JPS6234762Y2 - - Google Patents
Info
- Publication number
- JPS6234762Y2 JPS6234762Y2 JP13674583U JP13674583U JPS6234762Y2 JP S6234762 Y2 JPS6234762 Y2 JP S6234762Y2 JP 13674583 U JP13674583 U JP 13674583U JP 13674583 U JP13674583 U JP 13674583U JP S6234762 Y2 JPS6234762 Y2 JP S6234762Y2
- Authority
- JP
- Japan
- Prior art keywords
- plate
- steel
- copper
- copper alloy
- steel plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
- 229910000831 Steel Inorganic materials 0.000 claims description 41
- 239000010959 steel Substances 0.000 claims description 41
- RYGMFSIKBFXOCR-UHFFFAOYSA-N Copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 claims description 18
- 229910000881 Cu alloy Inorganic materials 0.000 claims description 18
- PXHVJJICTQNCMI-UHFFFAOYSA-N Nickel Chemical compound [Ni] PXHVJJICTQNCMI-UHFFFAOYSA-N 0.000 claims description 18
- 229910052802 copper Inorganic materials 0.000 claims description 18
- 239000010949 copper Substances 0.000 claims description 18
- 229910052759 nickel Inorganic materials 0.000 claims description 9
- 239000010935 stainless steel Substances 0.000 claims description 9
- 229910001220 stainless steel Inorganic materials 0.000 claims description 9
- 238000005253 cladding Methods 0.000 claims description 2
- 230000003373 anti-fouling effect Effects 0.000 description 7
- 230000007797 corrosion Effects 0.000 description 6
- 238000005260 corrosion Methods 0.000 description 6
- 239000013535 sea water Substances 0.000 description 6
- 238000010586 diagram Methods 0.000 description 4
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 description 4
- 239000000463 material Substances 0.000 description 3
- 230000007774 longterm Effects 0.000 description 2
- 241000238586 Cirripedia Species 0.000 description 1
- 230000000694 effects Effects 0.000 description 1
- 239000000155 melt Substances 0.000 description 1
- 239000003973 paint Substances 0.000 description 1
- 230000003746 surface roughness Effects 0.000 description 1
Landscapes
- Laminated Bodies (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13674583U JPS6046233U (ja) | 1983-09-05 | 1983-09-05 | 多重クラツド鋼板 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13674583U JPS6046233U (ja) | 1983-09-05 | 1983-09-05 | 多重クラツド鋼板 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6046233U JPS6046233U (ja) | 1985-04-01 |
JPS6234762Y2 true JPS6234762Y2 (US07534539-20090519-C00280.png) | 1987-09-04 |
Family
ID=30307366
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP13674583U Granted JPS6046233U (ja) | 1983-09-05 | 1983-09-05 | 多重クラツド鋼板 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6046233U (US07534539-20090519-C00280.png) |
-
1983
- 1983-09-05 JP JP13674583U patent/JPS6046233U/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6046233U (ja) | 1985-04-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS539246A (en) | Method of preventing corrosion of ironncontaining metal in aqueous medium*particularly sea water | |
NO305692B1 (no) | DobbeltskrogbÕt med nedsenkede hydrofoiler | |
US5820737A (en) | Anti-fouling laminate marine structures | |
US3971084A (en) | Hull construction and method for forming same | |
JPS6234762Y2 (US07534539-20090519-C00280.png) | ||
US3421990A (en) | Sacrificial anode | |
AU1512483A (en) | Anti-fouling treatment of boats, ships, buoys and other structures exposed to water | |
US4678692A (en) | Multilayer protection system | |
GB2040232A (en) | Submersible or semi-submersible structures | |
JPS61122090A (ja) | 大型鋼構造物の洋上建造法 | |
JPH0346305B2 (US07534539-20090519-C00280.png) | ||
Czyryca et al. | Corrosion of Aluminum Alloys in Exfoliation-Resistant Tempers Exposed to Marine Environments for Two Years | |
JPS5894459A (ja) | 積層溶射層 | |
Ross | Corrosion of steel in marine environments | |
Edyvean et al. | The effects of marine fouling on the corrosion of offshore structures | |
Klingel | Boat building with steel. | |
JPS5826695A (ja) | 防汚特性の優れた接水構造物外板 | |
Rozenfeld et al. | Special Features of Electrochemical and Corrosion Behavior of Metals in Sea Water. | |
JPS5942130B2 (ja) | 着底型海洋構造物の据付方法 | |
Raclot | Anodes for Cathodic Protection in Seawater. Choice and Efficiency | |
McDonald | Waving, not drowning | |
JPS61260001A (ja) | 防汚板 | |
JPS62156592A (ja) | 海上立地原子力発電プラント | |
Raghava et al. | Corrosion fatigue studies on stiffened steel tubular T joints | |
JPS5657590A (en) | Semisubmerged type twin-hull boat |