JPS58182598A - 放射性固体廃棄物の減容固化方法およびそれに用いられる装置 - Google Patents
放射性固体廃棄物の減容固化方法およびそれに用いられる装置Info
- Publication number
- JPS58182598A JPS58182598A JP6696982A JP6696982A JPS58182598A JP S58182598 A JPS58182598 A JP S58182598A JP 6696982 A JP6696982 A JP 6696982A JP 6696982 A JP6696982 A JP 6696982A JP S58182598 A JPS58182598 A JP S58182598A
- Authority
- JP
- Japan
- Prior art keywords
- capsule
- solid waste
- oxidizing agent
- metal capsule
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Processing Of Solid Wastes (AREA)
- Treatment Of Sludge (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6696982A JPS58182598A (ja) | 1982-04-20 | 1982-04-20 | 放射性固体廃棄物の減容固化方法およびそれに用いられる装置 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6696982A JPS58182598A (ja) | 1982-04-20 | 1982-04-20 | 放射性固体廃棄物の減容固化方法およびそれに用いられる装置 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS58182598A true JPS58182598A (ja) | 1983-10-25 |
JPS6331758B2 JPS6331758B2 (enrdf_load_stackoverflow) | 1988-06-27 |
Family
ID=13331353
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6696982A Granted JPS58182598A (ja) | 1982-04-20 | 1982-04-20 | 放射性固体廃棄物の減容固化方法およびそれに用いられる装置 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS58182598A (enrdf_load_stackoverflow) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03113399A (ja) * | 1989-09-28 | 1991-05-14 | Power Reactor & Nuclear Fuel Dev Corp | 放射性金属廃棄物の減容処理方法 |
JP2019521856A (ja) * | 2016-07-08 | 2019-08-08 | ラジェンドラ ペルサウド, | 核型熱間静水圧プレス |
-
1982
- 1982-04-20 JP JP6696982A patent/JPS58182598A/ja active Granted
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03113399A (ja) * | 1989-09-28 | 1991-05-14 | Power Reactor & Nuclear Fuel Dev Corp | 放射性金属廃棄物の減容処理方法 |
JP2019521856A (ja) * | 2016-07-08 | 2019-08-08 | ラジェンドラ ペルサウド, | 核型熱間静水圧プレス |
Also Published As
Publication number | Publication date |
---|---|
JPS6331758B2 (enrdf_load_stackoverflow) | 1988-06-27 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS59138997A (ja) | 放射性廃棄物の収容方法及びその容器 | |
CA1270073A (en) | Encapsulation of waste material | |
US4645624A (en) | Containment and densification of particulate material | |
GB1592519A (en) | Method of containing spent nuclear fuel or high-level nuclear fuel waste | |
JP2015092161A (ja) | 発電で使用される微粒子状金属燃料、リサイクルシステム、及び小型モジュール式反応炉 | |
EA023726B1 (ru) | Блок для хранения отходов | |
EP0044692A2 (en) | Arrangements for containing waste material | |
WO2013058772A1 (en) | Graphite thermal decontamination with reducing gases | |
US4280921A (en) | Immobilization of waste material | |
KR101544668B1 (ko) | 분말야금기술을 이용한 방사성 폐기물의 감용처리 방법 | |
JPS5811899A (ja) | 放射性廃棄物の減容固化方法 | |
JPS58182598A (ja) | 放射性固体廃棄物の減容固化方法およびそれに用いられる装置 | |
JP2020501125A (ja) | 廃棄物処理のための制御されたhipコンテナ圧潰 | |
Ji et al. | Sonochemical decontamination of magnesium and magnesium-zirconium alloys in mild conditions | |
US9040014B2 (en) | Graphite thermal decontamination with reducing gases | |
RU2106257C1 (ru) | Способ уплотнения самовоспламеняющихся и/или взрывоопасных металлических отходов | |
JPS58106492A (ja) | 原子炉核燃料要素にあって核燃料から構造用黒鉛を分離する方法 | |
JPS5821600A (ja) | 放射性金属廃棄物の減容固化方法 | |
JPH0544639B2 (enrdf_load_stackoverflow) | ||
AU597385B2 (en) | Encapsulation of waste materials | |
JP2002318298A (ja) | 放射性廃棄物処理方法及び処理設備 | |
US3838184A (en) | Process for producing fuel and breeder bodies for a nuclear reactor | |
JPS6239960B2 (enrdf_load_stackoverflow) | ||
RU2065221C1 (ru) | Способ отверждения радиоактивных отходов | |
JPS59201000A (ja) | 放射性固体廃棄物の収納方法 |