JPH05170597A - 酸化物超電導体薄膜の製造方法 - Google Patents
酸化物超電導体薄膜の製造方法Info
- Publication number
- JPH05170597A JPH05170597A JP3342991A JP34299191A JPH05170597A JP H05170597 A JPH05170597 A JP H05170597A JP 3342991 A JP3342991 A JP 3342991A JP 34299191 A JP34299191 A JP 34299191A JP H05170597 A JPH05170597 A JP H05170597A
- Authority
- JP
- Japan
- Prior art keywords
- thin film
- oxide superconductor
- based oxide
- torr
- substrate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E40/00—Technologies for an efficient electrical power generation, transmission or distribution
- Y02E40/60—Superconducting electric elements or equipment; Power systems integrating superconducting elements or equipment
Landscapes
- Inorganic Compounds Of Heavy Metals (AREA)
- Crystals, And After-Treatments Of Crystals (AREA)
- Superconductors And Manufacturing Methods Therefor (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3342991A JPH05170597A (ja) | 1991-12-25 | 1991-12-25 | 酸化物超電導体薄膜の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3342991A JPH05170597A (ja) | 1991-12-25 | 1991-12-25 | 酸化物超電導体薄膜の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH05170597A true JPH05170597A (ja) | 1993-07-09 |
| JPH05170597A5 JPH05170597A5 (enExample) | 1999-10-26 |
Family
ID=18358094
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3342991A Pending JPH05170597A (ja) | 1991-12-25 | 1991-12-25 | 酸化物超電導体薄膜の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH05170597A (enExample) |
-
1991
- 1991-12-25 JP JP3342991A patent/JPH05170597A/ja active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0387456B1 (en) | Method for vapor-phase growth of an oxide thin film | |
| US5439876A (en) | Method of making artificial layered high Tc superconductors | |
| KR910007382B1 (ko) | 초전도 재료 및 초전도 박막의 제조방법 | |
| EP0406126B2 (en) | Substrate having a superconductor layer | |
| CN101705469A (zh) | 通过反应蒸发进行的原位薄膜的生长 | |
| EP0446145B1 (en) | Process for preparing high-temperature superconducting thin films | |
| Ohbayashi et al. | As‐grown superconducting Bi2Si2Ca2Cu3O x thin films with T c zero of 102 K prepared by rf magnetron sputtering | |
| US5116811A (en) | Cvd method for the formation of bi-containing superconducting thin films | |
| EP0410868A2 (en) | Superconducting thin film of compound oxide and process for preparing the same | |
| JP3579690B2 (ja) | 複合酸化物系薄膜の作製方法及びその装置並びにそれにより作製した複合酸化物系薄膜。 | |
| Kirlin et al. | Growth of High TcYBaCuO Thin Films by Metalorganic Chemical Vapor Deposition | |
| JP3253295B2 (ja) | 酸化物薄膜の製造方法 | |
| JP2530492B2 (ja) | 酸化物超伝導薄膜の作製方法及びそれに用いる基板 | |
| US5260267A (en) | Method for forming a Bi-containing superconducting oxide film on a substrate with a buffer layer of Bi2 O3 | |
| JPS63236794A (ja) | 酸化物超伝導薄膜の作製方法 | |
| JPH035397A (ja) | 酸化物結晶薄膜の気相成長方法 | |
| JP2551983B2 (ja) | 化学気相成長を用いた酸化物超伝導膜の作成方法 | |
| Norton | Epitaxial growth of superconducting cuprate thin films | |
| EP0401031A2 (en) | Oxide thin film and method of epitaxially growing same | |
| JPH0288426A (ja) | 超電導薄膜の製造方法 | |
| JPH02210718A (ja) | 酸化物超伝導体の気相成長方法 | |
| Erbil | Crystalline metal-semiconductor superlattices to search for excitonic superconductivity | |
| Norton | Thin Films | |
| KR950008862B1 (ko) | 금속 키레이트화합물을 사용한 화학증착법을 이용한 YBa₂Cu₃O_7-x(X=0-0.5)초전도체의 합성방법 | |
| JPS6424323A (ja) | 超電導体薄膜の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A02 | Decision of refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A02 Effective date: 20010501 |