JPS5792152A - External parts for pocket watch - Google Patents

External parts for pocket watch

Info

Publication number
JPS5792152A
JPS5792152A JP16872480A JP16872480A JPS5792152A JP S5792152 A JPS5792152 A JP S5792152A JP 16872480 A JP16872480 A JP 16872480A JP 16872480 A JP16872480 A JP 16872480A JP S5792152 A JPS5792152 A JP S5792152A
Authority
JP
Japan
Prior art keywords
corrosion resistance
added
external parts
superior corrosion
pocket watch
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP16872480A
Other languages
Japanese (ja)
Other versions
JPH0125820B2 (en
Inventor
Takeshi Ito
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Seiko Epson Corp
Suwa Seikosha KK
Original Assignee
Seiko Epson Corp
Suwa Seikosha KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Seiko Epson Corp, Suwa Seikosha KK filed Critical Seiko Epson Corp
Priority to JP16872480A priority Critical patent/JPS5792152A/en
Publication of JPS5792152A publication Critical patent/JPS5792152A/en
Publication of JPH0125820B2 publication Critical patent/JPH0125820B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE: To obtain the titled inexpensive external parts with superior corrosion resistance and workability by adding Cr, Mo and Cu to Ni as a base in a well- balanced state, adding a specified amount of Fe while maintaining the corrosion resistance, and further adding W.
CONSTITUTION: To Ni as a base are added, by wt., 16W25% Cr, 5W10% Mo, 1W4% Cu, 5W10% Fe, 1W5% W, <0.03% C, <0.5% Si, <0.4% V, <1% Mn and <1% Ti, Nb or Ta, or <2% in total of two or more among Ti, Nb and Ta. Thus, to Ni with superior corrosion resistance are added Cr with superior corrosion resistance under oxidizing conditions and Mo and Cu with superior corrosion resistance under nonoxidizing conditions, and in order to use the elements as a ferroalloy, Fe is added to reduce the cost. C, Si, V, Ti, etc. added by such very small amounts maintain the corrosion resistance after brazing.
COPYRIGHT: (C)1982,JPO&Japio
JP16872480A 1980-11-28 1980-11-28 External parts for pocket watch Granted JPS5792152A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP16872480A JPS5792152A (en) 1980-11-28 1980-11-28 External parts for pocket watch

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP16872480A JPS5792152A (en) 1980-11-28 1980-11-28 External parts for pocket watch

Publications (2)

Publication Number Publication Date
JPS5792152A true JPS5792152A (en) 1982-06-08
JPH0125820B2 JPH0125820B2 (en) 1989-05-19

Family

ID=15873248

Family Applications (1)

Application Number Title Priority Date Filing Date
JP16872480A Granted JPS5792152A (en) 1980-11-28 1980-11-28 External parts for pocket watch

Country Status (1)

Country Link
JP (1) JPS5792152A (en)

Also Published As

Publication number Publication date
JPH0125820B2 (en) 1989-05-19

Similar Documents

Publication Publication Date Title
JPS55134160A (en) Fe alloy with superior molten zinc erosion resistance
JPS5681661A (en) Heat resistant cast alloy
JPS57134542A (en) Ferrite stainless steel with superior corrosion resistance
JPS56136951A (en) Brazing al material
JPS572865A (en) P-containing corrosion resistant steel with high weldability
JPS5713137A (en) Amorphous alloy for magnetic head
JPS57185958A (en) High-manganese nonmagnetic steel with remarkably high specific resistance
JPS5792152A (en) External parts for pocket watch
JPS5792151A (en) External parts for pocket watch
JPS5785953A (en) Carbide dispersion type sintered iron alloy with superior wear resistance
JPS5629657A (en) High silicon two phase stainless steel
JPS5792153A (en) External parts for pocket watch
JPS57126959A (en) High strength and high toughness steel for pipe line with excellent hydrogen sulfide crack resistance
JPS5562145A (en) Corrosion resistant, high permeability alloy
JPS5747852A (en) High-cr low-ni two-phase stainless steel
JPS5562144A (en) Corrosion resistant, high permeability alloy
JPS57143467A (en) Low c-low si-cr-mo steel used in wet vapor
JPS5792154A (en) External parts for pocket watch
JPS5658942A (en) Exterior decoration parts for pocket watch
JPS56169755A (en) Heat-resisting alloy
JPS57126958A (en) Low alloy steel for rotor
JPS57110656A (en) Free cutting austenite stainless steel
JPS57158355A (en) Sintered fe alloy with superior wear and corrosion resistance
JPS5365213A (en) Low alloy high toughness steel with excellent delayed fracture resistantproperty
JPS5792155A (en) External parts for pocket watch