JPS6172637A - 板ガラスの強化方法 - Google Patents

板ガラスの強化方法

Info

Publication number
JPS6172637A
JPS6172637A JP19271784A JP19271784A JPS6172637A JP S6172637 A JPS6172637 A JP S6172637A JP 19271784 A JP19271784 A JP 19271784A JP 19271784 A JP19271784 A JP 19271784A JP S6172637 A JPS6172637 A JP S6172637A
Authority
JP
Japan
Prior art keywords
cooling
glass
nozzles
blast
nozzle
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP19271784A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6343327B2 (xx
Inventor
Shinichi Araya
眞一 荒谷
Tadashi Muramoto
正 村本
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Central Glass Co Ltd
Original Assignee
Central Glass Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Central Glass Co Ltd filed Critical Central Glass Co Ltd
Priority to JP19271784A priority Critical patent/JPS6172637A/ja
Priority to GB08427114A priority patent/GB2149777B/en
Priority to FR848416587A priority patent/FR2554805B1/fr
Priority to DE19843439871 priority patent/DE3439871A1/de
Priority to US06/842,723 priority patent/US4662926A/en
Publication of JPS6172637A publication Critical patent/JPS6172637A/ja
Publication of JPS6343327B2 publication Critical patent/JPS6343327B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Re-Forming, After-Treatment, Cutting And Transporting Of Glass Products (AREA)
JP19271784A 1983-11-16 1984-09-17 板ガラスの強化方法 Granted JPS6172637A (ja)

Priority Applications (5)

Application Number Priority Date Filing Date Title
JP19271784A JPS6172637A (ja) 1984-09-17 1984-09-17 板ガラスの強化方法
GB08427114A GB2149777B (en) 1983-11-16 1984-10-26 Method of toughening glass sheet by quenching
FR848416587A FR2554805B1 (fr) 1983-11-16 1984-10-30 Procede pour tremper une feuille de verre par refroidissement brusque, et feuille de verre obtenue
DE19843439871 DE3439871A1 (de) 1983-11-16 1984-10-31 Verfahren zum haerten einer glasschicht durch abschrecken
US06/842,723 US4662926A (en) 1983-11-16 1986-03-20 Method of toughening glass sheet by quenching

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP19271784A JPS6172637A (ja) 1984-09-17 1984-09-17 板ガラスの強化方法

Publications (2)

Publication Number Publication Date
JPS6172637A true JPS6172637A (ja) 1986-04-14
JPS6343327B2 JPS6343327B2 (xx) 1988-08-30

Family

ID=16295887

Family Applications (1)

Application Number Title Priority Date Filing Date
JP19271784A Granted JPS6172637A (ja) 1983-11-16 1984-09-17 板ガラスの強化方法

Country Status (1)

Country Link
JP (1) JPS6172637A (xx)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US9296638B2 (en) 2014-07-31 2016-03-29 Corning Incorporated Thermally tempered glass and methods and apparatuses for thermal tempering of glass
US11485673B2 (en) 2017-08-24 2022-11-01 Corning Incorporated Glasses with improved tempering capabilities
US11643355B2 (en) 2016-01-12 2023-05-09 Corning Incorporated Thin thermally and chemically strengthened glass-based articles
US11697617B2 (en) 2019-08-06 2023-07-11 Corning Incorporated Glass laminate with buried stress spikes to arrest cracks and methods of making the same
US11708296B2 (en) 2017-11-30 2023-07-25 Corning Incorporated Non-iox glasses with high coefficient of thermal expansion and preferential fracture behavior for thermal tempering
US11795102B2 (en) 2016-01-26 2023-10-24 Corning Incorporated Non-contact coated glass and related coating system and method
US11891324B2 (en) 2014-07-31 2024-02-06 Corning Incorporated Thermally strengthened consumer electronic glass and related systems and methods

Cited By (14)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US10077204B2 (en) 2014-07-31 2018-09-18 Corning Incorporated Thin safety glass having improved mechanical characteristics
US9296638B2 (en) 2014-07-31 2016-03-29 Corning Incorporated Thermally tempered glass and methods and apparatuses for thermal tempering of glass
US9783448B2 (en) 2014-07-31 2017-10-10 Corning Incorporated Thin dicing glass article
US9802853B2 (en) 2014-07-31 2017-10-31 Corning Incorporated Fictive temperature in damage-resistant glass having improved mechanical characteristics
US9975801B2 (en) 2014-07-31 2018-05-22 Corning Incorporated High strength glass having improved mechanical characteristics
US10005691B2 (en) 2014-07-31 2018-06-26 Corning Incorporated Damage resistant glass article
US9776905B2 (en) 2014-07-31 2017-10-03 Corning Incorporated Highly strengthened glass article
US10233111B2 (en) 2014-07-31 2019-03-19 Corning Incorporated Thermally tempered glass and methods and apparatuses for thermal tempering of glass
US11891324B2 (en) 2014-07-31 2024-02-06 Corning Incorporated Thermally strengthened consumer electronic glass and related systems and methods
US11643355B2 (en) 2016-01-12 2023-05-09 Corning Incorporated Thin thermally and chemically strengthened glass-based articles
US11795102B2 (en) 2016-01-26 2023-10-24 Corning Incorporated Non-contact coated glass and related coating system and method
US11485673B2 (en) 2017-08-24 2022-11-01 Corning Incorporated Glasses with improved tempering capabilities
US11708296B2 (en) 2017-11-30 2023-07-25 Corning Incorporated Non-iox glasses with high coefficient of thermal expansion and preferential fracture behavior for thermal tempering
US11697617B2 (en) 2019-08-06 2023-07-11 Corning Incorporated Glass laminate with buried stress spikes to arrest cracks and methods of making the same

Also Published As

Publication number Publication date
JPS6343327B2 (xx) 1988-08-30

Similar Documents

Publication Publication Date Title
JP2567438B2 (ja) 強化ガラスとその製造方法及び装置
FI60696C (fi) Glasskiva foer anvaendning som sido- eller bakruta i ett motorfordon och foerfarande foer framstaellning av denna glasskiva
JP2653708B2 (ja) 強化ガラス板の製造方法
JPS6172637A (ja) 板ガラスの強化方法
JP2002326830A (ja) 強化ガラス板
JPH026343A (ja) 凸状ガラス板の冷却工程及び装置
US4662926A (en) Method of toughening glass sheet by quenching
EP0000268B1 (en) Method for thermally toughening glass sheets, in particular to be used as motor vehicle side or rear windows
JP2000103632A (ja) 強化ガラス、強化ガラスの製造方法およびその装置
JPS62158128A (ja) 薄板ガラスの強化方法
JPS5891042A (ja) 強化ガラス
US4508783A (en) Method for the differentiated hardening of glass sheets, especially of automobile windshields, and tempered glass sheet
JPH0623068B2 (ja) 板ガラスの強化方法
US3294519A (en) Glass sheet tempering apparatus
US10519058B2 (en) Method for tempering glass sheets
US5112377A (en) Method of toughening glass sheet by quenching
JP2000103631A (ja) 強化ガラスの製造方法およびその装置
CN109468521A (zh) 高速铁路用钢轨生产方法及其约束装置
US3827872A (en) Glass tempering method
JPS605033A (ja) 板ガラスの強化方法
JPS6247819B2 (xx)
JPS5950033A (ja) 改良されたガラス板の強化方法
JPS60108331A (ja) 板ガラスの強化方法
JPH11310821A (ja) 金型の焼入れ方法
RU2189882C2 (ru) Способ изготовления заготовок при производстве изделий типа колес