JPS6167724A - 高融点活性金属及びその合金の真空ア−ク溶解方法 - Google Patents
高融点活性金属及びその合金の真空ア−ク溶解方法Info
- Publication number
- JPS6167724A JPS6167724A JP19005584A JP19005584A JPS6167724A JP S6167724 A JPS6167724 A JP S6167724A JP 19005584 A JP19005584 A JP 19005584A JP 19005584 A JP19005584 A JP 19005584A JP S6167724 A JPS6167724 A JP S6167724A
- Authority
- JP
- Japan
- Prior art keywords
- melting
- alloys
- active metals
- vacuum arc
- melting point
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacture And Refinement Of Metals (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19005584A JPS6167724A (ja) | 1984-09-10 | 1984-09-10 | 高融点活性金属及びその合金の真空ア−ク溶解方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19005584A JPS6167724A (ja) | 1984-09-10 | 1984-09-10 | 高融点活性金属及びその合金の真空ア−ク溶解方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6167724A true JPS6167724A (ja) | 1986-04-07 |
JPH0429722B2 JPH0429722B2 (enrdf_load_stackoverflow) | 1992-05-19 |
Family
ID=16251589
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP19005584A Granted JPS6167724A (ja) | 1984-09-10 | 1984-09-10 | 高融点活性金属及びその合金の真空ア−ク溶解方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6167724A (enrdf_load_stackoverflow) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2007291453A (ja) * | 2006-04-25 | 2007-11-08 | Kobe Steel Ltd | 消耗電極 |
CN113462904A (zh) * | 2021-07-22 | 2021-10-01 | 西安汉唐分析检测有限公司 | 一种高Mo含量Ti-Mo合金真空自耗电极棒的压制方法 |
-
1984
- 1984-09-10 JP JP19005584A patent/JPS6167724A/ja active Granted
Non-Patent Citations (2)
Title |
---|
TITANIUM 1980 SCIENCE AND TECHNOLOGY=1980 * |
TITANIUM AND TITANIUM ALLOYS=1976 * |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2007291453A (ja) * | 2006-04-25 | 2007-11-08 | Kobe Steel Ltd | 消耗電極 |
CN113462904A (zh) * | 2021-07-22 | 2021-10-01 | 西安汉唐分析检测有限公司 | 一种高Mo含量Ti-Mo合金真空自耗电极棒的压制方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0429722B2 (enrdf_load_stackoverflow) | 1992-05-19 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US8668760B2 (en) | Method for the production of a β-γ-TiAl base alloy | |
US3649253A (en) | Deoxidation of aluminum-killed molten steel | |
JPH05239584A (ja) | 高強度アルミニウム合金圧延板およびその製造方法 | |
EP0202336B1 (en) | Process for producing a thin plate of a high ferrosilicon alloy | |
US3737981A (en) | Process of manufacturing forged or rolled rod steel from ledeburitic tool steel | |
JPS6167724A (ja) | 高融点活性金属及びその合金の真空ア−ク溶解方法 | |
JPH0559483A (ja) | 商用周波数帯トランス用非晶質合金薄帯の製造方法 | |
US20200199711A1 (en) | Processes for producing superalloys and superalloys obtained by the processes | |
JPS5935642A (ja) | Mo合金インゴツトの製造方法 | |
JPS63111172A (ja) | タ−ゲツト材の製造方法 | |
JP3322806B2 (ja) | 鋼中の酸化物の微細分散法 | |
JPS629746A (ja) | 鋳塊製造方法 | |
DE69317489T2 (de) | Verfahren zur Herstellung von weich-magnetischen Legierungen hoher permeabilität und Legierungen | |
US1975310A (en) | Process of making ferrous alloys | |
JPH0971827A (ja) | 工業用純チタンインゴットの製造方法 | |
JP2926169B2 (ja) | 連鋳片の加熱方法 | |
JPS619554A (ja) | 冷間圧延用鍛鋼ロ−ル | |
JP3658488B2 (ja) | 共晶黒鉛鋳鉄の製造方法 | |
JPH07136740A (ja) | チタン合金の鋳造方法 | |
JPH08120366A (ja) | チタン鋳塊の連続鋳造方法 | |
US3550671A (en) | Steel making practice | |
JPS6137954A (ja) | モリブデン又はモリブデン合金の溶接方法 | |
JPH06335750A (ja) | Al−Zr系合金の製造方法 | |
CN112941393A (zh) | 一种五元中间合金材料及其制备方法和用途 | |
US3387968A (en) | Free-cutting steels |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
LAPS | Cancellation because of no payment of annual fees |