Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP4344178A
Other languages
Japanese (ja)
Inventor
Takao Mihara
Toshiaki Morichika
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kubota Corp
Original Assignee
Kubota Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kubota Corp filed Critical Kubota Corp
Priority to JP4344178A priority Critical patent/JPS54135643A/en
Publication of JPS54135643A publication Critical patent/JPS54135643A/en
Pending legal-status Critical Current

Links

Landscapes

  • Arc Welding In General (AREA)

Abstract

PURPOSE: To carry out the crater treatment without producing blowhole, burn through or crater crack etc., by regulating feeding angle of core wire at a proper extent and directly feeding the core wire in molten pool.
CONSTITUTION: Relative advance of the basic material 3 and the torch 2 at the crater part, is stopped at the time of finished welding and feeding of the core wire 1 to the crater part, is started lowering flowing quantity of center gas. On this occasion, the angle α of the wire 1 is made within the extent of more than 50° and less than 80° and tip end of the wire 1 is dipped in the molten pool 4. Hereby, arc heat is transmitted in the pool 4 and outer surface of the pool 4 is solidified after the center gas is passed through to the outer face. Accordingly, blowhole is not remained and the back bead 5 is not projected and also trouble of crater crack is not taken place. Also, the above effect is obtained even when the basic material is thick and small diameter or much Cr, Ni components are contained.
COPYRIGHT: (C)1979,JPO&Japio
JP4344178A 1978-04-12 1978-04-12 Treating method for crater of plasma keyhole welding Pending JPS54135643A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP4344178A JPS54135643A (en) 1978-04-12 1978-04-12 Treating method for crater of plasma keyhole welding

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP4344178A JPS54135643A (en) 1978-04-12 1978-04-12 Treating method for crater of plasma keyhole welding

Publications (1)

Publication Number Publication Date
JPS54135643A true JPS54135643A (en) 1979-10-22

Family

ID=12663776

Family Applications (1)

Application Number Title Priority Date Filing Date
JP4344178A Pending JPS54135643A (en) 1978-04-12 1978-04-12 Treating method for crater of plasma keyhole welding

Country Status (1)

Country Link
JP (1) JPS54135643A (en)

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS49133250A (en) * 1973-04-26 1974-12-20
JPS502642A (en) * 1973-05-12 1975-01-11

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS49133250A (en) * 1973-04-26 1974-12-20
JPS502642A (en) * 1973-05-12 1975-01-11

Similar Documents

Publication Publication Date Title
JPS54135643A (en) Treating method for crater of plasma keyhole welding
JPS57103783A (en) Method for continuous gouging of stainless steel clad steel in water
JPS5691992A (en) Laser welding method and laser working head
JPS53130241A (en) Welding method for manufacture of thick walled steel pipe
JPS5570479A (en) Narrow groove co2 gas shielded arc welding method
JPS5684172A (en) 2-electrode tig welding method
JPS5573474A (en) Butt welding method of thin-wall tubular bodiy
JPS53106361A (en) Submerged arc welding method for steel plate
JPS55117564A (en) Build-up welding method
JPS5636376A (en) Crater treating method of plasma arc welding
JPS57181763A (en) Vertical narrow groove mag welding method for short size
SU585003A1 (en) Device for gas-shielding of welding bath, weld and electrode
JPS5330983A (en) Treating method for solid waste by electric melting
JPS5633170A (en) Cutting method for thick metallic plate
JPS5575882A (en) Gta welding method
JPS5677091A (en) Welding method using electro-slag welding consumable nozzle and consumable nozzle to be used for this purpose
JPS5542136A (en) Crack preventive method of welded part
JPS5764478A (en) Method for automatic welding
JPS5633192A (en) Welding process for copper and copper alloy
JPS5594779A (en) Method and device for tig welding
JPS5666387A (en) Submerged stud welding method
JPS53144850A (en) Automatic arc welding process using non-consumable electrode
JPS5395850A (en) Multiple wire submerged arc welding method
JPS53137043A (en) Inert gas arc welding method for steel for low temperature use
JPS5781954A (en) Forming method for edge welded joint