JPS6456855A - Austenitic stainless steel for boiler for soda recovery - Google Patents

Austenitic stainless steel for boiler for soda recovery

Info

Publication number
JPS6456855A
JPS6456855A JP21391487A JP21391487A JPS6456855A JP S6456855 A JPS6456855 A JP S6456855A JP 21391487 A JP21391487 A JP 21391487A JP 21391487 A JP21391487 A JP 21391487A JP S6456855 A JPS6456855 A JP S6456855A
Authority
JP
Japan
Prior art keywords
boiler
stainless steel
austenitic stainless
stock
soda recovery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP21391487A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0431020B2 (enrdf_load_stackoverflow
Inventor
Satoshi Araki
Tsunetoshi Takahashi
Yukio Onoyama
Masatomo Shinohara
Yorimasa Takeda
Takashi Oguro
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Heavy Industries Ltd
Nippon Steel Corp
Original Assignee
Mitsubishi Heavy Industries Ltd
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Heavy Industries Ltd, Nippon Steel Corp filed Critical Mitsubishi Heavy Industries Ltd
Priority to JP21391487A priority Critical patent/JPS6456855A/ja
Publication of JPS6456855A publication Critical patent/JPS6456855A/ja
Publication of JPH0431020B2 publication Critical patent/JPH0431020B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Cleaning And De-Greasing Of Metallic Materials By Chemical Methods (AREA)
  • Heat Treatment Of Steel (AREA)
JP21391487A 1987-08-27 1987-08-27 Austenitic stainless steel for boiler for soda recovery Granted JPS6456855A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP21391487A JPS6456855A (en) 1987-08-27 1987-08-27 Austenitic stainless steel for boiler for soda recovery

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP21391487A JPS6456855A (en) 1987-08-27 1987-08-27 Austenitic stainless steel for boiler for soda recovery

Publications (2)

Publication Number Publication Date
JPS6456855A true JPS6456855A (en) 1989-03-03
JPH0431020B2 JPH0431020B2 (enrdf_load_stackoverflow) 1992-05-25

Family

ID=16647124

Family Applications (1)

Application Number Title Priority Date Filing Date
JP21391487A Granted JPS6456855A (en) 1987-08-27 1987-08-27 Austenitic stainless steel for boiler for soda recovery

Country Status (1)

Country Link
JP (1) JPS6456855A (enrdf_load_stackoverflow)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH03153847A (ja) * 1989-11-13 1991-07-01 Nippon Steel Corp クリープ破断特性のすぐれたNi―Crオーステナイト系ステンレス鋼
EP0937783A1 (en) * 1998-02-18 1999-08-25 Sandvik Aktiebolag New use of a high strength stainless steel

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS62199753A (ja) * 1986-02-25 1987-09-03 Nippon Steel Corp 高温環境下での時効後靭性および耐高温粒界腐食性に優れたオ−ステナイトステンレス鋼

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS62199753A (ja) * 1986-02-25 1987-09-03 Nippon Steel Corp 高温環境下での時効後靭性および耐高温粒界腐食性に優れたオ−ステナイトステンレス鋼

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH03153847A (ja) * 1989-11-13 1991-07-01 Nippon Steel Corp クリープ破断特性のすぐれたNi―Crオーステナイト系ステンレス鋼
EP0937783A1 (en) * 1998-02-18 1999-08-25 Sandvik Aktiebolag New use of a high strength stainless steel
US6174386B1 (en) 1998-02-18 2001-01-16 Sandvik Ab NaOH evaporator comprising at least one component formed by a high strength stainless steel

Also Published As

Publication number Publication date
JPH0431020B2 (enrdf_load_stackoverflow) 1992-05-25

Similar Documents

Publication Publication Date Title
Herbsleb et al. Precipitation of intermetallic compounds, nitrides and carbides in AF 22 duplex steel and their influence on corrosion behavior in acids
KR950000912A (ko) 기계 가공성이 개선된 마르텐시틱 스테인레스강
SE7713611L (sv) Hogtemperaturbearbetbart, austenitiskt rostfritt stal
TW208044B (enrdf_load_stackoverflow)
SE8106975L (sv) Stal
JPS5591960A (en) High silicon-nickel-chromium steel with resistance to concentrated
US4390367A (en) High-alloyed steel being resistive to corrosion by natural gas
JPS5681658A (en) Austenitic alloy pipe with superior hot steam oxidation resistance
JPS572869A (en) Austenite stainless steel for hot corrosive environment
JPS6456855A (en) Austenitic stainless steel for boiler for soda recovery
US4102677A (en) Austenitic stainless steel
JPS5672156A (en) Low-alloy heat-resistant steel for high temperature use
EP0780483B1 (en) High-strength austenitic heat-resisting steel having improved weldability
JPS6468450A (en) Austenitic stainless steel for seawater corrosion resistance
Keown et al. Niobium in stainless steels
GB2123031A (en) High-nickel austenitic alloys for sour well service
GB905238A (en) Improvements in or relating to austenitic stainless steels
JPH0835009A (ja) 耐食性の優れたマルテンサイトステンレス鋼の製造方法
SE8701871L (sv) Utskiljningsherdade nickelbaserade legeringar med god motstandskraft mot spenningskorrosion
JPS5662949A (en) Steel products for steam turbine moving blade or the like
JPS565949A (en) High tensile steel with superior sulfide corrosion crack resistance and superior corrosion resistance
JPH0430463B2 (enrdf_load_stackoverflow)
JPS57143467A (en) Low c-low si-cr-mo steel used in wet vapor
Vineberg et al. 12 Cr--Mo Steels With Improved Rupture Strength and Weldability
Johansson et al. Formability of stainless steels

Legal Events

Date Code Title Description
R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

R250 Receipt of annual fees

Free format text: JAPANESE INTERMEDIATE CODE: R250

EXPY Cancellation because of completion of term
FPAY Renewal fee payment (prs date is renewal date of database)

Year of fee payment: 16

Free format text: PAYMENT UNTIL: 20080525