JPS54128415A - Direct reduction furnace - Google Patents
Direct reduction furnaceInfo
- Publication number
- JPS54128415A JPS54128415A JP3701878A JP3701878A JPS54128415A JP S54128415 A JPS54128415 A JP S54128415A JP 3701878 A JP3701878 A JP 3701878A JP 3701878 A JP3701878 A JP 3701878A JP S54128415 A JPS54128415 A JP S54128415A
- Authority
- JP
- Japan
- Prior art keywords
- sic
- furnace
- refractories
- lining
- direct reduction
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacture Of Iron (AREA)
- Furnace Housings, Linings, Walls, And Ceilings (AREA)
- Ceramic Products (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP53037018A JPS5917347B2 (ja) | 1978-03-29 | 1978-03-29 | 回転還元炉 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP53037018A JPS5917347B2 (ja) | 1978-03-29 | 1978-03-29 | 回転還元炉 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS54128415A true JPS54128415A (en) | 1979-10-05 |
JPS5917347B2 JPS5917347B2 (ja) | 1984-04-20 |
Family
ID=12485912
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP53037018A Expired JPS5917347B2 (ja) | 1978-03-29 | 1978-03-29 | 回転還元炉 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5917347B2 (ja) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6028956U (ja) * | 1983-07-29 | 1985-02-27 | 新日本製鐵株式会社 | 取鍋ライニング残存確認れんが |
EP2530051A1 (en) * | 2011-06-03 | 2012-12-05 | Evonik Solar Norge AS | Reduction furnace body |
JP2022507411A (ja) * | 2018-11-13 | 2022-01-18 | サン-ゴバン セラミックス アンド プラスティクス,インコーポレイティド | 耐火物およびその形成方法 |
-
1978
- 1978-03-29 JP JP53037018A patent/JPS5917347B2/ja not_active Expired
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6028956U (ja) * | 1983-07-29 | 1985-02-27 | 新日本製鐵株式会社 | 取鍋ライニング残存確認れんが |
JPS637419Y2 (ja) * | 1983-07-29 | 1988-03-02 | ||
EP2530051A1 (en) * | 2011-06-03 | 2012-12-05 | Evonik Solar Norge AS | Reduction furnace body |
WO2012163530A1 (en) * | 2011-06-03 | 2012-12-06 | Evonik Solar Norge As | Components of plant, such as reduction furnace body and/or electrode, in particular for a reduction furnace |
JP2022507411A (ja) * | 2018-11-13 | 2022-01-18 | サン-ゴバン セラミックス アンド プラスティクス,インコーポレイティド | 耐火物およびその形成方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS5917347B2 (ja) | 1984-04-20 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS54128415A (en) | Direct reduction furnace | |
GB1262328A (en) | Refractory brick composition | |
CA2124151A1 (en) | High Alumina Refractory Shapes | |
IE40377L (en) | Refractory linings on hot metallurgical ladles. | |
Nagai | BEHAVIOUR OF MAGNESIA CARBON BRICKS CONTAINING ALUMINIUM UNDER VACUUM AT HIGH TEMPERATURE | |
Toritani | Effect of metallic additives on the oxidation-reduction reaction of magnesia-carbon brick | |
GB1109647A (en) | Basic steelmaking | |
JPS5792145A (en) | Tuyere part of refining furnace for metal | |
JPS52134805A (en) | Slag discharge prevention during converter tapping | |
ES8307193A1 (es) | Procedimiento de obtencion de un articulo refractario resistente al desgaste o erosion al metal fundido. | |
ES8306077A1 (es) | "un metodo de fabricar un cuerpo refractario". | |
JPS5294805A (en) | Suppression of local injury in pig iron tapping spout in blast furnace | |
WECHT | THE ROLE OF SILICON CARBIDE IN THE REFRACTORY LINING OF REFUSE INCINERATOR PLANTS | |
JPS51133198A (en) | The manufacturing technique of the nitrided ferrosilicon | |
JPS531605A (en) | Structure of refractory lining of treating vessel and trouch for molten iron | |
JPS5589412A (en) | Preventing method of collapse of converter slag and electric furnace slag | |
BEELEN | THE DEVELOPMENT OF A RENEWED REFRACTORY BRICK FOR THE STEEL CONVERTER | |
Borisov et al. | Improving Converter Lining Life | |
JPS54103717A (en) | Slag forming material | |
JPS55164004A (en) | Prevention of furnace bottom of blast furnace from corrosion | |
JPS54157707A (en) | Prevention of dmage to lined bricks of molten metal container | |
SU589260A1 (ru) | Брикет дл выплавки синтетического шлака | |
JPS572817A (en) | Refining method of molten steel | |
LAMING | BRAVE NEW WORLD. PTS. 1 AND 2 | |
JPS5514811A (en) | Metal mixing car |