Device for gas-shielding of welding bath, weld and electrodeInfo
- Publication number
- SU585003A1 SU585003A1 SU7502124486A SU2124486A SU585003A1 SU 585003 A1 SU585003 A1 SU 585003A1 SU 7502124486 A SU7502124486 A SU 7502124486A SU 2124486 A SU2124486 A SU 2124486A SU 585003 A1 SU585003 A1 SU 585003A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- electrode
- gas
- weld
- pressure plates
- shielding
- Prior art date
Description
(54) УСТРОЙСТВО ДЛЯ ГАЗОВОЙ ЗАШИТЫ ШВА И- ЭЛЕКТРОДА СВАРОЧНОЙ ВАННЫ,(54) DEVICE FOR GAS PROTECTION OF THE SEAM AND ELECTRODE OF THE WELDING BATH,
;. ;.
конструкций из листового титанового сплава ВТ1 толщиной от 0,5 до 5 мм с длиной шва от 5 до 100 мм. Планки 3 размером 110x10x4 устройства изготавливались из гранулированного порошка олов нистой бронзы фракции 0,315, 0,4 и 0,6 мм. Рассто ние между планками, образуюш,ими зону защиты, было равно 12 мм. В качестве защитного газа использовали аргон марки А ГОСТ 10157-62, расход газа составл л 4 л/мин. Сварку проводили на установке «УДАР - режим сварки: 1 15-18 А, и 18-20 В, УСЬ 45м/час, использовали горелку «РГА - 150 без сопла. Качество щва соответствовало требовани м отраслевой инструкции ПИ-126-67 «Дугова сварка сплавов титана в среде защитных газов.structures made of sheet titanium alloy VT1 with a thickness of 0.5 to 5 mm with a seam length of 5 to 100 mm. The trims 3 with a size of 110x10x4 devices were made of granulated tin-bronze powder with a fraction of 0.315, 0.4 and 0.6 mm. The distance between the slats, forming, by them, the protection zone, was equal to 12 mm. Argon of grade A of GOST 10157-62 was used as a shielding gas, the gas consumption was 4 l / min. The welding was carried out on the installation “KICK - welding mode: 1 15-18 A, and 18-20 V, ACP 45m / h, used a torch“ RSA - 150 without a nozzle. The quality of the spike complied with the requirements of the branch instruction PI-126-67 "Arc welding of titanium alloys in protective gas.
Использование устройства дл газовой защиты сварочной ванны, шва и электрода обеспечивает увеличение скорости сварки не ниже чем в 1,5 раза, улучшение обзора зоны сварки и повышение надежности газовой защиты, а также расширение номенклатуры свариваемых де585003The use of a device for gas protection of the weld pool, weld and electrode provides an increase in the welding speed of not less than 1.5 times, improving the overview of the welding zone and improving the reliability of gas protection, as well as expanding the range of welded materials.
талей, что значительно повышает производительность процесса и качество сварки.hoists, which significantly improves the performance of the process and the quality of welding.
Claims (2)