JPS5845927B2 - Manufacturing method of artificial decorative veneer - Google Patents
Manufacturing method of artificial decorative veneerInfo
- Publication number
- JPS5845927B2 JPS5845927B2 JP55010905A JP1090580A JPS5845927B2 JP S5845927 B2 JPS5845927 B2 JP S5845927B2 JP 55010905 A JP55010905 A JP 55010905A JP 1090580 A JP1090580 A JP 1090580A JP S5845927 B2 JPS5845927 B2 JP S5845927B2
- Authority
- JP
- Japan
- Prior art keywords
- adhesive
- veneers
- manufacturing
- flitch
- veneer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【発明の詳細な説明】
本発明は、人工化粧単板の製造方法に関するものである
。DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a method for manufacturing artificially decorated veneers.
従来の人工化粧単板の製造方法にあっては接着剤が塗布
された単板を複数枚積層すると共に上下の上型と下型と
の間に上記の積層した単板を挾んで圧締してフリッチを
形成し、このフリッチをスライスして人工化粧単板を形
成している。In the conventional manufacturing method of artificial decorative veneers, multiple veneers coated with adhesive are laminated, and the laminated veneers are sandwiched and pressed between upper and lower molds. The flitch is then sliced to form an artificial decorative veneer.
しかしながら従来例にあっては、接着剤の硬化が遅いの
でフリッチを形成して上型と下型を開いたとき単板が剥
離したりするという欠点があった。However, in the conventional example, since the adhesive hardens slowly, a flitch is formed and the veneer may peel off when the upper and lower molds are opened.
本発明は叙述の点に鑑みてなされたものであって、圧締
時接着剤を湿潤させて硬化を早め製造時間の短縮を計る
ことのできる人工化粧単板の製造方法を提供することを
目的とするものである。The present invention has been made in view of the above-mentioned points, and an object of the present invention is to provide a method for manufacturing artificial decorative veneers that can accelerate curing by moistening the adhesive during pressing, thereby shortening the manufacturing time. That is.
以下本発明を図面により詳細に説明する。The present invention will be explained in detail below with reference to the drawings.
第1図及び第2図のようにプレスの下型1に多数のノズ
ル孔2を穿孔し、このノズル孔2にホース3を接続し、
下型1のノズル孔2から高圧の湿り蒸気が噴出するよう
にしである。As shown in FIGS. 1 and 2, a large number of nozzle holes 2 are bored in the lower die 1 of the press, and a hose 3 is connected to the nozzle holes 2.
High pressure wet steam is blown out from the nozzle hole 2 of the lower mold 1.
単板は原木をロータリレースにて切削したり、又スライ
ス切削したものである。Veneer is made by cutting raw wood with a rotary race or cutting it into slices.
ウレタン接着剤のような接着剤(接着剤の塗布量は例え
ば100〜2oor/rr?)を塗布された状態の単板
4を数10枚(例えば30〜50枚)プレスの上型5と
下型1の間に積層し、然るのち例えば10〜20驚のプ
レス圧にて圧締すると共に下型1のノズル孔2より湿り
蒸気を吹き付けて単板4の接着剤の硬化を図り、薄肉の
フリッチ素体6を形成する。Several tens (for example, 30 to 50 pieces) of veneer 4 coated with an adhesive such as urethane adhesive (the amount of adhesive applied is, for example, 100 to 2 oor/rr) are pressed into the upper mold 5 and the lower part of the press. The veneer 4 is laminated between the molds 1, and then pressed together with a press pressure of, for example, 10 to 20 degrees, and wet steam is blown from the nozzle hole 2 of the lower mold 1 to harden the adhesive of the veneer 4. A flitch element body 6 is formed.
この場合湿り蒸気を吹き付けることにより、接着剤の硬
化を5分短縮することができて生産性の向上を図ること
ができるものである。In this case, by spraying wet steam, the curing time of the adhesive can be shortened by 5 minutes, thereby improving productivity.
接着剤が完全に硬化すると上型5を引き上げ、下型1上
に新たな接着剤を塗布した単板4を数10枚積層して再
度圧締を行ない、2倍厚の変形フリッチ素体6を形成す
る。When the adhesive is completely cured, the upper mold 5 is lifted up, several dozen veneers 4 coated with new adhesive are laminated on the lower mold 1, and pressed together again to form a double-thick deformed flitch element 6. form.
この場合フリッチ素体6は上型5の下面に接着しており
、フリッチ素体6は上型5と共に上昇し、単板4の下型
1への積層が簡単になるようにしである。In this case, the flitch element body 6 is adhered to the lower surface of the upper die 5, and the flitch element body 6 rises together with the upper die 5, so that the veneer 4 can be easily laminated onto the lower die 1.
また湿り蒸気の噴出により、接着剤の硬化を完全にしで
あるため、上型5の上昇時に単板4が落下したりすると
いうことがないものである。Furthermore, since the adhesive is completely cured by the ejection of wet steam, there is no possibility that the veneer 4 will fall when the upper die 5 is raised.
このような作業(第3図口〜二の作業)を繰返して次第
に単板4を積み増し、最終的に所定層のフリッチ8(第
3図ホ)を形成する。By repeating such operations (operations 2 to 3 in Figure 3), the number of veneers 4 is gradually increased, and finally a predetermined layer of flitches 8 (FIG. 3, E) is formed.
然るのちこのフリッチ8をスライスして第3図へのよう
な年輪となる部分の層が明確な太い線となって表われる
人工化粧単板8を形成する。Afterwards, this flitch 8 is sliced to form an artificial decorative veneer 8 in which the layer of the part that will become the annual ring appears as a clear thick line as shown in Fig. 3.
本発明は叙述の如く積層した単板を上型と下型とで圧締
する際下型に設けた多数個のノズル孔より高圧の湿り蒸
気を吹付は湿潤させて接着剤を硬化させているので、複
数層の接着剤層を同時に湿潤させて硬化を早めることが
できると共に圧締するとき同時に湿潤させるので湿潤さ
せるのに特別な工程を要しないものであって、接着剤の
硬化を早めることができる上、製造時間の短縮化が計れ
るものである。As described above, when the laminated veneer is pressed between the upper mold and the lower mold, high-pressure wet steam is sprayed from multiple nozzle holes provided in the lower mold to moisten and harden the adhesive. Therefore, multiple adhesive layers can be moistened at the same time to accelerate curing, and since they are moistened at the same time when compressed, no special process is required for wetting, and the adhesive can be cured quickly. In addition to this, the manufacturing time can be shortened.
第1図は本発明の実施例で使用するプレスの下型の局部
断面斜視図、第2図は本発明の実施例におけるプレス状
態を示す縦断面図、第3図イルへは本発明の実施例の作
業順序を示す説明図である。Fig. 1 is a partial cross-sectional perspective view of the lower die of a press used in an embodiment of the present invention, Fig. 2 is a longitudinal sectional view showing a press state in an embodiment of the present invention, and Fig. 3 is a perspective view of a lower die of a press used in an embodiment of the present invention. It is an explanatory diagram showing an example work order.
Claims (1)
下の上型と下型との間に上記の積層した単板を挾んで圧
締してフリッチを形成し、このフリッチをスライスして
人工化粧単板を形成する人工化粧単板の製造方法におい
て、積層した単板を上型と下型とで圧締する際下型に設
けた多数個のノズル孔より高圧の湿り蒸気を吹付けて湿
潤させて接着剤を硬化させることを特徴とする人工化粧
単板の製造方法。1 Laminate multiple veneers coated with adhesive, sandwich and press the laminated veneers between the upper and lower upper and lower molds to form a flitch, and slice this flitch. In the method for manufacturing artificial decorative veneers, when the laminated veneers are pressed between an upper mold and a lower mold, high-pressure moist steam is sprayed from multiple nozzle holes provided in the lower mold. A method for producing an artificial decorative veneer, characterized by curing the adhesive by moistening the adhesive.