JPH059912B2 - - Google Patents

Info

Publication number
JPH059912B2
JPH059912B2 JP1211570A JP21157089A JPH059912B2 JP H059912 B2 JPH059912 B2 JP H059912B2 JP 1211570 A JP1211570 A JP 1211570A JP 21157089 A JP21157089 A JP 21157089A JP H059912 B2 JPH059912 B2 JP H059912B2
Authority
JP
Japan
Prior art keywords
heating element
temperature
ferroelectric
specimen
voltage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP1211570A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0388294A (ja
Inventor
Shii Yui Chen
Hon Uen Wan
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TSUAITOWANFUAAREN KONIEJISHUIENJIOYUEN
Original Assignee
TSUAITOWANFUAAREN KONIEJISHUIENJIOYUEN
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TSUAITOWANFUAAREN KONIEJISHUIENJIOYUEN filed Critical TSUAITOWANFUAAREN KONIEJISHUIENJIOYUEN
Priority to JP21157089A priority Critical patent/JPH0388294A/ja
Publication of JPH0388294A publication Critical patent/JPH0388294A/ja
Publication of JPH059912B2 publication Critical patent/JPH059912B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Constitution Of High-Frequency Heating (AREA)
JP21157089A 1989-08-18 1989-08-18 強誘電体セラミック発熱素子 Granted JPH0388294A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP21157089A JPH0388294A (ja) 1989-08-18 1989-08-18 強誘電体セラミック発熱素子

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP21157089A JPH0388294A (ja) 1989-08-18 1989-08-18 強誘電体セラミック発熱素子

Publications (2)

Publication Number Publication Date
JPH0388294A JPH0388294A (ja) 1991-04-12
JPH059912B2 true JPH059912B2 (de) 1993-02-08

Family

ID=16607970

Family Applications (1)

Application Number Title Priority Date Filing Date
JP21157089A Granted JPH0388294A (ja) 1989-08-18 1989-08-18 強誘電体セラミック発熱素子

Country Status (1)

Country Link
JP (1) JPH0388294A (de)

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5724974A (en) * 1980-07-22 1982-02-09 Canon Inc Fixing device
JPS57194479A (en) * 1981-05-25 1982-11-30 Ngk Insulators Ltd Heating element
JPS5845785A (ja) * 1981-09-15 1983-03-17 レノツクス・インステイテユ−ト・フオ−・リサ−チ・インク 浮選とろ過とにより水を浄化する方法および装置

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5724974A (en) * 1980-07-22 1982-02-09 Canon Inc Fixing device
JPS57194479A (en) * 1981-05-25 1982-11-30 Ngk Insulators Ltd Heating element
JPS5845785A (ja) * 1981-09-15 1983-03-17 レノツクス・インステイテユ−ト・フオ−・リサ−チ・インク 浮選とろ過とにより水を浄化する方法および装置

Also Published As

Publication number Publication date
JPH0388294A (ja) 1991-04-12

Similar Documents

Publication Publication Date Title
El-Mallah AC Electrical Conductivity and Dielectric Properties of Perovskite (Pb,Ca)TiO_3 Ceramic
US4620262A (en) Pyroelectric energy converter element comprising vinylidene fluoride-trifluoroethylene copolymer
KR20100134563A (ko) 가변용량 소자와 그 제어 방법, 전자 디바이스 및 통신 모바일 기기
Aparna et al. Effect of lanthanum doping on electrical and electromechanical properties of Ba 1− x La x TiO 3
Zhigao et al. An impedance study of Pb2KNb5O15 ferroelectric ceramics
Hsiao-Lin Structure and dielectric properties of perovskite–Barium Titanate (BaTiO3)
Hoh Conversion of thermal to electrical energy with ferroelectric materials
Chan et al. A poling study of PZT/P (VDF-TrFE) copolymer 0-3 composites
CN109678501B (zh) 一种烟雾报警器专用压电振子瓷料配方及其制备方法
JPH059912B2 (de)
Sharma et al. Dielectric and pyroelectric characteristics of PZT doped with gadolinium
Sanlialp et al. Direct electrocaloric measurements using a differential scanning calorimeter
Thongrueng et al. Properties and Degradation of Polarization Reversal of Soft BaTiO3 Ceramics for Ferroelectric Thin-Film Devices
JPS6255281B2 (de)
Anokhin et al. Investigation of time and frequency characteristics of the electrocaloric response in ferroelectric materials
Wang et al. Ferroelectric heater by use of Pb (ZrTi) O3 and BaTiO3 ceramics
WO2021234984A1 (ja) 発電システム
Zhao et al. Effect of Pre-Field on the Dielectric Properties of BaTiO 3-based Equalizing Ceramics Capacitors of Surge Arrester
JPS6230682B2 (de)
Pramila et al. Pyroelectric, dielectric and resistivity studies on samarium modified PZT ceramics
Jamadar et al. Pyroelectric properties of lead-barium titanate and lead-strontium titanate
JPH056826U (ja) コンデンサ
Ploss et al. Poling of P (VDF-TrFE) with ferroelectrically applied dielectric displacement
JPH06100505B2 (ja) 温度センサ及びそれを用いた温度検知器
JPH09301778A (ja) 磁器材料の焼成方法及び焼結装置、並びに圧電材料