JPS59159966A - 応力除去焼なましによるじん性劣化が少ない大入熱溶接用調質高張力鋼 - Google Patents
応力除去焼なましによるじん性劣化が少ない大入熱溶接用調質高張力鋼Info
- Publication number
- JPS59159966A JPS59159966A JP3250383A JP3250383A JPS59159966A JP S59159966 A JPS59159966 A JP S59159966A JP 3250383 A JP3250383 A JP 3250383A JP 3250383 A JP3250383 A JP 3250383A JP S59159966 A JPS59159966 A JP S59159966A
- Authority
- JP
- Japan
- Prior art keywords
- weight
- less
- heat input
- steel
- input welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Articles (AREA)
- Heat Treatment Of Steel (AREA)
- Arc Welding In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3250383A JPS59159966A (ja) | 1983-02-28 | 1983-02-28 | 応力除去焼なましによるじん性劣化が少ない大入熱溶接用調質高張力鋼 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3250383A JPS59159966A (ja) | 1983-02-28 | 1983-02-28 | 応力除去焼なましによるじん性劣化が少ない大入熱溶接用調質高張力鋼 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59159966A true JPS59159966A (ja) | 1984-09-10 |
| JPH0351780B2 JPH0351780B2 (enExample) | 1991-08-07 |
Family
ID=12360787
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3250383A Granted JPS59159966A (ja) | 1983-02-28 | 1983-02-28 | 応力除去焼なましによるじん性劣化が少ない大入熱溶接用調質高張力鋼 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59159966A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61190016A (ja) * | 1985-02-19 | 1986-08-23 | Kobe Steel Ltd | 大入熱溶接構造用鋼の製造方法 |
| JPS6286119A (ja) * | 1985-10-09 | 1987-04-20 | Kobe Steel Ltd | 耐溶接割れ性のすぐれた大入熱溶接構造用鋼の製造方法 |
-
1983
- 1983-02-28 JP JP3250383A patent/JPS59159966A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61190016A (ja) * | 1985-02-19 | 1986-08-23 | Kobe Steel Ltd | 大入熱溶接構造用鋼の製造方法 |
| JPS6286119A (ja) * | 1985-10-09 | 1987-04-20 | Kobe Steel Ltd | 耐溶接割れ性のすぐれた大入熱溶接構造用鋼の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0351780B2 (enExample) | 1991-08-07 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR100260578B1 (ko) | 입열 500kj/cm이상의 대입열 용접용강 및 그 제조방법 | |
| JPS6352090B2 (enExample) | ||
| JP3762700B2 (ja) | 成形性と化成処理性に優れた高強度鋼板およびその製造方法 | |
| JPS61139648A (ja) | 強度及び溶接性に優れた低炭素極厚鋼板 | |
| JP2500948B2 (ja) | 溶接性の優れた厚手80kgf/mm2 級高張力鋼の製造法 | |
| JP2671732B2 (ja) | 溶接性に優れた高張力鋼の製造方法 | |
| JPS6033340A (ja) | 溶接性の優れた低炭素極厚鋼板 | |
| JPH0351780B2 (enExample) | ||
| JP2634961B2 (ja) | 溶接性の優れた80kgf/mm2級高張力鋼の製造法 | |
| JPH0329861B2 (enExample) | ||
| JP2546888B2 (ja) | 溶接性、靭性の優れた高張力鋼板の製造方法 | |
| JP2529042B2 (ja) | 冷間成形による建築用低降伏比鋼管の製造法 | |
| JP3007246B2 (ja) | 溶接性の優れた降伏比80%以下の590N/mm2級高張力鋼の製造法 | |
| JPH06192729A (ja) | 溶接性の優れた低温用鋼の製造方法 | |
| JPS62149845A (ja) | 溶接部じん性のすぐれたCu析出型鋼材とその製造方法 | |
| JP3007247B2 (ja) | 溶接性の優れた降伏比80%以下のTS590N/mm2級高張力鋼の製造法 | |
| JPH02163342A (ja) | 大人熱溶接用高張力鋼 | |
| JPS61295320A (ja) | 引張強さ58〜85Kgf/mm↑2の高強度鋼の製造方法 | |
| JP4967373B2 (ja) | 非調質高張力鋼板およびその製造方法 | |
| JPH06340924A (ja) | 低降伏比高張力鋼の製造方法 | |
| JP3114493B2 (ja) | 厚鋼板の製造方法 | |
| JPH0841582A (ja) | 大入熱溶接部靱性の優れた低合金耐熱鋼 | |
| JPH045741B2 (enExample) | ||
| JPH02217437A (ja) | 冷間加工用綱 | |
| JPH0762489A (ja) | アーク溶接部の疲労特性に優れた高張力鋼 |