JPS56165564A - Arc welding method - Google Patents
Arc welding methodInfo
- Publication number
- JPS56165564A JPS56165564A JP6894380A JP6894380A JPS56165564A JP S56165564 A JPS56165564 A JP S56165564A JP 6894380 A JP6894380 A JP 6894380A JP 6894380 A JP6894380 A JP 6894380A JP S56165564 A JPS56165564 A JP S56165564A
- Authority
- JP
- Japan
- Prior art keywords
- current
- time
- base
- base current
- pulse
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To make the arc stable, shift globules smoothly and obtain the weld zone of high quality by limiting the current change width between peak current and base current and pulse current time.
CONSTITUTION: The current change width IP-IB between peak current IP and base current IB is adjusted to ≥300A, and the time TP from the start of rise of the pulse current IP till the start of fall thereof is kept within a 0.2ms≤4ms range. Further, when the time of the base current IB is short in a spray region, and arc sound is produced within the prescribed current change width, the value of the base current IB is increased, average current value Im is increased and base current time TB is made long. To shift one globule surely with one time of pulse, the peak current IP and the peak current time TP are so set as to attain IPK.TP=C. At this time, C is the constant determined by the diameter and material of a wire, and K is 1.9W 2.5. Further it is possible to make the adjustment of welding current much easier by associating wire feed speed and the base current time.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6894380A JPS56165564A (en) | 1980-05-26 | 1980-05-26 | Arc welding method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6894380A JPS56165564A (en) | 1980-05-26 | 1980-05-26 | Arc welding method |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS56165564A true JPS56165564A (en) | 1981-12-19 |
JPS6339349B2 JPS6339349B2 (en) | 1988-08-04 |
Family
ID=13388249
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6894380A Granted JPS56165564A (en) | 1980-05-26 | 1980-05-26 | Arc welding method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS56165564A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61199581A (en) * | 1985-03-01 | 1986-09-04 | Hitachi Seiko Ltd | Arc welding method |
JPS62151272A (en) * | 1985-12-26 | 1987-07-06 | Mitsubishi Heavy Ind Ltd | Detecting method for droplet transfer time |
DE4023155A1 (en) * | 1989-07-21 | 1991-02-07 | Hitachi Seiko Kk | AC CURRENT PROTECTIVE GAS ARC WELDING PROCESS WITH CONSUMABLE ELECTRODE AND DEVICE THEREFOR |
-
1980
- 1980-05-26 JP JP6894380A patent/JPS56165564A/en active Granted
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61199581A (en) * | 1985-03-01 | 1986-09-04 | Hitachi Seiko Ltd | Arc welding method |
JPH0435265B2 (en) * | 1985-03-01 | 1992-06-10 | Hitachi Seiko Kk | |
JPS62151272A (en) * | 1985-12-26 | 1987-07-06 | Mitsubishi Heavy Ind Ltd | Detecting method for droplet transfer time |
DE4023155A1 (en) * | 1989-07-21 | 1991-02-07 | Hitachi Seiko Kk | AC CURRENT PROTECTIVE GAS ARC WELDING PROCESS WITH CONSUMABLE ELECTRODE AND DEVICE THEREFOR |
Also Published As
Publication number | Publication date |
---|---|
JPS6339349B2 (en) | 1988-08-04 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS56165564A (en) | Arc welding method | |
JPS5662674A (en) | Pulse arc welding method | |
GB2171267A (en) | Welding power supply | |
CA2049666A1 (en) | Method for reducing the energy consumption and minimizing the martensite formation when joining a connecting piece of metal with a metal surface by pin brazing and arrangement forcarrying out the method | |
JPS57130770A (en) | Arc welding method | |
EP0178680A3 (en) | Feed length control device for consumable electrode welding operations | |
JPS57124572A (en) | Arc welding method | |
JPS55147479A (en) | Automatic welding method | |
JPS57130769A (en) | Arc welding method | |
JPS5419445A (en) | Arc welding method | |
JPS5719173A (en) | Consumable electrode type pulse arc welding machine | |
JPS6431574A (en) | Consumable electrode type and welding method | |
JPS56119673A (en) | Nonconsumable electrode arc welding method | |
JPS56141969A (en) | Power source for pulse arc welding machine | |
JPS566790A (en) | Controlling method of flash welding machine | |
JPS55126382A (en) | Arc welding equipment | |
JPS5781960A (en) | Pulsed arc welding | |
JPS57184576A (en) | Cutting method by plasma arc | |
JPS5548480A (en) | Single-electrode swing submerging arc welding method | |
JPS5781961A (en) | Pulse arc welding | |
JPS5554271A (en) | Arc starting method in dcsp-tig welding of aluminum material | |
JPS5481158A (en) | Manufacture of welded tube | |
JPS53103955A (en) | Arc welder | |
JPS571589A (en) | Electron beam welding method | |
JPS56134075A (en) | Method for large-current pulse one-side welding of steel for low temperature |