JPH052609Y2 - - Google Patents
Info
- Publication number
- JPH052609Y2 JPH052609Y2 JP1986187591U JP18759186U JPH052609Y2 JP H052609 Y2 JPH052609 Y2 JP H052609Y2 JP 1986187591 U JP1986187591 U JP 1986187591U JP 18759186 U JP18759186 U JP 18759186U JP H052609 Y2 JPH052609 Y2 JP H052609Y2
- Authority
- JP
- Japan
- Prior art keywords
- insulating panel
- basket
- anode chamber
- porous insulating
- porous
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Electroplating Methods And Accessories (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1986187591U JPH052609Y2 (enrdf_load_html_response) | 1986-12-05 | 1986-12-05 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1986187591U JPH052609Y2 (enrdf_load_html_response) | 1986-12-05 | 1986-12-05 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6394971U JPS6394971U (enrdf_load_html_response) | 1988-06-18 |
JPH052609Y2 true JPH052609Y2 (enrdf_load_html_response) | 1993-01-22 |
Family
ID=31138191
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1986187591U Expired - Lifetime JPH052609Y2 (enrdf_load_html_response) | 1986-12-05 | 1986-12-05 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH052609Y2 (enrdf_load_html_response) |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS558622U (enrdf_load_html_response) * | 1978-06-30 | 1980-01-21 | ||
JPS6089277U (ja) * | 1983-11-22 | 1985-06-19 | 川崎製鉄株式会社 | 高電流密度電解用陽極 |
-
1986
- 1986-12-05 JP JP1986187591U patent/JPH052609Y2/ja not_active Expired - Lifetime
Also Published As
Publication number | Publication date |
---|---|
JPS6394971U (enrdf_load_html_response) | 1988-06-18 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN101855390B (zh) | 电镀用阳极组件 | |
US4459189A (en) | Electrode coated with lead or a lead alloy and method of use | |
KR101077000B1 (ko) | 전기도금용 애노드 | |
US3300396A (en) | Electroplating techniques and anode assemblies therefor | |
SE433022B (sv) | Artikel for anvendning som en stomme i en elektrod, serskilt for en blyackumulator, eller som en elektrod for elektrokemiska forfaranden, anvendning av artikeln som en elektrodstomme i en elektrod for en blyackumulator | |
US3821097A (en) | Current density redistributing anode | |
SE425009B (sv) | Bipoler elektrod samt forfarande for framstellning av en bipoler elektrod | |
JPH052609Y2 (enrdf_load_html_response) | ||
CN1847466B (zh) | 不溶性阳极 | |
EP3976861B1 (en) | An electrode assembly for electrochemical processes | |
CA2052587A1 (en) | Insoluble anode for electrolyses in aqueous solutions | |
JPH052610Y2 (enrdf_load_html_response) | ||
JP3928013B2 (ja) | めっき用不溶性陽極 | |
US5720867A (en) | Process for the electrochemical recovery of the metals copper, zinc, lead, nickel or cobalt | |
JPS63143295A (ja) | バスケツト型陽極室 | |
CN217378064U (zh) | 带有退镀功能的电镀装置 | |
US4203808A (en) | Electroplating cathodes for electrochemical synthesis | |
JPH08376Y2 (ja) | 不溶解性陽極を用いたメッキ装置 | |
JPH07180078A (ja) | 複極式電解槽 | |
US3661757A (en) | Anode | |
CN219099371U (zh) | 一种圆柱形脉冲电镀不溶性阳极装置 | |
JPS6333971Y2 (enrdf_load_html_response) | ||
CN215925131U (zh) | 用于镀膜机的钛蓝、钛蓝组件及镀膜机 | |
JPS6220452Y2 (enrdf_load_html_response) | ||
US1486546A (en) | Electrolytic separation |