JPS6126520A - 溶融低粘性ガラスゴブの成形方法 - Google Patents
溶融低粘性ガラスゴブの成形方法Info
- Publication number
- JPS6126520A JPS6126520A JP14448084A JP14448084A JPS6126520A JP S6126520 A JPS6126520 A JP S6126520A JP 14448084 A JP14448084 A JP 14448084A JP 14448084 A JP14448084 A JP 14448084A JP S6126520 A JPS6126520 A JP S6126520A
- Authority
- JP
- Japan
- Prior art keywords
- glass
- mold
- blade
- upper plate
- tip
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 238000000034 method Methods 0.000 title claims abstract description 18
- 239000006060 molten glass Substances 0.000 title claims abstract description 13
- 238000000465 moulding Methods 0.000 title claims description 4
- 239000011521 glass Substances 0.000 claims abstract description 68
- 206010040925 Skin striae Diseases 0.000 abstract description 8
- 230000007547 defect Effects 0.000 abstract description 5
- 238000005520 cutting process Methods 0.000 description 5
- 239000005304 optical glass Substances 0.000 description 4
- 230000000694 effects Effects 0.000 description 3
- 239000011324 bead Substances 0.000 description 2
- 238000002347 injection Methods 0.000 description 2
- 239000007924 injection Substances 0.000 description 2
- 239000000203 mixture Substances 0.000 description 2
- 230000003213 activating effect Effects 0.000 description 1
- 239000000853 adhesive Substances 0.000 description 1
- 230000001070 adhesive effect Effects 0.000 description 1
- 239000005356 container glass Substances 0.000 description 1
- 238000007796 conventional method Methods 0.000 description 1
- 238000001816 cooling Methods 0.000 description 1
- 238000005336 cracking Methods 0.000 description 1
- 238000004031 devitrification Methods 0.000 description 1
- 238000004519 manufacturing process Methods 0.000 description 1
- 238000002844 melting Methods 0.000 description 1
- 230000008018 melting Effects 0.000 description 1
- 230000000717 retained effect Effects 0.000 description 1
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 description 1
- 238000009736 wetting Methods 0.000 description 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B19/00—Other methods of shaping glass
- C03B19/02—Other methods of shaping glass by casting molten glass, e.g. injection moulding
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B7/00—Distributors for the molten glass; Means for taking-off charges of molten glass; Producing the gob, e.g. controlling the gob shape, weight or delivery tact
- C03B7/10—Cutting-off or severing the glass flow with the aid of knives or scissors or non-contacting cutting means, e.g. a gas jet; Construction of the blades used
- C03B7/12—Cutting-off or severing a free-hanging glass stream, e.g. by the combination of gravity and surface tension forces
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Manufacturing & Machinery (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14448084A JPS6126520A (ja) | 1984-07-13 | 1984-07-13 | 溶融低粘性ガラスゴブの成形方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14448084A JPS6126520A (ja) | 1984-07-13 | 1984-07-13 | 溶融低粘性ガラスゴブの成形方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6126520A true JPS6126520A (ja) | 1986-02-05 |
| JPH0143689B2 JPH0143689B2 (enExample) | 1989-09-22 |
Family
ID=15363286
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14448084A Granted JPS6126520A (ja) | 1984-07-13 | 1984-07-13 | 溶融低粘性ガラスゴブの成形方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6126520A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS63199049A (ja) * | 1987-02-13 | 1988-08-17 | Sumitomo Electric Ind Ltd | 連続結晶成長方法 |
-
1984
- 1984-07-13 JP JP14448084A patent/JPS6126520A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS63199049A (ja) * | 1987-02-13 | 1988-08-17 | Sumitomo Electric Ind Ltd | 連続結晶成長方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0143689B2 (enExample) | 1989-09-22 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0615476B1 (en) | Casting of light metal alloys | |
| CN208483224U (zh) | 一种适用于激光选区熔化金属打印机的铺粉装置 | |
| DE69012092T2 (de) | Verfahren und Vorrichtung zum horizontalen Stranggiessen von Metallband. | |
| US4381932A (en) | Laminated gob for pressing glass articles | |
| KR100218174B1 (ko) | 유리성형장치 및 성형방법 | |
| JP2002160041A (ja) | 金属薄肉成形体用金型およびそれを用いた金属薄肉成形体の製法 | |
| JPS6126520A (ja) | 溶融低粘性ガラスゴブの成形方法 | |
| CN211708081U (zh) | 一种防冷料散热片压铸模具 | |
| JPH0466818B2 (enExample) | ||
| TWI774551B (zh) | 澆道截斷式塑膠鏡片成型裝置 | |
| CN114536698A (zh) | 一种可智能调控的注塑装置及其工艺 | |
| US7082985B2 (en) | Moulding apparatus | |
| CN210679547U (zh) | 一种雨刮器浇口切除模 | |
| CN210679546U (zh) | 一种空调压缩机缸体浇口切除模 | |
| CN209006633U (zh) | 一种自动锡球铸造机 | |
| US4390593A (en) | Laminated gob for pressing glass articles | |
| JP7645587B1 (ja) | ガラス製光学部品成形用金型 | |
| US2745151A (en) | Method and apparatus for continuous casting | |
| PT86221B (pt) | Metodo de moldacao por injeccao de um micro-pipeta | |
| JPS5837057B2 (ja) | バッテリグリッドの連続鋳造装置 | |
| JPH01202349A (ja) | 連続鋳造方法 | |
| JPS5841730A (ja) | ガラス溶融装置 | |
| JP4359826B2 (ja) | 金属材料成形装置 | |
| KR19990009025U (ko) | 금속박판제조용 턴디쉬 | |
| JPH05132325A (ja) | 溶融ガラスの成形方法 |