JPS6219430Y2 - - Google Patents
Info
- Publication number
- JPS6219430Y2 JPS6219430Y2 JP1981092482U JP9248281U JPS6219430Y2 JP S6219430 Y2 JPS6219430 Y2 JP S6219430Y2 JP 1981092482 U JP1981092482 U JP 1981092482U JP 9248281 U JP9248281 U JP 9248281U JP S6219430 Y2 JPS6219430 Y2 JP S6219430Y2
- Authority
- JP
- Japan
- Prior art keywords
- die
- powder
- molded product
- punch
- green compact
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
- 239000000843 powder Substances 0.000 description 17
- 238000000465 moulding Methods 0.000 description 9
- 230000006835 compression Effects 0.000 description 6
- 238000007906 compression Methods 0.000 description 6
- 239000000446 fuel Substances 0.000 description 6
- 239000008188 pellet Substances 0.000 description 5
- 238000005336 cracking Methods 0.000 description 3
- OOAWCECZEHPMBX-UHFFFAOYSA-N oxygen(2-);uranium(4+) Chemical compound [O-2].[O-2].[U+4] OOAWCECZEHPMBX-UHFFFAOYSA-N 0.000 description 3
- 230000002093 peripheral effect Effects 0.000 description 3
- FCTBKIHDJGHPPO-UHFFFAOYSA-N uranium dioxide Inorganic materials O=[U]=O FCTBKIHDJGHPPO-UHFFFAOYSA-N 0.000 description 3
- 238000005056 compaction Methods 0.000 description 2
- 229910001315 Tool steel Inorganic materials 0.000 description 1
- 229910001093 Zr alloy Inorganic materials 0.000 description 1
- 238000013459 approach Methods 0.000 description 1
- 238000005253 cladding Methods 0.000 description 1
- 238000007796 conventional method Methods 0.000 description 1
- 230000007547 defect Effects 0.000 description 1
- 230000006866 deterioration Effects 0.000 description 1
- 230000002542 deteriorative effect Effects 0.000 description 1
- 238000010586 diagram Methods 0.000 description 1
- 230000000694 effects Effects 0.000 description 1
- 238000001125 extrusion Methods 0.000 description 1
- 238000004904 shortening Methods 0.000 description 1
- 238000005245 sintering Methods 0.000 description 1
- 230000003746 surface roughness Effects 0.000 description 1
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 description 1
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E30/00—Energy generation of nuclear origin
- Y02E30/30—Nuclear fission reactors
Landscapes
- Powder Metallurgy (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1981092482U JPS6219430Y2 (US07582779-20090901-C00044.png) | 1981-06-23 | 1981-06-23 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1981092482U JPS6219430Y2 (US07582779-20090901-C00044.png) | 1981-06-23 | 1981-06-23 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57204898U JPS57204898U (US07582779-20090901-C00044.png) | 1982-12-27 |
JPS6219430Y2 true JPS6219430Y2 (US07582779-20090901-C00044.png) | 1987-05-18 |
Family
ID=29887511
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1981092482U Expired JPS6219430Y2 (US07582779-20090901-C00044.png) | 1981-06-23 | 1981-06-23 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6219430Y2 (US07582779-20090901-C00044.png) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6137399A (ja) * | 1984-07-30 | 1986-02-22 | Hitachi Powdered Metals Co Ltd | 圧粉体の成形方法とその装置 |
-
1981
- 1981-06-23 JP JP1981092482U patent/JPS6219430Y2/ja not_active Expired
Also Published As
Publication number | Publication date |
---|---|
JPS57204898U (US07582779-20090901-C00044.png) | 1982-12-27 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US5043123A (en) | Method and apparatus for manufacturing finished parts as composite bodies from pulverulent rolling materials | |
US5156854A (en) | Press forming apparatus for sintered parts | |
JPS6219430Y2 (US07582779-20090901-C00044.png) | ||
US3949027A (en) | Manufacturing process for improved nuclear fuel tablets | |
JPS639562B2 (US07582779-20090901-C00044.png) | ||
US5019307A (en) | Method and apparatus for the manufacture of hollow ceramic beams using multiple molding mandrels | |
JPH0832922B2 (ja) | ボス付き成形体の粉末成形方法およびその装置 | |
JP2864392B2 (ja) | セラミックス成形型 | |
JPH0313281B2 (US07582779-20090901-C00044.png) | ||
JPS639561B2 (US07582779-20090901-C00044.png) | ||
JPH0344880B2 (US07582779-20090901-C00044.png) | ||
JP2001003104A (ja) | 粉末から成形体を成形する方法 | |
JP2851326B2 (ja) | 原子燃料ペレットの製造装置 | |
CN217134193U (zh) | 一种带逃料槽的磁芯模具 | |
JPH0570802A (ja) | 長尺圧粉体の成形方法 | |
JP2501820Y2 (ja) | 粉末成形用金型 | |
JP2594691B2 (ja) | セラミックス管成形素地体の成形方法 | |
JPS6233281B2 (US07582779-20090901-C00044.png) | ||
JPH07120579A (ja) | 低密度部を有する核燃料ペレット及びその製造方法 | |
JP2906259B2 (ja) | セラミックス成形型 | |
JPH05156305A (ja) | 焼結部品の成形装置 | |
JPS6054361B2 (ja) | 多孔磁石板の製造方法 | |
SU816692A1 (ru) | Устройство дл прессовани металлическихпОРОшКОВ | |
JPH02250903A (ja) | 環状部材の製造方法 | |
JPH0740493Y2 (ja) | 粉末成形用金型への原料供給装置 |