JPS56152939A - Exterior decorative parts for pocket watch - Google Patents
Exterior decorative parts for pocket watchInfo
- Publication number
- JPS56152939A JPS56152939A JP5724380A JP5724380A JPS56152939A JP S56152939 A JPS56152939 A JP S56152939A JP 5724380 A JP5724380 A JP 5724380A JP 5724380 A JP5724380 A JP 5724380A JP S56152939 A JPS56152939 A JP S56152939A
- Authority
- JP
- Japan
- Prior art keywords
- corrosion resistance
- superior corrosion
- decorative parts
- exterior decorative
- pocket watch
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 230000007797 corrosion Effects 0.000 abstract 5
- 238000005260 corrosion Methods 0.000 abstract 5
- 239000000463 material Substances 0.000 abstract 3
- 229910052804 chromium Inorganic materials 0.000 abstract 2
- 229910052750 molybdenum Inorganic materials 0.000 abstract 2
- 229910052758 niobium Inorganic materials 0.000 abstract 2
- VEXZGXHMUGYJMC-UHFFFAOYSA-M Chloride anion Chemical compound [Cl-] VEXZGXHMUGYJMC-UHFFFAOYSA-M 0.000 abstract 1
- 229910000640 Fe alloy Inorganic materials 0.000 abstract 1
- 229910045601 alloy Inorganic materials 0.000 abstract 1
- 239000000956 alloy Substances 0.000 abstract 1
- 230000002708 enhancing effect Effects 0.000 abstract 1
- 230000001590 oxidative effect Effects 0.000 abstract 1
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5724380A JPS56152939A (en) | 1980-04-30 | 1980-04-30 | Exterior decorative parts for pocket watch |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP5724380A JPS56152939A (en) | 1980-04-30 | 1980-04-30 | Exterior decorative parts for pocket watch |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS56152939A true JPS56152939A (en) | 1981-11-26 |
| JPH0149783B2 JPH0149783B2 (enrdf_load_stackoverflow) | 1989-10-26 |
Family
ID=13050085
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP5724380A Granted JPS56152939A (en) | 1980-04-30 | 1980-04-30 | Exterior decorative parts for pocket watch |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS56152939A (enrdf_load_stackoverflow) |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4876721A (enrdf_load_stackoverflow) * | 1972-01-19 | 1973-10-16 | ||
| JPS49126511A (enrdf_load_stackoverflow) * | 1973-04-11 | 1974-12-04 | ||
| JPS52120220A (en) * | 1976-04-03 | 1977-10-08 | Nippon Musical Instruments Mfg | Corrosion resistant nickel based alloy |
-
1980
- 1980-04-30 JP JP5724380A patent/JPS56152939A/ja active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4876721A (enrdf_load_stackoverflow) * | 1972-01-19 | 1973-10-16 | ||
| JPS49126511A (enrdf_load_stackoverflow) * | 1973-04-11 | 1974-12-04 | ||
| JPS52120220A (en) * | 1976-04-03 | 1977-10-08 | Nippon Musical Instruments Mfg | Corrosion resistant nickel based alloy |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0149783B2 (enrdf_load_stackoverflow) | 1989-10-26 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS55100959A (en) | Invar alloy with excellent welding high temperature crack resistance and strain corrosion crack resistance | |
| JPS55134160A (en) | Fe alloy with superior molten zinc erosion resistance | |
| JPS57134542A (en) | Ferrite stainless steel with superior corrosion resistance | |
| JPS56136951A (en) | Brazing al material | |
| TW583315B (en) | Free cutting steel | |
| JPS57185958A (en) | High-manganese nonmagnetic steel with remarkably high specific resistance | |
| JPS56152939A (en) | Exterior decorative parts for pocket watch | |
| JPS5360303A (en) | Amorphous alloy of high magnetic permeability | |
| JPS5337992A (en) | Sintered diamond | |
| JPS53113216A (en) | High magnetic permeable amorphous alloy excellent in corrosion resistance | |
| JPS57126959A (en) | High strength and high toughness steel for pipe line with excellent hydrogen sulfide crack resistance | |
| JPS5365213A (en) | Low alloy high toughness steel with excellent delayed fracture resistantproperty | |
| JPS5729563A (en) | Austenite type stainless steel with excellent corrosion resistance | |
| JPS5411015A (en) | Iron alloy | |
| JPS5335610A (en) | W base sintered alloy having high toughness | |
| JPS563649A (en) | Sintered hard alloy having superior corrosion resistance | |
| JPS5792151A (en) | External parts for pocket watch | |
| JPS53129679A (en) | Watch parts such as watch cases, winding crowns, watch bands | |
| JPS57126958A (en) | Low alloy steel for rotor | |
| JPS5696059A (en) | High manganese stainless steel with low melting point | |
| JPS5337110A (en) | Preparation of overlays | |
| JPS53100913A (en) | Wear resistant cu alloy | |
| JPS53141115A (en) | High chromium alloy having good anticorrosion resistance and weldability against mixed acid consisting of nitric acid and fluoric acid | |
| JPS57131340A (en) | Alloy for oil well pipe with superior stress corrosion cracking resistance | |
| JPS55141543A (en) | Mo-containing hard alloy |