JPS63162812A - 肌焼鋼の製造方法 - Google Patents
肌焼鋼の製造方法Info
- Publication number
- JPS63162812A JPS63162812A JP30830686A JP30830686A JPS63162812A JP S63162812 A JPS63162812 A JP S63162812A JP 30830686 A JP30830686 A JP 30830686A JP 30830686 A JP30830686 A JP 30830686A JP S63162812 A JPS63162812 A JP S63162812A
- Authority
- JP
- Japan
- Prior art keywords
- steel
- case
- heat treatment
- coarsening
- hardening steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP30830686A JPS63162812A (ja) | 1986-12-26 | 1986-12-26 | 肌焼鋼の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP30830686A JPS63162812A (ja) | 1986-12-26 | 1986-12-26 | 肌焼鋼の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63162812A true JPS63162812A (ja) | 1988-07-06 |
| JPH0568528B2 JPH0568528B2 (enExample) | 1993-09-29 |
Family
ID=17979462
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP30830686A Granted JPS63162812A (ja) | 1986-12-26 | 1986-12-26 | 肌焼鋼の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63162812A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02147148A (ja) * | 1988-11-28 | 1990-06-06 | Daido Steel Co Ltd | 肌焼鋼製品の製造方法 |
| JPH03122218A (ja) * | 1989-10-06 | 1991-05-24 | Nippon Steel Corp | 肌焼鋼の製造方法 |
| JPH04350113A (ja) * | 1991-05-28 | 1992-12-04 | Nippon Steel Corp | 浸炭熱処理時に結晶粒が粗大化しない肌焼鋼の製造方法 |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0638987U (ja) * | 1992-11-05 | 1994-05-24 | デンケンエンジニアリング株式会社 | 介護老人用肛門洗浄装置 |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6033311A (ja) * | 1983-07-29 | 1985-02-20 | Kawasaki Steel Corp | 大入熱溶接特性に優れた鋼材の製造方法 |
-
1986
- 1986-12-26 JP JP30830686A patent/JPS63162812A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6033311A (ja) * | 1983-07-29 | 1985-02-20 | Kawasaki Steel Corp | 大入熱溶接特性に優れた鋼材の製造方法 |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02147148A (ja) * | 1988-11-28 | 1990-06-06 | Daido Steel Co Ltd | 肌焼鋼製品の製造方法 |
| JPH03122218A (ja) * | 1989-10-06 | 1991-05-24 | Nippon Steel Corp | 肌焼鋼の製造方法 |
| JPH04350113A (ja) * | 1991-05-28 | 1992-12-04 | Nippon Steel Corp | 浸炭熱処理時に結晶粒が粗大化しない肌焼鋼の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0568528B2 (enExample) | 1993-09-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US9062359B2 (en) | High carbon chromium bearing steel, and preparation method thereof | |
| KR102131530B1 (ko) | 구상화 열처리성이 우수한 선재 및 그 제조방법 | |
| KR102131523B1 (ko) | 구상화 열처리성이 우수한 선재 및 그 제조방법 | |
| CN113366136B (zh) | 高碳热轧钢板和其制造方法 | |
| CN112996940B (zh) | 使得能够省略软化热处理的钢线材及其制造方法 | |
| KR102131529B1 (ko) | 구상화 열처리성이 우수한 선재 및 그 제조방법 | |
| JPH0568528B2 (enExample) | ||
| JPH01176031A (ja) | 熱間鍛造用非調質鋼の製造方法 | |
| JPH0112815B2 (enExample) | ||
| JPH04350113A (ja) | 浸炭熱処理時に結晶粒が粗大化しない肌焼鋼の製造方法 | |
| JPH04371522A (ja) | 浸炭用鋼材の製造方法 | |
| JPS5816024A (ja) | 高温浸炭用はだ焼鋼の製造方法 | |
| JPH10176242A (ja) | 耐焼割れ性に優れた軸受鋼 | |
| JP7530427B2 (ja) | 球状化熱処理性に優れた線材及びその製造方法 | |
| JPS62253725A (ja) | 高靭性熱間鍛造用非調質棒鋼の製造方法 | |
| JP4564189B2 (ja) | 熱間鍛造用高靭性非調質鋼 | |
| JP3903996B2 (ja) | 被削性、冷間鍛造性および焼き入れ・焼き戻し後の疲労強度特性に優れた冷間鍛造用棒鋼および機械構造用部材 | |
| JP2001011571A (ja) | 被削性、冷間鍛造性および焼入れ性に優れた機械構造用鋼材 | |
| JPH08295981A (ja) | 耐粗粒化肌焼鋼および強度と靱性に優れた表面硬化部品並びにその製造方法 | |
| JPH03260010A (ja) | 熱間鍛造非調質部品の製造方法 | |
| KR100554748B1 (ko) | 신선용 고강도 선재의 제조방법 | |
| KR100611201B1 (ko) | 내거침성이 우수한 열간압연용 원심주조 고속도공구강복합롤 | |
| JPH0967625A (ja) | 耐遅れ破壊性に優れた浸炭高強度ネジの製造方法 | |
| JPH02163319A (ja) | 高靭性鋼の製造方法および高靭性鋼部品の製造方法 | |
| JPS6299416A (ja) | 肌焼鋼の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |