JPS5651214B2 - - Google Patents
Info
- Publication number
- JPS5651214B2 JPS5651214B2 JP1921877A JP1921877A JPS5651214B2 JP S5651214 B2 JPS5651214 B2 JP S5651214B2 JP 1921877 A JP1921877 A JP 1921877A JP 1921877 A JP1921877 A JP 1921877A JP S5651214 B2 JPS5651214 B2 JP S5651214B2
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D7/00—Modifying the physical properties of iron or steel by deformation
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Grinding And Polishing Of Tertiary Curved Surfaces And Surfaces With Complex Shapes (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1921877A JPS53104531A (en) | 1977-02-25 | 1977-02-25 | Surface processing method decreasing stress corrosion cracking |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1921877A JPS53104531A (en) | 1977-02-25 | 1977-02-25 | Surface processing method decreasing stress corrosion cracking |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS53104531A JPS53104531A (en) | 1978-09-11 |
| JPS5651214B2 true JPS5651214B2 (enExample) | 1981-12-03 |
Family
ID=11993218
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1921877A Granted JPS53104531A (en) | 1977-02-25 | 1977-02-25 | Surface processing method decreasing stress corrosion cracking |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS53104531A (enExample) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4609917A (en) * | 1983-01-17 | 1986-09-02 | Lexidata Corporation | Three-dimensional display system |
| JPH0629458B2 (ja) * | 1984-10-25 | 1994-04-20 | 愛知製鋼株式会社 | 時効割れ防止可能な鋼材の製造方法 |
| JPH1017986A (ja) | 1996-06-28 | 1998-01-20 | Nippon Steel Corp | パイプラインの耐外面scc特性に優れた鋼 |
| JP4513311B2 (ja) * | 2002-11-18 | 2010-07-28 | Jfeスチール株式会社 | 疲労強度特性に優れた溶接継手 |
| DE602005021286D1 (de) * | 2004-09-15 | 2010-07-01 | Sumitomo Metal Ind | Stahl-Rohr mit ausgezeichneter Beständigkeit gegen Abblättern auf der inneren Oberfläche |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5324169B2 (enExample) * | 1974-03-07 | 1978-07-19 |
-
1977
- 1977-02-25 JP JP1921877A patent/JPS53104531A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS53104531A (en) | 1978-09-11 |