JPH0784612B2 - Ca快削鋼の溶製方法 - Google Patents
Ca快削鋼の溶製方法Info
- Publication number
- JPH0784612B2 JPH0784612B2 JP6368991A JP6368991A JPH0784612B2 JP H0784612 B2 JPH0784612 B2 JP H0784612B2 JP 6368991 A JP6368991 A JP 6368991A JP 6368991 A JP6368991 A JP 6368991A JP H0784612 B2 JPH0784612 B2 JP H0784612B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- inclusions
- free
- composition
- machinability
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Treatment Of Steel In Its Molten State (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6368991A JPH0784612B2 (ja) | 1991-03-06 | 1991-03-06 | Ca快削鋼の溶製方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6368991A JPH0784612B2 (ja) | 1991-03-06 | 1991-03-06 | Ca快削鋼の溶製方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH04280911A JPH04280911A (ja) | 1992-10-06 |
| JPH04280911A5 JPH04280911A5 (enExample) | 1994-04-19 |
| JPH0784612B2 true JPH0784612B2 (ja) | 1995-09-13 |
Family
ID=13236599
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6368991A Expired - Lifetime JPH0784612B2 (ja) | 1991-03-06 | 1991-03-06 | Ca快削鋼の溶製方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0784612B2 (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2003293027A (ja) * | 2002-04-09 | 2003-10-15 | Daido Steel Co Ltd | カルシウム快削ステンレス鋼の製造方法 |
| JP5137082B2 (ja) * | 2008-12-19 | 2013-02-06 | 新日鐵住金株式会社 | 機械構造用鋼材およびその製造方法 |
-
1991
- 1991-03-06 JP JP6368991A patent/JPH0784612B2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH04280911A (ja) | 1992-10-06 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Luyckx et al. | Sulfide shape control in high strength low alloy steels | |
| Yang et al. | Optimum composition of CaO-SiO2-Al2O3-MgO slag for spring steel deoxidized by Si and Mn in production | |
| PL148685B1 (en) | Ferrosilicon inoculant for cast iron | |
| CN105734397A (zh) | 一种高强度灰铸铁材料及其熔炼浇注工艺 | |
| JP6937190B2 (ja) | Ni−Cr−Mo−Nb合金およびその製造方法 | |
| LU502587B1 (en) | Low-cost, high-strength ferritic nodular cast iron, and preparation method and use thereof | |
| JPH06128618A (ja) | 介在物の少ない電磁鋼板の製造方法 | |
| Seidu et al. | Control of chilling tendency in grey cast iron reuse | |
| JP2991796B2 (ja) | マグネシウム脱酸による薄鋼板の溶製方法 | |
| CN116516111A (zh) | 一种硬线钢的高效脱硫低铝合成渣及冶炼工艺 | |
| SU1002392A1 (ru) | Раскислитель | |
| JP5199543B2 (ja) | アルミキルド鋼の溶製方法 | |
| JPH04280911A (ja) | Ca快削鋼の溶製方法 | |
| CN114134391A (zh) | 控制含硫低合金钢硫含量的冶炼方法 | |
| JP4107801B2 (ja) | 磁気特性に優れたFe−Ni系パーマロイ合金の製造方法 | |
| RU2269577C1 (ru) | Способ получения стали в дуговой электросталеплавильной печи | |
| Riposan et al. | Benefits of residual aluminum in ductile iron | |
| RU2070603C1 (ru) | Модификатор для быстрорежущей стали | |
| RU2051984C1 (ru) | Сталь | |
| SU1044653A1 (ru) | Сплав дл раскислени легировани и модифицировани стали | |
| Aydemir | Use of aluminium dross for slag treatment in secondary steelmaking to decrease amount of reducible oxides in ladle furnace | |
| SU1617031A1 (ru) | Лигатура дл стали | |
| SU1633002A1 (ru) | Лигатура дл стали | |
| RU1770438C (ru) | Жаростойкий алюминиевый чугун | |
| JP4357082B2 (ja) | 含クロム溶鋼の脱炭精錬方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 Effective date: 19960227 |