있던 보강사(13)는 상기와 같은 성형온도로 가열되면 상기 낚싯대 본체의 성형과정과 마찬가지로 원단에 함유된 열가소성수지에 의해 원단과 강하게 결합된다.When the reinforcement yarn 13 attached to the long groove 12 of the mold is heated to the molding temperature as described above, the reinforcement yarn 13 is strongly bonded to the fabric by the thermoplastic resin contained in the fabric as in the forming process of the rod body.

따라서, 성형공정을 거친 후 낚싯대 본체와 금형(11)을 분리시키게 되면 보강사는 낚싯대 본체 내부면에 결합되어 금형과 분리된다.Therefore, when the fishing rod main body and the mold 11 are separated after the molding process, the reinforcing yarn is coupled to the fishing rod main body and separated from the mold.

그 다음 낚싯대 본체(10)를 금형(11)과 분리시킨 후 낚싯대 표면의 고온 테이프를 풀어내고 절단 및 표면가공, 연마공정 등의 작업을 통하여 성형공정(S2)을 완료한다. Then, after separating the fishing rod body 10 from the mold 11, the high temperature tape on the surface of the fishing rod is released, and the molding process (S2) is completed through operations such as cutting, surface processing, and polishing.

그런 다음 마지막 공정인 제 3공정은, 상기 소재성형공정(S2)에서 가공된 낚싯대 본체(10)의 표면에 다양한 형태의 도료를 도포하는 도장공정(S3)단계로, 우선 표면의 굴곡 현상과 미세구멍을 제거하기 위해 하도층을 페인팅 한 후, 그 표면을 연마하는 순으로 5회 이상 반복 시행함으로써 낚싯대 본체(10)의 표면을 일층 매끄럽게 가공한다. Then, the third step, which is the last step, is a coating step (S3) of applying various types of paint to the surface of the fishing rod main body 10 processed in the material forming step (S2). After painting the undercoat layer to remove the hole, the surface of the fishing rod main body 10 is smoothly processed by repeating five or more times in the order of polishing the surface.

그 후, 중도층 페인팅 공정을 실시하는 바, 원하는 색상의 도료를 선택하고 이를 빼내기식 혹은 스프레이식 등의 방법을 통하여 상기 하도층이 완료된 낚싯대 본체(10) 상면에 도포하는 것으로써, 이는 낚싯대 본체(10)의 바탕색을 원하는 형태로 형성하도록 하며 바탕색의 색상만큼 반복하여 도장한 뒤 연마한다. Then, the middle layer painting process is performed, by selecting a paint of a desired color and applying it to the upper surface of the fishing rod body 10 on which the undercoat is completed by a method such as extraction or spraying, which is a rod body Form the background color of (10) in the desired shape and repeat the coating as the color of the background color and polish.

그런 다음 상기 색상을 형성시킨 중도층 페인팅 공정을 완료한 후에는 미려한 광택을 형성시키기 위한 상도층 페인팅 공정을 실시하는 바, 우레탄 클리어 등의 투명 페인트를 빼내기식 도장방법을 통하여 표면을 도장한 상도층 페인팅을 완료함으로써 도장작업을 완료하며, 상기와 같이 여러 단계를 거쳐서 형성된 도장 층은 색상의 박리 현상이 없어서 보존성이 좋고, 마모나 변질이 되지 않으며 방수효과가 우수하여 수분접촉에 따라 들뜨는 현상이 없으며 복합적으로 소재가 반복 도장된 피막층의 두께로 표면강도가 좋은 장점이 있다. Then, after completing the middle layer painting process in which the color is formed, the top layer painting process is performed to form a beautiful luster, and the top coat layer is coated with a surface by drawing a transparent paint method such as urethane clear. The painting work is completed by completing the painting, and the coating layer formed through the various steps as described above has no preservation of color, and thus has good preservation, does not wear or deteriorate, and has excellent waterproof effect. Composite has the advantage of good surface strength as the thickness of the coating layer repeatedly coated material.

상기 제1공정에서 제3공정을 반복하여 직경이 각각 다른 낚싯대 본체를 여러 개 제조한 후 직경이 작은 것에서부터 큰 것으로 순차적으로 다단 결합함으로써 하나의 낚싯대를 완성한다.By repeating the third step in the first step to manufacture several fishing rod bodies of different diameters, and then to a single fishing rod by completing a plurality of fishing rods sequentially from the smallest diameter to the larger.

도 1은 종래의 낚싯대 본체를 도시한 정면도1 is a front view showing a conventional fishing rod body

도 2는 본 발명 낚싯대 제조방법을 보여주는 사시도Figure 2 is a perspective view showing a fishing rod manufacturing method of the present invention

도 3은 본 발명 낚싯대 본체의 단면도3 is a cross-sectional view of the present invention fishing rod body

도 4는 본 발명 낚싯대의 제조공정도Figure 4 is a manufacturing process of the present invention fishing rod

도 2는 본 발명의 단면도 2 is a cross-sectional view of the present invention

[도면의 주요부분에 대한 부호의 설명][Explanation of symbols on the main parts of the drawings]

10 : 낚싯대 본체 11 : 금형10: rod body 11: mold

12 : 장홈 13 : 보강사12: long groove 13: reinforcement

14 : 원단14: fabric

Claims (2)

낚싯대 제조방법에 있어서, In the fishing rod manufacturing method, 금형(11)에 보강사(13)를 삽입 부착할 수 있도록 길이방향으로 장홈(12)을 형성하여 금형을 제작하는 금형제조공정(S1)과;A mold manufacturing step (S1) of forming a long groove 12 in the longitudinal direction so as to attach and insert the reinforcement yarn 13 into the mold 11 to manufacture a mold; 상기 장홈(12)에 보강사(13)를 부착한 뒤 그 상면에 수지가 함침된 유리섬유와 카본섬유 중 어느 하나로 구성된 원단(14)을 금형(11)에 접착 권취한 후 120℃로 가열 성형하는 성형공정(S2)과;After attaching the reinforcing yarn 13 to the long groove 12, the fabric (14) consisting of any one of glass fiber and carbon fiber impregnated with resin on the upper surface of the mold 11, the adhesive wound on the mold 11 and then heated to 120 ℃ Forming step (S2) and; 상기 성형이 완료된 낚싯대 본체(10)를 금형(11)으로부터 분리한 후, 표면을 하도, 중도, 상도도장의 3단계로 도장 및 연마하는 도장공정(S3)으로 이루어지는 것을 특징으로 하는 낚싯대의 제조방법.The method of manufacturing a fishing rod, comprising a coating step (S3) of separating and removing the fishing rod main body (10) from the mold (11), and then painting and polishing the surface in three stages of undercoat, middle coat, and top coat. . 제 1항에 있어서, The method of claim 1, 금형제조공정(S1)에 의해 제작된 금형(11)은 테이퍼진 금속 환봉으로 구성되되, 그 외부면에는 길이방향으로 보강사(13)가 삽입될 수 있도록 반구형상의 장홈(12)이 3 내지 7개가 형성되는 것을 특징으로 하는 낚싯대의 제조방법.Mold 11 produced by the mold manufacturing process (S1) is composed of a tapered metal round bar, the outer surface of the hemispherical long groove 12 is 3 to 7 so that the reinforcing yarn 13 can be inserted in the longitudinal direction Fishing rod manufacturing method characterized in that the dog is formed.
KR1020080074935A 2008-07-31 2008-07-31 The manufacturing method of the fishing rod KR101008826B1 (en)