JPS6081764A - 即用式密閉形鉛蓄電池 - Google Patents
即用式密閉形鉛蓄電池Info
- Publication number
- JPS6081764A JPS6081764A JP58188820A JP18882083A JPS6081764A JP S6081764 A JPS6081764 A JP S6081764A JP 58188820 A JP58188820 A JP 58188820A JP 18882083 A JP18882083 A JP 18882083A JP S6081764 A JPS6081764 A JP S6081764A
- Authority
- JP
- Japan
- Prior art keywords
- electrolyte
- storage battery
- battery
- sealed lead
- ready
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/06—Lead-acid accumulators
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Sealing Battery Cases Or Jackets (AREA)
- Filling, Topping-Up Batteries (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58188820A JPS6081764A (ja) | 1983-10-08 | 1983-10-08 | 即用式密閉形鉛蓄電池 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58188820A JPS6081764A (ja) | 1983-10-08 | 1983-10-08 | 即用式密閉形鉛蓄電池 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6081764A true JPS6081764A (ja) | 1985-05-09 |
| JPH0443385B2 JPH0443385B2 (enrdf_load_stackoverflow) | 1992-07-16 |
Family
ID=16230385
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58188820A Granted JPS6081764A (ja) | 1983-10-08 | 1983-10-08 | 即用式密閉形鉛蓄電池 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6081764A (enrdf_load_stackoverflow) |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5534611U (enrdf_load_stackoverflow) * | 1978-08-25 | 1980-03-06 |
-
1983
- 1983-10-08 JP JP58188820A patent/JPS6081764A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5534611U (enrdf_load_stackoverflow) * | 1978-08-25 | 1980-03-06 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0443385B2 (enrdf_load_stackoverflow) | 1992-07-16 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US3855000A (en) | Air depolarization primary cell and process for production thereof | |
| US4576879A (en) | Sealed lead acid battery | |
| JPS6081764A (ja) | 即用式密閉形鉛蓄電池 | |
| JP2002008634A (ja) | 電 池 | |
| JPH0471309B2 (enrdf_load_stackoverflow) | ||
| JPH0531814Y2 (enrdf_load_stackoverflow) | ||
| JPH0517814Y2 (enrdf_load_stackoverflow) | ||
| JPS61171061A (ja) | 円筒形電池の真空注液方法 | |
| JPS63152856A (ja) | 蓄電池の電解液注液装置 | |
| JPH0580104B2 (enrdf_load_stackoverflow) | ||
| JPH0621172Y2 (ja) | 密閉型電池 | |
| JPH0322859Y2 (enrdf_load_stackoverflow) | ||
| JPH0218926Y2 (enrdf_load_stackoverflow) | ||
| JPH0218927Y2 (enrdf_load_stackoverflow) | ||
| JPH05205767A (ja) | 密閉形鉛蓄電池 | |
| JPH0538534Y2 (enrdf_load_stackoverflow) | ||
| JPH0525178Y2 (enrdf_load_stackoverflow) | ||
| JPH0735304Y2 (ja) | 密閉形鉛蓄電池 | |
| JPH074771Y2 (ja) | 蓄電池用電解液容器 | |
| JP2959099B2 (ja) | 密閉形鉛蓄電池の製造方法 | |
| JPS62103989A (ja) | 密閉鉛蓄電池 | |
| JPH0877984A (ja) | 蓄電池 | |
| JPH0652884A (ja) | 密閉形鉛蓄電池 | |
| JPH062218Y2 (ja) | 蓄電池 | |
| JPH0193066A (ja) | 密閉形鉛蓄電池の製造法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |