JPH07240203A5 - - Google Patents

Info

Publication number
JPH07240203A5
JPH07240203A5 JP6-27919A JP2791994A JPH07240203A5 JP H07240203 A5 JPH07240203 A5 JP H07240203A5 JP 2791994 A JP2791994 A JP 2791994A JP H07240203 A5 JPH07240203 A5 JP H07240203A5
Authority
JP
Japan
Prior art keywords
mixing
lead
water
sulfuric acid
kneading
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP6-27919A
Other languages
English (en)
Japanese (ja)
Other versions
JPH07240203A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP6027919A priority Critical patent/JPH07240203A/ja
Priority claimed from JP6027919A external-priority patent/JPH07240203A/ja
Publication of JPH07240203A publication Critical patent/JPH07240203A/ja
Publication of JPH07240203A5 publication Critical patent/JPH07240203A5/ja
Pending legal-status Critical Current

Links

JP6027919A 1994-02-25 1994-02-25 鉛蓄電池用負極板ペーストの製造方法 Pending JPH07240203A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP6027919A JPH07240203A (ja) 1994-02-25 1994-02-25 鉛蓄電池用負極板ペーストの製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP6027919A JPH07240203A (ja) 1994-02-25 1994-02-25 鉛蓄電池用負極板ペーストの製造方法

Publications (2)

Publication Number Publication Date
JPH07240203A JPH07240203A (ja) 1995-09-12
JPH07240203A5 true JPH07240203A5 (enExample) 1999-12-14

Family

ID=12234298

Family Applications (1)

Application Number Title Priority Date Filing Date
JP6027919A Pending JPH07240203A (ja) 1994-02-25 1994-02-25 鉛蓄電池用負極板ペーストの製造方法

Country Status (1)

Country Link
JP (1) JPH07240203A (enExample)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN114558490A (zh) * 2022-02-24 2022-05-31 天能电池集团(马鞍山)新能源科技有限公司 一种负合膏乳化浆料添加方法及应用其的合膏方法

Similar Documents

Publication Publication Date Title
JPH10270013A5 (enExample)
JPS57208079A (en) Rechargeable lithium cell
JPH07296849A5 (enExample)
JPH0554881A5 (enExample)
JP3178015B2 (ja) 鉛蓄電池用正極板およびその製造法
JPS58147961A (ja) 鉛蓄電池の陰極板製造方法
JPS5930722A (ja) 過酸化銀板の製造方法
JPH0547382A5 (enExample)
CA1163406A (en) Method of forming negative plate utilizing barium carbonate as expander
JP2004055417A (ja) 正極用ペースト状活物質の製造方法及びそれを用いた鉛蓄電池
JPS5682571A (en) Thin alkaline battery
JPH088103B2 (ja) 鉛蓄電池の極板製造法
JPS5945186B2 (ja) 鉛蓄電池用陰極板の製造法
JPS61142666A (ja) 鉛蓄電池用陽極板の製造法
JPS5615560A (en) Alkaline battery
JPH01187771A (ja) 鉛蓄電池用正極板の製造方法
JPH07240203A (ja) 鉛蓄電池用負極板ペーストの製造方法
JPH0322353A (ja) 釦蓄電池用極板の製造法
JPH11162455A (ja) 鉛蓄電池
JPS6489263A (ja) 鉛蓄電池用陽極板
JPS57162264A (en) Method for manufacturing unconverted pasted plate for lead battery
JPH0724216B2 (ja) アルカリ蓄電池用非焼結式カドミウム陰極
JPS57162263A (en) Method for manufacturing unconverted pasted plate for lead battery
JPS6110857A (ja) 密閉形アルカリ蓄電池用カドミウム陰極板の製造法
JPS607062A (ja) 鉛蓄電池用陰極板の製造法