JPH0471964B2 - - Google Patents
Info
- Publication number
- JPH0471964B2 JPH0471964B2 JP1746888A JP1746888A JPH0471964B2 JP H0471964 B2 JPH0471964 B2 JP H0471964B2 JP 1746888 A JP1746888 A JP 1746888A JP 1746888 A JP1746888 A JP 1746888A JP H0471964 B2 JPH0471964 B2 JP H0471964B2
- Authority
- JP
- Japan
- Prior art keywords
- iron
- nozzle
- molten iron
- containing cold
- pine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Carbon Steel Or Casting Steel Manufacturing (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1746888A JPH01195233A (ja) | 1988-01-29 | 1988-01-29 | 含鉄冷材の溶解方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1746888A JPH01195233A (ja) | 1988-01-29 | 1988-01-29 | 含鉄冷材の溶解方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPH01195233A JPH01195233A (ja) | 1989-08-07 |
JPH0471964B2 true JPH0471964B2 (enrdf_load_stackoverflow) | 1992-11-17 |
Family
ID=11944851
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1746888A Granted JPH01195233A (ja) | 1988-01-29 | 1988-01-29 | 含鉄冷材の溶解方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH01195233A (enrdf_load_stackoverflow) |
-
1988
- 1988-01-29 JP JP1746888A patent/JPH01195233A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPH01195233A (ja) | 1989-08-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP3058039B2 (ja) | 転炉製鉄法 | |
JP2735774B2 (ja) | 冶金反応容器での反応を強化する方法 | |
US4936908A (en) | Method for smelting and reducing iron ores | |
EP2796569B1 (en) | Converter steelmaking method | |
JP2865639B2 (ja) | 金属酸化物を精錬することによりステンレス鋼を製造する方法 | |
US4410360A (en) | Process for producing high chromium steel | |
JP2007002305A (ja) | キュポラによる溶銑の溶製方法 | |
JPS5935407B2 (ja) | 転炉内の鉄融成物への炭素供給法 | |
JPH0471964B2 (enrdf_load_stackoverflow) | ||
US2741554A (en) | Method of refining iron | |
US4090869A (en) | Process of manufacturing alloy steels in a continuously charged arc furnace | |
JPH0471965B2 (enrdf_load_stackoverflow) | ||
US3615356A (en) | Basic steelmaking process | |
US3234011A (en) | Process for the production of steel | |
JP3286114B2 (ja) | 屑鉄から高炭素溶融鉄を製造する方法 | |
JP2836192B2 (ja) | 低硫黄溶銑の製造方法 | |
JP3764543B2 (ja) | 含鉄冷材の溶解方法 | |
JPH02166256A (ja) | 中・低炭素フェロマンガンの溶製方法 | |
JP2783894B2 (ja) | 鉄浴式の溶融還元法 | |
JPS62247013A (ja) | 鉄系溶融金属の製造装置 | |
JPS62116712A (ja) | スプラツシユランスを有する溶解・製錬容器 | |
JPS62167809A (ja) | 含クロム溶銑の製造法 | |
JPH08260022A (ja) | 屑鉄の溶解方法 | |
JPH0368712A (ja) | 転炉の床上げコーティング方法 | |
JPH01283312A (ja) | 含鉄冷材の溶解方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
FPAY | Renewal fee payment (prs date is renewal date of database) |
Year of fee payment: 15 Free format text: PAYMENT UNTIL: 20071117 |
|
FPAY | Renewal fee payment (prs date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20081117 Year of fee payment: 16 |
|
EXPY | Cancellation because of completion of term | ||
FPAY | Renewal fee payment (prs date is renewal date of database) |
Year of fee payment: 16 Free format text: PAYMENT UNTIL: 20081117 |