JPS6096725A - 耐応力腐食割れ性にすぐれた高張力電縫鋼管の製造方法 - Google Patents
耐応力腐食割れ性にすぐれた高張力電縫鋼管の製造方法Info
- Publication number
- JPS6096725A JPS6096725A JP20100583A JP20100583A JPS6096725A JP S6096725 A JPS6096725 A JP S6096725A JP 20100583 A JP20100583 A JP 20100583A JP 20100583 A JP20100583 A JP 20100583A JP S6096725 A JPS6096725 A JP S6096725A
- Authority
- JP
- Japan
- Prior art keywords
- less
- stress corrosion
- corrosion cracking
- cracking resistance
- steel pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
- C21D8/02—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of plates or strips
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Strip Materials And Filament Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20100583A JPS6096725A (ja) | 1983-10-28 | 1983-10-28 | 耐応力腐食割れ性にすぐれた高張力電縫鋼管の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP20100583A JPS6096725A (ja) | 1983-10-28 | 1983-10-28 | 耐応力腐食割れ性にすぐれた高張力電縫鋼管の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6096725A true JPS6096725A (ja) | 1985-05-30 |
| JPS638166B2 JPS638166B2 (enExample) | 1988-02-22 |
Family
ID=16433912
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP20100583A Granted JPS6096725A (ja) | 1983-10-28 | 1983-10-28 | 耐応力腐食割れ性にすぐれた高張力電縫鋼管の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6096725A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0382282U (enExample) * | 1989-12-15 | 1991-08-22 |
-
1983
- 1983-10-28 JP JP20100583A patent/JPS6096725A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS638166B2 (enExample) | 1988-02-22 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH11140580A (ja) | 低温靱性に優れた高強度鋼用の連続鋳造鋳片およびその製造法、および低温靱性に優れた高強度鋼 | |
| CN1989266B (zh) | 声各向异性小的焊接性优异的高强度钢板及其制造方法 | |
| JPS6145685B2 (enExample) | ||
| JPS6141968B2 (enExample) | ||
| JPH0320408A (ja) | 低温靭性に優れた高張力鋼材の製造法 | |
| JPH06128631A (ja) | 低温靱性の優れた高マンガン超高張力鋼の製造方法 | |
| JPH01116032A (ja) | 高強度・高靭性非調質鋼の製造方法 | |
| JPH04157117A (ja) | 母材および溶接部靭性の優れた圧延形鋼の製造方法 | |
| JPS6096725A (ja) | 耐応力腐食割れ性にすぐれた高張力電縫鋼管の製造方法 | |
| JPS602364B2 (ja) | 低温靭性にすぐれた非調質高張力鋼板の製造法 | |
| JP2706159B2 (ja) | 溶接性の良好な低降伏比高張力鋼の製造方法 | |
| JP2543282B2 (ja) | 靭性の優れた制御圧延形鋼の製造方法 | |
| JPH03207814A (ja) | 低降伏比高張力鋼板の製造方法 | |
| JPH09295067A (ja) | 優れた溶接金属部靱性を有する高強度ベンド管の製造法 | |
| JPS6256523A (ja) | 溶接性付与高強度レ−ルの製造法 | |
| JPS62970B2 (enExample) | ||
| JPS59153841A (ja) | 一様な強度を有する高張力電縫鋼管の製造方法 | |
| JPS63145711A (ja) | 低温靭性にすぐれる高張力鋼板の製造方法 | |
| JPH0247525B2 (enExample) | ||
| JP2001158936A (ja) | 耐水素誘起割れ性に優れた薄肉鋼板およびその製造方法 | |
| JPS6046318A (ja) | 耐硫化物割れ性の優れた鋼の製造方法 | |
| JPH09263831A (ja) | 低温靭性の優れた極厚高強度ベンド管の製造法 | |
| JPS5835579B2 (ja) | 溶接金属の高靭性化方法 | |
| JPH0116283B2 (enExample) | ||
| JPS60174820A (ja) | 低温じん性及び大入熱溶接性が優れた調質高張力鋼の製造方法 |