JPS5858198A - ヘドロまたは汚泥の固化方法 - Google Patents

ヘドロまたは汚泥の固化方法

Info

Publication number
JPS5858198A
JPS5858198A JP56156417A JP15641781A JPS5858198A JP S5858198 A JPS5858198 A JP S5858198A JP 56156417 A JP56156417 A JP 56156417A JP 15641781 A JP15641781 A JP 15641781A JP S5858198 A JPS5858198 A JP S5858198A
Authority
JP
Japan
Prior art keywords
sludge
alkali metal
blast furnace
hydroxide
granulated slag
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP56156417A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0124559B2 (enrdf_load_html_response
Inventor
Hiroshi Isozaki
磯崎 啓
Koji Nakagawa
中川 晃次
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Denka Co Ltd
Original Assignee
Denki Kagaku Kogyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Denki Kagaku Kogyo KK filed Critical Denki Kagaku Kogyo KK
Priority to JP56156417A priority Critical patent/JPS5858198A/ja
Publication of JPS5858198A publication Critical patent/JPS5858198A/ja
Publication of JPH0124559B2 publication Critical patent/JPH0124559B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Processing Of Solid Wastes (AREA)
  • Treatment Of Sludge (AREA)
JP56156417A 1981-10-01 1981-10-01 ヘドロまたは汚泥の固化方法 Granted JPS5858198A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP56156417A JPS5858198A (ja) 1981-10-01 1981-10-01 ヘドロまたは汚泥の固化方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP56156417A JPS5858198A (ja) 1981-10-01 1981-10-01 ヘドロまたは汚泥の固化方法

Publications (2)

Publication Number Publication Date
JPS5858198A true JPS5858198A (ja) 1983-04-06
JPH0124559B2 JPH0124559B2 (enrdf_load_html_response) 1989-05-12

Family

ID=15627292

Family Applications (1)

Application Number Title Priority Date Filing Date
JP56156417A Granted JPS5858198A (ja) 1981-10-01 1981-10-01 ヘドロまたは汚泥の固化方法

Country Status (1)

Country Link
JP (1) JPS5858198A (enrdf_load_html_response)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100436396B1 (ko) * 2002-01-29 2004-06-16 주식회사 포스코건설 유기성슬러지의 고형화, 안정화를 통한 자원화 방법 및이를 위한 장치
WO2005039702A1 (en) * 2003-10-28 2005-05-06 Nanyang Technological University A method and composition for stabilizing waste mercury compounds using ladle furnace slag

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100436396B1 (ko) * 2002-01-29 2004-06-16 주식회사 포스코건설 유기성슬러지의 고형화, 안정화를 통한 자원화 방법 및이를 위한 장치
WO2005039702A1 (en) * 2003-10-28 2005-05-06 Nanyang Technological University A method and composition for stabilizing waste mercury compounds using ladle furnace slag

Also Published As

Publication number Publication date
JPH0124559B2 (enrdf_load_html_response) 1989-05-12

Similar Documents

Publication Publication Date Title
Wang et al. Hydration behavior and immobilization mechanism of MgO–SiO2–H2O cementitious system blended with MSWI fly ash
JP5946107B2 (ja) セメント組成物の製造方法
Chindaprasirt et al. Characterizations of FBC/PCC fly ash geopolymeric composites
JP6137850B2 (ja) 水硬性組成物
JP5800387B2 (ja) 土質改良材
CN104338730B (zh) 含有重金属类的固体废弃物的无害化方法
JPS63289498A (ja) 放射性廃棄物の固化剤
JP3970201B2 (ja) セメント組成物、コーティング材料、及びそれを用いた遮塩方法
Zhang et al. Preparation and hydration process of copper slag-granulated blast furnace slag-cement composites
JPH0337145A (ja) セメント用急結剤
JP6957922B2 (ja) 石炭灰硬化物
JP2008029937A (ja) 副生物の処理方法
JP6292257B2 (ja) 脱硫スラグを用いた水和固化体
JPH10165920A (ja) 泥状物の団粒化剤、それを用いた固化剤
JPS5858198A (ja) ヘドロまたは汚泥の固化方法
JPH0214308B2 (enrdf_load_html_response)
JP5015435B2 (ja) 固化材
GB2077251A (en) Slag Cement Composition
JP2716758B2 (ja) セメント混和材
ES2592953B1 (es) Material cementante a partir de mezclas de residuos y/o subproductos industriales y procedimiento de fabricación
JPS5953229B2 (ja) 石炭灰を主原料とする硬化体の製造方法
JP2503235B2 (ja) 硬化促進材
JP3549635B2 (ja) 混合セメントの刺激材及び混合セメント組成物
JPH0339984B2 (enrdf_load_html_response)
Ponomarenko Magazine of Civil Engineering