JPS55144388A - Welding method of round bar and plate material - Google Patents
Welding method of round bar and plate materialInfo
- Publication number
- JPS55144388A JPS55144388A JP5231279A JP5231279A JPS55144388A JP S55144388 A JPS55144388 A JP S55144388A JP 5231279 A JP5231279 A JP 5231279A JP 5231279 A JP5231279 A JP 5231279A JP S55144388 A JPS55144388 A JP S55144388A
- Authority
- JP
- Japan
- Prior art keywords
- wire
- plate
- electrodes
- contact
- electric current
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To improve the bonding strength of weld zone by providing the curved surface form ridge part intersecting orthogonally with the axial direction of an Mo wire on the contact surface of a welding electrode end in contact with an Mo plate at the time of welding the Mo wire and Mo plate by supplying electric current under pressure thereto by the electrodes from their above and below.
CONSTITUTION: An Mo wire material A and Mo plate material B are contacted. While they are being pressed by upper and lower electrodes 1, 2, electric current is flowed between the electrodes 1, 2 to weld the Mo wire A and Mo plate B. At this time, the end face 2a of the lower electrode 2 in contact with the Mo plate B is formed to the semicircular shape of a radius of curvature R. Hence, it has a ridge part 3 in the direction orthogonal to the axial direction of the Mo wire A. When pressure is applied and electric current is supplied by the electrodes 1, 2 in this state, the central part of the contact area D of the Mo wire A and Mo plate B recrystallizes and has smaller mechanical strength but in the peripheral part the rate of recrystallization is less becuase contact resistance is smallest in the central part and becomes gradually large in the periperal part thereof, thus the weld zone of high mechanical strength is formed.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5231279A JPS5935718B2 (en) | 1979-04-27 | 1979-04-27 | How to weld round bars and plates |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP5231279A JPS5935718B2 (en) | 1979-04-27 | 1979-04-27 | How to weld round bars and plates |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS55144388A true JPS55144388A (en) | 1980-11-11 |
JPS5935718B2 JPS5935718B2 (en) | 1984-08-30 |
Family
ID=12911258
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP5231279A Expired JPS5935718B2 (en) | 1979-04-27 | 1979-04-27 | How to weld round bars and plates |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5935718B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03114682A (en) * | 1989-09-28 | 1991-05-15 | Tanaka Kikinzoku Kogyo Kk | Electrode for welding brush wire bundle |
-
1979
- 1979-04-27 JP JP5231279A patent/JPS5935718B2/en not_active Expired
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03114682A (en) * | 1989-09-28 | 1991-05-15 | Tanaka Kikinzoku Kogyo Kk | Electrode for welding brush wire bundle |
Also Published As
Publication number | Publication date |
---|---|
JPS5935718B2 (en) | 1984-08-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS55144387A (en) | Welding equipment of bar material and plate material | |
US3346350A (en) | Electrical contact tape | |
JPS55144388A (en) | Welding method of round bar and plate material | |
US2832127A (en) | Method of making electrical contacts | |
UA7227A1 (en) | Contact flat wire | |
EP0332337A3 (en) | Electrode and construction thereof | |
EP0399334A3 (en) | Method of producing contact tip | |
JPH04339573A (en) | Electrode for resistance welding and its forming method | |
JP2798825B2 (en) | Electrode for resistance welding | |
JPS57105960A (en) | Preparation of lead battery electrode group | |
US4514033A (en) | Arc welding clamp | |
US4385222A (en) | Apparatus for spot welding galvanized sheet metal | |
JPS5662681A (en) | Welding method of spring material | |
JPS5728683A (en) | Electrode structure of electric welder | |
JPS6454706A (en) | Organic positive temperature coefficient thermistor | |
JPS5586688A (en) | Welding method of pipe materials | |
JPH07314141A (en) | Bar shaped body for welding | |
JPS5732569A (en) | Manufacture of battery with coiled electrode body | |
JPS5669038A (en) | Electric discharge machining electrode | |
JPS566791A (en) | Welding method of nut | |
JPS5588995A (en) | Welding method of tube body | |
SU677849A1 (en) | Resistance welding method | |
JPS57121886A (en) | Method and device for welding of very thin wire | |
JPS5527428A (en) | Fusion welding method of screen and other metal | |
JPS6127186A (en) | Forming equipment of resistance welding electrode |