JPS61212483A - 耐食性の優れた二相ステンレス溶接管の製造方法 - Google Patents
耐食性の優れた二相ステンレス溶接管の製造方法Info
- Publication number
- JPS61212483A JPS61212483A JP5510385A JP5510385A JPS61212483A JP S61212483 A JPS61212483 A JP S61212483A JP 5510385 A JP5510385 A JP 5510385A JP 5510385 A JP5510385 A JP 5510385A JP S61212483 A JPS61212483 A JP S61212483A
- Authority
- JP
- Japan
- Prior art keywords
- stainless steel
- welding
- corrosion resistance
- duplex stainless
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5510385A JPS61212483A (ja) | 1985-03-19 | 1985-03-19 | 耐食性の優れた二相ステンレス溶接管の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5510385A JPS61212483A (ja) | 1985-03-19 | 1985-03-19 | 耐食性の優れた二相ステンレス溶接管の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61212483A true JPS61212483A (ja) | 1986-09-20 |
JPH0333071B2 JPH0333071B2 (enrdf_load_stackoverflow) | 1991-05-15 |
Family
ID=12989410
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP5510385A Granted JPS61212483A (ja) | 1985-03-19 | 1985-03-19 | 耐食性の優れた二相ステンレス溶接管の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61212483A (enrdf_load_stackoverflow) |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS51145454A (en) * | 1975-06-10 | 1976-12-14 | Nippon Steel Corp | Method for manufacture of electriccweld steel pipe |
JPS5550757A (en) * | 1978-10-06 | 1980-04-12 | Hitachi Denshi Ltd | Signal change-over control device |
-
1985
- 1985-03-19 JP JP5510385A patent/JPS61212483A/ja active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS51145454A (en) * | 1975-06-10 | 1976-12-14 | Nippon Steel Corp | Method for manufacture of electriccweld steel pipe |
JPS5550757A (en) * | 1978-10-06 | 1980-04-12 | Hitachi Denshi Ltd | Signal change-over control device |
Also Published As
Publication number | Publication date |
---|---|
JPH0333071B2 (enrdf_load_stackoverflow) | 1991-05-15 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Qiao et al. | Microstructural evolution and deformation behavior of friction stir welded twin-induced plasticity steel | |
JPS60133996A (ja) | クリ−プ破断延性の優れた溶接材料 | |
JPS61212483A (ja) | 耐食性の優れた二相ステンレス溶接管の製造方法 | |
US3663217A (en) | Brazing alloy for elevated temperature service | |
JPH02185940A (ja) | 酸化雰囲気中での接合が可能な液相拡散接合用合金箔 | |
JP2639798B2 (ja) | オーステナイト系ステンレス鋼の製造方法 | |
JPH02151377A (ja) | 酸化雰囲気中で接合可能なCr含有材料の液相拡散接合用合金箔 | |
JP2002285239A (ja) | 溶接熱影響部靱性に優れた非調質厚肉高張力鋼の製造方法 | |
CN116590629B (zh) | 一种环焊热影响区低温韧性良好的x80钢管制造方法 | |
JPH02151378A (ja) | 酸化雰囲気中で接合可能なCr含有材料の液相拡散接合用合金箔 | |
JP2002275590A (ja) | 溶接部の加工性に優れた溶接用フェライト系ステンレス鋼 | |
JPS5832583A (ja) | 大径鋼管の造管溶接法 | |
CN110193682B (zh) | 钎料及其制备方法 | |
JPH0649233B2 (ja) | ステンレス鋼の溶接方法 | |
Wright | Mechanical behavior and weldability of a high chromium ferritic stainless steel as a function of purity | |
JPH04325628A (ja) | 電縫溶接部の硬化の少ない電縫鋼管の製造方法 | |
JPH0698500B2 (ja) | 耐サワーガス性に優れた大径鋼管の製造方法 | |
JP2911333B2 (ja) | 高温特性及び耐食性の優れたボイラー用電縫鋼管 | |
JPH09209100A (ja) | α+β型チタン合金溶接部材の後熱処理方法 | |
JPS63157837A (ja) | 溶接作業性と溶接部の加工性に優れたフエライト系耐熱ステンレス鋼 | |
JP3146918B2 (ja) | オーステナイト系ステンレス鋼溶接管の製造方法 | |
JP3678321B2 (ja) | 高温強度に優れたエンジン排ガス経路部材用フェライト系ステンレス鋼パイプ | |
JPH09155574A (ja) | 耐炭酸ガス腐食性に優れたマルテンサイト系ステンレス鋼溶接管の製造方法 | |
JPS60216993A (ja) | 高温部材用溶接材料 | |
JPS626618B2 (enrdf_load_stackoverflow) |