JPS60146812A - Thickening and gelling composition - Google Patents

Thickening and gelling composition

Info

Publication number
JPS60146812A
JPS60146812A JP59001588A JP158884A JPS60146812A JP S60146812 A JPS60146812 A JP S60146812A JP 59001588 A JP59001588 A JP 59001588A JP 158884 A JP158884 A JP 158884A JP S60146812 A JPS60146812 A JP S60146812A
Authority
JP
Japan
Prior art keywords
thickening
oil
phospholipid
polyhydric alcohol
agent composition
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP59001588A
Other languages
Japanese (ja)
Inventor
Shunji Yamada
俊二 山田
Satoru Nakada
悟 中田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nonogawa Shoji Ltd
Original Assignee
Nonogawa Shoji Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nonogawa Shoji Ltd filed Critical Nonogawa Shoji Ltd
Priority to JP59001588A priority Critical patent/JPS60146812A/en
Publication of JPS60146812A publication Critical patent/JPS60146812A/en
Pending legal-status Critical Current

Abstract

PURPOSE:A composition that is composed of phospholipid and polyhydric alcohol to thicken and gelatinize oil which is used in drugs and cosmetics, thus making it hydrophilic and giving good feeling, when applied. CONSTITUTION:Phospholipid and polyhydric alcohol are used to give the objective composition for thickening and gelatinize oil preparation. Soybean and yolk phospholipids and their hydrogenated products are used as phospholipid, and, as polyhydric alcohol, alkylene glycol, polyalkylene glycol, glycerol, polyglycerol and sugar alcohol are used. They are used so that the phospholipid is included in the polyhydric alcohol by 0.05-50wt%, preferably 0.5-35wt%. Gelatinization is effected by adding the phospholipid to the polyhydric alcohol to form a homogeneous solution and adding the oil to the composition under stirring. The oil can be added as much as 8-10 times the quantity of the composition.

Description

【発明の詳細な説明】 本発明はリン脂質及び多価アルコールから成ることを特
徴とする油剤の増粘−ゲル化剤組成物tこ関するもので
ある。
DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a thickening and gelling agent composition for oils, which is characterized by comprising a phospholipid and a polyhydric alcohol.

一般tこ医薬品や化粧品に使用される油剤は、液状のも
のがほとんどであり、これらを粘度調整することeこよ
り、使用形態を変えることは非常tこ興味あることであ
る。また従来の油の多い製品のほとんどは親油性であり
、最近の傾向として親水性の製品が望まれてきたが、こ
うした製品はほとんど見られなかった。本発明者等はリ
ン脂質と多価アルコール1こよって調整した増粘−ゲル
化剤組成物が、極めて容易にかつ良好tこ油剤を増粘、
ゲル化し、製品価値の高いものが得られることを見い出
した。得られた製品は親水性であり、使用感eこ優れて
いる特性を持つている。さらEこ本発明の増粘−ゲル化
剤組成物は、油剤の量を調節することにより、容易tこ
粘度調整ができることを見い出した。
Most of the oils used in general medicines and cosmetics are liquid, and it is very interesting to change their usage form by adjusting their viscosity. Furthermore, most conventional oil-rich products are lipophilic, and although there has been a recent trend toward hydrophilic products, such products have rarely been seen. The present inventors have discovered that a thickening-gelling agent composition prepared using phospholipids and a polyhydric alcohol can thicken oil agents very easily and successfully.
It has been found that it can be gelled and a product with high product value can be obtained. The resulting product is hydrophilic and has excellent properties such as ease of use. Furthermore, it has been found that the viscosity of the thickening-gelling agent composition of the present invention can be easily adjusted by adjusting the amount of oil.

本発明tこ用いられるリン脂質は、大豆リン脂質および
卵黄リン脂質であり、これらを水添した水添大豆リン脂
質および水添卵黄リン脂質も同様tこ用いることが可能
である。
The phospholipids used in the present invention are soybean phospholipids and egg yolk phospholipids, and hydrogenated soybean phospholipids and hydrogenated egg yolk phospholipids obtained by hydrogenating these can also be used.

大豆リン脂質の主成分は、ホスファチジルコリン、ホス
ファチジルエタノールアミン、ホスファチジルイノシト
ールであり、卵黄リン脂質の主成分は、ホスファチジル
コリン、ホスファチジルエタノールアミン、リゾホスフ
ァチジルコリンである。本発明者等はこれらを分割し、
鋭意研究の結果、それぞれの化合物が多価アルコールを
含むこと1こより、油剤を増粘、ゲル化することを見い
出した。
The main components of soybean phospholipids are phosphatidylcholine, phosphatidylethanolamine, and phosphatidylinositol, and the main components of egg yolk phospholipids are phosphatidylcholine, phosphatidylethanolamine, and lysophosphatidylcholine. The inventors divided these into
As a result of intensive research, it was discovered that each compound contains polyhydric alcohol, which thickens and gels the oil.

本発明tこ用いられるリン脂質の多価アルコール溶液中
の濃度としては、005〜50重景%であれば増粘、ゲ
ル化は可能で、好ましくは0.5〜35重量%である。
The concentration of the phospholipid used in the present invention in the polyhydric alcohol solution is 0.05 to 50% by weight, allowing for thickening and gelling, and preferably 0.5 to 35% by weight.

リン脂質が005重量%未満あるいは50重量係以上の
場合においては、リン脂質−多価アルコールの均−系の
中1こ油剤を均一に加えることができない為に増粘、ゲ
ル化力jおこらず、本発明tこおいては不適である。
If the phospholipid content is less than 0.05% by weight or more than 50% by weight, thickening and gelling power will not occur because the oil agent cannot be added uniformly to the homogeneous phospholipid-polyhydric alcohol system. , is not suitable for the present invention.

本発明1こ用いられる多価アルコールとしては、水溶性
で1分子中に水酸基を2個以上有するものの中から自由
に選択することができる。例えばエチレングリコール、
ジエチレングリコール、それ以上のポリエチレングリコ
ール類、プロピレングリコール、ジプロピレングリコー
ル、ソれ以上のポリプロピレングリコール類、グリセリ
ン、ジグリセリン、それ以上のポリグリセリン類、マル
チトール、ソルビトール、キシリトール、マンニトール
等の糖アルコール、グリコース、シュークロース、フラ
クトース、マルトース、ガラクトース等の糖類等である
The polyhydric alcohol used in the present invention can be freely selected from those that are water-soluble and have two or more hydroxyl groups in one molecule. For example, ethylene glycol
Diethylene glycol, higher polyethylene glycols, propylene glycol, dipropylene glycol, higher polypropylene glycols, glycerin, diglycerin, higher polyglycerins, maltitol, sorbitol, xylitol, mannitol and other sugar alcohols, glycose , sucrose, fructose, maltose, galactose, and other sugars.

本発明の増粘−ゲル化剤組成物によって増粘、ゲル化で
きる油剤は非常eこ多くあり、100℃以下で液状又は
ペースト状tこなるものであれば、はとんどすべてのも
のが可能である。例えば流動パラフィン、スクワラン等
の炭化水素類、ミンク油、ホホバ油、アボカド油等の動
植物油、セチルイソオクタノエート、イソプロピルミリ
ステート、インセチルミリステート等のエステル類、セ
チルアルコール、イソステアリルアルコール、ベヘニル
アルコール等の高級アルコール類、ステアリン酸、パル
ミチン酸、ベヘニン酸等の高級脂肪酸類、メチルポリシ
ロキサン、メチルフェニルポリシロキサン、環状ジメチ
ルポリシロキサン、その他のシリコン誘導体等である。
There are a large number of oils that can be thickened and gelled by the thickening-gelling agent composition of the present invention, and almost all of them can be used as long as they become liquid or paste at temperatures below 100°C. It is possible. For example, hydrocarbons such as liquid paraffin and squalane, animal and vegetable oils such as mink oil, jojoba oil, and avocado oil, esters such as cetyl isooctanoate, isopropyl myristate, and incetyl myristate, cetyl alcohol, isostearyl alcohol, These include higher alcohols such as behenyl alcohol, higher fatty acids such as stearic acid, palmitic acid, and behenic acid, methylpolysiloxane, methylphenylpolysiloxane, cyclic dimethylpolysiloxane, and other silicon derivatives.

本発明における増粘、ゲル化の方法としては、まず多価
アルコールtこリン脂質を加えて均一に混合溶解し、増
粘−ゲル化剤組成物を調整する。
As a method for thickening and gelling in the present invention, first, a polyhydric alcohol and a phospholipid are added and uniformly mixed and dissolved to prepare a thickening-gelling agent composition.

次いでこの増粘−ゲル化剤組成物tこ攪拌しながら油剤
を加え製品とする。油剤を多く加えていくにつれて系の
粘度は上昇して流動性を失うという現象が見られた。油
剤の増粘、ゲル化を行なう場合、油剤は増粘−ゲル化剤
組成物1こ対して、重量で8〜10倍量まで加えること
ができる。
Next, an oil agent is added to this thickening/gelling agent composition while stirring to form a product. As more oil was added, the viscosity of the system increased and fluidity was lost. When thickening or gelling an oil agent, the oil agent can be added in an amount of 8 to 10 times the weight of one thickening-gelling agent composition.

尚、本発明tこおいて、製品の均質安定化、粘度調整等
の目的で更に水を添加してもよい。
In the present invention, water may be further added for the purpose of stabilizing the homogeneity of the product, adjusting the viscosity, etc.

次1こ本発明の実施例を例示して、本発明を具体的1こ
説明する。尚、実施例中の%は重量%である。
Next, the present invention will be specifically explained by illustrating one embodiment of the present invention. In addition, % in an example is weight %.

実施例1 親水性ゲルクレンジングクリーム 本発明増粘−ゲル化剤組成物 20% 流動パラフィン 6o% セチルイソオクタノエート 20% まずグリセリン1こ大豆リン脂質を加え、塞流tこて均
−tこ混合溶解し増粘−ゲル化剤組成物を調製した。次
いでこの増粘−ゲル化剤組成物を約70℃tこ加熱し、
攪拌しながら油剤を滴下すると半透明のゲル状のクレン
ジングクリームを得た。得られたクレンジングクリーム
は、ファンデーシコンの落ちが良く、また水洗性eこ優
れている。
Example 1 Hydrophilic gel cleansing cream Thickening-gelling agent composition of the present invention 20% Liquid paraffin 6% Cetyl iso-octanoate 20% First, 1 glycerin and soybean phospholipid were added, and the mixture was evaporated with a trowel. A thickening-gelling agent composition was prepared by mixing and dissolving. This thickening-gelling agent composition was then heated to about 70°C,
When the oil agent was added dropwise while stirring, a translucent gel-like cleansing cream was obtained. The resulting cleansing cream removes foundation easily and has excellent water washability.

実施例2 ナリシングオイル 本発明増粘−ゲル化剤組成物 30% スクワラン 60% ホホバ油 15% 七チルイソオクタノエート 20% 精製水 5% 実施例1と同様な方法tこより半透明の粘稠なナリシン
グオイルを得た。このナリシングオイルit 非’WE
 tこエモリエント効果が高い。
Example 2 Nourishing oil Thickening-gelling agent composition of the present invention 30% Squalane 60% Jojoba oil 15% Heptylisooctanoate 20% Purified water 5% A translucent viscosity was obtained by the same method as in Example 1. Obtained a thick nourishing oil. This Nourishing Oil It's Not We
It has a high emollient effect.

実施例3 ポマード 本発明増粘−ゲル化剤組成物 15% ヒマシ油 40% 流動パラフィン 40% セチルアルコール 5% 実施例1と同様な方法tこより半透明のゲル状のポマー
ドを得た。このポマードは整髪力が強く、水洗性がある
Example 3 Pomade Thickening-gelling agent composition of the present invention 15% Castor oil 40% Liquid paraffin 40% Cetyl alcohol 5% A translucent gel-like pomade was obtained in the same manner as in Example 1. This pomade has strong hair styling power and is washable.

実施例4 バスミルク 本発明増粘−ゲル化剤組成物 50% 卵黄リン脂質 5% グリセリン 80% ジエチレングリコール 15% イソプロピルミリステート 20傳 流動パラフイン 20% 精製水 10% 実施例1と同様な方法により半透明の粘稠なバスミルク
を得た。このバスミルクは浴槽中で容易eこ乳化する。
Example 4 Bath milk Thickening-gelling agent composition of the present invention 50% Egg yolk phospholipids 5% Glycerin 80% Diethylene glycol 15% Isopropyl myristate 20% Liquid paraffin 20% Purified water 10% A clear viscous bath milk was obtained. This bath milk easily emulsifies in the bathtub.

実施例5 サンオイル 本発明増粘−ゲル化剤組成物 25% オリーブ油 50% 流動パラフィン 20% イソステアリン酸 5% 実施例1と同様な方法?こより半透明の粘稠なサンオイ
ルを得た。
Example 5 Sunoil Thickening-gelling agent composition of the present invention 25% Olive oil 50% Liquid paraffin 20% Isostearic acid 5% Same method as in Example 1? A translucent and viscous sun oil was obtained from this.

Claims (5)

【特許請求の範囲】[Claims] (1)リン脂質及び多価アルフールから成ることを特徴
とする油剤の増粘−ゲル化剤組成物。
(1) A thickening-gelling agent composition for an oil agent, characterized by comprising a phospholipid and a polyhydric alfur.
(2)リン脂質が大豆又は鶏卵黄由来である、特許請求
の範囲第(1)項記載の増粘−ゲル化剤組成物。
(2) The thickening-gelling agent composition according to claim (1), wherein the phospholipid is derived from soybean or chicken egg yolk.
(3) 多価アルコールがアルキレングリコール、ポリ
アルキレンダリコール、グリセリン、ポリグリセリン、
糖アルコール、糖あるいはこれらの混合物である、特許
請求の範囲第(1)項記載の増粘−ゲル化剤組成物。
(3) Polyhydric alcohol is alkylene glycol, polyalkylene dalicol, glycerin, polyglycerin,
The thickening-gelling agent composition according to claim 1, which is a sugar alcohol, sugar, or a mixture thereof.
(4)油剤が炭化水素類、動植物油、エステル類、高級
アルコール類、高級脂肪酸類、シリコン類あるいはこれ
らの混合物である、特許請求の範囲第(1)項記載の増
粘−ゲル化剤組成物。
(4) The thickening-gelling agent composition according to claim (1), wherein the oil agent is a hydrocarbon, an animal or vegetable oil, an ester, a higher alcohol, a higher fatty acid, a silicone, or a mixture thereof. thing.
(5) 多価アルコール溶液中tこリン脂質が005〜
50重量%存在する、特許請求の範囲第(1)項記載の
増粘−ゲル化剤組成物。
(5) The phospholipid in the polyhydric alcohol solution is 005~
Thickening-gelling agent composition according to claim 1, present in an amount of 50% by weight.
JP59001588A 1984-01-09 1984-01-09 Thickening and gelling composition Pending JPS60146812A (en)