JPS5895678A - 耐熱性セラミツクコ−テイング方法 - Google Patents
耐熱性セラミツクコ−テイング方法Info
- Publication number
- JPS5895678A JPS5895678A JP56191824A JP19182481A JPS5895678A JP S5895678 A JPS5895678 A JP S5895678A JP 56191824 A JP56191824 A JP 56191824A JP 19182481 A JP19182481 A JP 19182481A JP S5895678 A JPS5895678 A JP S5895678A
- Authority
- JP
- Japan
- Prior art keywords
- heat
- resistant ceramic
- layer
- cooling
- cooling holes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Turbine Rotor Nozzle Sealing (AREA)
- Coating By Spraying Or Casting (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56191824A JPS5895678A (ja) | 1981-12-01 | 1981-12-01 | 耐熱性セラミツクコ−テイング方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56191824A JPS5895678A (ja) | 1981-12-01 | 1981-12-01 | 耐熱性セラミツクコ−テイング方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5895678A true JPS5895678A (ja) | 1983-06-07 |
| JPS6153424B2 JPS6153424B2 (cg-RX-API-DMAC7.html) | 1986-11-18 |
Family
ID=16281125
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56191824A Granted JPS5895678A (ja) | 1981-12-01 | 1981-12-01 | 耐熱性セラミツクコ−テイング方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5895678A (cg-RX-API-DMAC7.html) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6024954A (ja) * | 1983-07-20 | 1985-02-07 | Canon Inc | インクジエツトプリンタのインク残量検知方法 |
| JPS61174385A (ja) * | 1984-09-10 | 1986-08-06 | Hitachi Ltd | セラミツク被覆耐熱部材及びその製造方法 |
| JPH03140451A (ja) * | 1989-10-27 | 1991-06-14 | Shinagawa Refract Co Ltd | 溶射基材の冷却装置 |
| JPH03223455A (ja) * | 1990-01-29 | 1991-10-02 | Sugitani Kinzoku Kogyo Kk | セラミック溶射材料 |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4985602A (cg-RX-API-DMAC7.html) * | 1972-01-25 | 1974-08-16 | ||
| JPS509104A (cg-RX-API-DMAC7.html) * | 1973-05-09 | 1975-01-30 | ||
| JPS5547229B2 (cg-RX-API-DMAC7.html) * | 1972-03-29 | 1980-11-28 |
-
1981
- 1981-12-01 JP JP56191824A patent/JPS5895678A/ja active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4985602A (cg-RX-API-DMAC7.html) * | 1972-01-25 | 1974-08-16 | ||
| JPS5547229B2 (cg-RX-API-DMAC7.html) * | 1972-03-29 | 1980-11-28 | ||
| JPS509104A (cg-RX-API-DMAC7.html) * | 1973-05-09 | 1975-01-30 |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6024954A (ja) * | 1983-07-20 | 1985-02-07 | Canon Inc | インクジエツトプリンタのインク残量検知方法 |
| JPS61174385A (ja) * | 1984-09-10 | 1986-08-06 | Hitachi Ltd | セラミツク被覆耐熱部材及びその製造方法 |
| JPH03140451A (ja) * | 1989-10-27 | 1991-06-14 | Shinagawa Refract Co Ltd | 溶射基材の冷却装置 |
| JPH03223455A (ja) * | 1990-01-29 | 1991-10-02 | Sugitani Kinzoku Kogyo Kk | セラミック溶射材料 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6153424B2 (cg-RX-API-DMAC7.html) | 1986-11-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6296447B1 (en) | Gas turbine component having location-dependent protective coatings thereon | |
| US6387527B1 (en) | Method of applying a bond coating and a thermal barrier coating on a metal substrate, and related articles | |
| US4328285A (en) | Method of coating a superalloy substrate, coating compositions, and composites obtained therefrom | |
| US5894053A (en) | Process for applying a metallic adhesion layer for ceramic thermal barrier coatings to metallic components | |
| JP3258599B2 (ja) | 断熱バリヤコーティングシステム | |
| JP4279104B2 (ja) | マスキング用囲いで部分的にマスクされたガスタービン翼を気相アルミナイド処理する方法 | |
| US6361878B2 (en) | Roughened bond coat and method for producing using a slurry | |
| JPH0715141B2 (ja) | 耐熱部品 | |
| JP2007255415A (ja) | 焼結されたプリフォームを有するhpt側壁の修理方法 | |
| CZ302983B6 (cs) | Zpusob aplikování vazebního povlaku odolného pri vysokých teplotách, a s tímto zpusobem související kašovité suspenze a výrobky | |
| US6623790B2 (en) | Method of adjusting the size of cooling holes of a gas turbine component | |
| CN101205833A (zh) | 隔热涂层 | |
| CN100510153C (zh) | Ni基合金制部件的修补方法 | |
| US7422771B2 (en) | Methods for applying a hybrid thermal barrier coating | |
| JP2008063657A (ja) | 高温耐フレッティング摩耗コーティングを施工する方法 | |
| JP4579383B2 (ja) | 緻密セラミック遮熱皮膜を表面から除去する方法 | |
| US6521053B1 (en) | In-situ formation of a protective coating on a substrate | |
| JP3219594B2 (ja) | 高温酸化防止用遮熱コーティング方法 | |
| US6190785B1 (en) | Spray coating powder material and high-temperature components coated therewith | |
| US4503122A (en) | High-temperature protection layer | |
| JPS6153424B2 (cg-RX-API-DMAC7.html) | ||
| JP2008002468A (ja) | 耐酸化性金属リン酸塩皮膜 | |
| US6656605B1 (en) | Low-sulfur article coated with a platinum-group metal and a ceramic layer, and its preparation | |
| JP4643546B2 (ja) | アルミナイド表面上にボンディングコート及び断熱皮膜を施工する方法 | |
| JPH10110279A (ja) | セラミック被覆耐熱部材とその用途及びガスタービン |