JPS62279076A - Brazing method for fit joint part without gap - Google Patents
Brazing method for fit joint part without gapInfo
- Publication number
- JPS62279076A JPS62279076A JP11913886A JP11913886A JPS62279076A JP S62279076 A JPS62279076 A JP S62279076A JP 11913886 A JP11913886 A JP 11913886A JP 11913886 A JP11913886 A JP 11913886A JP S62279076 A JPS62279076 A JP S62279076A
- Authority
- JP
- Japan
- Prior art keywords
- brazing
- fitting
- joint
- marking
- engagement
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【発明の詳細な説明】
3発明の詳細外説明
〔産業上の利用分野〕
本発明は、隙間(クリアランス)のない嵌め合い継手部
をろう付接合するようにしたろう付方法に関する。DETAILED DESCRIPTION OF THE INVENTION 3. Detailed Description of the Invention [Field of Industrial Application] The present invention relates to a brazing method for brazing fitting fitting joints having no clearance.
従来のろう付方法は、第5図に示すように、ろう付継手
部に隙間(クリアランス)9があり、その隙間に溶融ろ
うが流れ込む際、毛細管現像が生じ、隙間9にろうが満
たされた状態で溶融ろうが凝固することによりろう付接
合を実施していた。しかしながら、隙間のない嵌め合い
継手部では、充分なろう付品質が得られない問題があっ
た。In the conventional brazing method, as shown in Figure 5, there is a gap (clearance) 9 in the brazed joint, and when molten solder flows into the gap, capillary development occurs and the gap 9 is filled with wax. Brazed joints were performed by solidifying the molten solder in this state. However, there has been a problem that sufficient brazing quality cannot be obtained in a fitting joint portion without a gap.
表お、第5図において% 1はメス側部品、2はオス側
部品、3はろう行動の組立て品、4はろう付接合品%6
はろう材を示す。In Table 5, % 1 is the female side part, 2 is the male side part, 3 is the soldering assembly, 4 is the brazed joint %6
indicates filler metal.
従来方法では、継手部に隙間(クリアランス)があり、
隙間の量だけ継手が偏心したり、倒れたりするので、継
手の寸法品質要求が厳しいものに対しては、細心の注意
を払って継手を切組み、さらに固定治具を使用して固定
して寸法要求を満足させていたが、ろう材処理温度(約
1100℃)が高く、治具の熱膨張および熱変形があり
、2回目以降継続して同じ治具でろう行処理する時は、
継手部の寸法要求が満足しなく表る。又、その都度、新
しい治具を使用する方法では、量産に適さない。In the conventional method, there is a gap (clearance) at the joint,
The joint will become eccentric or fall by the amount of the gap, so if the joint has strict dimensional quality requirements, cut the joint with great care and then fix it using a fixing jig. Although the dimensional requirements were met, the brazing metal processing temperature (approximately 1100℃) was high and the jig was subject to thermal expansion and thermal deformation.
It appears that the dimensional requirements of the joint are not satisfied. Furthermore, the method of using a new jig each time is not suitable for mass production.
本発明は、上記問題点を解消し、容易に高品質のろう付
ができるようにした隙間(クリアランス)のない嵌め合
い継手部のろう付方法を提供しようとするものでおる。The present invention aims to solve the above-mentioned problems and provide a method of brazing a fitting joint portion without any clearance, which allows high-quality brazing to be easily performed.
本発明は、冷し嵌め法、焼き嵌め法あるいは圧入法等に
より形成した隙間のない継手部をろう相接合する方法に
おいて、メス側部品又はオス側部品の接合表面のどちら
か一方又は両方に外部に通ずるケガキ傷を入れて、ろう
相接合を行うことt−特徴とする隙間のない嵌め合い継
手部のろう付方法に関する。The present invention provides a method for braze-phase joining a joint portion with no gap formed by a cold fitting method, a shrink fitting method, a press fitting method, etc. The present invention relates to a brazing method for a fitting joint portion without a gap, characterized in that the brazing phase joint is performed by making a scribe mark that leads to the above.
本発明では、寸法要求を満足させるためK、冷し嵌め法
、焼き嵌め法又は圧入法により隙間(クリアランス)の
ない嵌め合い継手にする。In the present invention, in order to satisfy the dimensional requirements, a fitting joint with no clearance is formed by a cold fitting method, a shrink fitting method, or a press fitting method.
隙間(クリアランス)のないろう付に対しては、嵌め合
い前に第4図に示すようにケガキ傷5を、機械加工表面
ライン(マシンミゾ)10を横切シ、外部に通ずるよう
に遊子方向に設ける。この2つの要因(隙間のない嵌め
合い、ケガキ傷)により、寸法品質とろう付品質とを同
時に満足させることができる。For brazing without any clearance, before fitting, as shown in Figure 4, mark scratches 5 across the machined surface line (machine groove) 10 and in the direction of the playback so that it leads to the outside. establish. Due to these two factors (fitting without gaps, scribing scratches), dimensional quality and brazing quality can be satisfied at the same time.
なお、第4図は下記に詳述する第1図のオス側部品の詳
細図であシ、同図において、03)は、(A)のl−1
1矢視断面を示す。In addition, Fig. 4 is a detailed view of the male side parts of Fig. 1, which will be explained in detail below.
A cross section taken in the direction of arrow 1 is shown.
本発明方法は、以下のようにして行われる。The method of the present invention is carried out as follows.
先づ、継手部オス側の嵌め合い寸法をメス側の嵌め合り
寸法より大きくする。又、オス側部品とメス側部品の継
手部のどちらか一方あるいは両方にケガキ傷を設ける。First, the fitting dimensions on the male side of the joint are made larger than the fitting dimensions on the female side. Also, provide a scribing mark on one or both of the joint parts of the male side part and the female side part.
次に、冷し嵌め、焼き嵌めあるいは圧入等によりメス側
部品とオス側部品とを隙間(クリアランス)のない嵌め
合いをする。嵌め合い後、継手部一端にろう材を置く。Next, the female part and the male part are fitted together without any clearance by cold fitting, shrink fitting, press fitting, or the like. After fitting, place a filler metal on one end of the joint.
その状態で、適正な加熱温度で加熱することによりろう
相接合を行なうと、ろう材が毛細管現像によりケガキ部
及び機械加工表面ミゾをったいろうが充填され寸法品質
とろう付品質とを同時に満足させることができる。In this state, when solder phase bonding is performed by heating at an appropriate heating temperature, the solder fills the scribed area and the grooves on the machined surface by capillary development, satisfying both dimensional quality and brazing quality. can be done.
次K、本発明を図面に基づき説明する。Next, the present invention will be explained based on the drawings.
第1図は、本発明によるろう付方法の一例を示す説明図
である。図において、メス側部品1゜オス側部品2、ろ
う付前の組立品3、ろう付接合品4を表わし、オス側部
め合い寸法8は、メス側部め合い寸法7より大きくしで
ある。又、オス側部品2の継手部にケガキ傷5を数本設
ける。次に1冷し嵌め法、焼き嵌め法あるいは圧入法に
よりろう付前の組立品3になるように嵌め合いする。そ
の後、ろう材6を継手部一端に置き、適正温度に加熱し
てろう相接合することKよシ、ろう付接合品4を製作す
ることができる。この場合、ろう回夛部は、嵌め合い部
全域であシ、ケガキ傷5に加えてマシンミゾ10[屯及
ぶ。FIG. 1 is an explanatory diagram showing an example of the brazing method according to the present invention. In the figure, the female side part 1, the male side part 2, the assembly before brazing 3, and the brazed joint 4 are shown, and the male side fitting dimension 8 is larger than the female side fitting dimension 7. . Also, several scratches 5 are provided on the joint portion of the male part 2. Next, they are fitted together by a cold fitting method, a shrink fitting method, or a press fitting method so as to become an assembled product 3 before brazing. Thereafter, the brazing material 6 is placed on one end of the joint, heated to an appropriate temperature, and brazed phase welded, thereby producing the brazed joint 4. In this case, the solder recovery part covers the entire area of the fitting part, and in addition to the marking scratches 5, it also extends to the machine groove 10.
第2図は、本発明によるろう付方法の他の例を示す説明
図である。その構成は、第1図の例とほぼ同じであるが
、ケガキ傷5をメス側部品1の継手部に数本設ける点で
異なる。その後は第1回の例と同じ方法で嵌め合いおよ
びろう相接合して、ろう付接合品4を製作することがで
きる。FIG. 2 is an explanatory diagram showing another example of the brazing method according to the present invention. Its structure is almost the same as the example shown in FIG. 1, but differs in that several scribes 5 are provided at the joint portion of the female part 1. Thereafter, the soldered parts 4 can be manufactured by fitting and soldering in the same manner as in the first example.
第3図は、本発明によるろう付方法のもう一つの例を示
す説明図である。その構成は、第1図の例と、ケガキ傷
51!1:オス側部2とメス側部品10両方の継手部に
各数本設ける点で異なる。FIG. 3 is an explanatory diagram showing another example of the brazing method according to the present invention. The configuration differs from the example shown in FIG. 1 in that several marking scratches 51!1 are provided at the joint portions of both the male side part 2 and the female side part 10.
次に、第1図の例と同じ方法で嵌め合いおよびろう相接
合して、ろう付接合品4t−製作することができる。Next, the parts are fitted and soldered together in the same manner as in the example shown in FIG. 1 to produce a soldered product 4t.
継手部の倒れ・同心度等の寸法要求は、冷し嵌め法、焼
き嵌め法あるいは圧入法による嵌め合りで満足させるこ
とができる。又、ろう付接合率要求は、ケガキ傷により
満足させることができる。その両方の効果により、寸法
・ろう付の品質を保証することができる。Dimensional requirements such as inclination and concentricity of the joint can be satisfied by fitting by cold fitting, shrink fitting, or press fitting. Further, the brazing joint rate requirement can be satisfied by scribing scratches. Due to both effects, dimensions and brazing quality can be guaranteed.
第1図乃至第3図は、本発明によるろう付方法の説明図
、第4図・け、ケガキ傷の説明図でちる。第5図は、従
来のろう付方法の説明図である。1 to 3 are explanatory diagrams of the brazing method according to the present invention, and FIG. 4 is an explanatory diagram of scribing scratches. FIG. 5 is an explanatory diagram of a conventional brazing method.
Claims (1)
た隙間のない継手部をろう付接合する方法において、メ
ス側部品又はオス側部品の接合表面のどちらか一方又は
両方に外部に通ずるケガキ傷を入れて、ろう付接合を行
うことを特徴とする隙間のない嵌め合い継手部のろう付
方法。Scratches that lead to the outside on either or both of the joining surfaces of the female side part or the male side part in the method of brazing joints with no gaps formed by cold fitting, shrink fitting, press fitting, etc. A brazing method for a fitting joint portion with no gaps, characterized by performing a brazing joint by inserting the