JPS623213B2 - - Google Patents
Info
- Publication number
- JPS623213B2 JPS623213B2 JP55001742A JP174280A JPS623213B2 JP S623213 B2 JPS623213 B2 JP S623213B2 JP 55001742 A JP55001742 A JP 55001742A JP 174280 A JP174280 A JP 174280A JP S623213 B2 JPS623213 B2 JP S623213B2
- Authority
- JP
- Japan
- Prior art keywords
- temperature
- rolling
- strength
- stainless steel
- cold rolling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D7/00—Modifying the physical properties of iron or steel by deformation
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP174280A JPS56102519A (en) | 1980-01-12 | 1980-01-12 | Cold rolling method for stainless steel of high strength |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP174280A JPS56102519A (en) | 1980-01-12 | 1980-01-12 | Cold rolling method for stainless steel of high strength |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS56102519A JPS56102519A (en) | 1981-08-17 |
| JPS623213B2 true JPS623213B2 (cs) | 1987-01-23 |
Family
ID=11510010
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP174280A Granted JPS56102519A (en) | 1980-01-12 | 1980-01-12 | Cold rolling method for stainless steel of high strength |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS56102519A (cs) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0768584B2 (ja) * | 1986-06-09 | 1995-07-26 | 日新製鋼株式会社 | ばね特性に優れたばね用ステンレス鋼材の製造方法 |
| JPS6310009A (ja) * | 1986-06-27 | 1988-01-16 | Kawasaki Steel Corp | ステンレス鋼帯の連続温間圧延方法及びその設備 |
| US7082910B2 (en) | 1999-01-19 | 2006-08-01 | Aktiebolaget Electrolux | Two-stroke internal combustion engine |
| SE0000095L (sv) | 2000-01-14 | 2001-07-15 | Electrolux Ab | Spjäll för reglering av tillsatsluft till tvåtakts förbränningsmotorer |
| TWI623622B (zh) * | 2016-01-14 | 2018-05-11 | Ak鋼鐵資產公司 | 溫軋含介穩態奧氏體的鋼 |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5811489B2 (ja) * | 1976-03-01 | 1983-03-03 | 川崎製鉄株式会社 | 塑性歪比の面内異方性の小さいオ−ステナイト系ステンレス鋼帯板の製造方法 |
| JPS6054122B2 (ja) * | 1977-12-12 | 1985-11-28 | 日新製鋼株式会社 | 準安定オ−ステナイト系ステンレス鋼の冷間圧延方法 |
| JPS5561303A (en) * | 1978-11-02 | 1980-05-09 | Takasago Tekko Kk | Low temperature rolling method for metastable austenitic stalnless steel strip |
-
1980
- 1980-01-12 JP JP174280A patent/JPS56102519A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS56102519A (en) | 1981-08-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN107287489B (zh) | 基于全无头薄板坯连铸连轧流程生产钛微合金钢的方法 | |
| US3947293A (en) | Method for producing high-strength cold rolled steel sheet | |
| CN108441759B (zh) | 一种540MPa级热轧酸洗钢板及其制造方法 | |
| KR930017636A (ko) | 고강도 캔용 강판의 제조방법 | |
| US4323403A (en) | Continuous annealing method for cold reduced steel strip | |
| CN109182918A (zh) | 一种钒铌微合金化低碳热轧窄带钢及其制备方法 | |
| CN113996651A (zh) | 一种低碳钢及提高csp流程铁素体轧制低碳钢性能均匀性的制造方法 | |
| JPS623213B2 (cs) | ||
| JPS61207521A (ja) | 複合組織鋼ストリツプの製造方法 | |
| RU2164248C2 (ru) | Способ производства тонколистовой горячекатаной стали | |
| ATE104362T1 (de) | Verfahren zum herstellen eines alterungsbestaendigen bandstahles mit hoher kaltumformbarkeit. | |
| US2457420A (en) | Process of making corrugated galvanized steel sheets | |
| CN115747632A (zh) | 一种薄规格热轧钢及其制备方法 | |
| US3513036A (en) | Process for producing coiled,hotrolled,pickled steel strip | |
| CN115537682A (zh) | 一种薄规格热轧1200MPa钢及其制备方法 | |
| US3099592A (en) | Process of annealing low carbon steel | |
| JPS5573824A (en) | Production of rigid cold-rolled steel plate for drawing | |
| JPH0545653B2 (cs) | ||
| JPS56119732A (en) | Manufacture of high-strength cold rolled steel plate with superior press formability | |
| JPS59177325A (ja) | 高強度熱延ベイナイト鋼板の製造方法 | |
| US2405946A (en) | Production of non-aging steel | |
| KR100368835B1 (ko) | 온간압연법을이용한고강도강의제조방법 | |
| SU1710155A1 (ru) | Способ производства проката на непрерывных мелкосортных и проволочных станах | |
| SU1318318A1 (ru) | Способ тепловой правки стального проката | |
| JPS61238919A (ja) | 面内異方性の小さい絞り用冷延鋼板の製造方法 |