KR102196311B1 - Heat fusion fixing a float - Google Patents

Heat fusion fixing a float Download PDF

Info

Publication number
KR102196311B1
KR102196311B1 KR1020180151611A KR20180151611A KR102196311B1 KR 102196311 B1 KR102196311 B1 KR 102196311B1 KR 1020180151611 A KR1020180151611 A KR 1020180151611A KR 20180151611 A KR20180151611 A KR 20180151611A KR 102196311 B1 KR102196311 B1 KR 102196311B1
Authority
KR
South Korea
Prior art keywords
buoy
members
heater
bonding surfaces
bonding
Prior art date
Application number
KR1020180151611A
Other languages
Korean (ko)
Other versions
KR20200065292A (en
Inventor
백정호
김경진
홍점자
Original Assignee
주식회사 부선
주식회사 대성에프앤비
홍점자
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 부선, 주식회사 대성에프앤비, 홍점자 filed Critical 주식회사 부선
Priority to KR1020180151611A priority Critical patent/KR102196311B1/en
Publication of KR20200065292A publication Critical patent/KR20200065292A/en
Application granted granted Critical
Publication of KR102196311B1 publication Critical patent/KR102196311B1/en

Abstract

부표(100)에 있어서
상기 부표는 두 개의 부재(101, 102)가 결합되어 구성되되
상기 부재(101, 102)는 내부에 형성된 공간부;와 상기 부재의 일측에 상기 공간부와 통공되면서 상기 부재들을 결합하기 위한 결합부(103, 104);가 구비되어
상기 부재들을 대응되게 위치시킨 후 상기 결합부(103, 104)를 통해 상기 부재(101, 102)들을 결합하여 형성되며,
상기 결합부(103, 104)는 접합면적을 넓힐 수 있도록 상기 공간부의 가장자리를 따라 외부로 돌출되는 플랜지부와 상기 플랜지부의 일면인 접합면(105, 106)을 포함하며), 상기 접합면(105, 106)이 서로 마주보도록 위치시키고 상기 접합면(105, 106) 사이에 히터를 삽입하여 상기 서로 마주보는 접합면(105, 106)을 용융시킨 다음, 상기 히터는 추출되고, 상기 용융된 접합면(105, 106)이 서로 맞닿도록 가압하여 결합되는 것을 특징으로 하는 열융착 고정 부표.
In the buoy (100)
The buoy is composed of two members (101, 102) combined
The members 101 and 102 are provided with a space portion formed therein; and a coupling portion 103 and 104 for coupling the members while passing through the space portion at one side of the member.
It is formed by placing the members correspondingly and then combining the members 101 and 102 through the coupling portions 103 and 104,
The coupling portions 103 and 104 include a flange portion protruding to the outside along an edge of the space portion and a joint surface 105 and 106 which are one surface of the flange portion so as to increase the joint area), the joint surface ( 105 and 106 are positioned to face each other and a heater is inserted between the bonding surfaces 105 and 106 to melt the facing bonding surfaces 105 and 106, and then the heater is extracted and the molten bonding Heat-sealing fixed buoy, characterized in that the surface (105, 106) is coupled by pressing so as to contact each other.

Figure 112018119866677-pat00001
Figure 112018119866677-pat00001

Description

열융착 고정 부표{Heat fusion fixing a float} Heat fusion fixing a float}

본 발명은 물에 뜨는 부표 구조에 관한 것으로서, 보다 상세하게는 분할 형성되는 한 쌍의 부재의 접착부를 히터로 용융한 후 가압하여 열융착시킨 타원형체의 부표 구조에 관한 것이다.The present invention relates to a buoy structure that floats in water, and more particularly, to a buoy structure of an elliptical body in which the adhesive portions of a pair of divided members are melted with a heater and then pressurized and thermally fused.

일반적으로, 부표는 수면에 띄운 부체(浮體)다. 부표는 어구나 닻 등 물 속에 있는 물체의 위치를 나타내기 위해 사용되며, 일정 범위에 어류, 및 조류 등을 양식하기 위해 설치된 그물을 고정시키기 위해 사용된다.In general, buoys are floating bodies on the surface. The buoy is used to indicate the location of objects in the water such as fishing gear or anchors, and is used to fix the net installed to cultivate fish and algae in a certain range.

또한 부표는 바다에 뜰 수 있도록 부력을 가지고 있으며, 부표를 와이어, 어구용 밧줄을 이용하여 매어 달아 기구에 의해 해저의 바닥 또는 위치가 고정될 수 있는 중량물에 고정된다. In addition, the buoy has buoyancy so that it can float on the sea, and the buoy is hung using a wire or a fishing rope, and is fixed to the bottom of the sea floor or a heavy object that can be fixed in position by a mechanism.

일반적인 부표는 합성수지를 발포 성형한 발포 수지재로 제작되어, 합성수지를 발포하면 발포제품내에는 많은 공극이 형성되어 물에 뜰 수 있는 부력을 가지고 있다. General buoys are made of a foamed resin material obtained by foam molding of synthetic resin, and when the synthetic resin is foamed, many voids are formed in the foamed product and have the buoyancy to float in water.

이러한 부표는 어구용 밧줄에 고정하기 위한 고정구가 필요하고, 발포된 합성수지는 충격강도에 약해 파손되는 단점이 있다.These buoys require a fixture to be fixed to the fishing gear, and the foamed synthetic resin has a disadvantage of being damaged due to weak impact strength.

또한, 발포된 부표에서 파손되어 나온 작은 조각들은 해양어류가 먹을 수 있어, 어족 자원 보존에 나쁜 영향을 미치고, 해양오염의 원인이 되고 있다.In addition, the small pieces that are damaged from the foamed buoy can be eaten by marine fish, which adversely affects the conservation of fish stocks and causes marine pollution.

이와 같은 문제점을 개선하기 위한 구조의 부표로서, 어구용 밧줄을 쉽게 고정시키기 위한 고정끈 삽입부와, 부표의 외주면 원통부에 다수개의 고리부를 부가하여 그물이나, 기구들을 쉽게 부착할 수 있는 구조로 하며,As a buoy with a structure to improve such problems, it is a structure in which a net or equipment can be easily attached by adding a fixing string insertion part to easily fix the fishing gear rope and a plurality of hooks on the outer circumferential cylindrical part of the buoy. And

부표의 재질을 합성수지로 성형하여 해저 수압에 견딜 수 있는 강도를 가지며, 분할 성형된 한 쌍의 부재의 접착부를 히터로 용융한 후 가압하여 열융착 시켜 제조가 간단하며 내구성이 있는 부표를 제작하기 위한 것이다.The material of the buoy is molded with synthetic resin to have the strength to withstand the water pressure on the sea floor, and the bonding part of a pair of split-molded members is melted with a heater and then pressurized and thermally fused to produce a buoy that is simple and durable. will be.

: 대한민국 등록실용신안공보 제20-0446171호: Republic of Korea Utility Model Publication No. 20-0446171 : 대한민국 등록특허공보 제0795144호: Korean Patent Publication No. 0795144 : 일본국 공개특허공보 JP2000-128087호: Japanese Patent Application Publication No. JP2000-128087 : 대한민국 등록특허공보 제10-1829898호: Korean Patent Publication No. 10-1829898

본 발명은 상기와 같은 문제를 해결하기 위하여 안출된 것으로, 분할 형성되는 한 쌍의 부재의 접착부를 히터로 용융한 후 가압하여 열융착 시키는 타원형체의 부표를 제작하는데 그 목적이 있다.The present invention has been conceived to solve the above problems, and an object of the present invention is to produce an elliptical buoy that is thermally fused by melting and pressing the adhesive portion of a pair of members to be divided by a heater.

또한 부표의 몸통 외면부에는 반원통 형상의 오목 홈부를 형성하고, 결합부에 상기 오목 홈부와 통공되게 관통구멍이 형성된 고정끈 삽입부를 형성하여 고정끈을 쉽게 부표에 묶을 수 있도록 형성되는 목적이 있다.In addition, there is an object of forming a semi-cylindrical concave groove on the outer surface of the buoy, and forming a fixing strap insertion portion in which a through hole is formed so as to penetrate the concave groove in the coupling portion so that the fixing strap can be easily tied to the buoy. .

또한 융착 결합된 부표의 결합부 양측에는 금속재질로 형성된 링형태의 보강링을 더 포함하며, 상기 양측의 보강링과 결합부를 고정끈 삽입부를 이용하여 강제 또는 고정끈으로 묶거나, 고정 결합하여 접합부의 접합강도를 증대되는 구조를 제공하는 것을 그 목적으로 한다.In addition, both sides of the bonding portion of the fusion-bonded buoy further include a ring-shaped reinforcing ring formed of a metal material, and the reinforcing ring and the connecting portion on both sides are tied with a force or a fixing string using a fixing string insertion part, or by a fixed connection. Its purpose is to provide a structure that increases the bonding strength of.

상기 목적을 달성하기 위한 본 발명에 따른 열융착 고정 부표 구조는The heat-sealed fixed buoy structure according to the present invention for achieving the above object

상기 부표는 두 개의 부재가 결합되어 구성되되The buoy is composed of two members combined.

상기 부재는 내부에 형성된 공간부;와 상기 부재의 일측에 상기 공간부와 통공되면서 상기 부재들을 결합하기 위한 결합부가 구비되어 The member is provided with a space part formed therein; and a coupling part for coupling the members while passing through the space part at one side of the member

상기 부재들을 대응되게 위치시킨 후, 상기 결합부를 통해 상기 부재들을 결합하여 형성하는 열융착 고정 부표를 특징으로 한다.After positioning the members correspondingly, it features a heat-sealing fixing buoy formed by combining the members through the coupling part.

바람직하게는 상기 결합부는 접합면적을 넓힐 수 있도록 상기 공간부의 가장자리를 따라 외부로 돌출되는 플랜지부와 상기 플랜지부의 일면인 접합면을 포함하며, 상기 접합면이 서로 마주보도록 위치시키고 상기 접합면 사이에 히터를 삽입하여 상기 서로 마주보는 접합면을 용융시킨 다음, 상기 히터는 추출되고, 상기 용융된 접합면이 서로 맞닿도록 가압하여 결합되는 것을 특징으로 할 수 있다.Preferably, the coupling portion includes a flange portion protruding outward along the edge of the space portion and a bonding surface that is one surface of the flange portion so as to increase the bonding area, and the bonding surfaces are positioned so as to face each other, and between the bonding surfaces After inserting a heater into the bonding surface facing each other to melt, the heater is extracted, the melted bonding surface may be characterized in that the bonding by pressing so as to contact each other.

또한, 상기 접합면에는 융착되는 접촉면적을 넓힐 수 있도록 돌출부와 오목부가 형성되며, 상기 히터에서 상기 접합면에 접촉되는 부위에도 상기 접합면의 돌출부와 오목부에 대응되는 오목부와 돌출부가 형성되는 것을 특징으로 할 수 있다.In addition, a protruding portion and a concave portion are formed on the bonding surface to increase the contact area to be fused, and a concave portion and a concave portion corresponding to the protruding portion and the concave portion of the bonding surface are formed in a portion of the heater contacting the bonding surface. It can be characterized.

또한, 상기 부재의 몸통 외면부에는 반원통 형상의 오목 홈부를 더 포함되고, 상기 결합부에 상기 오목 홈부와 연통되는 관통구멍이 형성된 고정끈 삽입부를 형성될 수 있으며,In addition, a semi-cylindrical concave groove may be further included on the outer surface of the member, and a fixing strap insertion portion having a through hole communicating with the concave groove may be formed in the coupling portion,

또한, 상기 부재의 몸통부 원형부의 끝단에는 고정끈이 삽입되는 고리부가 구비되고, 플랜지부 외부면의 소정부위에는 일정한 간격으로 고정끈이 삽입되는 고리부가 구비되는 것을 특징으로 할 수 있다.In addition, it may be characterized in that a ring portion into which the fixing strap is inserted is provided at an end of the circular portion of the body of the member, and a ring portion into which the fixing strap is inserted at regular intervals is provided at a predetermined portion of the outer surface of the flange portion.

또한, 상기 부재는 내부에 형성된 공간부에 다수의 분할 공간을 갖도록 구획 형성된 격벽부재를 더 포함하며, 상기 부재의 외주면에는 외부로 돌출된 반원형의 리브를 부재의 길이방향을 따라 일정 간격 이격되게 형성된 것을 특징으로 할 수 있다.In addition, the member further includes a partition member formed to have a plurality of divided spaces in a space formed therein, and a semicircular rib protruding to the outside is formed on an outer circumferential surface of the member to be spaced apart at predetermined intervals along the length direction of the member. It can be characterized.

또한, 상기 부재가 내부에 수용되는 한 쌍의 지그틀과, In addition, a pair of jig frames in which the member is accommodated,

상기 지그틀에 수납되는 상기 부재는 접합면이 서로 마주보도록 배치되며, 상기 지그틀에는 수용되는 부재가 정확한 위치에 안착될 수 있도록 부재에 형성된 오목 홈부에 대응되는 안내부가 형성되며,The members accommodated in the jig frame are disposed so that the bonding surfaces face each other, and the jig frame has a guide portion corresponding to the concave groove formed in the member so that the member to be accommodated can be seated at an accurate position,

상기 지그틀에 부재를 수납할 때 상기 안내부에 의해 부재에 형성된 오목 홈부가 가이드 되며 수납되어 정확한 위치에 고정되는 것을 더 포함할 수 있으며,When the member is received in the jig frame, the concave groove portion formed in the member is guided by the guide portion and received and fixed to the correct position.

상기 지그틀은 유압 또는 공기압으로 가동되는 실린더로 이동 및 가압되도록 형성되고, The jigtle is formed to be moved and pressurized by a cylinder operated by hydraulic or pneumatic pressure,

상기 부재의 접합면 사이에 삽입되어 접촉되는 접합면을 용융되도록 가열하는 히터와,A heater inserted between the bonding surfaces of the member and heated to melt the bonding surfaces that are in contact;

상기 히터는 접촉되는 상기 접합면이 용융되면 상기 지그틀 사이에서 분리 추출되고, The heater is separated and extracted between the jig molds when the bonding surface to be in contact is melted,

상기 지그틀은 삽입된 접합면이 용융된 상태에서 가압하여 융착 결합하며,The jig frame is fusion bonded by pressing in a state in which the inserted bonding surface is melted,

상기 융착 결합된 부표를 상기 지그틀에서 분리하여 추출하기 위한 가압부재가 더 포함하여 이루어진다.A pressure member for separating and extracting the fusion-bonded buoy from the jig frame is further included.

또한, 상기 융착 결합된 부표의 결합부 양측에는 금속재질로 형성된 링형태의 보강링을 더 포함하며, 상기 양측의 보강링과 결합부를 고정끈 삽입부를 이용하여 강제 또는 고정끈으로 묶거나 고정 결합시켜 접합부의 접합강도를 증대시키는 것을 특징으로 하며,In addition, both sides of the coupling portion of the fusion-bonded buoy further include a ring-shaped reinforcing ring formed of a metal material, and the reinforcing ring and the coupling portion on both sides are tied or fixedly coupled with a force or a fixing string using a fixing string insertion part. It is characterized by increasing the bonding strength of the joint,

융착에 사용되는 히터의 표면온도는 450℃ ~700℃이고, 상기 히터와 접합면의 접촉 시간은 2~3초이고, The surface temperature of the heater used for fusion is 450°C to 700°C, and the contact time between the heater and the bonding surface is 2 to 3 seconds,

상기 접촉시간이 경과 후에 상기 히터를 분리 추출하고 0.2~0.3초 내로 가압하여 융착 결합시키는 것을 특징으로 한다.After the elapse of the contact time, the heater is separated and extracted and pressurized within 0.2 to 0.3 seconds to perform fusion bonding.

또한, 상기 부표의 크기는 길이 600㎜ 직경 400㎜이고, 부표 몸체의 두께는 3㎜이고, 반원형의 리브의 높이는 3㎜, 격벽부재의 두께는 3㎜, 결합부의 두께는 10~13㎜, 융착 결합된 두께는 20~25㎜로 형성된다.In addition, the size of the buoy is 600 mm in length and 400 mm in diameter, the thickness of the buoy body is 3 mm, the height of the semicircular rib is 3 mm, the thickness of the partition member is 3 mm, the thickness of the joint is 10 to 13 mm, and The combined thickness is formed from 20 to 25 mm.

또한, 열융착 결합된 부표의 표면에 용제, 실란, 아세트산으로 구성된 프라이머를 도포하여 프라이머 코팅층을 생성하고, In addition, a primer consisting of a solvent, silane, and acetic acid is applied to the surface of the heat-sealed buoy to create a primer coating layer,

상기 부표의 표면에 알루미나 분말이 포함된 제1 코팅제를 도포한 후 UV 차단제가 포함된 제2 코팅제를 도포하여 제2 코팅층을 생성하여 자외선 차단기능의 부여한 것을 특징으로 한다.After applying the first coating agent containing alumina powder on the surface of the buoy, a second coating layer containing a UV blocking agent is applied to create a second coating layer to provide a UV blocking function.

또한, 자외선 차단기능의 부여한 열융착 결합된 부표의 표면에는 야광테이프를 부착하거나 야광도료를 도포하여 표면에서 띠 형태를 이루는 야광반사부를 형성되되, 상기 야광반사부는 부체의 길이방향을 따라 일정 간격 이격되게 형성되는 것을 추가하여 부가할 수 있다.In addition, a luminous reflective part is formed on the surface of the heat-sealed-coupled buoy with a UV blocking function by attaching a luminous tape or applying a luminous paint, and the luminous reflecting part is spaced apart at regular intervals along the length direction of the float. It can be added by adding what is formed to be.

또한, 열융착 부표의 제조방법으로서In addition, as a method of manufacturing a heat-sealed buoy

합성수지로 내부에 형성되는 공간부와 결합부를 가지는 부재를 각각 형성하는 단계와; 상기 각각의 부재의 접합면이 대응되도록 지그틀에 각각 장착하는 단계와; 상기 지그틀에 삽입 결합된 부재의 접합면 사이에 히터를 장착하는 단계를 포함하며,Forming a member having a space portion and a coupling portion formed therein of synthetic resin, respectively; Mounting each member to the jig frame so that the bonding surfaces of the respective members correspond to each other; And mounting a heater between the bonding surfaces of the members inserted and coupled to the jig frame,

상기 히터가 부재의 접합면 사이에 장착하면, 제어부의 제어에 따라 450℃ ~700℃로 가열된 히터면과 상기 부재의 접합면을 2~3초간 접촉하여 용융하는 단계와; 상기 접합면이 용융되면, 히터를 접합면 사이에서 분리하여 추출한 후, 접합면을 0.2 ~ 0.5초간 가압하여 접합면의 융착부를 가압 융착하는 부표를 형성하는 단계를 포함하고,When the heater is mounted between the bonding surfaces of the members, melting by contacting the heater surface heated to 450°C to 700°C and the bonding surface of the member for 2 to 3 seconds under control of a control unit; When the bonding surface is melted, the heater is separated and extracted between the bonding surfaces, and then the bonding surface is pressurized for 0.2 to 0.5 seconds to form a buoy for pressing and bonding the fused portion of the bonding surface,

상기 성형된 부표를 지그틀 중 어느 하나에 장착된 가압부재의 가압으로 지그틀에서 분리되는 것이다. The molded buoy is separated from the jig frame by pressing a pressing member mounted on one of the jig frames.

상기와 같은 특징을 갖는 본 발명은, 내부에 형성된 공간부와 부재들을 결합하기 위한 결합부를 구비한 부재들을 대응되게 위치시킨 후에, 대응되는 부재의 결합부를 히터로 용융시킨 다음에 압축하는 압착으로 부표를 제작하므로, 접합 강도가 향상되고, 균일한 부력을 가지는 장점이 있다.The present invention having the above characteristics is a buoyant by compressing the members having a space portion formed therein and a coupling portion for coupling the members to be correspondingly positioned, and then melting the joint portion of the corresponding member with a heater and then compressing it. Since it is produced, there is an advantage of improving the bonding strength and having a uniform buoyancy.

또한, 부재의 몸통 외면부에 반원통 형상의 오목 홈부와 상기 오목 홈부와 연통되는 결합부의 관통구멍으로 형성된 고정끈 삽입부를 이용하여 부표 몸통부에 어구나 닻, 그물을 고정시키기 위해 고정끈을 쉽고 강력하게 묶을 수 있는 장점이 있다.In addition, by using a fixed strap insertion portion formed by a semi-cylindrical concave groove on the outer surface of the member and a through hole of the coupling portion communicating with the concave groove, it is easy to fix the fixing strap to the buoy body to fix the fishing, anchor, and net. It has the advantage of being able to bind strongly.

또한, 융착 결합된 부표의 결합부 양측에는 링형태의 보강링을 더 포함하고, 양측의 보강링과 결합부를 고정끈 삽입부를 이용하여 강제 또는 고정끈으로 묶거나, 고정 결합시켜 접합부의 접합강도를 증대시키고, 고정끈 삽입부의 파손을 방지하는 장점이 있다.In addition, a ring-shaped reinforcing ring is further included on both sides of the coupling part of the fusion-bonded buoy, and the reinforcing ring and the coupling part on both sides are tied with a force or a fixing string using a fixing string insertion part, or fixedly combined to increase the bonding strength of the junction. It has the advantage of increasing and preventing damage to the fixing strap insertion part.

또한, 부재 내부에 격벽부재를 더 포함하고, 상기 부재의 결합부를 융착 결합한 부표의 내부에는 상기 격벽에 의하여 분할된 공간마다 밀폐된 공기층으로 이루어지는 부력체를 형성하여, 분할된 일부 공간에서 부력이 상실되어도 나머지 공간에서 부력을 제공하는 장점이 있다.In addition, a buoyancy body formed of an air layer sealed in each space divided by the partition wall is formed in the buoy further comprising a partition member inside the member, and the joint portion of the member is fused and bonded, so that buoyancy is lost in the divided partial spaces. Even if it is, it has the advantage of providing buoyancy in the rest of the space.

도 1은 본 발명의 실시 예에 따른 완성된 열융착 고정 부표의 형상을 나타내는 사시도이다.
도 2은 본 발명의 실시 예에 따른 두 개의 부재가 결합된 열융착 고정 부표 구조를 예시한 입체도이다
도 3은 본 발명의 실시 예에 부재의 구조를 예시한 입체도이다
도 4는 본 발명의 또 다른 실시 따른 격벽을 구비한 부재가 열융착되고, 외면에 보강리부를 구비하는 부재가 결합된 열융착 고정 부표 구조를 예시한 입체도이다.
도 5는 본 발명의 실시 예에 따른 결합 지그틀과 지그틀의 작동과정을 그린 구조도이다.
도 6는 본 발명의 실시 예에 따른 열융착 고정 부표 사용한 그물망을 예시한 도면이다.
1 is a perspective view showing the shape of a completed heat-sealing fixing buoy according to an embodiment of the present invention.
2 is a three-dimensional view illustrating a heat-sealed fixed buoy structure in which two members are combined according to an embodiment of the present invention.
3 is a three-dimensional view illustrating the structure of a member in an embodiment of the present invention
FIG. 4 is a three-dimensional view illustrating a heat-sealed fixed buoy structure in which a member having a partition wall is thermally fused and a member having a reinforcement part on an outer surface thereof according to another embodiment of the present invention.
5 is a structural diagram illustrating an operation process of a joint jig frame and a jig frame according to an embodiment of the present invention.
6 is a view illustrating a net using a heat-sealing fixed buoy according to an embodiment of the present invention.

본 발명에서 사용되는 용어는 가능한 현재 널리 사용되는 일반적인 용어를 선택하였으나, 특정한 경우는 출원인이 임의로 선정한 용어도 있는데 이 경우에는 단순한 용어의 명칭이 아닌 발명을 실시하기 위한 구체적인 내용에 기재되거나 사용된 의미를 고려하여 그 의미가 파악되어야 할 것이다.As for terms used in the present invention, general terms that are currently widely used are selected, but in certain cases, some terms are arbitrarily selected by the applicant. In this case, the meanings described or used in the specific contents for carrying out the invention are not just the names of terms. The meaning should be grasped in consideration of.

이하, 첨부한 도면에 도시된 바람직한 실시 예들을 참조하여 본 발명의 기술적 구성을 상세하게 설명한다. 여기서, 상하좌우, 우측, 좌측, 저면 등 방향과 관련된 표현은 모두 제시한 도면을 기준으로 기재하고 있음을 밝혀둔다.Hereinafter, the technical configuration of the present invention will be described in detail with reference to exemplary embodiments illustrated in the accompanying drawings. Here, it should be noted that all expressions related to directions such as up, down, left, right, left, and bottom are described based on the presented drawings.

본 발명은 여러 가지 상이한 형태로 구현될 수 있으며 여기에서 설명하는 실시 예에 한정되지 않는다. 명세서 전체를 통하여 유사한 부분에 대해서는 동일한 도면 부호를 붙였다.The present invention may be implemented in various forms and is not limited to the embodiments described herein. The same reference numerals are assigned to similar parts throughout the specification.

도 1에 도시된 바와 같이, 본 발명의 실시 예에 따른 완성된 열융착 고정 부표의 형상을 나타내는 사시도이고, 부표의 가운데는 두 개의 부재가 결합된 결합부가 형성되며, 결합부의 양면에는 강재로 형성된 보강링 더 포함하고, 양 보강링과 결합부를 강재로 결합시켜 접합부의 강도를 증대시키고, 고정끈 삽입부의 파손을 방지는 입체도가 도시되어 있다. As shown in FIG. 1, it is a perspective view showing the shape of a completed heat-sealing fixing buoy according to an embodiment of the present invention, and a coupling part in which two members are combined is formed in the middle of the buoy, and both sides of the coupling part are formed of steel. A three-dimensional view is shown that further includes a reinforcing ring, and increases the strength of the joint by combining both reinforcing rings and the joint with a steel material, and prevents damage to the fixing strap insert.

도 2는 본 발명의 실시 예에 따른 두 개의 부재가 결합된 열융착 고정 부표 구조와 부재의 몸통 외면부에 반원통 형상의 오목 홈부와 상기 오목 홈부와 연통되는 결합부 관통구멍으로 형성된 고정끈 삽입부를 예시한 입체도가 도시되어 있다2 is a heat-sealing fixing buoy structure in which two members are combined according to an embodiment of the present invention, and a fixing strap inserted into a semi-cylindrical concave groove portion and a coupling portion through hole communicating with the concave groove portion on the outer surface of the body of the member A three-dimensional diagram illustrating wealth is shown.

도 3은 본 발명의 실시 예에 따른 부재의 구조를 예시한 입체도이다3 is a three-dimensional view illustrating the structure of a member according to an embodiment of the present invention

도 1 내지 도 3을 참고하면, 본 발명의 한 실시 예에 따른 열융착 고정 부표는 상기 부표는 두 개의 부재(101, 102)가 결합되는 구조로 구성되어 있으며,1 to 3, the heat-sealing fixed buoy according to an embodiment of the present invention is composed of a structure in which two members 101 and 102 are coupled,

상기 부재(101, 102)는 내부에 형성된 공간부가 형성되어 있어, 상기 공간부에 공기가 충전되는 것으로 상기 부재의 일측에 상기 공간부와 통공되면서 상기 부재들을 결합하기 위한 결합부(103, 104)가 구비되어 있다.The members 101 and 102 have a space part formed therein, so that air is filled in the space part, and a coupling part 103 and 104 for coupling the members while passing through the space part at one side of the member Is equipped.

그리고 부재(101, 102)의 재질은 폴리에틸렌(LDPE & HDPE), 폴리 프로필렌(PP), 폴리염화비닐(PVC), 폴리 스타이렌(PS), 폴리에스테르(PET), 스티렌 아크릴로니트릴 부타디엔(ABS)수지 및 나일론(PA) 중에 어느 하나 및 이들의 둘 이상의 혼합물에 의해 선택되어 진 합성수지로 이루어 질 수 있다.And the materials of the members 101 and 102 are polyethylene (LDPE & HDPE), polypropylene (PP), polyvinyl chloride (PVC), polystyrene (PS), polyester (PET), styrene acrylonitrile butadiene (ABS). ) It may be made of a synthetic resin selected by any one of resin and nylon (PA) and a mixture of two or more thereof.

합성수지는 고분자 화합물의 일종으로 썩지 않으며, 썩지 않는 합성 수지가 바다에 버려지게 되면 어류, 조류, 그리고 해초의 먹이 사슬을 파괴된다. Synthetic resin is a type of high molecular compound that does not rot. When non-perishable synthetic resin is thrown into the sea, the food chain of fish, algae, and seaweed is destroyed.

또한, 땅에 합성수지가 매립되면 원활한 공기 소통을 막아 토양을 오염시킨다. 이런, 공해 문제를 해결하고자 자연 상태에서 분해되는 분해성 플라스틱이 개발되어 있으므로, 상기 합성수지는 생분해성 플라스틱(bio-degradable plastic)으로 선택할 수 있다.In addition, when synthetic resin is buried in the ground, it contaminates the soil by preventing smooth air communication. In order to solve the pollution problem, since degradable plastics that decompose in nature have been developed, the synthetic resin may be selected as bio-degradable plastic.

또한, 상기와 같은 구성으로 형성된 상기 부재(101, 102)는 대응되도록 2개로 분할 제작된 것으로, 이를 결합시키기 위해서는 상기 부재들을 대응되게 위치시킨 후 상기 결합부(103, 104)를 통해 상기 부재(101, 102)들을 결합하여 형성되는 열융착 고정 부표를 특징으로 한다.In addition, the members 101 and 102 formed in the above configuration are divided into two so as to correspond to each other, and in order to combine them, the members are positioned correspondingly and then through the coupling portions 103 and 104, the member ( It features a heat-sealed fixed buoy formed by combining 101 and 102).

이러한 형식으로 제작된 열융착 고정 부표는 내부에는 공기층이 형성되고, 중간부에는 결합부가 형성되며 내부에 밀폐된 공기층으로 이루어지는 부력체로서 2개로 분할된 부재를 결합시켜 하나로 결합되어 부표(100)가 된다.The heat-sealed fixed buoy manufactured in this form is a buoyant body consisting of an air layer formed inside, a coupling part formed in the middle part, and a sealed air layer inside. The buoy 100 is combined into one by combining the members divided into two. do.

또한, 도 1, 2에 도시된 바와 같이In addition, as shown in Figures 1 and 2

상기 부재의 몸통 외면부에는 반원통 형상의 오목 홈부(111, 112)를 더 포함하고, 상기 결합부에 상기 오목 홈부(111, 112)와 연통되는 관통구멍을 형성하여 상기 오목 홈부(111, 112)와 상기 결합부의 관통구멍으로 이루어진 고정끈 삽입부(109, 110)를 형성할 수 있으며, 이렇게 형성된 고정끈 삽입부(109, 110)는 결합부의 외주면으로 돌출되지 않아 선박의 접안등에 의한 파손을 예방할 수 있는 장점이 있다.The member further includes a semi-cylindrical concave groove portion 111, 112 on the outer surface portion thereof, and a through hole communicating with the concave groove portion 111, 112 is formed in the coupling portion to form the concave groove portion 111, 112 ) And the through hole of the coupling part, and the fixing strap insertion parts 109 and 110 formed in this way do not protrude to the outer circumferential surface of the coupling part, thereby preventing damage due to the eyepiece of the ship, etc. There are advantages that can be prevented.

또한, 상기 융착 결합된 부표(100)의 결합부 양측에는 금속재질로 형성된 링 형태의 보강링(120, 130)을 더 포함하며, 상기 양측의 보강링과 결합부를 고정끈 삽입부(109, 110)를 이용하여 고정끈으로 묶어서 고정시킬 수 있다. In addition, both sides of the coupling portion of the fusion-bonded buoy 100 further include reinforcing rings 120 and 130 in the form of a ring formed of a metal material, and the reinforcing rings and the coupling portions at both sides of the fusion-bonded buoy 100 are fixed string insertion portions 109 and 110 ) Can be used to tie and fix it.

또한, 필요에 따라서는 고정끈외에 강선, 강제고리 등을 이용하여 보강할 수 있으므로 융착시킨 접합부의 접합강도를 증대시키는 것은 물론 보강된 보강링을 결합부에 형성된 고정끈 삽입부(109, 110)에 고정 끈을 묶어서 사용하므로, 파손 염려가 없는 강력한 고정끈 삽입부가 형성되어 편리하게 사용할 수 있다. In addition, if necessary, it can be reinforced using steel wires, steel rings, etc. in addition to the fixed straps, so as to increase the bonding strength of the fused joints, as well as the fixed strap inserts (109, 110) formed with reinforced reinforcing rings in the joints. Since it is used by tying up a fixing string, a strong fixing string insertion part is formed without fear of damage, so it can be used conveniently.

특히, 도 3 및 도 5를 참고하면, 상기 부재(101, 102)에는 상기 결합부(103, 104)의 접합면적을 넓힐 수 있도록 상기 공간부의 가장자리를 따라 외부로 돌출되는 플랜지부를 형성하고, 상기 플랜지부의 일면인 접합면(105, 106)을 포함하며, 상기 접합면(105, 106)을 서로 마주보도록 위치시키고 상기 접합면(105, 106) 사이에 히터를 삽입하여 상기 서로 마주보는 접합면(105, 106)을 용융시킨 다음, 상기 히터를 분리하여 추출하고, 상기 용융된 접합면(105, 106)이 서로 맞닿도록 가압하여 결합하는 것을 특징으로 할 수 있다.In particular, referring to FIGS. 3 and 5, a flange portion protruding outward along the edge of the space portion is formed on the members 101 and 102 so as to increase the bonding area of the coupling portions 103 and 104, It includes a bonding surface (105, 106) that is one side of the flange, and the bonding surface (105, 106) is positioned to face each other, and a heater is inserted between the bonding surfaces (105, 106) to face each other After melting the faces 105 and 106, the heater is separated and extracted, and the melted bonding faces 105 and 106 are pressed so as to contact each other to be combined.

또한, 상기 부재의 몸통부 원형부의 끝단에는 고정끈을 삽입할 수 있는 고리부(115, 116)를 필요에 따라 더 구비할 수 있고, 플랜지부 외부면에도 필요에 따라 소정부위에 일정한 간격으로 고정끈을 삽입하는 고리부(113, 114)가 구비된 것이 도시되어 두 개의 부재를 결합한 부표의 양단과 결합부에 일정한 간격으로 고리부를 형성하여 사용자의 필요에 따라, 어떠한 방향에서도 고정 끈을 묶어서 편리하게 사용할 수 있다.In addition, at the ends of the circular portion of the trunk portion of the member, a ring portion 115 and 116 into which the fixing strap can be inserted may be further provided as needed, and the outer surface of the flange portion may be fixed at a predetermined interval at regular intervals as needed. It is shown that the ring portions 113 and 114 for inserting the string are provided, and by forming a ring portion at regular intervals at both ends of the buoy that combines the two members, it is convenient to tie the fixing string in any direction according to the needs of the user. Can be used.

또한, 도 4를 참조하여 보면,Further, referring to FIG. 4,

본 발명의 또 다른 실시 예로서 상기 부재(101, 102) 내부에 형성된 공간부에 다수의 분할 공간을 갖도록 구획 형성된 격벽부재(117, 118)를 더 포함하며, 상기 격벽부재(117, 118)의 수와 모양은 다양하게 부가할 수 있고, 상기 부재(101, 102)의 외주면에는 외부로 돌출된 반원형의 리브(109)를 부재의 길이방향을 따라 일정 간격 이격되게 부가하여 형성할 수 있다. As another embodiment of the present invention, the partition wall members 117 and 118 are partitioned to have a plurality of partitioned spaces in the spaces formed inside the members 101 and 102, and the partition wall members 117 and 118 The number and shape may be added in various ways, and semicircular ribs 109 protruding outward may be added to the outer circumferential surfaces of the members 101 and 102 at regular intervals along the length direction of the member.

상기와 같이 격벽부재(117, 118)를 더 포함된 부재(101, 102)의 결합부(103, 104)를 열융착시켜면 열융착 고정 부표의 내부에는 상기 격벽 부재에 의하여 다양하게 분할된 공간마다 밀폐된 공기층으로 이루어지는 부력체가 형성하게 된다.As described above, when the coupling portions 103 and 104 of the members 101 and 102 further including the partition members 117 and 118 are thermally fused, the space divided in various ways by the partition member is inside the heat fusion fixing buoy. Each buoyant body made of a sealed air layer is formed.

또한, 이와 같이 분할된 부력체를 형성하여, 분할된 일부 공간에서 부력을 상실하여도 나머지 공간에서는 부력을 유지할 수 있는 부표(100)가 된다.In addition, by forming the divided buoyancy body as described above, even if the buoyancy is lost in a part of the divided space, the buoy 100 can be maintained in the remaining space.

또한, 상기 부재의 외주면에 외부로 돌출된 반원형의 리브(109)를 부재의 길이방향을 따라 일정 간격 이격되게 반원형의 보강리브를 더 부가하여 형성할 수 있으며, 상기 보강리브는 배의 접안등으로 부표와 배 또는 부두와 접촉시에는 돌출된 리부 상부면에서 접촉하여, 접촉에 의한 마모 파손을 방지할 수 있고, 리브에 의하여 부표의 강도를 보강하여 파손을 방지한다.In addition, semicircular ribs 109 protruding outward from the outer circumferential surface of the member may be formed by adding semicircular reinforcing ribs at regular intervals along the length direction of the member, and the reinforcing ribs are When the buoy is in contact with the ship or the pier, it contacts from the upper surface of the protruding rib to prevent abrasion and damage due to contact, and the strength of the buoy is reinforced with ribs to prevent damage.

또한, 도 5를 참조하여 보면,Also, referring to FIG. 5,

2개의 부재(101, 102)를 결합시키기 위해 형성된 플랜지부와 상기 플랜지부의 일면인 접합면(105, 106)을 포함하며, 상기 접합면(105, 106)이 서로 마주보도록 위치시키고 상기 접합면(105, 106) 사이에 히터를 삽입하여 상기 서로 마주보는 접합면(105, 106) 사이에 삽입된 상기 히터면의 양면과 접합면(105, 106)을 접촉하여 용융한 다음, 상기 히터를 분리 추출하고, 상기 용융된 접합면(105, 106)이 서로 맞닿도록 가압하여 결합하는 장치와 이를 이용하는 구성을 도시한 예시 도면이며. It includes a flange portion formed to couple the two members 101 and 102 and a bonding surface 105 and 106 that is one surface of the flange portion, and the bonding surfaces 105 and 106 are positioned to face each other, and the bonding surface A heater is inserted between (105, 106) to contact and melt both sides of the heater surface inserted between the facing bonding surfaces (105, 106) and the bonding surfaces (105, 106), and then separate the heater. It is an exemplary view showing a device for extracting and bonding by pressing the molten bonding surfaces 105 and 106 to abut each other and a configuration using the same.

이를 상세하게 살펴보면,Looking at this in detail,

한 쌍의 부재(101, 102)를 내부에 수용되는 한 쌍의 지그틀(210, 220)과, 상기 지그틀(210, 220)에 수납되는 상기 부재는 접합면(105, 106)이 서로 마주보도록 배치된다.A pair of jig frames (210, 220) accommodated in the pair of members (101, 102), and the members accommodated in the jig (210, 220) have a bonding surface (105, 106) facing each other. It is arranged to see.

또한, 상기 지그틀(210, 220)에는 수용되는 부재(101, 102)가 정확한 위치에 안착될 수 있도록 부재에 형성된 오목 홈부(111, 112)에 대응되는 안내부(230, 240)가 형성되어 있고, In addition, guide portions 230 and 240 corresponding to the concave groove portions 111 and 112 formed in the member so that the accommodated members 101 and 102 can be seated in the correct position are formed in the jig frames 210 and 220. There,

상기 지그틀(210, 220)에 부재(101, 102)를 수납할 때 상기 안내부(230, 240)에 의하여 부재(101, 102)에 형성된 오목 홈부(111, 112)가 가이드 되며 수납되어 정확한 위치에 고정된다.When receiving the members 101 and 102 in the jig frames 210 and 220, the concave grooves 111 and 112 formed in the members 101 and 102 are guided and accommodated by the guide parts 230 and 240. Fixed in position.

또한, 상기 지그틀(210, 220)은 유압 또는 공기압으로 가동되는 실린더를 이용하여 수납과 가압할 수 있도록 이동 가능하게 형성된다.In addition, the jig frames 210 and 220 are formed to be movable so as to be accommodated and pressurized using a cylinder operated by hydraulic or pneumatic pressure.

또한, 상기 부재의 접합면(105, 106) 사이에 히터(300)가 삽입하여 상기 히터의 양면과 상기 접합면(105, 106)이 접촉되어 용융된다.In addition, the heater 300 is inserted between the bonding surfaces 105 and 106 of the member, so that both surfaces of the heater and the bonding surfaces 105 and 106 contact and melt.

또한, 상기 히터(300)와 접촉되는 상기 접합면(105, 106)이 용융되면 상기 히터(300)는 상기 지그틀(210, 220)에 삽입된 부재의 접합면(105, 106) 사이에서 분리하여 추출한 다음, 상기 지그틀(210, 220)은 삽입된 접합면(105, 106)이 용융된 상태에서 가압하여 융착 결합된다.In addition, when the bonding surfaces 105 and 106 in contact with the heater 300 are melted, the heater 300 is separated between the bonding surfaces 105 and 106 of the members inserted into the jigframes 210 and 220. Then, the jig molds 210 and 220 are fused and bonded by pressing the inserted bonding surfaces 105 and 106 in a melted state.

또한, 상기 융착 결합된 부표(100)를 상기 지그틀(210, 220)에서 분리하여 추출하기 위한 가압부재(250)가 더 포함하여 이루어진 구성임을 알 수 있다.In addition, it can be seen that the configuration further includes a pressing member 250 for separating and extracting the fusion-bonded buoy 100 from the jig frames 210 and 220.

또한, 상기 접합면(105, 106)에는 융착되는 접촉면적을 넓힐 수 있도록 돌출부(107)와 오목부(108)를 형성하며, 상기 히터에서 상기 접합면에 접촉되는 부위에도 상기 접합면의 돌출부(107)와 오목부(108)에 대응되는 오목부(109)와 돌출부(110)를 형성할 수 있으며, 상기 돌출부와 오목부는 서로 대칭되게 다양한 형상으로 변경할 수 있다.In addition, a protrusion 107 and a concave portion 108 are formed on the bonding surfaces 105 and 106 so as to increase the contact area to be fused, and a protrusion of the bonding surface ( The concave portion 109 and the protrusion 110 corresponding to the concave portion 107 and the concave portion 108 may be formed, and the protrusion and the concave portion may be changed into various shapes to be symmetrical to each other.

또한, 상기 부재의 결합부(103, 104)는 접합면적을 넓힐 수 있도록 상기 공간부의 가장자리를 따라 외부로 돌출되는 플랜지부를 형성하며, 상기 플랜지부의 일면인 접합면(105, 106)을 포함한다.In addition, the joining portions 103 and 104 of the member form a flange portion protruding outward along the edge of the space portion so as to increase the joining area, and include joining surfaces 105 and 106 that are one surface of the flange portion. do.

또한, 상기 접합면(105, 106)을 서로 마주보도록 위치시키고, 상기 접합면(105, 106) 사이에 히터를 삽입하여 상기 삽입된 히터의 가열된 양면과 접합면(105, 106)을 접촉하여 용융시킨 다음, 상기 히터는 분리 추출하고, 상기 용융된 접합면(105, 106)이 서로 맞닿도록 가압하여 결합되는 것을 특징으로 할 수 있다.In addition, by positioning the bonding surfaces 105 and 106 to face each other, and inserting a heater between the bonding surfaces 105 and 106, the heated both surfaces of the inserted heater and the bonding surfaces 105 and 106 After melting, the heater may be separated and extracted, and the melted bonding surfaces 105 and 106 may be pressed and bonded to abut each other.

또한, 상기 지그틀(210, 220)을 이용하여 최적의 융착 방법을 살펴 보면,In addition, looking at the optimal fusion method using the jig frame (210, 220),

지그틀(210, 220)에서 융착에 사용되는 히터(300)의 표면온도는 450℃ ~700℃이고, 상기 히터(300)와 접합면(105, 106)의 접촉 시간은 2~3초이고, The surface temperature of the heater 300 used for fusion in the jig molds 210 and 220 is 450°C to 700°C, and the contact time between the heater 300 and the bonding surfaces 105 and 106 is 2 to 3 seconds,

상기 접촉시간이 경과 후에 히터(300)가 분리 추출되면 0.2~0.3초 내로 가압하여 융착 결합시키는 것을 최적으로 조건으로 선택할 수 있으며,When the heater 300 is separated and extracted after the elapse of the contact time, it is possible to select an optimal condition to pressurize within 0.2 to 0.3 seconds to fusion bond,

상기 접촉시간이 경과 후에 접합면(105, 106) 사이에서 히터(300)가 분리 추출되면 0.2~0.3초 내로 가압하여 융착 결합시키는 것이다.When the heater 300 is separated and extracted between the bonding surfaces 105 and 106 after the elapse of the contact time, it is fused and bonded by pressing within 0.2 to 0.3 seconds.

상기와 같은 최적의 조건은 상기 융착에 사용되는 히터(300)의 표면온도를 450℃이하로 설정하면 지그틀(210, 220)에 삽입된 접합면(105, 106)이 용융되는 시간이 길어짐은 물론이고, 상기 접합면(105, 106)이 융착에 적합하게 용융되지 않고, 이와 같이 용융이 적합하지 않은 접합면을 가압하여 융착시켜도 접합강도가 약하게 된다.The optimum condition as described above is that if the surface temperature of the heater 300 used for the fusion is set to 450°C or less, the time for the bonding surfaces 105 and 106 inserted in the jigframes 210 and 220 to melt becomes longer. Of course, the bonding surfaces 105 and 106 are not melted appropriately for fusion, and the bonding strength is weakened even if the bonding surfaces that are not suitable for melting are pressed and fused together.

또한, 상기 히터(300)의 표면온도는 700℃이상으로 하면, 지그틀(210, 220)에 삽입된 접합면(105, 106)이 높은 온도로 인하여 필요 이상 용융되어 접합면(105, 106)에서 용융된 용융액이 히터면에 부착되거나 하부로 흘러내리게 된다.In addition, when the surface temperature of the heater 300 is 700° C. or higher, the bonding surfaces 105 and 106 inserted in the jig frames 210 and 220 melt more than necessary due to the high temperature, and the bonding surfaces 105 and 106 The molten liquid melted in is attached to the heater surface or flows down.

따라서, 융착에 사용되는 히터(300)의 최적 표면온도는 450℃ ~700℃이고, 상기 히터(300) 온도를 선택에 의하여, 히터와 접합면(105, 106)의 접촉 시간은 상기 히터(300)의 표면온도에 따라 2~3초 사이에서 시간을 선택할 수 있고, 상기 접촉시간이 경과되어 접합면(105, 106)이 용융되면, 상기 접합면(105, 106) 사이에 삽입된 히터(300)를 분리 추출한다.Therefore, the optimum surface temperature of the heater 300 used for fusion is 450°C to 700°C, and by selecting the temperature of the heater 300, the contact time between the heater and the bonding surfaces 105 and 106 is determined by the heater 300 ) Depending on the surface temperature, you can select a time between 2 and 3 seconds, and when the contact time elapses and the bonding surfaces 105 and 106 are melted, the heater 300 inserted between the bonding surfaces 105 and 106 ) Is separated and extracted.

또한, 상기 히터가 추출되면 지그틀은 유압 또는 공기압으로 가동되는 실린더를 이용하여 0.2~0.3초 내로 용융된 접합면을 맞닿도록 이동하고, 가압하여 융착 결합시키는 것이다.In addition, when the heater is extracted, the jigtle moves so as to contact the molten bonding surface within 0.2 to 0.3 seconds using a cylinder operated by hydraulic or pneumatic pressure, and pressurizes to fusion bond.

상기와 같이 히터(300)가 분리 추출되면 0.2~0.3초 내로 가압하는 조건중 0.2초는 히터와 접촉된 접합면(105, 106)의 분리 추출되는 시간이 필요하고, 0.3초 내로 가압하는 것은 용융된 접촉면이 냉각되기 전에 용융면을 접촉시켜 가압하도록 선정한 것이다. When the heater 300 is separated and extracted as described above, 0.2 seconds of the conditions of pressurization within 0.2 to 0.3 seconds require a time to separate and extract the bonding surfaces 105 and 106 in contact with the heater, and pressurization within 0.3 seconds is melted. It is selected to pressurize by contacting the molten surface before the contact surface is cooled.

또한, 상기와 같은 가압으로 융착되면 접합면을 자연 냉각시키거나 송풍하여 냉각한 후 에 지그틀(210, 220)에 고정된 부표를 가압부재(250)로 가압하여 추출 반출함으로서 부표가 완성됨을 알 수 있다.In addition, when fused with the above pressure, it is known that the buoy is completed by extracting and carrying out the buoy fixed to the jigtle (210, 220) after cooling by naturally cooling or by blowing. I can.

이러한 방법으로 제작된 부표(100)의 크기는 길이 600㎜ 직경 400㎜이고, 부표 몸체의 두께는 3㎜이고, 반원형의 리브의 높이는 3㎜, 격벽부재의 두께는 3㎜, 결합부(103, 104)의 두께는 10~13㎜, 융착 결합된 두께는 20~25㎜로 형성될 수 있으며, 이러한 수치는 최적의 수치로 이외 다양한 크기와 두께로 제작할 수 있다.The size of the buoy 100 manufactured in this way is 600 mm in length and 400 mm in diameter, the thickness of the buoy body is 3 mm, the height of the semi-circular rib is 3 mm, the thickness of the partition member is 3 mm, the coupling part 103, 104) may have a thickness of 10 to 13 mm and a fusion bonded thickness of 20 to 25 mm, and these values can be manufactured in various sizes and thicknesses other than the optimal values.

또한, 부표는 햇빛이 강한 바다에서 사용되므로 자외선 차단기능의 부여하여야 되며, 자외선 차단방법은 열융착 결합된 부표(100)의 표면에 용제, 실란, 아세트산으로 구성된 프라이머를 도포하여 프라이머 코팅층을 생성한다.In addition, since the buoy is used in the sea with strong sunlight, it must provide a UV blocking function, and the UV blocking method is to create a primer coating layer by applying a primer composed of a solvent, silane, and acetic acid on the surface of the buoy 100 bonded by heat fusion. .

또한, 상기 부표의 표면에 알루미나 분말이 포함된 제1 코팅제를 도포한 후 UV 차단제가 포함된 제2 코팅제를 도포하여 제2 코팅층을 생성하여 자외선 차단기능의 부여하는 것으로 선택할 수 있다.In addition, after applying the first coating agent containing alumina powder on the surface of the buoy, it may be selected to apply a second coating agent containing a UV blocking agent to create a second coating layer to provide a UV blocking function.

또한, 상기 프라이머는 실란 10 중량부에 용제 450 내지 550 중량부 및 아세트산 2 내지 4 중량부가 혼합되어 구성될 수 있으며, 상기 1차 도장단계는 스프레이 도장을 사용하고, 상기 2차 도장단계는 정전 도장을 선택할 수 있다.In addition, the primer may be configured by mixing 450 to 550 parts by weight of a solvent and 2 to 4 parts by weight of acetic acid in 10 parts by weight of silane, and the first painting step uses spray painting, and the second painting step is electrostatic painting You can choose.

또한, 상기 공정에서 자외선 차단기능의 부여한 열융착 결합된 부표(100)의 표면에는 야광테이프를 부착하거나 야광도료를 도포하여 부표 표면에 띠 형태의 야광 반사부를 이루도록 형성되되, 상기 야광 반사부는 부체의 길이방향을 따라 일정 간격 이격되게 형성하여 어두운 야간에 빛을 발광하도록 야광 기능을 부가할 수 있다. In addition, a luminous tape is attached or a luminous paint is applied to the surface of the buoy 100, which has a UV-blocking function, and is formed to form a band-shaped luminous reflector on the surface of the buoy. A luminous function can be added to emit light in a dark night by forming at regular intervals along the length direction.

또한, 열융착 부표의 제조방법을 살펴 보면, In addition, looking at the manufacturing method of the thermal bonding buoy,

열융착 부표의 제조방법으로서As a method of manufacturing a heat-sealing buoy

합성수지로 내부에 형성되는 공간부와, 결합부를 가지는 부재(101, 102)를 각각 형성하는 단계와; 상기 각각의 부재(101, 102)의 접합면(105, 106)이 대응되도록 지그틀(210, 220)에 각각 장착하는 단계이며,Forming members (101, 102) each having a space portion and a coupling portion formed therein of synthetic resin; It is a step of attaching to the jig frames 210 and 220 so that the bonding surfaces 105 and 106 of the respective members 101 and 102 correspond,

상기 지그틀(210, 220)에 삽입 결합된 부재의 접합면(105, 106) 사이에 히터(300)를 장착하는 단계와; 상기 히터(300)가 부재의 접합면(105, 106) 사이에 장착되면, 제어부의 제어에 따라 450℃ ~700℃로 가열된 히터면과 상기 접합면(105, 106)을 2~3초간 접촉하여 용융하는 단계로 이루어 지며,Mounting a heater 300 between the bonding surfaces 105 and 106 of the members inserted and coupled to the jig frames 210 and 220; When the heater 300 is mounted between the bonding surfaces 105 and 106 of the member, the heater surface heated to 450°C to 700°C and the bonding surfaces 105 and 106 are contacted for 2 to 3 seconds under the control of the controller. It consists of a step of melting,

상기 접합면(105, 106)이 용융되면, 히터를 접합면(105, 106) 사이에서 분리 추출한 후, 접합면(105, 106)을 0.2 ~ 0.5초간 가압하여 접합면(105, 106)의 융착부가 가압 융착되는 부표를 형성하는 단계로 이루어지며,When the bonding surfaces 105 and 106 are melted, the heater is separated and extracted between the bonding surfaces 105 and 106, and then the bonding surfaces 105 and 106 are pressed for 0.2 to 0.5 seconds to fuse the bonding surfaces 105 and 106. It consists of the step of forming a buoy to be fused by additional pressure,

상기 부표를 지그틀(210, 220) 중 어느 하나에 장착된 가압부재(250)의 가압으로 지그틀(210, 220)에서 분리되어 완성되는 단계로 이루어 짐을 알 수 있다.It can be seen that the buoy is separated from the jig holders 210 and 220 by pressing the pressing member 250 mounted on one of the jig frames 210 and 220 and is completed.

이상의 설명은 본 발명을 예시적으로 설명한 것이고, 명세서에 게시된 실시 예는 본 발명의 기술사상을 한정하기 위한 것이 아니라 설명하기 위한 것이므로 본 발명이 속하는 기술분야에서 통상의 지식을 가진 자라면 본 발명의 기술사상을 벗어나지 않는 범위에서 다양한 수정 및 변형이 가능할 것이다. 그러므로 본 발명의 보호범위는 청구범위에 기재된 사항에 의해 해석되고, 그와 균등한 범위 내에 있는 기술적 사항도 본 발명의 권리범위에 포함되는 것으로 해석되어야 할 것이다.The above description is an illustrative description of the present invention, and the embodiments published in the specification are not intended to limit the technical idea of the present invention, but to describe the present invention. Various modifications and variations will be possible without departing from the technical idea of Therefore, the scope of protection of the present invention is interpreted by the matters described in the claims, and technical matters within the scope equivalent thereto should be construed as being included in the scope of the present invention.

101, 102 : 부재 103, 104 : 결합부
105, 106 : 접합면 107, 110 : 돌출부
108, 109: 오목부 111, 112 : 오목 홈부
113, 114, 115, 116 : 고리부 117, 118 : 격벽
119 : 리브 120, 130 : 보강링
210, 220 : 지그틀 230, 240 : 안내부재
250: 가압부재 300: 히터
101, 102: member 103, 104: coupling portion
105, 106: bonding surface 107, 110: protrusion
108, 109: concave portion 111, 112: concave groove portion
113, 114, 115, 116: ring portion 117, 118: bulkhead
119: rib 120, 130: reinforcing ring
210, 220: jig frame 230, 240: guide member
250: pressure member 300: heater

Claims (8)

부표(100)에 있어서
상기 부표는 두 개의 부재(101, 102)가 결합되어 구성되되
상기 부재(101, 102)는 내부에 형성된 공간부;와 상기 부재의 일측에 상기 공간부와 통공되면서 상기 부재들을 결합하기 위한 결합부(103, 104);가 구비되어
상기 부재들을 대응되게 위치시킨 후 상기 결합부(103, 104)를 통해 상기 부재(101, 102)들을 결합하여 형성되되,
상기 결합부(103, 104)는 접합면적을 넓힐 수 있도록 상기 공간부의 가장자리를 따라 외부로 돌출되는 플랜지부와 상기 플랜지부의 일면인 접합면(105, 106)을 포함하며, 상기 접합면(105, 106)이 서로 마주보도록 위치시키고,
상기 접합면(105, 106) 사이에 히터를 삽입하여 상기 서로 마주보는 접합면(105, 106)을 용융시킨 다음, 상기 히터는 분리 추출하고, 상기 용융된 접합면(105, 106)이 서로 맞닿도록 가압하여 결합하며
상기 결합부(103, 104)의 양측에는 금속재질로 형성된 링형태의 보강링(120, 130)을 더 포함하며, 상기 결합부(103, 104)의 양측의 보강링과 상기 결합부를 상기 결합부에 형성된 고정끈 삽입부(109, 110)를 이용하여 강재 또는 고정끈으로 묶거나 고정 결합시켜 접합부의 접합강도를 증대시키는 것을 특징으로 하는 열융착 고정 부표.
In the buoy (100)
The buoy is composed of two members (101, 102) combined
The members 101 and 102 are provided with a space portion formed therein; and a coupling portion 103 and 104 for coupling the members while passing through the space portion at one side of the member.
After positioning the members correspondingly, formed by combining the members 101 and 102 through the coupling portions 103 and 104,
The coupling portions 103 and 104 include a flange portion protruding outward along an edge of the space portion and a joint surface 105 and 106 which are one surface of the flange portion so as to increase the joint area, and the joint surface 105 , 106) are positioned to face each other,
A heater is inserted between the bonding surfaces 105 and 106 to melt the bonding surfaces 105 and 106 facing each other, and then the heater is separated and extracted, and the melted bonding surfaces 105 and 106 abut each other. Pressurized and combined
Both sides of the coupling portions 103 and 104 further include ring-shaped reinforcing rings 120 and 130 formed of a metal material, and reinforcing rings on both sides of the coupling portions 103 and 104 and the coupling portion Thermal fusion fixing buoy, characterized in that to increase the bonding strength of the joint by binding or fixedly coupled with a steel material or a fixing string using the fixing string insertion portions (109, 110) formed in the.
삭제delete 제1항에 있어서
상기 부재의 몸통부 원형부의 끝단에는 고정끈이 삽입되는 고리부(115, 116)가 구비되고, 플랜지부 외부면의 소정부위에는 일정한 간격으로 고정끈이 삽입되는 고리부(113, 114)가 구비되는 것을 특징으로 하는 열융착 고정 부표.
According to claim 1
Ring portions 115 and 116 are provided at the ends of the circular portion of the trunk portion of the member, and ring portions 113 and 114 into which the fixing straps are inserted at regular intervals are provided at a predetermined portion of the outer surface of the flange portion. Heat-sealed fixed buoy, characterized in that the.
제3항에 있어서
상기 부재(101, 102)는 내부에 형성된 공간부에 다수의 분할 공간을 갖도록 구획 형성된 격벽부재(117, 118)를 포함하며, 상기 부재의 외주면에는 외부로 돌출된 반원형의 리브(119)를 부재의 길이방향을 따라 일정 간격 이격되게 형성된 것을 특징으로 하는 열융착 고정 부표.
According to claim 3
The members 101 and 102 include partition wall members 117 and 118 partitioned to have a plurality of divided spaces in a space formed therein, and a semicircular rib 119 protruding outward is formed on the outer circumferential surface of the member. Heat-sealed fixed buoys, characterized in that formed at a certain interval along the longitudinal direction of.
제4항에 있어서
상기 부재(101, 102)가 내부에 수용되는 한 쌍의 지그틀(210, 220)과, 상기 지그틀(210, 220)에 수납되는 상기 부재는 접합면(105, 106)이 서로 마주보도록 배치되며,
상기 지그틀(210, 220)은 유압 또는 공기압으로 가동되는 실린더로 이동 및 가압되도록 형성하고,
상기 부재의 접합면(105, 106) 사이에 삽입하여 접촉되는 접합면(105, 106)을 용융되도록 가열하는 히터(300)와,
상기 히터(300)는 접촉되는 상기 접합면(105, 106)이 용융되면 상기 지그틀(210, 220)사이에서 분리 추출하고,
상기 지그틀(210, 220)은 삽입된 접합면(105, 106)이 용융된 상태에서 가압하여 융착 결합하며,
상기 융착 결합된 부표(100)를 상기 지그틀(210, 220)에서 분리하여 추출하기 위한 가압부재(250)를 더 포함하는 것을 특징으로 하는 열융착 고정 부표.
According to claim 4
A pair of jig frames 210 and 220 in which the members 101 and 102 are accommodated, and the members accommodated in the jig frames 210 and 220 are arranged so that the bonding surfaces 105 and 106 face each other. And
The jig frames 210 and 220 are formed to be moved and pressurized by a cylinder operated by hydraulic or pneumatic pressure,
A heater 300 for heating the bonding surfaces 105 and 106 in contact by being inserted between the bonding surfaces 105 and 106 of the member to melt,
The heater 300 separates and extracts between the jig frames 210 and 220 when the contact surfaces 105 and 106 are melted,
The jig frame (210, 220) is fusion bonded by pressing the inserted bonding surface (105, 106) in a molten state,
A heat-sealing fixed buoy further comprising a pressing member 250 for separating and extracting the fusion-bonded buoy 100 from the jig frames 210 and 220.
삭제delete 제1항에 있어서
열융착 결합된 부표(100)의 표면에 용제, 실란, 아세트산으로 구성된 프라이머를 도포하여 프라이머 코팅층을 생성하고,
상기 부표의 표면에 알루미나 분말이 포함된 제1 코팅제를 도포한 후 UV 차단제가 포함된 제2 코팅제를 도포하여 제2 코팅층을 생성하여 자외선 차단기능을 부여한 것을 특징으로 하는 열융착 고정 부표.
According to claim 1
To create a primer coating layer by applying a primer composed of a solvent, silane, and acetic acid on the surface of the heat-sealed buoy 100,
A heat-sealing fixed buoy, characterized in that after applying a first coating agent containing alumina powder on the surface of the buoy, and then applying a second coating agent containing a UV blocking agent to create a second coating layer to provide a UV blocking function.
제7항에 있어서
자외선 차단기능을 부여한 열융착 결합된 부표(100)의 표면에 야광테이프를 부착하거나 야광도료를 도포하여 부표의 표면에서 띠 형태를 이루도록 형성하는 것을 특징으로 하는 열융착 고정 부표.
According to claim 7
A heat-sealing fixed buoy, characterized in that forming a band shape on the surface of the buoy by attaching a luminous tape or applying a luminous paint to the surface of the heat-sealing-coupled buoy 100 with a UV blocking function.
KR1020180151611A 2018-11-30 2018-11-30 Heat fusion fixing a float KR102196311B1 (en)