JPH0817432A - 充放電式水素電池 - Google Patents
充放電式水素電池Info
- Publication number
- JPH0817432A JPH0817432A JP6180382A JP18038294A JPH0817432A JP H0817432 A JPH0817432 A JP H0817432A JP 6180382 A JP6180382 A JP 6180382A JP 18038294 A JP18038294 A JP 18038294A JP H0817432 A JPH0817432 A JP H0817432A
- Authority
- JP
- Japan
- Prior art keywords
- charge
- hydrogen
- cathode
- palladium
- discharge type
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】
【目的】 水素吸蔵物質と水により充放電電池を作る。
【構成】 水素吸蔵物質の陰極に直流電源で水を電気分
解して水素を吸蔵させる。直流電源をはずせば、水素吸
蔵物質を陰極とした電池になる。
解して水素を吸蔵させる。直流電源をはずせば、水素吸
蔵物質を陰極とした電池になる。
Description
【0001】
【産業上の利用分野】この発明は水素吸蔵物質を陰極に
用いた充放電式水素電池である。
用いた充放電式水素電池である。
【0002】
【従来の技術】以前までの充放電式電池は、金属イオン
と酸またはアルカリイオンとの交換によって充電・放電
がなされていた。
と酸またはアルカリイオンとの交換によって充電・放電
がなされていた。
【0003】
【発明が解決しようとする課題】本発明は水素吸蔵物質
を陰極にし、水だけを用いて充放電式電池を作ることを
可能にするものである。
を陰極にし、水だけを用いて充放電式電池を作ることを
可能にするものである。
【0004】
(イ)水素吸蔵物質の陰極に直流電源で水を電気分解し
て水素を吸蔵させる。 (ロ)直流電源をはずせば、水素吸蔵物質を陰極とした
電池になる。
て水素を吸蔵させる。 (ロ)直流電源をはずせば、水素吸蔵物質を陰極とした
電池になる。
【0005】
【作用】水素吸蔵物質の陰極に直流電源で水を電気分解
して水素を吸蔵させる。直流電源をはずせば、水素吸蔵
物質を陰極とした電池になる。
して水素を吸蔵させる。直流電源をはずせば、水素吸蔵
物質を陰極とした電池になる。
【0006】
【実施例】水素をよく吸蔵するパラジウムを陰極に用
い、伝導性物質を陽極にして、直流電源で水を電気分解
して水素をパラジウムに吸蔵させる。その後、直流電源
をはずせば、パラジウムを陰極とする電池ができる。
い、伝導性物質を陽極にして、直流電源で水を電気分解
して水素をパラジウムに吸蔵させる。その後、直流電源
をはずせば、パラジウムを陰極とする電池ができる。
Claims (1)
- 【請求項1】(イ)水素吸蔵物質の陰極に直流電源で水
を電気分解して水素を吸蔵させる。 (ロ)直流電源をはずせば、水素吸蔵物質を陰極とした
電池になる。 以上により充放電式水素電池を作る。