JPH0790946A - Sealing material and sealing method for concrete panel - Google Patents
Sealing material and sealing method for concrete panelInfo
- Publication number
- JPH0790946A JPH0790946A JP20731893A JP20731893A JPH0790946A JP H0790946 A JPH0790946 A JP H0790946A JP 20731893 A JP20731893 A JP 20731893A JP 20731893 A JP20731893 A JP 20731893A JP H0790946 A JPH0790946 A JP H0790946A
- Authority
- JP
- Japan
- Prior art keywords
- sealing
- sealing material
- concrete panel
- adhesive
- release
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【0001】[0001]
【産業上の利用分野】本発明は、コンクリートパネルの
シーリング用材及びシーリング工法に関するものであ
る。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a sealing material for concrete panels and a sealing method.
【0002】[0002]
【従来の技術及び発明が解決しようとする課題】従来、
軽量気泡コンクリートパネル(以下、ALCパネルとい
う。)の目地のシーリングは、図16に示すような、弾
性を有する長尺状のバックアップ材本体51と、その一
側面に付着された粘着材52と、その粘着材52に添着
された剥離紙53とを備えたバックアップ材50を使用
し、図17〜図19に示すような工法で行われていた。2. Description of the Related Art Conventionally, the problems to be solved by the invention
As shown in FIG. 16, the sealing of the joints of the lightweight cellular concrete panel (hereinafter referred to as ALC panel) has a long elastic backup material main body 51 and an adhesive material 52 attached to one side surface thereof. The backup material 50 provided with the release paper 53 attached to the adhesive material 52 is used, and the method is as shown in FIGS.
【0003】すなわち、剥離紙53を粘着材52から剥
し、図17に示すように、先に建込んだ一方のALCパ
ネル55の端面に、バックアップ材50の一側面を粘着
材52により貼着する。続いて、図18に矢印で示すよ
うに、前記バックアップ材50の他側面に、後に建込む
ALCパネル56の端面を当接させる。そして、図19
に示すように、バックアップ材50を目地底として生じ
たALCパネル55,56の両端面間の目地57にシー
ル材58を充填する。That is, the release paper 53 is peeled from the adhesive material 52 and, as shown in FIG. 17, one side surface of the backup material 50 is attached to the end surface of one of the ALC panels 55 which has been previously installed by the adhesive material 52. . Subsequently, as shown by the arrow in FIG. 18, the end surface of the ALC panel 56 to be built later is brought into contact with the other side surface of the backup material 50. And in FIG.
As shown in FIG. 5, the seal material 58 is filled in the joints 57 between the both end surfaces of the ALC panels 55 and 56 which are formed by using the backup material 50 as the joint bottom.
【0004】ところが、前記シール材58の充填作業は
面倒であり、多くの手間、時間、コスト等がかかるとい
う問題があった。また、シール材58は目地57に完全
に充填されるとは限らず、シール材58とALCパネル
55,56の端面との間に隙間ができ、図19に矢印で
示すように、この隙間からパネル外の雨水等が浸入する
ことがあった。このような場合、バックアップ材50の
一側面は、粘着材52により一方のALCパネル55の
端面に貼着しているので、前記雨水等をパネル内に通さ
ない。しかし、バックアップ材50の他側面は、他方の
ALCパネル56の端面に当接しているだけなので、前
記雨水等をパネル内に通すことがあった。However, the filling work of the sealing material 58 is troublesome, and there is a problem that much labor, time and cost are required. Further, the seal material 58 is not always completely filled in the joint 57, and a gap is formed between the seal material 58 and the end faces of the ALC panels 55 and 56, and as shown by an arrow in FIG. Rainwater outside the panel sometimes entered. In such a case, since one side surface of the backup material 50 is attached to the end surface of the one ALC panel 55 by the adhesive material 52, the rainwater or the like cannot pass through the panel. However, since the other side surface of the backup material 50 is only in contact with the end surface of the other ALC panel 56, the rainwater or the like may pass through the panel.
【0005】上記の問題は、バックアップ材50の他側
面にも粘着材を付着させれば解決できるように思われる
が、従来はそれができなかった。なぜなら、バックアッ
プ材50の他側面にも粘着材を付着させると、その粘着
材に、後に建込む他方のALCパネル56の端面が少し
触れただけで粘着してしまうため、その建込み作業が難
しくなるとか、粘着したバックアップ材50が連れ動い
て破損するとかという問題があったからである。It seems that the above-mentioned problem can be solved by attaching an adhesive material to the other side surface of the backup material 50, but it has not been possible so far. This is because if the adhesive material is attached to the other side surface of the backup material 50, the adhesive material will adhere to the adhesive material even if the end surface of the other ALC panel 56 to be installed later is slightly touched. This is because there is a problem that the backup material 50 that adheres is moved and damaged.
【0006】上記の問題に対応した技術として、実開平
4−20506号公報に開示された粘着剤入りパッキン
が知られている。図20に示すように、このパッキン6
0は、支柱部61と対のリップ62と剥離フィルム63
付き剥離用片64とによって囲まれた収納部65に粘着
剤66を充填してなり、これを一対のパネル67,68
の間に押し込むように挿入し、その後、剥離用片64を
パッキン本体から剥離除去して、粘着剤66をパネル6
7,68の端面に接合するという工法をとるものであ
る。このパッキン60及び工法によれば、リップ62と
粘着剤66とにより水密・気密に密閉できる効果があ
る。As a technique for dealing with the above problem, a packing containing an adhesive, which is disclosed in Japanese Utility Model Laid-Open No. 4-20506, is known. As shown in FIG. 20, this packing 6
0 is a support part 61, a pair of lips 62 and a release film 63.
The accommodating portion 66 is filled in the storage portion 65 surrounded by the peeling strip 64 and the pair of panels 67 and 68.
It is inserted so as to be pushed in between, and then the peeling piece 64 is peeled and removed from the packing main body, and the adhesive 66 is attached to the panel 6.
This is a method of joining to the end faces of 7,68. According to the packing 60 and the method of construction, there is an effect that the lip 62 and the adhesive 66 can seal in a watertight and airtight manner.
【0007】ところが、一対のパネル67,68の間に
挿入したパッキン60の剥離用片64を抓んで剥離する
のは極めて困難であり、同公報の開示の範囲では、現実
に施工することはできなかった。However, it is extremely difficult to carry out the peeling by peeling off the peeling piece 64 of the packing 60 inserted between the pair of panels 67 and 68, and within the scope of the disclosure of the publication, it cannot be actually applied. There wasn't.
【0008】本発明の目的は、上記課題を解決し、コン
クリートパネルの建込み作業を妨げることなく、雨水等
をパネル内に通さない確実なシーリングを実現できると
ともに、施工時に剥離材を容易に引剥すことができ、も
って簡単に施工できる新規なコンクリートパネルのシー
リング用材及びシーリング工法を提供することにある。An object of the present invention is to solve the above problems, to realize a reliable sealing that does not allow rainwater to pass through the panel without hindering the construction work of the concrete panel, and to easily remove the release material during construction. It is an object of the present invention to provide a sealing material for a concrete panel and a sealing method which can be peeled off and can be easily installed.
【0009】[0009]
【課題を解決するための手段】上記目的を達成するため
に、本発明の第一のシーリング用材は、弾性を有する長
尺状のシーリング用材本体と、前記シーリング用材本体
の一側面及び他側面にそれぞれ付着された第一粘着材及
び第二粘着材と、前記第一粘着材及び第二粘着材にそれ
ぞれ添着された第一剥離材及び第二剥離材と、前記第二
剥離材の一部から手前側又は奥側へ延設された引剥用リ
ップとを備えた構成とした。In order to achieve the above object, a first sealing material of the present invention comprises an elongated sealing material body having elasticity and one side surface and another side surface of the sealing material body. First adhesive material and second adhesive material respectively attached, the first release material and the second release material attached to the first adhesive material and the second adhesive material, respectively, from a part of the second release material A peeling lip extending to the front side or the back side is provided.
【0010】本発明の第二のシーリング用材は、弾性を
有する長尺状のシーリング用材本体と、前記シーリング
用材本体の一側面及び他側面にそれぞれ付着された第一
粘着材及び第二粘着材と、前記第一粘着材及び第二粘着
材にそれぞれ添着された第一剥離材及び第二剥離材と、
前記第一剥離材及び第二剥離材のそれぞれの一部から手
前側又は奥側へ延設された引剥用リップとを備えた構成
とした。A second sealing material according to the present invention comprises an elongated sealing material body having elasticity, a first adhesive material and a second adhesive material attached to one side surface and the other side surface of the sealing material body, respectively. A first release material and a second release material respectively attached to the first adhesive material and the second adhesive material,
The peeling lip is provided so as to extend from a part of each of the first release material and the second release material toward the front side or the back side.
【0011】これらのシーリング用材において、シーリ
ング用材本体の材質としては、発泡ゴム、発泡樹脂、ゴ
ム、樹脂、金属等を例示でき、樹脂、金属等を使用する
場合にはその形状を円筒状、U字状等にして弾性をもた
せればよい。粘着材の材質としては、ブチルゴム、樹脂
系粘着材等を例示できる。剥離材の材質は、コンクリー
トパネルが摺っても破損しない強度と、後述する引剥し
が可能な柔軟性とを有していることが好ましく、合成樹
脂、紙、布等を例示できる。但し、第一のシーリング用
材における第一剥離材の材質は、通常の剥離性を有して
いれば何でもよく、例えば安価な紙等で足りる。引剥用
リップは、剥離材の端部を手前側又は奥側へ折り曲げて
なるものでもよいし、剥離材とは別体に形成して第二剥
離材の一部に接続したものでもよい。In these sealing materials, examples of the material of the sealing material body include foamed rubber, foamed resin, rubber, resin and metal. When resin or metal is used, the shape is cylindrical or U. It may be formed in a letter shape or the like to have elasticity. Examples of the material of the adhesive material include butyl rubber and resin-based adhesive material. The material of the release material preferably has strength that does not damage even when the concrete panel is slid and has flexibility that allows peeling, which will be described later, and examples thereof include synthetic resin, paper, and cloth. However, the material of the first release material in the first sealing material may be any material as long as it has normal releasability, and for example, inexpensive paper or the like is sufficient. The peeling lip may be formed by bending the end portion of the release material toward the front side or the back side, or may be formed separately from the release material and connected to a part of the second release material.
【0012】次に、本発明の第一のシーリング工法は、
上記第一のシーリング用材を使用し、前記シーリング用
材から第一剥離材を剥し、隣接させて建込む二つのコン
クリートパネルのうち先に建込んだ第一コンクリートパ
ネルの端面に、前記シーリング用材を第一粘着材により
貼着する工程と、前記シーリング用材の第二剥離材に、
後に建込む第二コンクリートパネルの端面を当接させる
工程と、前記引剥用リップを引張ることにより、前記シ
ーリング用材から第二剥離材を引剥して除去し、第二コ
ンクリートパネルの端面にシーリング用材を第二粘着材
により貼着する工程とを含む構成とした。Next, the first sealing method of the present invention is
Using the first sealing material, peeling the first release material from the sealing material, on the end surface of the first concrete panel built first of the two concrete panels to be built adjacently, the sealing material A step of sticking with one adhesive material, and a second release material of the sealing material,
A step of abutting the end surface of the second concrete panel to be built later, by pulling the peeling lip, the second peeling material is peeled and removed from the sealing material, and a sealing material is attached to the end surface of the second concrete panel. And a step of adhering with a second adhesive material.
【0013】また、本発明の第二のシーリング工法は、
上記第二のシーリング用材を使用し、隣接させて建込ん
だ第一コンクリートパネル及び第二コンクリートパネル
の両端面間に前記シーリング用材を介装し、第一剥離材
及び第二剥離材に該両端面を当接させる工程と、前記引
剥用リップを引張ることにより、前記シーリング用材か
ら第一剥離材及び第二剥離材を引剥して除去し、第一コ
ンクリートパネル及び第二コンクリートパネルの両端面
にシーリング用材を第一粘着材及び第二粘着材により貼
着する工程とを含む構成とした。The second sealing method of the present invention is
Using the second sealing material, the sealing material is interposed between both end surfaces of the first concrete panel and the second concrete panel built adjacently, and the both ends of the first peeling material and the second peeling material. By abutting the surface and pulling the peeling lip, the first peeling material and the second peeling material are peeled and removed from the sealing material, and both end surfaces of the first concrete panel and the second concrete panel are removed. And a step of adhering the sealing material with the first adhesive material and the second adhesive material.
【0014】これらのシーリング工法において、前記シ
ーリング用材を第一コンクリートパネル及び第二コンク
リートパネルの両端面間の正面縁よりやや奥に位置さ
せ、シーリング用材を目地底として生じた第一コンクリ
ートパネル及び第二コンクリートパネルの両端面間の目
地にシール材を充填することができる。シール材は特定
のものに限定されないが、ゴム状の弾性シール材が一般
的であり、アクリル系、シリコン系、ポリサルファイド
系、ポリウレタン系等を例示できる。In these sealing methods, the sealing material is positioned slightly behind the front edge between the end faces of the first concrete panel and the second concrete panel, and the sealing material is used as a joint bottom to form the first concrete panel and the second concrete panel. The joint material between the two end faces of the two concrete panels can be filled with the sealing material. The sealing material is not limited to a specific one, but a rubber-like elastic sealing material is generally used, and examples thereof include acrylic, silicone, polysulfide, and polyurethane.
【0015】また、前記シーリング用材を第一コンクリ
ートパネル及び第二コンクリートパネルの両端面間の正
面縁に位置させ、シーリング用材、第一コンクリートパ
ネル及び第二コンクリートパネルの各正面に連続した塗
装を施すこともできる。Further, the sealing material is positioned at a front edge between both end surfaces of the first concrete panel and the second concrete panel, and continuous coating is applied to each front surface of the sealing material, the first concrete panel and the second concrete panel. You can also
【0016】[0016]
【作用】本発明の第一のシーリング用材又は第一のシー
リング工法によれば、シーリング用材の第二剥離材に、
後に建込む第二コンクリートパネルの端面を当接させる
際、該第二コンクリートパネルの端面が第二剥離材に粘
着しないので、その建込み作業を容易に行える。また、
第二コンクリートパネルの建込み位置を容易に調節で
き、その調節時にシーリング用材が連れ動いて破損する
こともない。また、第二剥離材は引剥用リップの存在に
より手前側又は奥側から容易に引張ることができ、第二
コンクリートパネルとの間から容易に除去できる。そし
て、シーリング用材の両側面が第一及び第二粘着材によ
り第一及び第二コンクリートパネルの両端面に貼着する
ので、雨水等をパネル内に通さない。According to the first sealing material or the first sealing method of the present invention, a second release material for the sealing material,
Since the end surface of the second concrete panel does not adhere to the second release material when the end surface of the second concrete panel to be installed later is brought into contact with the second concrete panel, the installation work can be easily performed. Also,
The installation position of the second concrete panel can be easily adjusted, and the sealing material does not move and be damaged during the adjustment. Further, the second peeling material can be easily pulled from the front side or the back side due to the existence of the peeling lip, and can be easily removed from between the second concrete panel and the second concrete panel. Then, since both side surfaces of the sealing material are attached to both end surfaces of the first and second concrete panels by the first and second adhesive materials, rainwater and the like cannot pass through the panel.
【0017】また、本発明の第二のシーリング用材又は
第二のシーリング工法によれば、シーリング用材の第二
剥離材に、後に建込む第二コンクリートパネルの端面を
当接させる際、該第二コンクリートパネルの端面が第二
剥離材に粘着しないので、その建込み作業を容易に行え
る。また、第二コンクリートパネルの建込み位置を容易
に調節でき、その調節時にシーリング用材が連れ動いて
破損することもない。また、第二剥離材は引剥用リップ
の存在により手前側又は奥側から容易に引張ることがで
き、第二コンクリートパネルとの間から容易に除去でき
る。そして、シーリング用材の両側面が第一及び第二粘
着材により第一及び第二コンクリートパネルの両端面に
貼着するので、雨水等をパネル内に通さない。According to the second sealing material or the second sealing method of the present invention, when the end surface of the second concrete panel to be built later is brought into contact with the second release material of the sealing material, the second sealing material is used. Since the end surface of the concrete panel does not adhere to the second release material, the building work can be performed easily. Further, the installation position of the second concrete panel can be easily adjusted, and the sealing material does not move and be damaged during the adjustment. Further, the second peeling material can be easily pulled from the front side or the back side due to the existence of the peeling lip, and can be easily removed from between the second concrete panel and the second concrete panel. Then, since both side surfaces of the sealing material are attached to both end surfaces of the first and second concrete panels by the first and second adhesive materials, rainwater and the like cannot pass through the panel.
【0018】さらに、前記シーリング用材を第一コンク
リートパネル及び第二コンクリートパネルの両端面間の
正面縁よりやや奥に位置させ、シーリング用材を目地底
として生じた第一コンクリートパネル及び第二コンクリ
ートパネルの両端面間の目地にシール材を充填すれば、
シーリング用材にシール材が加わるので、前記の雨水等
の遮断がより完全になる。Furthermore, the sealing material is located slightly behind the front edge between the both end faces of the first concrete panel and the second concrete panel, and the sealing material is used as a joint bottom to form the first concrete panel and the second concrete panel. If you fill the joint between both end faces with a sealant,
Since the sealing material is added to the sealing material, the interception of rainwater and the like becomes more complete.
【0019】また、前記シーリング用材を第一コンクリ
ートパネル及び第二コンクリートパネルの両端面間の正
面縁に位置させ、シーリング用材、第一コンクリートパ
ネル及び第二コンクリートパネルの各正面に連続した塗
装を施せば、シーリング用材のみによりシーリングを図
ることができるので、面倒なシール材の充填作業が不要
になる。Further, the sealing material is positioned at a front edge between both end surfaces of the first concrete panel and the second concrete panel, and continuous coating is applied to each front surface of the sealing material, the first concrete panel and the second concrete panel. For example, since sealing can be achieved only with the sealing material, troublesome filling work of the sealing material becomes unnecessary.
【0020】[0020]
【実施例】以下、本発明をALCパネルのシーリング用
材及びシーリング工法に具体化した実施例について、図
面を参照して説明する。EXAMPLES Examples in which the present invention is embodied in a sealing material for ALC panels and a sealing method will be described with reference to the drawings.
【0021】まず、図1に示す第一実施例のシーリング
用材1は、長尺四角棒状のシーリング用材本体2を備
え、該本体2は弾性を有する発泡EPDM(エチレン・
プロピレンゴム)により、後述する目地幅(例えば10
mm)より幅広(例えば20mm)に形成されている。
シーリング用材本体2の一側面及び他側面にはそれぞれ
第一粘着材3及び第二粘着材4が付着され、これらの粘
着材には例えば厚さ0.5〜3.0mmのブチルゴムが
使用されている。一側面の第一粘着材3には第一剥離材
5が引剥し可能に添着され、該第一剥離材5には公知の
剥離紙が使用されている。First, the sealing material 1 of the first embodiment shown in FIG. 1 is provided with a long rectangular rod-shaped sealing material main body 2, and the main body 2 is a foamed EPDM (ethylene.
The joint width (for example, 10
mm) wider (for example, 20 mm).
A first adhesive material 3 and a second adhesive material 4 are attached to one side surface and the other side surface of the sealing material body 2, respectively. For example, butyl rubber having a thickness of 0.5 to 3.0 mm is used for these adhesive materials. There is. A first release material 5 is detachably attached to the first adhesive material 3 on one side, and a known release paper is used for the first release material 5.
【0022】他側面の第二粘着材4には第二剥離材6が
引剥し可能に添着され、該第二剥離材6には、ALCパ
ネルが摺っても破損しない強度と後述する引剥しが可能
な柔軟性とを有する合成樹脂テープが使用されている。
また、第二剥離材6の端部には、その端部を手前側へ折
り曲げてなる引剥用リップ7が設けられており、従って
第二粘着材4の端部は露出している。A second peeling material 6 is detachably attached to the second adhesive material 4 on the other side, and the second peeling material 6 has a strength that does not damage the ALC panel even if it slides and a peeling strength described later. A synthetic resin tape having flexibility that can be used is used.
A peeling lip 7 formed by bending the end of the second peeling material 6 toward the front side is provided, and thus the end of the second adhesive material 4 is exposed.
【0023】次に、ALCパネルの目地のシーリング
は、上記シーリング用材1を使用し、図2〜図5に示す
ような工法で行われる。以下、工程順に詳述する。Next, the sealing of the joint of the ALC panel is performed by using the above-mentioned sealing material 1 by the method as shown in FIGS. The steps will be described in detail below.
【0024】まず、シーリング用材1から第一剥離材5
を剥し、隣接させて建込む二つのALCパネルのうち先
に建込んだ第一ALCパネル11の端面に、図2に示す
ように、シーリング用材1を第一粘着材3により貼着す
る。First, the sealing material 1 to the first release material 5
2 is peeled off, and the sealing material 1 is attached to the end surface of the first ALC panel 11 built first out of the two adjacent ALC panels as shown in FIG. 2 by the first adhesive material 3.
【0025】次に、図3に示すように、前記シーリング
用材1の第二剥離材6に、後に建込む第二ALCパネル
12の端面を当接させる。シーリング用材1はその弾性
に抗して幅が狭まる。この当接作業は、第二剥離材6が
第二粘着材4に添着された状態のまま行うので、第二A
LCパネル12の端面は第二剥離材6に触れても粘着せ
ずに滑り、容易に建込み作業を行うことができる。ま
た、ALCパネル12の建込み位置を容易に調節でき、
その調節時にシーリング用材1が連れ動いて破損するこ
ともない。この当接作業後は、第二剥離材6の引剥用リ
ップ7がパネル外にとび出した状態となる。Next, as shown in FIG. 3, the end surface of the second ALC panel 12 to be built later is brought into contact with the second release material 6 of the sealing material 1. The sealing material 1 narrows in width against its elasticity. This contacting work is performed while the second release material 6 is still attached to the second adhesive material 4, so that the second A
Even if the end surface of the LC panel 12 touches the second release material 6, the end surface of the LC panel 12 slides without sticking, and the building work can be easily performed. Also, the installation position of the ALC panel 12 can be easily adjusted,
The sealing material 1 will not move and be damaged during the adjustment. After this contacting work, the peeling lip 7 of the second release material 6 is in a state of protruding outside the panel.
【0026】続いて、図4に示すように、引剥用リップ
7を引張ることにより、シーリング用材1の第二粘着材
4から第二剥離材6を引剥して、第二ALCパネル12
との間から除去する。このとき、第二剥離材6は引剥用
リップ7の存在により手前側から容易に引張ることがで
き、また、第二剥離材6は柔軟性を有しているので容易
に除去できる。このように第二剥離材6を除去すれば、
当然、第二ALCパネル12の端面にシーリング用材1
が第二粘着材4により貼着する。同図は、シーリング用
材1を第一ALCパネル11及び第二ALCパネル12
の両端面間の正面縁よりやや奥に位置させた場合を示し
ている。Subsequently, as shown in FIG. 4, by pulling the peeling lip 7, the second peeling material 6 is peeled from the second adhesive material 4 of the sealing material 1, and the second ALC panel 12 is removed.
Remove from between. At this time, the second peeling material 6 can be easily pulled from the front side due to the existence of the peeling lip 7, and the second peeling material 6 has flexibility and can be easily removed. By removing the second release material 6 in this way,
Naturally, the sealing material 1 is attached to the end surface of the second ALC panel 12.
Are attached by the second adhesive material 4. In the figure, the sealing material 1 is provided with a first ALC panel 11 and a second ALC panel 12.
It shows a case where it is located slightly behind the front edge between both end faces of.
【0027】そして、図5に示すように、前記シーリン
グ用材1を目地底とするALCパネル11,12の両端
面間の目地にシール材14を充填する。シール材14に
は例えばアクリル系を使用する。但し、このシール材1
4は必ずしも完全に目地13に充填されるとは限らず、
シール材14とALCパネル11,12の端面との間に
隙間ができ、同図に矢印で示すように、この隙間からパ
ネル外の雨水等が浸入することがある。しかし、本実施
例によれば、シーリング用材1の両側面が第一及び第二
粘着材3,4により第一及び第二ALCパネル11,1
2の両端面に貼着しているので、前記雨水等をパネル内
に通さない。なお、シール材14、第一及び第二ALC
パネル11,12の各正面には、通常、塗装(図示略)
を施す。Then, as shown in FIG. 5, the sealing material 14 is filled in the joints between the both end surfaces of the ALC panels 11 and 12 having the sealing material 1 as the joint bottom. Acrylic is used for the sealing material 14, for example. However, this sealing material 1
4 is not always completely filled in the joint 13,
A gap is formed between the seal material 14 and the end faces of the ALC panels 11 and 12, and rainwater and the like outside the panel may intrude through the gap as shown by an arrow in the figure. However, according to the present embodiment, the first and second ALC panels 11, 1 are formed on both side surfaces of the sealing material 1 by the first and second adhesive materials 3, 4.
Since it is attached to both end faces of 2, the rainwater and the like do not pass through the panel. In addition, the sealing material 14, the first and second ALC
Normally, a coating (not shown) is provided on each front surface of the panels 11 and 12.
Give.
【0028】上記第一実施例はシーリング用材1をシー
ル材14のバックアップ材として使用する工法であっ
た。これに対し、図6は第一実施例のシーリング工法の
変更例を示し、シーリング用材1を第一及び第二ALC
パネル11,12の両端面の正面縁に位置させ、前記シ
ール材の充填は行わないようにしたものである。そし
て、シーリング用材1の正面に塗装下地としてのプライ
マ処理(図示略)を行った後、シーリング用材1、第一
及び第二ALCパネル11,12の各正面に連続した塗
装15を施して完了とする。なお、この変更例を採用す
る場合、シーリング用材本体2は非通水性又は難通水性
であることが好ましく、従って、該本体2が発泡体の場
合、独立発泡が好ましい。一方、上記第一実施例のシー
リング工法を採用する場合、シーリング用材本体2は通
水性でもよく、従って、該本体2が発泡体の場合、独立
発泡を潰して柔軟性を高めたものでもよい。The above-mentioned first embodiment is a construction method in which the sealing material 1 is used as a backup material for the sealing material 14. On the other hand, FIG. 6 shows a modification of the sealing method of the first embodiment, in which the sealing material 1 is the first and second ALC.
The panels 11 and 12 are located at the front edges of both end surfaces so that the sealing material is not filled. Then, after performing a primer treatment (not shown) as a coating base on the front surface of the sealing material 1, a continuous coating 15 is applied to each front surface of the sealing material 1 and the first and second ALC panels 11 and 12 to complete. To do. When this modified example is adopted, the sealing material body 2 is preferably water-impermeable or water-impermeable, and therefore, when the body 2 is a foam, independent foaming is preferable. On the other hand, when the sealing method of the first embodiment is adopted, the sealing material main body 2 may be water permeable, and therefore, when the main body 2 is a foam, it may be one in which independent foaming is crushed to enhance flexibility.
【0029】この変更例によれば、面倒なシール材の充
填作業が不要になるので、シーリング工法に要する手
間、時間、コスト等を大幅に削減でき、資源の節約にも
貢献できる。According to this modified example, since the troublesome filling work of the sealing material becomes unnecessary, the labor, time, cost, etc. required for the sealing method can be greatly reduced, and the resource can be saved.
【0030】次に、図7に示す第二実施例のシーリング
用材21は、シーリング用材本体と第二剥離材において
のみ第一実施例と相違する。すなわち、本実施例のシー
リング用材本体22は発泡EPDMにより長尺円筒状に
形成され、その外径は目地幅より幅広に形成されてい
る。また、第二剥離材26は強化紙が使用されている。
27は引剥用リップである。なお、第一実施例と同様の
部材については、図に共通の符号を付して重複説明を避
ける。Next, the sealing material 21 of the second embodiment shown in FIG. 7 differs from the first embodiment only in the sealing material body and the second release material. That is, the sealing material main body 22 of the present embodiment is formed of foamed EPDM into a long cylindrical shape, and its outer diameter is formed wider than the joint width. The second release material 26 is reinforced paper.
27 is a peeling lip. It should be noted that the same members as those in the first embodiment are designated by common reference numerals in the drawings to avoid redundant description.
【0031】このシーリング用材21も、上記第一実施
例又はその変更例と同様のシーリング工法に使用するこ
とができる。すなわち、図8は、第二剥離材26をシー
リング用材21と第二ALCパネル12との間から除去
する工程を示し、シーリング用材本体22はALCパネ
ル11,12に挾まれて楕円形に変形している。この工
程後、目地にシール材を充填すればよい。また、図9
は、シーリング用材21、第一及び第二ALCパネル1
1,12の各正面に連続した塗装15を施した状態を示
している。This sealing material 21 can also be used in the same sealing method as in the first embodiment or its modification. That is, FIG. 8 shows a step of removing the second release material 26 from between the sealing material 21 and the second ALC panel 12, and the sealing material body 22 is sandwiched between the ALC panels 11 and 12 and deformed into an elliptical shape. ing. After this step, the joint material may be filled with the sealing material. In addition, FIG.
Is a sealing material 21, first and second ALC panel 1
It shows a state in which a continuous coating 15 is applied to each of the front surfaces 1 and 12.
【0032】次に、図10に示す第三実施例のシーリン
グ用材31も、シーリング用材本体と第二剥離材におい
てのみ第一実施例と相違する。すなわち、本実施例のシ
ーリング用材本体32は金属薄板により断面変形U字状
に形成され、目地幅より幅広に形成されている。また、
第二剥離材36は表面の平滑な布が使用されている。3
7は引剥用リップである。なお、第一実施例と同様の部
材については、図に共通の符号を付して重複説明を避け
る。Next, the sealing material 31 of the third embodiment shown in FIG. 10 also differs from the first embodiment only in the sealing material body and the second release material. That is, the sealing material main body 32 of the present embodiment is formed of a thin metal plate in a U-shaped cross-section and is wider than the joint width. Also,
As the second release material 36, a cloth having a smooth surface is used. Three
7 is a peeling lip. It should be noted that the same members as those in the first embodiment are designated by common reference numerals in the drawings to avoid redundant description.
【0033】このシーリング用材31も、上記第一実施
例又はその変更例と同様のシーリング工法に使用するこ
とができる。すなわち、図11は、第二剥離材36をシ
ーリング用材31と第二ALCパネル12との間から除
去する工程を示し、シーリング用材本体32はALCパ
ネル11,12に挾まれて幅狭に変形している。この工
程後、目地にシール材を充填すればよい。This sealing material 31 can also be used in the same sealing method as in the first embodiment or its modification. That is, FIG. 11 shows a step of removing the second release material 36 from between the sealing material 31 and the second ALC panel 12, and the sealing material body 32 is sandwiched between the ALC panels 11 and 12 and deformed to a narrow width. ing. After this step, the joint material may be filled with the sealing material.
【0034】続いて、図12はシーリング用材の他の実
施例を示し、(a)の第四実施例のシーリング用材41
は発泡EPDMよりなる丸棒状のシーリング用材本体4
2を備えたもの、(b)の第五実施例のシーリング用材
51は発泡EPDMよりなる半丸棒状のシーリング用材
本体52を備えたもの、(c)の第六実施例のシーリン
グ用材61は発泡EPDMよりなる半円筒状のシーリン
グ用材本体62を備えたものである。また、(d)の第
七実施例のシーリング用材71は合成樹脂又は金属製の
薄板よりなる断面U字状のシーリング用材本体72を備
えたもの、(e)の第八実施例のシーリング用材81は
合成樹脂又は金属製の薄壁よりなる円筒状のシーリング
用材本体82を備えたものである。これらのシーリング
用材の他の部材は第一実施例と同様であり、シーリング
工法も同様である。Next, FIG. 12 shows another embodiment of the sealing material, which is the sealing material 41 of the fourth embodiment of FIG.
Is a round bar-shaped sealing material body 4 made of foamed EPDM
2, the sealing material 51 of the fifth embodiment shown in (b) has a semicircular rod-shaped sealing material body 52 made of foamed EPDM, and the sealing material 61 of the sixth embodiment shown in (c) is foamed. A semi-cylindrical sealing material body 62 made of EPDM is provided. The sealing material 71 of the seventh embodiment (d) includes a sealing material body 72 having a U-shaped cross section made of a synthetic resin or metal thin plate, and the sealing material 81 of the eighth embodiment (e). Is provided with a cylindrical sealing material body 82 made of a synthetic resin or a metal thin wall. The other members of these sealing materials are the same as in the first embodiment, and the sealing method is also the same.
【0035】次に、図13及び図14は第一実施例の変
更例を示し、シーリング用材1の引剥用リップ7の長さ
を数十cm〜十数mと長くしたものである。こうするこ
とにより、図13に示すように、第一ALCパネル11
及び第二ALCパネル12の近傍に障害物16等があっ
て、シーリング用材1付近まで手を伸ばせないようなと
きでも、長くとび出した引剥用リップ7を遠方から引張
ることにより、剥離材(図示略)を容易に引剥すことが
できる。また、図14に示すように、複数のシーリング
用材1の引剥用リップ7を一箇所に束ねて遠方から引張
ることにより、複数の剥離材(図示略)を同時に引剥す
こともできる。Next, FIGS. 13 and 14 show a modification of the first embodiment, in which the peeling lip 7 of the sealing material 1 is made as long as several tens cm to tens of m. By doing so, as shown in FIG. 13, the first ALC panel 11
Also, even when there is an obstacle 16 or the like in the vicinity of the second ALC panel 12 and the hand cannot reach the vicinity of the sealing material 1, the peeling material (illustrated in the figure Can be easily peeled off. Further, as shown in FIG. 14, a plurality of peeling materials (not shown) can be peeled off at the same time by bundling the peeling lips 7 of the plurality of sealing materials 1 in one place and pulling them from a distance.
【0036】図15も第一実施例の変更例を示し、その
シーリング用材1は、第一剥離材5の端部にも引剥用リ
ップ7が手前側へ延設されている点においてのみ、第一
実施例と相違している。また、そのシーリング工法は、
隣接させて建込んだ第一ALCパネル11及び第二AL
Cパネル12の両端面間にシーリング用材1を介装し、
第一剥離材5及び第二剥離材6に該両端面を当接させた
後、両剥離材5,6の引剥用リップ7を引張ることによ
り、シーリング用材1から両剥離材5,6を引剥して除
去し、両ALCパネル11,12の両端面にシーリング
用材1を第一粘着材3及び第二粘着材4により貼着する
というものである。この変更例によっても、第一実施例
と同様の効果が得られる。FIG. 15 also shows a modification of the first embodiment, in which the sealing material 1 has a peeling lip 7 extending toward the front side at the end of the first peeling material 5 as well. This is different from the first embodiment. In addition, the sealing method is
First ALC panel 11 and second AL built adjacent to each other
The sealing material 1 is interposed between both end surfaces of the C panel 12,
After the both end surfaces are brought into contact with the first release material 5 and the second release material 6, the peeling lips 7 of both release materials 5, 6 are pulled to remove both release materials 5, 6 from the sealing material 1. It is peeled off and removed, and the sealing material 1 is attached to both end surfaces of both ALC panels 11 and 12 by the first adhesive material 3 and the second adhesive material 4. Also with this modification, the same effect as that of the first embodiment can be obtained.
【0037】なお、本発明は前記実施例の構成に限定さ
れず、例えば非発泡のコンクリートパネルのシーリング
に具体化する等、発明の趣旨から逸脱しない範囲で適宜
変更して具体化することもできる。The present invention is not limited to the construction of the above-mentioned embodiment, and may be embodied by appropriately modifying it within a range not departing from the spirit of the invention, for example, embodying it in a non-foaming concrete panel sealing. .
【0038】[0038]
【発明の効果】以上詳述した通り、本発明に係る請求項
1、2、3又は4記載のシーリング用材又はシーリング
工法によれば、コンクリートパネルの建込み作業を妨げ
ることなく、雨水等をパネル内に通さない確実なシーリ
ングを実現できるとともに、施工時に剥離材を容易に引
剥すことができ、もって簡単に施工できるという優れた
効果を奏する。As described in detail above, according to the sealing material or the sealing method according to the first aspect of the present invention, rainwater or the like is applied to the panel without hindering the concrete panel construction work. It is possible to realize a reliable sealing that does not pass through the inside, and the peeling material can be easily peeled off at the time of construction, which is an excellent effect that construction can be performed easily.
【0039】さらに、請求項5記載のシーリング工法に
よれば、前記の雨水等の遮断がより完全になる。Furthermore, according to the sealing method of the fifth aspect, the interception of rainwater and the like becomes more complete.
【0040】また、請求項6記載のシーリング工法によ
れば、面倒なシール材の充填作業が不要になり、シーリ
ング工法に要する手間、時間、コスト等を大幅に削減で
き、資源の節約にも貢献できる。Further, according to the sealing method of the sixth aspect, the troublesome filling work of the sealing material becomes unnecessary, and the labor, time, cost, etc. required for the sealing method can be greatly reduced, and also contributes to resource saving. it can.
【図1】本発明の第一実施例のシーリング用材を示す斜
視図である。FIG. 1 is a perspective view showing a sealing material according to a first embodiment of the present invention.
【図2】同実施例のシーリング工法における第一ALC
パネルへのシーリング用材の貼着工程を示し、(a)は
正面図、(b)は断面図である。FIG. 2 is a first ALC in the sealing method of the embodiment.
The sticking process of the sealing material to a panel is shown, (a) is a front view, (b) is sectional drawing.
【図3】同じく第二ALCパネルの建込み工程を示し、
(a)は正面図、(b)は断面図である。FIG. 3 also shows a second ALC panel installation process,
(A) is a front view and (b) is a sectional view.
【図4】同じくシーリング用材からの第二剥離材の除去
工程を示し、(a)は正面図、(b)は同(a)のIV
b−IVb線断面図、(c)は同(a)のIVc−IV
c線断面図である。4A and 4B also show a step of removing the second release material from the sealing material, wherein FIG. 4A is a front view and FIG. 4B is IV of FIG. 4A.
b-IVb line sectional drawing, (c) is IVc-IV of the same (a)
It is a c line sectional view.
【図5】同じく目地へのシール材の充填工程を示し、
(a)は正面図、(b)は断面図である。FIG. 5 also shows a process of filling the joint with the sealing material,
(A) is a front view and (b) is a sectional view.
【図6】同実施例の変更例のシーリング工法を示す断面
図である。FIG. 6 is a cross-sectional view showing a sealing method of a modified example of the same embodiment.
【図7】第二実施例のシーリング用材を示す斜視図であ
る。FIG. 7 is a perspective view showing a sealing material of a second embodiment.
【図8】同実施例のシーリング工法におけるシーリング
用材からの第二剥離材の除去工程を示し、(a)は正面
図、(b)は同(a)のVIII b−VIII b線断面図、
(c)は同(a)のVIII c−VIII c線断面図であ
る。FIG. 8 shows a step of removing the second release material from the sealing material in the sealing method of the embodiment, (a) is a front view, (b) is a sectional view taken along line VIIIb-VIIIb of (a),
(C) is a VIII c-VIII c line sectional view of the same (a).
【図9】同実施例の変更例のシーリング工法を示す断面
図である。FIG. 9 is a sectional view showing a sealing method of a modified example of the same embodiment.
【図10】第三実施例のシーリング用材を示す斜視図で
ある。FIG. 10 is a perspective view showing a sealing material of a third embodiment.
【図11】同実施例のシーリング工法におけるシーリン
グ用材からの第二剥離材の除去工程を示し、(a)は正
面図、(b)は同(a)のXIb−XIb線断面図、
(c)は同(a)のXIc−XIc線断面図である。FIG. 11 shows a step of removing the second release material from the sealing material in the sealing method of the embodiment, (a) is a front view, (b) is a sectional view taken along line XIb-XIb of (a),
(C) is the XIc-XIc sectional view taken on the line of the same (a).
【図12】他の実施例のシーリング用材を示す断面図で
ある。FIG. 12 is a sectional view showing a sealing material of another example.
【図13】第一実施例の変更例のシーリング用材及びシ
ーリング工法を示す正面図である。FIG. 13 is a front view showing a sealing material and a sealing method according to a modified example of the first embodiment.
【図14】同変更例の別の用法を示す正面図である。FIG. 14 is a front view showing another usage of the modification.
【図15】第一実施例の別の変更例を示し、(a)は正
面図、(b)は同(a)のXVb−XVb線断面図、
(c)は同(a)のXVc−XVc線断面図である。FIG. 15 shows another modification of the first embodiment, (a) is a front view, (b) is a sectional view taken along line XVb-XVb in (a),
(C) is the XVc-XVc line sectional view of the same (a).
【図16】従来例のシーリング用材を示す斜視図であ
る。FIG. 16 is a perspective view showing a sealing material of a conventional example.
【図17】従来例のシーリング工法における一方のAL
Cパネルへのシーリング用材の貼着工程を示し、(a)
は正面図、(b)は断面図である。FIG. 17: One AL in the conventional sealing method
The step of attaching the sealing material to the C panel is shown (a)
Is a front view and (b) is a sectional view.
【図18】同じく他方のALCパネルの建込み工程を示
し、(a)は正面図、(b)は断面図である。FIG. 18 is a view showing the assembling process of the other ALC panel, (a) is a front view and (b) is a sectional view.
【図19】同じく目地へのシール材の充填工程を示し、
(a)は正面図、(b)は断面図である。FIG. 19 also shows a process of filling the joint with the sealing material,
(A) is a front view and (b) is a sectional view.
【図20】従来例のパッキンを示し、(a)はパッキン
の断面図、(b)はそのシーリング工法の斜視図であ
る。す断面図である。FIG. 20 shows a packing of a conventional example, (a) is a sectional view of the packing, and (b) is a perspective view of the sealing method. FIG.
1 シーリング用材 2 シーリング
用材本体 3 第一粘着材 4 第二粘着材 5 第一剥離材 6 第二剥離材 7 引剥用リップ 11 第一ALC
パネル 12 第二ALCパネル 13 目地 14 シール材 15 塗装 21 シーリング用材 22 シーリン
グ用材本体 26 第二剥離材 27 引剥用リ
ップ 31 シーリング用材 32 シーリン
グ用材本体 36 第二剥離材 37 引剥用リ
ップ 41 シーリング用材 42 シーリン
グ用材本体 51 シーリング用材 52 シーリン
グ用材本体 61 シーリング用材 62 シーリン
グ用材本体 71 シーリング用材 72 シーリン
グ用材本体 81 シーリング用材 82 シーリン
グ用材本体1 Sealing Material 2 Sealing Material Main Body 3 First Adhesive Material 4 Second Adhesive Material 5 First Release Material 6 Second Release Material 7 Peeling Lip 11 First ALC
Panel 12 Second ALC panel 13 Joint 14 Sealing material 15 Coating 21 Sealing material 22 Sealing material body 26 Second peeling material 27 Peeling lip 31 Sealing material 32 Sealing material body 36 Second peeling material 37 Peeling lip 41 Sealing material 42 Sealing Material Body 51 Sealing Material 52 Sealing Material Body 61 Sealing Material 62 Sealing Material Body 71 Sealing Material 72 Sealing Material Body 81 Sealing Material 82 Sealing Material Body
─────────────────────────────────────────────────────
─────────────────────────────────────────────────── ───
【手続補正書】[Procedure amendment]
【提出日】平成5年10月1日[Submission date] October 1, 1993
【手続補正1】[Procedure Amendment 1]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】特許請求の範囲[Name of item to be amended] Claims
【補正方法】変更[Correction method] Change
【補正内容】[Correction content]
【特許請求の範囲】[Claims]
【手続補正2】[Procedure Amendment 2]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】0009[Correction target item name] 0009
【補正方法】変更[Correction method] Change
【補正内容】[Correction content]
【0009】[0009]
【課題を解決するための手段】上記目的を達成するため
に、本発明の第一のシーリング用材は、弾性を有する長
尺状のシーリング用材本体と、前記シーリング用材本体
の一側面及び他側面にそれぞれ付着された第一粘着材及
び第二粘着材と、前記第一粘着材及び第二粘着材にそれ
ぞれ添着された第一剥離材及び第二剥離材と、前記第二
剥離材の一部から延設された引剥用リップとを備えた構
成とした。In order to achieve the above object, a first sealing material of the present invention comprises an elongated sealing material body having elasticity and one side surface and another side surface of the sealing material body. First adhesive material and second adhesive material respectively attached, the first release material and the second release material attached to the first adhesive material and the second adhesive material, respectively, from a part of the second release material The peeling lip extended is provided.
【手続補正3】[Procedure 3]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】0010[Correction target item name] 0010
【補正方法】変更[Correction method] Change
【補正内容】[Correction content]
【0010】本発明の第二のシーリング用材は、弾性を
有する長尺状のシーリング用材本体と、前記シーリング
用材本体の一側面及び他側面にそれぞれ付着された第一
粘着材及び第二粘着材と、前記第一粘着材及び第二粘着
材にそれぞれ添着された第一剥離材及び第二剥離材と、
前記第一剥離材及び第二剥離材のそれぞれの一部から延
設された引剥用リップとを備えた構成とした。A second sealing material according to the present invention comprises an elongated sealing material body having elasticity, a first adhesive material and a second adhesive material attached to one side surface and the other side surface of the sealing material body, respectively. A first release material and a second release material respectively attached to the first adhesive material and the second adhesive material,
Extend from a part of each of the first release material and the second release material
The peeling lip is provided.
Claims (6)
体と、前記シーリング用材本体の一側面及び他側面にそ
れぞれ付着された第一粘着材及び第二粘着材と、前記第
一粘着材及び第二粘着材にそれぞれ添着された第一剥離
材及び第二剥離材と、前記第二剥離材の一部から手前側
又は奥側へ延設された引剥用リップとを備えたコンクリ
ートパネルのシーリング用材。1. A long elastic sealing material body, a first adhesive material and a second adhesive material attached to one side surface and the other side surface of the sealing material body, the first adhesive material and the second adhesive material, respectively. (2) Sealing of a concrete panel provided with a first release material and a second release material respectively attached to an adhesive material, and a peeling lip extending from a part of the second release material to the front side or the back side. Lumber.
体と、前記シーリング用材本体の一側面及び他側面にそ
れぞれ付着された第一粘着材及び第二粘着材と、前記第
一粘着材及び第二粘着材にそれぞれ添着された第一剥離
材及び第二剥離材と、前記第一剥離材及び第二剥離材の
それぞれの一部から手前側又は奥側へ延設された引剥用
リップとを備えたコンクリートパネルのシーリング用
材。2. An elongate sealing material body having elasticity, a first adhesive material and a second adhesive material attached to one side surface and the other side surface of the sealing material body, the first adhesive material and the second adhesive material, respectively. (2) a first release material and a second release material which are respectively attached to the adhesive material, and a peeling lip extending from a part of each of the first release material and the second release material to the front side or the back side. Sealing material for concrete panels with.
体と、前記シーリング用材本体の一側面及び他側面にそ
れぞれ付着された第一粘着材及び第二粘着材と、前記第
一粘着材及び第二粘着材にそれぞれ添着された第一剥離
材及び第二剥離材と、前記第二剥離材の一部から手前側
又は奥側へ延設された引剥用リップとを備えたコンクリ
ートパネルのシーリング用材を使用し、 前記シーリング用材から第一剥離材を剥し、隣接させて
建込む二つのコンクリートパネルのうち先に建込んだ第
一コンクリートパネルの端面に、前記シーリング用材を
第一粘着材により貼着する工程と、 前記シーリング用材の第二剥離材に、後に建込む第二コ
ンクリートパネルの端面を当接させる工程と、 前記引剥用リップを引張ることにより、前記シーリング
用材から第二剥離材を引剥して除去し、第二コンクリー
トパネルの端面にシーリング用材を第二粘着材により貼
着する工程とを含むコンクリートパネルのシーリング工
法。3. An elongate sealing material body having elasticity, a first adhesive material and a second adhesive material attached to one side surface and the other side surface of the sealing material body, the first adhesive material and the second adhesive material, respectively. (2) Sealing of a concrete panel provided with a first release material and a second release material respectively attached to an adhesive material, and a peeling lip extending from a part of the second release material to the front side or the back side. Using a material, peel the first release material from the sealing material, and attach the sealing material with a first adhesive material to the end surface of the first concrete panel built first of the two concrete panels to be built adjacent to each other. And a step of bringing the end surface of a second concrete panel to be built into contact with the second release material of the sealing material, and pulling the peeling lip to remove the sealing material. The second peeling material is peeled off and removed, and the sealing material is attached to the end surface of the second concrete panel with the second adhesive material.
体と、前記シーリング用材本体の一側面及び他側面にそ
れぞれ付着された第一粘着材及び第二粘着材と、前記第
一粘着材及び第二粘着材にそれぞれ添着された第一剥離
材及び第二剥離材と、前記第一剥離材及び第二剥離材の
それぞれの一部から手前側又は奥側へ延設された引剥用
リップとを備えたコンクリートパネルのシーリング用材
を使用し、 隣接させて建込んだ第一コンクリートパネル及び第二コ
ンクリートパネルの両端面間に前記シーリング用材を介
装し、第一剥離材及び第二剥離材に該両端面を当接させ
る工程と、 前記引剥用リップを引張ることにより、前記シーリング
用材から第一剥離材及び第二剥離材を引剥して除去し、
第一コンクリートパネル及び第二コンクリートパネルの
両端面にシーリング用材を第一粘着材及び第二粘着材に
より貼着する工程とを含むコンクリートパネルのシーリ
ング工法。4. An elongate sealing material body having elasticity, a first adhesive material and a second adhesive material attached to one side surface and the other side surface of the sealing material body, the first adhesive material and the second adhesive material, respectively. (2) a first release material and a second release material which are respectively attached to the adhesive material, and a peeling lip extending from a part of each of the first release material and the second release material to the front side or the back side. Using a sealing material for a concrete panel provided with, the sealing material is interposed between both end faces of the first concrete panel and the second concrete panel that are built adjacent to each other. A step of bringing the both end surfaces into contact with each other, by pulling the peeling lip, the first peeling material and the second peeling material are peeled and removed from the sealing material,
A method for sealing a concrete panel, comprising a step of attaching a sealing material to both end faces of the first concrete panel and the second concrete panel with the first adhesive material and the second adhesive material.
パネル及び第二コンクリートパネルの両端面間の正面縁
よりやや奥に位置させ、シーリング用材を目地底として
生じた第一コンクリートパネル及び第二コンクリートパ
ネルの両端面間の目地にシール材を充填することを特徴
とする請求項3又は4記載のコンクリートパネルのシー
リング工法。5. The first concrete panel and the second concrete panel, wherein the sealing material is located slightly behind the front edge between both end faces of the first concrete panel and the second concrete panel, and the sealing material is used as a joint bottom. The sealing method for a concrete panel according to claim 3 or 4, wherein the joint material between both end faces is filled with a sealing material.
パネル及び第二コンクリートパネルの両端面間の正面縁
に位置させ、シーリング用材、第一コンクリートパネル
及び第二コンクリートパネルの各正面に連続した塗装を
施すことを特徴とする請求項3又は4記載のコンクリー
トパネルのシーリング工法。6. The sealing material is located at a front edge between both end faces of the first concrete panel and the second concrete panel, and continuous coating is applied to each front surface of the sealing material, the first concrete panel and the second concrete panel. The concrete panel sealing method according to claim 3 or 4, characterized in that.