JPS5545523A - Heat effect reducing method of inside surface of butt welded joint part of reaction pipe for chemical machinery - Google Patents

Heat effect reducing method of inside surface of butt welded joint part of reaction pipe for chemical machinery

Info

Publication number
JPS5545523A
JPS5545523A JP11749278A JP11749278A JPS5545523A JP S5545523 A JPS5545523 A JP S5545523A JP 11749278 A JP11749278 A JP 11749278A JP 11749278 A JP11749278 A JP 11749278A JP S5545523 A JPS5545523 A JP S5545523A
Authority
JP
Japan
Prior art keywords
heat effect
inside surface
chemical machinery
joint part
welded joint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP11749278A
Other languages
Japanese (ja)
Inventor
Tadashi Nosaka
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Power Ltd
Original Assignee
Babcock Hitachi KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Babcock Hitachi KK filed Critical Babcock Hitachi KK
Priority to JP11749278A priority Critical patent/JPS5545523A/en
Publication of JPS5545523A publication Critical patent/JPS5545523A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To suppress the deposition of carbide which becomes the point for initiation of crazing by taking the root face of the root pass portion larger thereby reducing heat effect extending to the inside surface side of the pipe of the second and subsequent passes.
CONSTITUTION: In the case of butt welding reaction pipes for chemical machinery, the root pass 2 fusion bonds the base pipes 1 by a keyhole method of plasma welding. Here, the root face 5 is taken about 5mm or over. Then, the distance up to the inside surface of the pipe becomes larger and the heat effect at the forming of the deposited metal 3 of the second and subsequent passes by using wire cores becomes relatively smaller. Hence, the deposition of the carbide 4 deposited owing to this heat effect is suppressed and the fortification of the joint is achieved.
COPYRIGHT: (C)1980,JPO&Japio
JP11749278A 1978-09-26 1978-09-26 Heat effect reducing method of inside surface of butt welded joint part of reaction pipe for chemical machinery Pending JPS5545523A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP11749278A JPS5545523A (en) 1978-09-26 1978-09-26 Heat effect reducing method of inside surface of butt welded joint part of reaction pipe for chemical machinery

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP11749278A JPS5545523A (en) 1978-09-26 1978-09-26 Heat effect reducing method of inside surface of butt welded joint part of reaction pipe for chemical machinery

Publications (1)

Publication Number Publication Date
JPS5545523A true JPS5545523A (en) 1980-03-31

Family

ID=14713057

Family Applications (1)

Application Number Title Priority Date Filing Date
JP11749278A Pending JPS5545523A (en) 1978-09-26 1978-09-26 Heat effect reducing method of inside surface of butt welded joint part of reaction pipe for chemical machinery

Country Status (1)

Country Link
JP (1) JPS5545523A (en)

Similar Documents

Publication Publication Date Title
JPS5592285A (en) Welding method of hard metal
JPS5431062A (en) Manufacture of structure superior in stress corrosion cracking resistivity
JPS5545523A (en) Heat effect reducing method of inside surface of butt welded joint part of reaction pipe for chemical machinery
JPS53130241A (en) Welding method for manufacture of thick walled steel pipe
JPS53141140A (en) Process for forming weld joint of pipeline or vessel
JPS54155153A (en) Preventing method for stress corrosion cracking for sensitized zone of welding
JPS5478340A (en) Butt welding method for aluminum clad steel
JPS5584279A (en) Narrow groove submerged arc welding method
JPS56131083A (en) Welded joint method for stainless steel tube
JPS574395A (en) Welding method
JPS53142348A (en) Welding method for metallic pipe
JPS53130242A (en) Welding method for manufacture of thick-walled large diameter welded steel pipe
JPS5545572A (en) Welding method
JPS5542128A (en) Repair welding method of stainless steel pipe welded joint
JPS52118615A (en) Specials welded joint
JPS564392A (en) Connecting method of piping
JPS5397964A (en) Preparation of electric welded steel tube
JPS5411045A (en) Preventing method for crack initiation of deposited metal
JPS5542136A (en) Crack preventive method of welded part
JPS53119772A (en) Manufacture of force welded pipe
JPS5469540A (en) Joining method for tube and tube plate in heat exchanger or the like
JPS52153192A (en) Cable joint process and composite lead pipe
JPS5345713A (en) Production for porcelain enamel tank
JPS53131941A (en) Method of forming gap of thick pipe welded portion
JPS5318814A (en) Strengthening structure for steel pipe bending