JPS58208365A - 脆性体の破壊剤 - Google Patents

脆性体の破壊剤

Info

Publication number
JPS58208365A
JPS58208365A JP9127382A JP9127382A JPS58208365A JP S58208365 A JPS58208365 A JP S58208365A JP 9127382 A JP9127382 A JP 9127382A JP 9127382 A JP9127382 A JP 9127382A JP S58208365 A JPS58208365 A JP S58208365A
Authority
JP
Japan
Prior art keywords
calcareous
water
agent
clinker
brittle
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP9127382A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0138428B2 (enrdf_load_stackoverflow
Inventor
Mitsuo Hanada
花田 光雄
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yoshizawa Lime Industry Co Ltd
Original Assignee
Yoshizawa Lime Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yoshizawa Lime Industry Co Ltd filed Critical Yoshizawa Lime Industry Co Ltd
Priority to JP9127382A priority Critical patent/JPS58208365A/ja
Publication of JPS58208365A publication Critical patent/JPS58208365A/ja
Publication of JPH0138428B2 publication Critical patent/JPH0138428B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Drilling And Exploitation, And Mining Machines And Methods (AREA)
  • Working Measures On Existing Buildindgs (AREA)
  • Disintegrating Or Milling (AREA)
JP9127382A 1982-05-31 1982-05-31 脆性体の破壊剤 Granted JPS58208365A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP9127382A JPS58208365A (ja) 1982-05-31 1982-05-31 脆性体の破壊剤

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP9127382A JPS58208365A (ja) 1982-05-31 1982-05-31 脆性体の破壊剤

Publications (2)

Publication Number Publication Date
JPS58208365A true JPS58208365A (ja) 1983-12-05
JPH0138428B2 JPH0138428B2 (enrdf_load_stackoverflow) 1989-08-14

Family

ID=14021839

Family Applications (1)

Application Number Title Priority Date Filing Date
JP9127382A Granted JPS58208365A (ja) 1982-05-31 1982-05-31 脆性体の破壊剤

Country Status (1)

Country Link
JP (1) JPS58208365A (enrdf_load_stackoverflow)

Also Published As

Publication number Publication date
JPH0138428B2 (enrdf_load_stackoverflow) 1989-08-14

Similar Documents

Publication Publication Date Title
CN102010169B (zh) 一种静态破碎剂
JPS5910280B2 (ja) 廃液又はスラツジの固定法
JPS601904B2 (ja) 脆性物体の破壊剤
CN101016198A (zh) 超细碳酸盐岩粉混凝土复合掺合料及其制备方法
KR101680348B1 (ko) 말뚝 주입재 조성물
WO2017085565A2 (en) Portland cement free activation of ground granulated blast furnace slag
JPS58101178A (ja) 岩石またはコンクリ−トの静的破砕剤
JPS6311508B2 (enrdf_load_stackoverflow)
KR101638079B1 (ko) 심층혼합공법용 고화재
KR100900333B1 (ko) 저발열 저수축 시멘트 조성물
JP2009504545A (ja) 石灰非依存性セメント混合物
KR880001586B1 (ko) 파괴용이제
JPS58208365A (ja) 脆性体の破壊剤
JPH03503629A (ja) ポルトランドクリンカーの製造方法
JP4009045B2 (ja) 地盤改良材料および複合地盤ならびに地盤改良工法
JP2001059217A (ja) 地盤改良材料および地盤改良工法
KR101636282B1 (ko) 심층혼합공법용 고화재
JP4578920B2 (ja) 地盤改良方法
KR101636278B1 (ko) 경소백운석을 활용한 심층혼합공법용 고화재
JPH0375706B2 (enrdf_load_stackoverflow)
RU2251619C1 (ru) Способ получения невзрывного разрушающего средства
JPH0216789B2 (enrdf_load_stackoverflow)
JP4583148B2 (ja) 泥土の改質方法
JPS62253737A (ja) バインダ−の製造方法
US20090205539A1 (en) Production method and cement compositions with rapidly acquire good strength and which are resistant to corrosion