JPS55122853A - Welded steel tube having superior butted portion toughness - Google Patents

Welded steel tube having superior butted portion toughness

Info

Publication number
JPS55122853A
JPS55122853A JP3090879A JP3090879A JPS55122853A JP S55122853 A JPS55122853 A JP S55122853A JP 3090879 A JP3090879 A JP 3090879A JP 3090879 A JP3090879 A JP 3090879A JP S55122853 A JPS55122853 A JP S55122853A
Authority
JP
Japan
Prior art keywords
steel tube
welded steel
superior
toughness
butted portion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP3090879A
Other languages
Japanese (ja)
Other versions
JPS5853707B2 (en
Inventor
Yoji Yamaguchi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP54030908A priority Critical patent/JPS5853707B2/en
Publication of JPS55122853A publication Critical patent/JPS55122853A/en
Publication of JPS5853707B2 publication Critical patent/JPS5853707B2/en
Expired legal-status Critical Current

Abstract

PURPOSE: To provide high toughness to the weld zone of an electric welded steel tube consisting of a respectively specified ratio of C, Si, Mn, P, S and sol. Al, N esp. 0.0030% or less and the balance Fe and manufactured esp. by high or low frequency electric resistance welding.
CONSTITUTION: This welded steel tube is made of carbon steel consisting of C≤ 0.3%, Si≤1.00%, Mn 0.2W2.00%, P≤0.05%, S≤0.05%, sol. Al 0.01W0.10%, N≤0.0030%, and the balance Fe and inevitable impurities. Nb 0.01W0.15% and/or V 0.01W0.20% may be added to the compsn. to further enhance the strength. By controlling the N content of the steel to 0.0030% or less a toughness lowering due to the influence of residual strain and working strain in the manufacturing process and the influence of heat and working strain in use can be minimized.
COPYRIGHT: (C)1980,JPO&Japio
JP54030908A 1979-03-15 1979-03-15 ERW steel pipe with excellent butt toughness Expired JPS5853707B2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP54030908A JPS5853707B2 (en) 1979-03-15 1979-03-15 ERW steel pipe with excellent butt toughness

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP54030908A JPS5853707B2 (en) 1979-03-15 1979-03-15 ERW steel pipe with excellent butt toughness

Publications (2)

Publication Number Publication Date
JPS55122853A true JPS55122853A (en) 1980-09-20
JPS5853707B2 JPS5853707B2 (en) 1983-11-30

Family

ID=12316803

Family Applications (1)

Application Number Title Priority Date Filing Date
JP54030908A Expired JPS5853707B2 (en) 1979-03-15 1979-03-15 ERW steel pipe with excellent butt toughness

Country Status (1)

Country Link
JP (1) JPS5853707B2 (en)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6418015U (en) * 1987-07-21 1989-01-30

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS502847A (en) * 1973-05-10 1975-01-13
JPS50139013A (en) * 1974-04-27 1975-11-06

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS502847A (en) * 1973-05-10 1975-01-13
JPS50139013A (en) * 1974-04-27 1975-11-06

Also Published As

Publication number Publication date
JPS5853707B2 (en) 1983-11-30

Similar Documents

Publication Publication Date Title
JPS56122681A (en) Manufacture of titanium or titanium alloy clad steel plate by rolling and pressure welding
JPS5458615A (en) Niobium-containing line pipe steel with superior weldability
JPS5723050A (en) Heat resistant steel with excellent high temp. strength
JPS55122854A (en) Welded steel tube having superior butted portion toughness
JPS55122853A (en) Welded steel tube having superior butted portion toughness
JPS57154395A (en) Welding material
JPS6468451A (en) High strength low alloy heat-resistant steel having excellent strength of its weld zone
JPS5735625A (en) Manufacture of high tensile steel pipe with superior toughness at low temperature
JPS56108860A (en) Super-high tensile steel with superior corrosion resistance
JPS55100960A (en) High tensile steel with low subsequent crack sensitivity
JPS5465115A (en) Boron-added high tensile steel with superior low temperature toughness
JPS5693858A (en) High temp. steel with excellent creep embrittlement resistance
SU1411112A1 (en) Composition of welding wire
JPS5726147A (en) High strength steel for flash butt welding
JPS57202981A (en) Highly tenacious ac mig welding method
JPS5726139A (en) Weld cracking resistant steel
JPS5582752A (en) High strength steel with superior reheating crack resistance for high temperature use
JPS5528307A (en) Heat resistant alloy with superior weld crack resistance
JPS57104648A (en) Seam welded steel pipe with superior groove corrosion resistance
JPS5527481A (en) Wire for welding cast iron
JPS56252A (en) Cr-mo steel of excellent strength and tenacity to be hot- worked
JPS55131158A (en) Heat resistant cast alloy
JPS56150167A (en) Corrosion resistant alloy for molten borax
JPS5623249A (en) Hot rolled steel strip for high tensile electric welded tube having superior flattening performance
JPS54112719A (en) Nonmagnetic steel with good electron beam weldability