JPS5845288A - 石炭・水スラリ−流動性改良法 - Google Patents
石炭・水スラリ−流動性改良法Info
- Publication number
- JPS5845288A JPS5845288A JP14398581A JP14398581A JPS5845288A JP S5845288 A JPS5845288 A JP S5845288A JP 14398581 A JP14398581 A JP 14398581A JP 14398581 A JP14398581 A JP 14398581A JP S5845288 A JPS5845288 A JP S5845288A
- Authority
- JP
- Japan
- Prior art keywords
- coal
- slurry
- fluidity
- water slurry
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Liquid Carbonaceous Fuels (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14398581A JPS5845288A (ja) | 1981-09-14 | 1981-09-14 | 石炭・水スラリ−流動性改良法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14398581A JPS5845288A (ja) | 1981-09-14 | 1981-09-14 | 石炭・水スラリ−流動性改良法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5845288A true JPS5845288A (ja) | 1983-03-16 |
| JPH0132876B2 JPH0132876B2 (enrdf_load_html_response) | 1989-07-10 |
Family
ID=15351622
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14398581A Granted JPS5845288A (ja) | 1981-09-14 | 1981-09-14 | 石炭・水スラリ−流動性改良法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5845288A (enrdf_load_html_response) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN102391901A (zh) * | 2011-07-12 | 2012-03-28 | 石河子市明升科技有限责任公司 | 一种用于兰炭粉生产型焦的粘合剂及其制备方法 |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5834896A (ja) * | 1981-08-26 | 1983-03-01 | Nippon Oil & Fats Co Ltd | 石炭−水スラリ−用添加剤 |
-
1981
- 1981-09-14 JP JP14398581A patent/JPS5845288A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5834896A (ja) * | 1981-08-26 | 1983-03-01 | Nippon Oil & Fats Co Ltd | 石炭−水スラリ−用添加剤 |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN102391901A (zh) * | 2011-07-12 | 2012-03-28 | 石河子市明升科技有限责任公司 | 一种用于兰炭粉生产型焦的粘合剂及其制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0132876B2 (enrdf_load_html_response) | 1989-07-10 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4304572A (en) | Production of solid fuel-water slurries | |
| CA1072330A (en) | Preparation of solid fuel-water slurries | |
| CN106967469B (zh) | 高浓度生物质浆料及其制备方法与应用 | |
| CN111690447B (zh) | 一种水煤浆添加剂及其制备方法和应用 | |
| CN101225336B (zh) | 碱木素-磺化丙酮-甲醛缩聚物水煤浆添加剂 | |
| CN103265984A (zh) | 一种酚水水煤浆用木质素系分散剂及其制备方法与应用 | |
| CN105695001A (zh) | 一种复合原料制备焦油型水煤浆添加剂及生产工艺 | |
| EP3158031A1 (en) | Carbonaceous material suspension | |
| JPS5845288A (ja) | 石炭・水スラリ−流動性改良法 | |
| JPS5845287A (ja) | 石炭・水スラリ−流動性改良方法 | |
| CN109777531A (zh) | 一种萘系水煤浆分散剂及其应用 | |
| JPS5845289A (ja) | 石炭・水スラリ−の流動性を改良する方法 | |
| CN102559305A (zh) | 一种复合高效水煤浆添加剂及其制备方法 | |
| CN100430122C (zh) | 两亲型水煤浆添加剂及其制备方法 | |
| JPS5845290A (ja) | 石炭・水スラリ−流動性の改良方法 | |
| CN114133967A (zh) | 一种水煤浆添加剂及其制备方法以及一种水煤浆 | |
| CN1340604A (zh) | 一种焦水煤气化料浆的制备方法及工艺 | |
| CN112852513A (zh) | 水煤浆及其制备方法和合成气的制备方法 | |
| JPH0237392B2 (enrdf_load_html_response) | ||
| CN109943372B (zh) | 褐煤或长焰煤处理改性制备水煤浆的方法 | |
| CN107353952B (zh) | 一种水煤浆分散剂及其制备方法 | |
| CA1091016A (en) | Production of solid fuel-water slurries | |
| KR840002293B1 (ko) | 착화탄용 점결제의 제조방법 | |
| CN106867605A (zh) | 一种纤维素基水煤浆添加剂及其制备方法与应用 | |
| JPS59152994A (ja) | 高濃度コ−クス−水スラリ−用減粘剤 |