JPH0694543B2 - 塗 料 - Google Patents

塗 料

Info

Publication number
JPH0694543B2
JPH0694543B2 JP62002980A JP298087A JPH0694543B2 JP H0694543 B2 JPH0694543 B2 JP H0694543B2 JP 62002980 A JP62002980 A JP 62002980A JP 298087 A JP298087 A JP 298087A JP H0694543 B2 JPH0694543 B2 JP H0694543B2
Authority
JP
Japan
Prior art keywords
interference
paint
particles
color
film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP62002980A
Other languages
English (en)
Other versions
JPS63172779A (ja
Inventor
健 魚谷
明穂 飯田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Motors Corp
Original Assignee
Mitsubishi Motors Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Motors Corp filed Critical Mitsubishi Motors Corp
Priority to JP62002980A priority Critical patent/JPH0694543B2/ja
Publication of JPS63172779A publication Critical patent/JPS63172779A/ja
Publication of JPH0694543B2 publication Critical patent/JPH0694543B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【発明の詳細な説明】 〔発明の目的〕 (産業上の利用分野) 本発明は、たとえば自動車の車体塗装用であり、干渉色
を得るための粒子を顔料の一成分として混入した塗料に
関する。
(従来の技術) たとえば自動車の車体外装用である塗料として、従来よ
り種々のものが採用されている。特に塗装対象物として
の自動車においては、きれいな色を得るばかりでなく、
目立つことも大切な要素である。そこで、この条件を満
足するために、車体の一部を干渉色で塗装することがな
された。干渉色とは、いわゆる「玉虫色」あるいは「虹
色(レインボーカラー)」などと呼ばれ、見る位置に応
じて微妙に色彩が変化するとともに、鮮かでかつ落着い
て見えるところから、車体外装遥として最適である。
従来用いられた干渉色を呈する塗料としては、雲母を使
用した干渉パール塗料がある。これは第2図に示すよう
に、雲母a…をある程度細分化して顔料の一成分とな
し、他の添加材などともに塗料bに混入し、被塗装物で
あるたとえば車体cに塗装する。雲母a…は適当に拡散
し、塗料bの一部として車体c表面に密着して光を反射
し、干渉色を見せる。
しかしながらこのような塗料bでは、雲母a…自体の反
射量が低いために、強い干渉色が得られなかった。換言
すれば、目立たない干渉色であり、塗装に用いた意味が
ない。さらにまた、雲母a…の形状が制約されるため、
限定された干渉パターンしか得られないとともに、雲母
a…は自然物であるために高価であり、塗料化するとコ
ストに悪影響がある。
ところで近時、干渉色を有するフィルムが開発され、自
動車の車室内装品として採用されることがある。たとえ
ば、社名もしくは車種を表わすマークなどを上記フィル
ムで形取って車室に貼着すると、見る位置によって色の
変化があり、美麗である。上記フィルムは、その一面に
幅寸法が0.1〜10μ,深さ寸法が0.1〜10μの無数の溝が
刻まれ、この溝により透過または反射回折格子を形成し
たものであり、廉価であるとともに高い干渉性を有す
る。したがって、上記フィルムをなんらかの手段で塗料
化することができれば都合がよい。
(発明が解決しようとする問題点) 本発明は、上述したような雲母を用いることによる干渉
色の弱さを充分カバーして、高い干渉性による美観およ
び商品価値の向上と、コストの低減を得る塗料を提供す
ることを目的とする。
〔発明の構成〕
(問題点を解決するための手段) すなわち本発明は、少なくとも二面が並行であり、その
片面に幅寸法が0.1〜10μ,深さ寸法が0.1〜10μの無数
の溝が刻まれ、かつ該溝により透過または反射回折格子
が形成した干渉粒子を、顔料の一成分として混入したこ
とを特徴とする塗料である。
(作用) このような構成によれば、干渉性を有するフィルムと全
く同様、高い干渉色の塗装ができ、干渉パターンをある
程度任意にコントロールできて見栄えがよい。
(実施例) 以下、本発明の一実施例を第1図にもとづいて説明す
る。たとえば自動車の車体cを干渉色を有する塗料1で
塗装する。上記塗料1は、溶剤や添加材および顔料で構
成されるが、上記顔料の一成分として後述する干渉粒子
2…が混入される。
すなわち干渉粒子2は、少なくとも二面が並行であり、
その片面に幅寸法が0.1〜10μ,深さ寸法が0.1〜10μの
無数の溝が刻まれた透過または反射回折格子を形成した
約50μ程度の粒子である。この干渉粒子2…の製造方法
は、現在市販されているアルミもしくはアルミ蒸着され
たポリエステル,ポリカーボネイトなどの樹脂フィルム
を、公知のカラーアルミ粒子製造法と同法により粒子化
したものである。
このような干渉粒子2…を塗料1に混入し、かつ塗装す
ることにより、車体cは高い干渉性の塗料膜で覆われる
こととなる。すなわち、干渉粒子の溝に光が入り復屈折
し、光が干渉することで干渉色が際立って極めて美麗で
ある。
さらにまた、干渉粒子2…の大きさおよび塗料1に対す
る混入量を変えることにより、干渉パターンをある程度
調節可能である。
なお上記実施例においては、被塗装物cとして自動車の
車体を適用したが、これに限定されるものではなく、要
は見栄えをよくして商品価値の向上を図るもの全てに適
用できること言う迄もない。
〔発明の効果〕
以上説明したように本発明によれば、高い干渉性を有
し、干渉パターンもある程度任意に調節できて、極めて
美麗な干渉色の塗装を得ることができ、コストに悪影響
を与えることなく商品価値の向上を図れるなどの効果を
要する。
【図面の簡単な説明】
第1図は本発明の一実施例を示す干渉粒子を有する塗装
膜の縦断面図、第2図は本発明の従来例を示す干渉粒子
を有する塗装膜の縦断面図である。 2……干渉粒子、1……塗料、c……被塗装物。

Claims (1)

    【特許請求の範囲】
  1. 【請求項1】少なくとも二面が並行であり、その片面に
    幅寸法が0.1〜10μ,深さ寸法が0.1〜10μの無数の溝が
    刻まれ、かつ該溝により透過または反射回折格子が形成
    された干渉粒子を、顔料の一成分として混入したことを
    特徴とする塗料。
JP62002980A 1987-01-09 1987-01-09 塗 料 Expired - Lifetime JPH0694543B2 (ja)