Prior art keywords
leakage current
capacitor
electrolyte
histidine
reduce
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP19469587A
Other languages
Japanese (ja)
Inventor
Hideki Shimamoto
Hisao Nagara
Keiji Mori
Shingo Yoshida
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panasonic Holdings Corp
Original Assignee
Matsushita Electric Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Matsushita Electric Industrial Co Ltd filed Critical Matsushita Electric Industrial Co Ltd
Priority to JP19469587A priority Critical patent/JPS6437826A/en
Publication of JPS6437826A publication Critical patent/JPS6437826A/en
Pending legal-status Critical Current

Links

Landscapes

  • Electric Double-Layer Capacitors Or The Like (AREA)

Abstract

PURPOSE:To reduce the initial leakage current or the leakage current after the title capacitor is left to stand with no-load and to reduce the capacity change at high temperature, by adding L-histidine at 0.005-0.5wt.% to the weight of an electrolytic solution which consists of a solvent and a solute. CONSTITUTION:L-histidine is added 0.005-0.4wt.% to the weight of electrolytic solution which consists of solvent and solute. If the addition is not more than 0.005wt.%, little effect is expected, and if more than 0.5wt.%, it is insoluble. Addition of L-histidine can improve the formation and reduce the leakage current. According to this constitution, a capacitor of little capacity change at high temperature can be obtained by reducing the initial leakage current and the leakage current after the capacitor is left to stand with no-load.
JP19469587A 1987-08-04 1987-08-04 Electrolyte for driving electrolytic capacitor Pending JPS6437826A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP19469587A JPS6437826A (en) 1987-08-04 1987-08-04 Electrolyte for driving electrolytic capacitor

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP19469587A JPS6437826A (en) 1987-08-04 1987-08-04 Electrolyte for driving electrolytic capacitor

Publications (1)

Publication Number Publication Date
JPS6437826A true JPS6437826A (en) 1989-02-08

Family

ID=16328738

Family Applications (1)

Application Number Title Priority Date Filing Date
JP19469587A Pending JPS6437826A (en) 1987-08-04 1987-08-04 Electrolyte for driving electrolytic capacitor

Country Status (1)

Country Link
JP (1) JPS6437826A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2019065524A1 (en) 2017-09-28 2019-04-04 日新製鋼株式会社 Metal wall material and wall construction method using same
US11261603B2 (en) 2017-05-23 2022-03-01 Nippon Steel Nisshin Co., Ltd. Metallic roof material and roofing method using same

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US11261603B2 (en) 2017-05-23 2022-03-01 Nippon Steel Nisshin Co., Ltd. Metallic roof material and roofing method using same
WO2019065524A1 (en) 2017-09-28 2019-04-04 日新製鋼株式会社 Metal wall material and wall construction method using same

Similar Documents

Publication Publication Date Title
DE3565913D1 (en) Process for stabilising primary electrochemical generators wih active anodes of zinc, aluminium or magnesium, and anode for a generator stabilised by this process
JPS6437826A (en) Electrolyte for driving electrolytic capacitor
JPS536213A (en) Carbon electrode coated with antioxidant for al electrolysis
JPS6437823A (en) Electrolyte for driving electrolytic capacitor
SU1045049A2 (en) Method of part running-in
JPS5653564A (en) Brushless self-excited synchronous generator
SU670981A1 (en) Method of manufacturing electrolytic capacitors with liquid electrolyte
JPS51139685A (en) Process for preparing glutathione
JPS6424411A (en) Electrolytic capacitor
JPS5749165A (en) Organic electrolytic cell
Barz et al. Hydrogen Evolution During Open-Circuit Corrosion and Anodic Polarization of Al, Mg and Li
JPS53124174A (en) Frame for electrolytic cell filter press type
JPS55142050A (en) Lacquer composition for highly dielectric film
JPS6475518A (en) Stabilization of electrolyte for electrolytic polymerization
JPS6486514A (en) Solid electrolytic capacitor
JPS6481307A (en) Electrolyte for aluminum electrolytic capacitor
JPS5332889A (en) Production of luminous electrolyte
JPS5334772A (en) Preparation of 2-benzothiazolines
JPS647512A (en) Electrolyte for electrolytic capacitor
JPS6430177A (en) Electrolyte for lithium secondary battery
JPS5339429A (en) Inverter
JPS55119363A (en) Nonaqueous electrolyte battery
JPS5235818A (en) Staring circuit for three-phase ac motor
JPS541824A (en) Inverter control circuit
JPS51136516A (en) Method for stopping the electric power supply for aluminium electrolytic cells