KR100662545B1 - Method and apparatus for forming oily make-up powder by pressing - Google Patents

Method and apparatus for forming oily make-up powder by pressing Download PDF

Info

Publication number
KR100662545B1
KR100662545B1 KR1020050040094A KR20050040094A KR100662545B1 KR 100662545 B1 KR100662545 B1 KR 100662545B1 KR 1020050040094 A KR1020050040094 A KR 1020050040094A KR 20050040094 A KR20050040094 A KR 20050040094A KR 100662545 B1 KR100662545 B1 KR 100662545B1
Authority
KR
South Korea
Prior art keywords
press
product container
molding
powder
upper punch
Prior art date
Application number
KR1020050040094A
Other languages
Korean (ko)
Other versions
KR20060117653A (en
Inventor
황선철
김형운
Original Assignee
(주)아모레퍼시픽
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by (주)아모레퍼시픽 filed Critical (주)아모레퍼시픽
Priority to KR1020050040094A priority Critical patent/KR100662545B1/en
Publication of KR20060117653A publication Critical patent/KR20060117653A/en
Application granted granted Critical
Publication of KR100662545B1 publication Critical patent/KR100662545B1/en

Abstract

본 발명은 투웨이 케익이나 파우더 팩트, 스킨 커버와 같은 메이크업 화장품을 생산하기 위한 것으로서, 특히 분말원료의 가압성형공정을 하부 프레스에 의한 1차 성형단계 및 2차 성형단계로 각각 구분하고, 각각의 가압성형공정에 있어 1차 가압성형공정에서는 1차 성형 및 오일제거가 이루어지게 하고, 2차 가압성형공정에서는 2차 성형 및 반복오일제거가 이루어지도록 함으로서, 균일한 압력에 의해 효과적으로 오일을 제거하므로 제품 전체에 고른 경도 및 건/습 상태가 유지되게 하면서도, 용기외부로 오일이 새어나오는 것을 방지하며, 상부펀치의 하부면이 오염되는 것을 방지하면서도 흡습지의 파손 또는 구겨짐을 방지할 수 있어, 고품질의 화장품을 얻게 하면서도 보다 안정된 품질을 지속적으로 유지할 수 있는 효과를 갖는 오일리 메이크업 분말의 가압성형방법 및 그 성형장치에 대한 것이다.The present invention is to produce a make-up cosmetics, such as two-way cake, powder pact, skin cover, in particular, the press molding process of the powder raw material is divided into the primary molding step and the secondary molding step by the lower press, respectively, each press In the pressurization process, the primary press molding process removes the primary molding and oil, and the secondary press molding process performs the secondary molding and repeating oil removal, effectively removing oil by uniform pressure. High-quality cosmetics, while maintaining even hardness and dry / humidity throughout, preventing oil from leaking out of the container, and preventing breakage or wrinkle of the absorbent paper while preventing the lower surface of the upper punch from being contaminated Oily makeup that has the effect of maintaining a more stable quality Press-molding method, and the end is on the molding apparatus.

메이크업, 분말원료, 화장품, 1차 가압성형, 2차 가압성형, 상부펀치, 오일제거 Makeup, powder raw material, cosmetics, 1st press molding, 2nd press molding, upper punch, oil removal

Description

오일리 메이크업 분말의 가압성형방법 및 그 성형장치{Method and apparatus for forming oily make-up powder by pressing}Method for forming oily make-up powder and pressing apparatus {Method and apparatus for forming oily make-up powder by pressing}

도 1은 본 발명에 따른 메이크업 분말 성형장치의 평면 전체구성도1 is a plan view of the overall makeup of the makeup powder molding apparatus according to the present invention

도 2는 본 발명에 따른 메이크업 분말 성형장치의 측면 전체구성도Figure 2 is a whole side view of the makeup powder molding apparatus according to the present invention

도 3은 본 발명에 따른 메이크업 분말 성형장치의 가압성형부 확대정면도Figure 3 is an enlarged front view of the press molding portion of the makeup powder molding apparatus according to the present invention

도 4는 본 발명에 따른 메이크업 분말 성형장치의 1차 가압성형부의 상부펀치 사시도Figure 4 is a perspective view of the upper punch of the primary pressing portion of the makeup powder molding apparatus according to the present invention

도 5는 도 4에 의한 상부펀치의 가압성형공정을 도시한 확대도5 is an enlarged view illustrating a press molding process of the upper punch according to FIG. 4.

도 6은 본 발명에 따른 메이크업 분말 성형장치의 2차 가압성형부의 상부펀치 사시도Figure 6 is a perspective view of the upper punch of the secondary pressing molded part of the makeup powder molding apparatus according to the present invention

도 7은 도 6에 의한 상부펀치의 가압성형공정을 도시한 확대도FIG. 7 is an enlarged view illustrating a press molding process of the upper punch according to FIG. 6.

도 8은 본 발명에 따른 메이크업 분말 성형장치의 상부펀치의 오일 배출작동도8 is an oil discharge operation of the upper punch of the makeup powder molding apparatus according to the present invention

도 9는 종래의 가압성형방식과 본 발명에 따른 가압성형방식의 비교도Figure 9 is a comparison between the conventional pressing method and the pressing method according to the invention

* 도면의 주요부분에 대한 부호의 설명 *Explanation of symbols on the main parts of the drawings

1 : 제품용기 2 : 이송치구1: Product container 2: Transfer jig

10 : 이송수단 20 : 액체정량주입기10: transfer means 20: liquid injection

30 : 1차가압성형장치 31 : 권취롤30: primary pressure molding apparatus 31: winding roll

32 : 흡습지 33 : 상부실린더32: hygroscopic paper 33: upper cylinder

34 : 가압판 35 : 하부실린더34: pressure plate 35: lower cylinder

36 : 상부펀치 37 : 배출공36: upper punch 37: discharge hole

38 : 공간부 39 : 통공38: space part 39: through hole

40 : 2차가압성형장치 41 : 권취롤40: secondary pressure molding apparatus 41: winding roll

42 : 흡습지 43 : 상부실린더42: moisture absorbing paper 43: upper cylinder

44 : 가압판 45 : 하부실린더44: pressure plate 45: lower cylinder

46 : 상부펀치 47 : 배출공46: upper punch 47: discharge hole

48 : 공간부 49 : 통공48: space 49: through

50 : 경계가압부50: boundary pressure part

본 발명은 투웨이 케익이나 파우더 팩트, 스킨 커버와 같은 메이크업 화장품을 생산하기 위한 것으로서, 특히 오일리(oily) 원료를 용기에 주입한 후, 이를 1차 가압성형공정 한 후 이를 다시 2차 가압성형하여 이에 의해, 오일리 원료로부터 그 오일성분을 용이하고 효과적으로 제거함으로서, 더욱 뛰어난 품질을 안정적으로 유지할 수 있게 한 오일리 메이크업 분말의 가압성형방법 및 그 성형장치에 관한 것이다.The present invention is to produce a make-up cosmetics, such as a two-way cake, powder pact, skin cover, in particular, after injecting the oily (oily) raw material into the container, it is subjected to the first press molding process and then again to the second press molding Thereby, the present invention relates to a pressurizing method for oily makeup powder and a molding apparatus thereof, by which the oil component is easily and effectively removed from the oily raw material, thereby making it possible to stably maintain excellent quality.

일반적으로 메이크업을 하기 위해서는, 사용자의 취향이나 피부의 특성에 따라 다양한 기능 및 형태를 갖는 수많은 종류 화장품을 사용하게 되는데, 가장 보편적으로는 메이크업 베이스 및 파우더, 투웨이 케익, 파우더 팩트, 스킨 커버 등이 주로 이용된다.In general, to make up, many kinds of cosmetics having various functions and shapes are used according to the user's taste or the characteristics of the skin. Most commonly, makeup base and powder, two-way cake, powder pact, and skin cover are mainly used. Is used.

이때, 상기한 바와 같은 메이크업용 화장품은 오일리 분말원료를 용기 내에 주입한 후 이를 프레스에 의해 가압 성형하여 만들어지는 것으로, 대부분 고형으로 압축되어 생산되는 것이다.In this case, the makeup cosmetics as described above are made by injecting the oily powder raw material into the container and press-molded it by a press, which is mostly compressed and produced.

특히, 상기한 오일성분은 탈크, 이산화티탄, 마이카, 실리카, 나일론 분말, 폴리메칠매타크릴레이크, 세리사이트, 카올린, 이연화, 옥시염화비스머스 등과 같은 기제에 색상을 나타내기 위한 색소 및 상기 성분들을 결합시키는 바인더로 작용하게 되는 것이며,In particular, the oil component is a pigment for coloring the base and the components such as talc, titanium dioxide, mica, silica, nylon powder, polymethyl methacrylate, sericite, kaolin, disintegration, bismuth oxychloride, and the like. Act as a binder to bind,

상기한 바인더는, 실리콘계 오일류, 탄화수소계 오일류, 고급 지방산계 오일류, 고급알콜계 오일류, 에스테르계 오일류, 글리세라이드계 오일류, 라놀린계 오일류, 동물성계 오일류, 식물성계 오일류 등이 선택적으로 사용되고 있다.As the binder, silicone oils, hydrocarbon oils, higher fatty acid oils, higher alcohol oils, ester oils, glyceride oils, lanolin oils, animal oils, vegetable oils and the like are selectively used.

이때, 상기한 베이스의 점도는 항상 일정하지 않으나, 일반적인 습식 성형방법에 의해 제조할 경우의 기본색 베이스 점도가 15,000~25,000cps 인데 반해, 유동성 반죽상의 점도는 20~50,000cps의 폭넓은 점도를 갖는 것을 사용할 수 있는 것이다.In this case, the viscosity of the base is not always constant, but the base color base viscosity when prepared by the general wet molding method is 15,000 ~ 25,000cps, whereas the viscosity of the flowable dough phase has a wide viscosity of 20 ~ 50,000cps It can be used.

따라서, 완성된 제품을 생산하기 위해서는 상기한 바와 같은 점도를 갖는 원료로부터 그 오일성분의 바인더를 제거해주어야 하는 것이며, 이러한 오일성분의 제거방법으로는 습식성형과정에 있어 원료의 가압성형과정 중에 그 가압치구로 배어나오는 오일을 강제로 흡입하여 배출하는 방법이 채택되고 있다.Therefore, in order to produce the finished product, it is necessary to remove the binder of the oil component from the raw material having the viscosity as described above, and the method of removing the oil component is pressurization during the press molding process of the raw material in the wet molding process. A method of forcibly inhaling and discharging oil coming into the jig has been adopted.

이러한, 메이크업용 화장품의 개략적인 생산과정을 살펴보면, 화장품 내부용기가 내장되어진 운반치구는 컨베이어 이송수단에 의해 순차적으로 이송되고, 운반치구의 이송과정 중에 오일리 원료의 투입공정과, 프레스에 의한 투입된 원료의 가압성형 및 오일배출공정을 거치게 되고, 오일이 제거된 용기를 취출하여 완성하는 것으로서,Looking at the outline of the production process of the cosmetic make-up, the conveying jig in which the inner container of the cosmetic is built is sequentially transferred by the conveyer conveying means, the process of adding the oily raw material and the raw material introduced by the press during the conveying jig of the conveying jig. Through the press molding and oil discharge process of, and to take out the container from which oil has been removed,

상기한 원료투입공정에서는 액체정량주입기가 사용되고, 액체정량주입기는 유동성 반죽상의 베이스를 건밸브와 자동 디스펜서에 의해 토출시키는 것이며,In the above-mentioned raw material injection process, a liquid metering injector is used, and the liquid metering injector ejects the base of the flowable dough by a gun valve and an automatic dispenser,

투입된 원료의 가압성형공정은, 그 용기의 상측에서 승강하는 가압치구에 의해 용기 내에 주입되어 있는 원료를 가압하게 되는 것이며, 이와 동시에 가압되는 원료로부터 발생하는 오일성분은 강제 흡입기에 의해 인공적으로 흡입하여 배출하는 오일배출공정을 수행하는 것이다.In the press molding step of the injected raw material, the raw material injected into the container is pressurized by the pressure jig lifting up from the upper side of the container. At the same time, the oil component generated from the pressurized raw material is artificially sucked by the forced suction unit. It is to carry out the oil draining process.

그러나, 상기한 바와 같은 메이크업 분말의 가압성형공정에 있어, 오일배출공정은, 상측으로부터 하강하는 프레스 및 가압치구의 압력에 의해 분말원료에 배어있던 오일을 강제 배출시켜 이를 제거하는 것이므로,However, in the press molding process of the makeup powder as described above, the oil discharge process is to forcibly discharge the oil soaked in the powder raw material by the pressure of the press and pressure jig falling from the upper side to remove it,

상측으로부터 강제적인 가압에 의해 오일이 배어나오게 함에 따라 용기 하측의 분말원료에 배합되어 있던 오일은 배출되지 않는 문제점이 있어 전체적으로 균 일한 건/습 상태를 유지할 수 없는 문제점이 있는 것이며,As oil is squeezed out by forcibly pressurized from the upper side, the oil mixed in the powder raw material at the lower side of the container is not discharged, and thus there is a problem that the overall dry and wet state cannot be maintained.

별도의 오일흡입수단에 의해 그 오일을 제거하므로 필요이상 과도한 시설투자비를 요구하면서도, 흡입소음 등에 의해 정숙하고 쾌적한 작업환경을 조성하지 못하게 되는 것이다.Since the oil is removed by means of a separate oil suction means, excessive facility investment cost is required, but it is unable to create a quiet and comfortable working environment by suction noise.

또한, 용기와 대응상의 형상을 갖는 가압치구는, 용기의 내측벽과 가압치구의 외주면 사이의 틈새로 오일리 원료가 새어나오는 문제점이 있으면서도, 전체적으로 균일한 압력이 부여되지 않아 원료의 점도 또는 고형의 정도가 균일하지 못한 문제점을 갖게 된다.In addition, the pressure jig having a shape corresponding to the container has a problem that oily raw material leaks out due to a gap between the inner wall of the container and the outer circumferential surface of the pressure jig. Has a non-uniform problem.

본 발명은 전기한 바와 같은 문제점을 극복하고자 안출된 것으로서, 분말원료의 가압성형공정을 하부 프레스에 의한 1차성형단계 및 2차성형단계로 각각 구분하고, 각각의 가압성형공정에 있어 1차 가압성형공정에서는 1차 성형 및 오일제거가 이루어지게 하고, 2차 가압성형공정에서는 2차 성형 및 반복오일제거가 이루어지도록 함으로서,The present invention has been made to overcome the problems described above, divided into a primary molding step and a secondary molding step of the press molding process of the powder raw material, respectively, the first press in each press molding process In the molding process, primary molding and oil removal are performed, and in the secondary press molding process, secondary molding and repeated oil removal are performed.

균일한 압력에 의해 효과적으로 오일을 제거하므로 제품 전체에 고른 경도 및 건/습상태가 유지되게 하면서도, 용기외부로 오일이 새어나오는 것을 방지하며, 상부펀치의 하부면이 오염되는 것을 방지하면서도 흡습지의 파손 또는 구겨짐을 방지할 수 있어, 고품질의 화장품을 얻게 하면서도 보다 안정된 품질을 지속적으로 유지할 수 있는 효과를 갖는 오일리 메이크업 분말의 가압성형방법 및 그 성형장치를 제공함에 본 발명의 목적이 있는 것이다. By removing the oil effectively by the uniform pressure, it maintains even hardness and dry / wet state throughout the product, prevents oil from leaking out of the container, and damages the absorbent paper while preventing the lower surface of the upper punch from being contaminated. Another object of the present invention is to provide a pressurizing method of the oily makeup powder and its molding apparatus, which can prevent wrinkles, thereby obtaining a cosmetic of high quality while maintaining a more stable quality.

이하, 본 발명의 바람직한 실시 예를 설명한다.Hereinafter, preferred embodiments of the present invention will be described.

도 1은 본 발명에 따른 메이크업 분말 성형장치의 평면 전체구성도이고, 도 2는 본 발명에 따른 메이크업 분말 성형장치의 측면 전체구성도이며, 도 3은 본 발명에 따른 메이크업 분말 성형장치의 가압성형부 확대정면도이다.1 is an overall plan view of the makeup powder molding apparatus according to the present invention, FIG. 2 is a side overall configuration diagram of the makeup powder molding apparatus according to the present invention, and FIG. 3 is a press molding of the makeup powder forming apparatus according to the present invention. This is an enlarged front view.

먼저, 본 발명에 따른 오일리 메이크업 분말의 가압성형방법을 살펴보면,First, looking at the pressure molding method of the oily makeup powder according to the present invention,

제품용기가 삽입된 이송치구가 순차적으로 이송되고, 이송된 이송치구의 제품용기의 내부에 액체정량주입기에 의해 분말원료를 투입한 후,After transporting the jig into which the product container is inserted, the powder raw material is introduced into the product container of the transported jig by the liquid metering injector.

상기 제품용기를 갖는 이송치구가 1차 가압성형수단에 위치되도록 하여, 상측의 흡습지 및 상부펀치와 하측의 가압프레스에 의해 1차 가압성형 및 오일제거공정을 수행케 하고,The transfer jig having the product container is positioned in the primary press forming means, and the primary press forming and oil removing process is performed by the upper absorbent paper, the upper punch and the lower press press.

1차 가압성형된 이송치구를 2차 가압성형수단으로 이동시켜, 상측의 흡습지 및 상부펀치와 하측의 가압프레스에 의해 2차 가압성형 및 오일제거공정을 수행케 하여,The primary press-molded transfer jig is moved to the secondary press forming means, and the secondary press forming and oil removing process is performed by the upper absorbent paper, the upper punch and the lower press press.

2단계의 가압성형공정에 의해 고른 경도 및 건/습 상태를 유지할 수 있게 하고, 하부 가압프레스에 의해 균일하고 안정된 오일 배출작용이 이루어지도록 한 것이다.By the two-stage press molding process, it is possible to maintain an even hardness and dry / wet state, and to ensure a uniform and stable oil discharge action by the lower pressure press.

이러한 가압성형방법을 이루기 위한 가압성형장치는,The press molding apparatus for achieving such a press molding method,

본체(100)의 상측에 마련된 컨베이어 이송수단(10)에 의해, 내부에 제품용기 (1)를 갖는 이송치구(2)가 연속적으로 이송되게 하고,By the conveyor conveying means 10 provided on the upper side of the main body 100, the conveying jig 2 having the product container 1 therein is continuously conveyed,

상기 이송치구(2)는, 액체정량주입기(20)와; 1차 가압성형장치(30)와; 2차 가압성형장치(40)를 따라 순차적으로 이송되게 하되,The transfer jig (2), and a liquid metering injector (20); Primary press molding apparatus 30; To be sequentially transported along the secondary press molding apparatus 40,

액체정량주입기(20)는, 적어도 하나 이상의 자동 디스펜서(21)에 의해 정량의 분말원료가 상기 제품용기(1)의 내부로 주입되게 형성하고,The liquid metering injector 20 is formed by at least one or more automatic dispensers 21 so that the quantitative powder raw material is injected into the inside of the product container 1,

1차 가압성형장치(30)는, 권취롤(31)에 의해 일정속도로 공급되는 흡습지(32)가 제품용기(1)의 상측에 위치되고, 그 흡습지(32)의 상측에는 상기 제품용기(1)의 내부형상과 동일한 상부펀치(36)를 갖는 상부실린더(33)가 위치하며, 상기 이송치구(2)의 하측에는 가압판(34)을 갖는 하부실린더(35)가 위치되어 구성되며,In the primary press-molding apparatus 30, the absorbent paper 32, which is supplied at a constant speed by the winding roll 31, is positioned above the product container 1, and above the absorbent paper 32, the product container ( The upper cylinder 33 having the same upper punch 36 as the internal shape of 1) is located, the lower cylinder 35 having a pressure plate 34 is positioned below the transfer jig 2,

2차 가압성형장치(40)는, 권취롤(41)에 의해 일정속도로 공급되는 흡습지(42)가 제품용기(1)의 상측에 위치되고, 그 흡습지(42)의 상측에는 상기 제품용기(1)의 내부형상과 동일한 상부펀치(46)를 갖는 상부실린더(43)가 위치하며, 상기 이송치구(2)의 하측에는 가압판(44)을 갖는 하부실린더(45)가 위치되게 구성되도록 한 것이다.In the secondary press-molding apparatus 40, the absorbent paper 42, which is supplied at a constant speed by the winding roll 41, is positioned above the product container 1, and above the absorbent paper 42, the product container ( The upper cylinder 43 having the upper punch 46 and the same as the inner shape of 1) is positioned, the lower cylinder 45 having the pressure plate 44 is positioned below the transfer jig (2). .

이때, 상기한 1차 가압성형장치(30)의 상부펀치(36)는, 그 하부 가장자리가 내측 경사면을 갖도록 융출된 경계가압부(50)를 형성하여, 오일성분이 용기와 상부펀치(32)의 경계틈으로 새어나오는 것을 방지하게 됨은 물론 그 가장자리측의 오일성분을 내측으로 집중시켜 보다 균일하고 효과적인 오일배출 작용을 할 수 있게 한 것이며,At this time, the upper punch 36 of the primary press-molding apparatus 30 forms a boundary pressure part 50 in which the lower edge thereof has an inner inclined surface, and the oil component is formed in the container and the upper punch 32. It prevents leaking into the boundary gap of the oil and also concentrates the oil component on the edge side to make the oil discharge function more uniform and effective.

상기 1차 가압성형장치(30)와 2차 가압성형장치(40)의 상부펀치(36)(46)는, 그 일측면에 배출공(37)(47)을 형성하여, 내측의 공간부(38)(48)와 연통되게 하고, 상기 공간부(38)(48)는 하측 방향으로 복수개 형성된 통공(39)(49)을 통해 하부면과 관통되게 형성된 것이다.The upper punches 36 and 46 of the primary press molding device 30 and the secondary press molding device 40 form discharge holes 37 and 47 on one side thereof, and the inner space portion ( 38 and 48, and the spaces 38 and 48 are formed to penetrate the lower surface through the plurality of through-holes 39 and 49 formed in the downward direction.

이상과 같은 방법 및 구성에 의한 본 발명 오일리 메이크업 분말의 가압성형방법 및 그 성형장치의 제조공정 및 작용을 첨부도면에 의해 보다 상세히 설명하면 다음과 같다.The pressure forming method of the oily make-up powder of the present invention and the manufacturing process and action of the molding apparatus according to the above-described method and configuration will be described in more detail with reference to the accompanying drawings.

도시와 같이 본 발명에 따른 가압성형장치는, 연속하여 배열된 이송치구(2)에 제품용기(1)를 각각 삽입한 후, 일정한 속도로 작동하는 컨베이어 이송수단(10)으로부터 상기한 이송치구(2)는 액체정량주입기(20)의 하측으로 이송된다.As shown in the figure, the press-molding apparatus according to the present invention inserts the product containers 1 into the continuous transfer jig 2 respectively, and then transfers the jig from the conveyor transfer means 10 operated at a constant speed. 2) is transferred to the lower side of the liquid injector 20.

이때, 단일의 이송치구(2) 만이 액체정량주입기(20)의 하측으로 이송되면, 그 액체정량주입기(20)의 디스펜서(21)로부터 오일리 겔상의 분말원료가 배출되어 상기 제품용기(1)의 내측으로 주입되는 것이며, 상기한 액체정량주입기(20)로부터 분말원료의 주입이 종료되면, 상기 컨베이어 이송수단(10)의 재작동에 의해 상기한 이송치구(2)는 1차 가압성형장치(30)의 하측으로 이동하게 된다.At this time, if only a single transfer jig 2 is transferred to the lower side of the liquid dosing injector 20, the oily gel-like powder raw material is discharged from the dispenser 21 of the liquid dosing injector 20, When the injection of the powder raw material from the above-mentioned liquid metering injector 20 is finished, the transfer jig 2 is reactivated by the conveyor transporting means 10 so that the transfer jig 2 is first press-molded. Will be moved to the lower side.

이와 같이 상기한 이송치구(2)가 1차 가압성형장치(30)의 하측으로 이동되면, 상기한 1차 가압성형장치(30)의 상부실린더(33)가 작동되어 그 하단의 상부펀치(36)를 하측으로 하강시켜 분말원료의 상측에 위치하게 되는데, 상기한 상부펀치(36)와 제품용기(1)의 사이에는 권취롤(31)에 의해 일정한 속도로 자동 공급되는 별도의 흡습지(32)가 위치하고 있어, 상기 흡습지(32)는 그 제품용기(1)의 상측에서 가장 근접된 위치로 접근하게 된다.As described above, when the transfer jig 2 is moved to the lower side of the primary pressing device 30, the upper cylinder 33 of the primary pressing device 30 is operated to operate the upper punch 36 at the lower end thereof. ) Is lowered to be positioned on the upper side of the powder raw material, between the upper punch 36 and the product container (1) a separate absorbent paper 32 is automatically supplied at a constant speed by the take-up roll (31) Is located, the absorbent paper 32 is close to the position closest to the upper side of the product container (1).

이러한 상부실린더(33)의 작동이 이루어지면, 이후에는 그 하부실린더(35)가 작동되어 하부실린더(35) 선단의 가압판(34)에 의해 상기 제품용기(1)를 상측으로 밀어 올리게 된다.When the operation of the upper cylinder 33 is made, the lower cylinder 35 is then operated to push up the product container 1 by the pressure plate 34 of the lower cylinder 35 front end.

따라서, 상측으로 밀려 올라가는 제품용기(1)에 의해 그 내측에 충진되어 있던 분말원료는 상부펀치(36)에 의한 가압작용에 의해 그 오일성분이 배출되는 것이며, 배출되는 오일성분은 상측표면의 흡습지(32)로 흡수되어 상당한 량의 오일성분이 제거되는 것이다.Therefore, the powder raw material filled in the inside by the product container 1 which is pushed upward is discharged by the upper punch 36, the oil component is discharged, and the discharged oil component is the absorbent paper on the upper surface. Absorbed in (32) to remove a significant amount of oil components.

또한, 상기한 오일제거작용과 동시에 제품용기(1)의 내측에 주입되어진 분말원료는 그 상부펀치(36)의 저면 형상대로 고형화가 되는 것인데, 상기한 상부펀치(36)는 도 4의 도시와 같이 그 저면 가장자리가 융출된 경계가압부(50)가 형성되어 있으므로, 상기한 경계가압부(50)에 의해 그 제품용기(1)의 내측 가장자리를 더욱 가압하게 되면 오일성분이 내측으로 모아지는 효과를 기대할 수 있어, 도 5의 도시와 같이 하부실린더(35)의 상승 가압시 그 오일성분이 상부펀치(36)와 제품용기(1)의 경계부로 새어나오지 않고 온전하게 그 흡습지(32)의 전체면으로 흡수되는 것이다.In addition, the powder raw material injected into the inside of the product container 1 at the same time as the oil removal action is to be solidified in the shape of the bottom of the upper punch 36, the upper punch 36 is shown in FIG. Since the boundary pressing portion 50 is formed in which the bottom edge is melted as described above, when the inner edge of the product container 1 is further pressed by the boundary pressing portion 50, the oil component is collected inwardly. As shown in FIG. 5, when the lower cylinder 35 is pressurized and pressurized, the oil component of the lower cylinder 35 does not leak to the boundary between the upper punch 36 and the product container 1. It is absorbed into cotton.

특히, 상기한 바와 같이 하부실린더(35)의 작동에 의해 그 분말원료를 성형 및 오일제거하는 공정은, 종래의 상부프레스 방식에 비해 제품의 표면 오염도를 크게 저하시킬 수 있어 보다 고품질의 제품을 양산할 수 있는 것이며, 상부실린더(33)의 행정거리가 짧아지므로 흡습지(32)의 파손이나 구겨짐 등이 발생하지 않아 불량율이 크게 감소하는 효과가 있다.In particular, as described above, the process of forming the powder raw material and removing the oil by the operation of the lower cylinder 35 can significantly reduce the surface contamination of the product compared to the conventional upper press method, thereby producing a higher quality product. Since the stroke length of the upper cylinder 33 is shortened, the breakage or wrinkle of the absorbent paper 32 does not occur, and the defective rate is greatly reduced.

이와 같이 1차 가압성형공정이 종료되면, 다시 컨베이어 이송수단(10)의 작동에 의해 상기한 이송치구(2)는 2차 가압성형장치(40)의 하측으로 이동하게 되는데, 상기한 2차 가압성형장치(40)는 주지된 1차 가압성형장치(30)와 마찬가지로 상부실린더(43)와 하부실린더(45)의 순차적인 작동에 의해 다시 한번 가압성형 및 오일제거를 하게 되는 것이다.As such, when the primary press molding process is completed, the transfer jig 2 is moved to the lower side of the secondary press forming apparatus 40 by the operation of the conveyor conveying means 10 again. The molding apparatus 40 is once again press-molded and oil removed by the sequential operation of the upper cylinder 43 and the lower cylinder 45 like the well-known primary press molding apparatus 30.

이와 같은 2차 가압성형공정은, 역시 권취롤(41)로부터 일정한 속도로 공급되는 흡습지(42)와, 도 7의 도시와 같이 이송치구(2)를 상측으로 밀어 올리는 가압판(44) 및 제품용기(1)의 내측형상과 동일한 형태를 갖는 상부펀치(46)로 이루어져 있는 것이다.This secondary press molding process, the absorbent paper 42 is also supplied from the take-up roll 41 at a constant speed, the pressing plate 44 and the product container for pushing up the transfer jig 2 as shown in FIG. It consists of an upper punch 46 having the same shape as the inner shape of (1).

이때, 상기한 상부펀치(46)는 1차 가압성형장치(30)의 상부펀치(36)와는 달리 도 6의 도시와 같이 그 저면이 평평한 형태로 제작되어 1차 가압성형공정에서 그 중앙부가 융출되게 성형된 분말원료의 중앙부를 눌러주어 평평한 제품면을 얻게 하면서도 중앙으로 집중된 오일성분을 재차 제거함과 동시에 제품 전체로 고른 건/습 상태를 유지하도록 펼쳐 가압하는 형태의 작용을 하게 된다.In this case, unlike the upper punch 36 of the primary press forming apparatus 30, the upper punch 46 is manufactured in a flat shape as shown in FIG. 6, and the central part is melted in the primary press molding process. Pressing the center part of the powder raw material so as to obtain a flat product surface while removing the oil component concentrated in the center and at the same time acts in the form of spreading to maintain a uniform dry / wet state throughout the product.

이와 같은 2단계의 가압성형공정에 의해 화장품은 고른 경도 및 건/습 상태를 유지하여 완성되는 것이며, 이렇게 2차 가압성형공정이 완료된 제품용기(1)는 다시 이동하여 별도의 취출수단(도면에는 미도시함.)에 의해 그 이송치구(2)로부터 분리되어 배출되는 것이다.The cosmetics are finished by maintaining a uniform hardness and dry / wet state by the two-step press molding process, and the product container 1 in which the second press molding process is completed is moved again to separate take-out means ( It is to be separated and discharged from the transfer jig (2) by the not shown.

본 발명에서는, 상기한 바와 같은 2단계의 가압성형공정으로부터, 보다 안정되고 균일한 고품질의 제품을 생산할 수 있게 한 것인데, 오일리 분말원료로부터 오일성분을 제거하는 과정에서 과도한 오일이 배출되는 경우에는 밀착된 흡습지(32)(42)가 충분히 제거하지 못할 수도 있으므로, 이를 대비하여 각각의 상부펀치(36)(46)에 별도의 오일배출수단을 형성하여 다량의 배출오일을 보다 용이하게 제거할 수 있도록 한 것이다.In the present invention, it is possible to produce a more stable and uniform high-quality product from the two-step press molding process as described above, if the excess oil is discharged in the process of removing the oil component from the oily powder raw material, the adhesion Since the absorbent papers 32 and 42 may not be sufficiently removed, a separate oil discharge means may be formed in each of the upper punches 36 and 46 so that a large amount of discharge oil may be more easily removed. It is.

즉, 상기한 각각의 상부펀치(36)(46)에는, 그 내부에 별도의 공간부(38)(48)가 형성되어 있고, 그 공간부(38)(48)는 일측으로 관통된 배출공(37)(47)이 형성되어 있으며, 상기한 공간부(38)(48)는 치구의 저면으로부터 수직 형성된 다수개의 통공(39)(49)에 의해 하부면과 관통되어 있는 것이다.That is, in each of the upper punches 36 and 46, separate spaces 38 and 48 are formed therein, and the spaces 38 and 48 are discharge holes penetrated to one side. 37 and 47 are formed, and the spaces 38 and 48 are penetrated with the lower surface by a plurality of through holes 39 and 49 vertically formed from the bottom of the jig.

따라서 도 8의 도시와 같이 하부실린더(35)(45)의 작동에 의해 제품용기(1)가 상승하면, 상부펀치(36)(46)와의 가압작용에 의해 분말원료로부터 오일이 배출되는 것이며, 흡습지(32)(42)로부터 충분한 오일흡수가 이루어지지 아니하고 과도하게 배출되는 오일은 상기 통공(39)(49)을 통해 치구 내측의 공간부(38)(48)로 모아지는 것이며, 일정하게 모아진 오일성분은 일측의 배출공(37)(47)을 통해 치구의 일측으로 흘러내리게 되므로,Therefore, when the product container 1 is raised by the operation of the lower cylinder 35, 45 as shown in Figure 8, the oil is discharged from the powder raw material by the pressure action with the upper punch (36) 46, The oil which is not sufficiently absorbed from the absorbent papers 32 and 42 and is excessively discharged is collected through the through holes 39 and 49 into the spaces 38 and 48 inside the jig, and is constantly collected. Since the oil component flows down to one side of the jig through the discharge holes 37 and 47 on one side,

이렇게 흘러내리는 오일을 상기한 흡습지(32)(42)가 빠르게 흡수하여 제거하는 형태를 갖게 되어, 결국 과도한 량의 오일이 일시에 배출되더라도 이를 효과적으로 제거할 수 있게 된다.The absorbing papers 32 and 42 absorb the oil flowing down in such a manner as to be quickly absorbed and removed, so that even if an excessive amount of oil is discharged at a time, the oil can be effectively removed.

따라서, 보다 뛰어난 고품질의 메이크업 화장품을 생산할 수 있게 되는 것이며, 상기한 메이크업용 화장품은 콤팩트(Compact), 투웨이 케익(Two way cake), 파우더 파운데이션(Powder foundation), 볼연지(Blusher), 아이새도우(Eye shadow) 등 각종 분말 메이크업 화장품에 모두 사용할 수 있는 것이다.Therefore, it is possible to produce a higher quality makeup cosmetics, the makeup cosmetics described above are compact (Compact), two way cake (Powder foundation), powder foundation (Blusher), eye shadow ( It can be used for all kinds of powder makeup cosmetics such as eye shadow.

이상과 같이 본 발명에 따른 가압성형과정 중에서 하부프레스에 의해 용기내의 내용물을 가압성형하는 방법은, 종래의 상부 가압성형방법에 비해 매우 뛰어난 효과 및 특징을 갖는 것인데 이를 보다 구체적으로 설명하면,As described above, the method of press-molding the contents of the container by the lower press during the press-molding process according to the present invention has a very excellent effect and characteristics compared to the conventional upper press-forming method.

도 9의 도시와 같이, 종래의 분말원료 성형방법은 내용물이 주입된 제품용기(101)를 갖는 이송치구(100)의 상측에만 단일적으로 설치되어 있는 상부실린더(102) 및 그 하단의 상부펀치(103)로만 제품을 성형하는 것으로, 이송치구(100)가 상부프레스의 하측으로 이송되어진 상태에서 상기한 상부실린더(102)가 하강하여 그 제품용기(101)로 주입되어진 분말원료를 가압 성형하는 형태를 갖게 된다.As shown in Figure 9, the conventional powder raw material forming method is the upper cylinder 102 and the upper punch at the bottom of which is installed only on the upper side of the transfer jig 100 having the product container 101 is injected into the contents By molding the product only by 103, the upper cylinder 102 is lowered in the state that the transfer jig 100 is transferred to the lower side of the upper press to press-mold the powder raw material injected into the product container 101. Form.

이후, 가압성형된 제품용기는 다소 긴 배출행정거리(L1)를 갖고 그 이송치구(100)로부터 배출되는 것이다.Thereafter, the press-molded product container has a rather long discharge stroke L1 and is discharged from the transfer tool 100.

그러나 상기한 바와 같은 상부 프레스에 의한 가압성형방식은, 상부펀치(103)의 가압행정거리가 길어짐에 따라 그 상부펀치(103)와 이송치구(2)의 사이에 각종 이물질이 끼어 제품을 오염시키게 되는 것이며, 용기의 배출행정거리(L1)가 매우 길어 신속한 자동 배출이 어려운 문제점이 있는 것이다.However, in the press molding method using the upper press as described above, as the pressure stroke of the upper punch 103 becomes longer, various foreign substances are caught between the upper punch 103 and the transfer tool 2 to contaminate the product. The discharge stroke (L1) of the container is very long, so that the automatic automatic discharge is difficult.

특히, 분말원료의 오일성분을 흡수 제거하는 흡습지는 제품용기(101)의 하부까지 내려가 오일성분을 흡수하게 되므로 상부펀치(103)와 이송치구(100)의 사이에 그 흡습지의 끼임이 발생하여 그 흡습지가 파손되는 문제점이 빈번하게 발생하고 있는 것이다.In particular, the absorbent paper absorbing and removing the oil component of the powder raw material is lowered to the lower portion of the product container 101 to absorb the oil component, so that the pinch of the absorbent paper occurs between the upper punch 103 and the transfer tool 100. The problem that the absorbent paper is broken frequently occurs.

또한, 상부 프레스 즉, 상부펀치(103)가 하강하여 가압 성형하는 방식의 경 우 상부펀치(103)의 하부면에 위치한 흡습지가 압착되므로 오일의 원활한 흡수 및 배출을 차단하는 문제점이 있는 것이다.In addition, when the upper press, that is, the upper punch 103 is lowered and press-molded, the absorbent paper located on the lower surface of the upper punch 103 is compressed, thereby preventing smooth absorption and discharge of oil.

반면에, 본 발명에 의해 개선되어진 하부 프레스에 의한 가압성형방식은,On the other hand, the press molding method by the lower press improved by the present invention,

상부실린더(33)(43)와 하부실린더(35)(45)가 상,하로 장착되어진 위치로 이송되어진 이송치구(2)를, 하부실린더(35)(45)가 상승하여 그 이송치구(2) 내측의 제품용기(1)를 상승시켜 이를 가압 성형하는 작동을 하게 됨으로서,The upper jig (33) 43 and the lower cylinder (35) 45 are transferred to a position where the upper and lower mounting jig (2), the lower cylinder 35, 45 is raised to the transfer jig (2) By raising the inner product container (1) to press-molding it,

상부펀치(36)의 직접적인 하강 가압이 아니라 하부실린더(35)(45)의 상승에 의한 간접 가압방식을 택함으로서, 가압성형 완료시 상승되어 있는 제품용기(1)의 배출행정거리(L2)가 크게 단축(L1>L2)되므로 이송치구(2)의 내부 오염 정도가 적어져 보다 고품질의 제품을 양산하게 되며, 자동 배출시 매우 신속하고 용이한 배출작업이 이루어지게 된다.By taking an indirect pressurization method by raising the lower cylinders 35 and 45 instead of directly lowering the upper punch 36, the discharge stroke distance L2 of the product container 1 which is raised at the completion of press molding is Since it is greatly shortened (L1> L2), the internal pollution degree of the transfer tool 2 is reduced, thereby producing a higher quality product, and a very quick and easy discharge operation is made during automatic discharge.

또한, 상부실린더(33)(43)가 하강하는 것이 아니라 그 제품용기(1)가 상승하여 가압 성형되는 것이므로, 상부실린더(33)(43)와 이송치구(2) 사이의 오염도가 크게 감소되므로 제품이 오염되는 것을 방지할 수 있으며,In addition, since the upper cylinder (33) 43 is not lowered, but the product container (1) is raised and pressure-molded, since the degree of contamination between the upper cylinder (33) 43 and the transfer tool (2) is greatly reduced Prevent contamination of the product,

오일리한 분말원료의 오일성분을 흡수 제거하는 흡습지(32)가 직접 하강되거나 이송치구(2)의 내측으로 삽입되지 않으므로 흡습지(32)가 파손되는 것을 방지할 수 있는 것이다.Since the absorbent paper 32 which absorbs and removes the oil component of the oily powder raw material is not directly lowered or inserted into the transfer jig 2, the absorbent paper 32 can be prevented from being damaged.

특히, 하부실린더(35)(45)의 상승에 의해 그 제품용기(1)가 상승하여 가압되는 구조를 채택함에 따라, 상기한 흡습지(32)가 강제 압착되는 것을 방지할 수 있으므로, 오일성분이 상부펀치(36)(46)의 배출공(37)(47)을 통해 보다 원활하게 배 출될 수 있는 통로를 제공하여 매우 뛰어난 오일흡수 작용을 하는 특징을 갖게 되는 것이다.In particular, by adopting a structure in which the product container 1 rises and is pressurized by the rise of the lower cylinders 35 and 45, the above-described absorbent paper 32 can be prevented from being forcedly compressed, so that the oil component By providing a passage that can be discharged more smoothly through the discharge hole (37) 47 of the upper punch (36) (46) will have the feature of having a very excellent oil absorption.

이와 같이 이송치구(2)의 하측에 하부실린더(35)(45)를 장착한 것은, 단순한 가압위치의 변경이 아니라, 보다 뛰어난 제품의 안정성 및 품질을 유지하기 위한 것이다.The lower cylinders 35 and 45 are attached to the lower side of the transfer jig 2 in this way, not to change the pressurization position, but to maintain more excellent product stability and quality.

한편, 이상과 같이 1차 가압성형장치와 2차 가압성형장치로 구성된 성형장치를 이용한 메이크업 화장품의 제조방법은 기존의 성형장치를 이용한 메이크업 화장품의의 단점을 개선하고 고품질의 메이크업 화장품을 제조하는 데 특징이 있다.On the other hand, as described above, the manufacturing method of the makeup cosmetics using the molding apparatus composed of the first press molding apparatus and the second press molding apparatus improves the disadvantages of the makeup cosmetics using the existing molding apparatus and manufactures high quality makeup cosmetics. There is a characteristic.

이상과 같은 본 발명 오일리 메이크업 분말의 가압성형방법 및 그 성형장치는, 균일한 압력에 의해 효과적으로 오일을 제거하므로 제품 전체에 고른 경도 및 건/습 상태가 유지되게 하면서도, 용기외부로 오일이 새어나오는 것을 방지하며, 상부펀치의 하부면이 오염되는 것을 방지하면서도 흡습지의 파손 또는 구겨짐을 방지할 수 있어, 고품질의 화장품을 얻게 하면서도 보다 안정된 품질을 지속적으로 유지할 수 있는 효과를 갖는 것이다.The pressure forming method of the oily makeup powder and the molding apparatus of the present invention as described above effectively remove oil by a uniform pressure, so that the oil is leaking out of the container while maintaining a uniform hardness and dry / wet state throughout the product. It can prevent and prevent the contamination of the lower surface of the upper punch, while preventing the breakage or wrinkle of the absorbent paper, to obtain a high-quality cosmetics while having the effect of maintaining a more stable quality.

Claims (7)

제품용기가 삽입된 이송치구가 순차적으로 이송되고, 이송된 이송치구의 제품용기 내부에 액체정량주입기에 의해 분말원료를 정량 투입한 후,After the transfer jig into which the product container is inserted is sequentially transferred, the powder raw material is quantitatively injected into the product container of the transferred jig by a liquid metering injector. 상기 제품용기를 갖는 이송치구가 1차 가압성형수단에 위치되도록 하여, 상측의 흡습지 및 상부펀치와 하측의 가압프레스에 의해 1차 가압성형 및 오일제거공정을 수행케 하고,The transfer jig having the product container is positioned in the primary press forming means, and the primary press forming and oil removing process is performed by the upper absorbent paper, the upper punch and the lower press press. 1차 가압성형된 이송치구를 2차 가압성형수단으로 이동시켜, 상측의 흡습지 및 상부펀치와 하측의 가압프레스에 의해 2차 가압성형 및 오일제거공정을 반복 수행케 하여,The primary press-molded transfer jig is moved to the secondary press forming means, and the secondary press forming and oil removing process are repeatedly performed by the upper absorbent paper, the upper punch and the lower press press. 2단계의 가압성형공정에 의해 고른 경도 및 건/습 상태를 유지할 수 있게 하고, 하부 가압프레스에 의해 균일하고 안정된 오일 배출작용이 이루어지도록 함을 특징으로 하는 오일리 메이크업 분말의 가압성형방법.The pressing process of the oily makeup powder, characterized in that to maintain a uniform hardness and dry / wet state by the two-step pressing process, and to achieve a uniform and stable oil discharge action by the lower pressure press. 제 1항에 있어서,The method of claim 1, 1차 가압성형수단 및 2차 가압성형수단은, 상부실린더가 우선 하강하여 상부펀치와 흡습지를 제품용기 상측에 근접 위치되게 한 후, 하부실린더가 상승 작동하여 그 제품용기를 밀어 올려 분말원료가 가압 성형되게 함을 특징으로 하는 오일리 메이크업 분말의 가압성형방법.In the first press molding means and the second press molding means, the upper cylinder is first lowered, so that the upper punch and the absorbent paper are located close to the upper side of the product container, and then the lower cylinder is pushed up to push up the product container to pressurize the powder raw material. Pressure molding method of the oily makeup powder characterized in that it is molded. 본체(100)의 상측에 마련된 컨베이어 이송수단(10)에 의해, 내부에 제품용기(1)를 갖는 이송치구(2)가 순차적으로 이송되게 하고,By the conveyor conveying means 10 provided on the upper side of the main body 100, the conveying jig 2 having the product container 1 therein is sequentially conveyed, 상기 이송치구(2)는, 액체정량주입기(20)와; 상,하실린더(33)(35)에 의한 1차 가압성형장치(30)와; 또 다른 상,하실린더(43)(45)에 의한 2차 가압성형장치(40)를 따라 순차적으로 이송되게 하되,The transfer jig (2), and a liquid metering injector (20); The primary press molding apparatus 30 by the upper and lower cylinders 33 and 35; Another phase, to be sequentially transported along the secondary pressure forming apparatus 40 by the cylinder 43, 45, 액체정량주입기(20)는, 적어도 하나 이상의 자동 디스펜서(21)에 의해 정량의 분말원료가 상기 제품용기(1)의 내부로 주입되게 구성함을 특징으로 하는 오일리 메이크업 분말의 가압성형장치.Liquid injection machine (20) is a pressurized molding apparatus for oily makeup powder, characterized in that configured to be injected into the interior of the product container (1) of the quantitative powder raw material by at least one automatic dispenser (21). 제 3항에 있어서,The method of claim 3, wherein 1차 가압성형장치(30)는, 귄취롤(31)에 의해 일정속도로 공급되는 흡습지(32)가 제품용기(1)의 상측에 위치되고, 그 흡습지(32)의 상측에는 상기 제품용기(1)의 내부형상과 동일한 상부펀치(36)를 갖는 상부실린더(33)가 위치하며, 상기 이송치구(2)의 하측에는 가압판(34)을 갖는 하부실린더(35)가 위치되어 구성되며,In the primary press-molding apparatus 30, the absorbent paper 32, which is supplied at a constant speed by the gusset roll 31, is positioned above the product container 1, and above the absorbent paper 32, the product container ( The upper cylinder 33 having the same upper punch 36 as the internal shape of 1) is located, the lower cylinder 35 having a pressure plate 34 is positioned below the transfer jig 2, 2차 가압성형장치(40)는, 권취롤(41)에 의해 일정속도로 공급되는 흡습지(42)가 제품용기(1)의 상측에 위치되고, 그 흡습지(42)의 상측에는 상기 제품용기(1)의 내부형상과 동일한 상부펀치(46)를 갖는 상부실린더(43)가 위치하며, 상기 이송치구(2)의 하측에는 가압판(44)을 갖는 하부실린더(45)가 위치되게 구성함을 특징으로 하는 오일리 메이크업 분말의 가압성형장치.In the secondary press-molding apparatus 40, the absorbent paper 42, which is supplied at a constant speed by the winding roll 41, is positioned above the product container 1, and above the absorbent paper 42, the product container ( The upper cylinder 43 having the same upper punch 46 as the inner shape of 1) is located, the lower cylinder 45 having a pressure plate 44 is located below the transfer jig 2 Pressing device for oily makeup powder. 제 4항에 있어서,The method of claim 4, wherein 1차 가압성형장치(30)의 상부펀치(36)는, 그 하부 가장자리가 내측 경사면을 갖도록 융출된 경계가압부(50)를 형성하여 됨을 특징으로 하는 오일리 메이크업 분말의 가압성형장치.The upper punch (36) of the primary pressure forming apparatus (30), the pressure forming apparatus of the oily makeup powder, characterized in that the lower edge is formed by the boundary pressing portion 50 is melted to have an inner inclined surface. 제 4항에 있어서,The method of claim 4, wherein 1차 가압성형장치(30)와 2차 가압성형장치(40)의 상부펀치(36)(46)는, 그 일측면에 배출공(37)(47)을 형성하여, 상부펀치(36)(46) 내측의 공간부(38)(48)와 서로 연통되게 하고, 상기 공간부(38)(48)는 하측 방향으로 복수개 형성된 통공(39)(49)을 통해 하부면과 관통되게 형성함을 특징으로 하는 오일리 메이크업 분말의 가압성형장치.The upper punches 36 and 46 of the primary press forming device 30 and the secondary press forming device 40 form discharge holes 37 and 47 on one side thereof, and the upper punch 36 ( 46) the inner spaces 38 and 48 communicate with each other, and the spaces 38 and 48 are formed to penetrate the lower surface through the plurality of through holes 39 and 49 formed in the downward direction. Pressing device for oily makeup powder characterized in that. 삭제delete
KR1020050040094A 2005-05-13 2005-05-13 Method and apparatus for forming oily make-up powder by pressing KR100662545B1 (en)