JPS54159359A - Mig arc welding method - Google Patents

Mig arc welding method

Info

Publication number
JPS54159359A
JPS54159359A JP6765478A JP6765478A JPS54159359A JP S54159359 A JPS54159359 A JP S54159359A JP 6765478 A JP6765478 A JP 6765478A JP 6765478 A JP6765478 A JP 6765478A JP S54159359 A JPS54159359 A JP S54159359A
Authority
JP
Japan
Prior art keywords
welding
arc
wire
molten
penetration
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP6765478A
Other languages
Japanese (ja)
Inventor
Akira Sato
Hiroshi Wachi
Satoshi Ogura
Eiji Ashida
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hitachi Ltd
Original Assignee
Hitachi Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Ltd filed Critical Hitachi Ltd
Priority to JP6765478A priority Critical patent/JPS54159359A/en
Publication of JPS54159359A publication Critical patent/JPS54159359A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To make large the amount of the deposited metal, and to execute the MIG arc welding with a good shape of penetration and a small rate of dilution, by feeding the arbitrary filler wire into the molten metal in which the molten particle of the welding wire is forced to cause the spray transfer.
CONSTITUTION: The electrode wire 1 contacts with the work 3 to be welded, the arc 4 is generated, and the welding is executed. While the welding work, when the spray transfer is caused in a small molten particle, the filler wire 5 is always fed into the molten metal 9 formed by the arc. According to this method, the generation of the spatter is prevented, the amount of the deposited metal is increased, and the shape of penetration is rounded. By this method, a great effect is given to the overlay welding and the joint welding.
COPYRIGHT: (C)1979,JPO&Japio
JP6765478A 1978-06-07 1978-06-07 Mig arc welding method Pending JPS54159359A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP6765478A JPS54159359A (en) 1978-06-07 1978-06-07 Mig arc welding method

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP6765478A JPS54159359A (en) 1978-06-07 1978-06-07 Mig arc welding method

Publications (1)

Publication Number Publication Date
JPS54159359A true JPS54159359A (en) 1979-12-17

Family

ID=13351218

Family Applications (1)

Application Number Title Priority Date Filing Date
JP6765478A Pending JPS54159359A (en) 1978-06-07 1978-06-07 Mig arc welding method

Country Status (1)

Country Link
JP (1) JPS54159359A (en)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5916680A (en) * 1982-07-16 1984-01-27 Mitsubishi Electric Corp Consumable electrode type arc welding device
JPH0663754A (en) * 1992-08-20 1994-03-08 Hitachi Zosen Corp Gas shielded arc welding method
JP2008207227A (en) * 2007-02-27 2008-09-11 Sumitomo Light Metal Ind Ltd Mig welded joint and mig welding process for aluminum material and steel
JP2008207226A (en) * 2007-02-27 2008-09-11 Sumitomo Light Metal Ind Ltd Mig welded joint and mig welding process for aluminum material and steel
JP2010069494A (en) * 2008-09-17 2010-04-02 Daihen Corp Two-wire welding method

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5916680A (en) * 1982-07-16 1984-01-27 Mitsubishi Electric Corp Consumable electrode type arc welding device
JPH0337469B2 (en) * 1982-07-16 1991-06-05 Mitsubishi Electric Corp
JPH0663754A (en) * 1992-08-20 1994-03-08 Hitachi Zosen Corp Gas shielded arc welding method
JP2008207227A (en) * 2007-02-27 2008-09-11 Sumitomo Light Metal Ind Ltd Mig welded joint and mig welding process for aluminum material and steel
JP2008207226A (en) * 2007-02-27 2008-09-11 Sumitomo Light Metal Ind Ltd Mig welded joint and mig welding process for aluminum material and steel
US8742294B2 (en) 2007-02-27 2014-06-03 Sumitomo Light Metal Industries, Ltd. MIG welded joint between aluminum and steel members and MIG welding process
JP2010069494A (en) * 2008-09-17 2010-04-02 Daihen Corp Two-wire welding method

Similar Documents

Publication Publication Date Title
JPS5788972A (en) Two electrode arc welding method
JPS54159359A (en) Mig arc welding method
JPS5573479A (en) Tandem system high speed arc welding method
JPS53103956A (en) Arc welding method
JPS53113734A (en) One-side arc welding method for 9% ni steel
JPS58176074A (en) Consumable electrode type pulse arc welding method
US4100389A (en) Method of high speed gas shielded arc welding
JPS5548479A (en) Arc welding method
JPS53115645A (en) Non-consuptive electrode type welding torch
JPS5510368A (en) Soldering method
JPS54132448A (en) Welding method for copper or copper alloy parts and ferro or nickel alloy parts
JPS564378A (en) Inert gas shielded arc welding method
JPS564381A (en) Two electrode submerged arc welding method
JPS5424240A (en) Non-consumable electrode type arc welding method
JPS57199564A (en) Build-up welding method by belt-like electrode type multiple electrodes
JPS5581068A (en) Tig welding method
JPS55156670A (en) Tig arc build-up weld method
JPS5433245A (en) Large current mig welding method of aluminum alloy
JP2534853B2 (en) High-speed Tig dressing method
JPS5542136A (en) Crack preventive method of welded part
JPS5432147A (en) Automatic arc welding method
JPS61216881A (en) Starting method for electroslag welding
JPS57159268A (en) Arc welding method
JPS54159361A (en) Preventing method for crack at starting point and toe of weld in mig welding
JPS53144850A (en) Automatic arc welding process using non-consumable electrode