JPH031472Y2 - - Google Patents

Info

Publication number
JPH031472Y2
JPH031472Y2 JP742986U JP742986U JPH031472Y2 JP H031472 Y2 JPH031472 Y2 JP H031472Y2 JP 742986 U JP742986 U JP 742986U JP 742986 U JP742986 U JP 742986U JP H031472 Y2 JPH031472 Y2 JP H031472Y2
Authority
JP
Japan
Prior art keywords
zone
continuous annealing
annealing furnace
plating
low
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP742986U
Other languages
Japanese (ja)
Other versions
JPS62122858U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP742986U priority Critical patent/JPH031472Y2/ja
Publication of JPS62122858U publication Critical patent/JPS62122858U/ja
Application granted granted Critical
Publication of JPH031472Y2 publication Critical patent/JPH031472Y2/ja
Expired legal-status Critical Current

Description

【考案の詳細な説明】 (産業上の利用分野) 本考案は溶融メツキ用連続焼鈍炉に関するもの
である。
[Detailed Description of the Invention] (Field of Industrial Application) The present invention relates to a continuous annealing furnace for hot-dip plating.

(従来技術とその問題点) 従来、一般に、溶融メツキ用連続焼鈍炉Tは、
第2図に示すように、予熱帯1、加熱帯2、還元
帯3、冷却帯4、低温保持帯5、下端をメツキ浴
槽7の溶融メツキ浴8に浸漬するスナウト部6と
からなる。
(Prior art and its problems) Conventionally, in general, the continuous annealing furnace T for fusion plating is
As shown in FIG. 2, it consists of a preheating zone 1, a heating zone 2, a reducing zone 3, a cooling zone 4, a low temperature holding zone 5, and a snout section 6 whose lower end is immersed in a molten plating bath 8 of a plating bath 7.

そして、鋼帯Sは前記予熱帯1から装入され、
ここで予熱されて加熱帯2に至り、加熱により鋼
帯Sの表面に付着されている油等を燃焼あるいは
熱分解により除去される。
Then, the steel strip S is charged from the preheating zone 1,
Here, it is preheated and reaches the heating zone 2, where oil and the like adhering to the surface of the steel strip S due to heating are removed by combustion or thermal decomposition.

この場合、鋼帯Sの表面は若干酸化されるた
め、つぎの還元帯3で還元するとともに、焼鈍す
る。
In this case, since the surface of the steel strip S is slightly oxidized, it is reduced and annealed in the next reduction zone 3.

ついで、この鋼帯Sは冷却帯4、低温保持帯5
に至り、所定のメツキ浴浸入温度まで冷却したの
ち、スナウト部6からメツキ浴槽7の溶融メツキ
浴8に浸漬してメツキされるものである。
Next, this steel strip S is passed through a cooling zone 4 and a low temperature holding zone 5.
After cooling to a predetermined plating bath immersion temperature, it is immersed from the snout portion 6 into the molten plating bath 8 of the plating bath 7 to be plated.

ところで、この種溶融メツキ用連続焼鈍炉にお
いては、メツキの種類をZnメツキからAlメツキ
等に変更することがある。そして、この場合に
は、低温保持帯5の露点を約−40℃に再調整する
必要があるが、この調整に約12時間も要し、生産
性が極めて悪いものであつた。
By the way, in this type of continuous annealing furnace for hot-dip plating, the type of plating may be changed from Zn plating to Al plating or the like. In this case, it is necessary to readjust the dew point of the low temperature holding zone 5 to about -40 DEG C., but this adjustment takes about 12 hours, resulting in extremely low productivity.

本考案者らは、前記問題点を解決すべく、種々
検討の結果、従来のものにおいては、前記低温保
持帯5は、その炉壁が総てレンガ張りであり、か
つ、炉温が最高でも650℃と低温であること、ま
た、スナウト部6にはシール装置が設けてある
が、メツキ浴の交換は、鋼帯Sを通板した状態で
行うため、このとき、スナウト部から酸素(空
気)が侵入する。
In order to solve the above-mentioned problems, the inventors of the present invention have conducted various studies and found that in the conventional low temperature holding zone 5, the furnace walls are all made of brick, and even when the furnace temperature is the highest, The temperature is as low as 650°C, and although a sealing device is installed in the snout section 6, the plating bath is replaced with the steel strip S passed through it, so oxygen (air) is removed from the snout section at this time. ) invades.

したがつて、前記スナウト部から入つた酸素
は、内張りレンガに吸蔵され、容易に排出されな
いことに起因するものであることが判明した。
Therefore, it was found that the oxygen that entered from the snout portion was occluded by the lining bricks and was not easily discharged.

(問題点を解決すべき手段) 本考案は、前記の点に鑑みてなされたもので、
溶融メツキ用連続焼鈍炉の低温保持帯を、レンガ
で内張りする代わりに、鋼板からなるマツフル構
造としたものである。
(Means to solve the problem) The present invention was made in view of the above points,
The low-temperature holding zone of a continuous annealing furnace for molten plating has a pine-full structure made of steel plates instead of being lined with bricks.

(実施例) つぎに、本考案を一実施例である図面にしたが
つて説明する。
(Example) Next, the present invention will be explained with reference to the drawings which are one example.

本考案は、前記第2図に示す溶融メツキ用連続
焼鈍炉Tにおいて、低温保持帯5を、第1図に示
すように、内張レンガに代えて、内部を鋼板や気
密性の材料からなるユニツト壁とし、このユニツ
ト壁を組み立ててマツフル構造9としたものであ
る。
In the present invention, in the continuous annealing furnace T for molten plating shown in FIG. 2, the low-temperature holding zone 5 is made of a steel plate or an airtight material instead of the lining brick, as shown in FIG. This is a unit wall, and the unit wall is assembled to form a muffle structure 9.

なお、このユニツト壁の外面は、セラミツクフ
エルト等の保温材10で被覆してある。また、1
1は搬送ロール、12は電熱ヒータ等の加熱装置
である。
The outer surface of this unit wall is covered with a heat insulating material 10 such as ceramic felt. Also, 1
1 is a conveyor roll, and 12 is a heating device such as an electric heater.

そして、溶融メツキ浴8を変える場合、メツキ
浴8とともにスナウト部6を取換え、各帯および
スナウト部6の雰囲気を必要に応じ調節する。
When changing the molten plating bath 8, the plating bath 8 and the snout section 6 are replaced, and the atmosphere of each band and the snout section 6 is adjusted as necessary.

(効果) 以上の説明で明らかなように、本考案によれ
ば、スナウト部に連接する低温保持帯は、マツフ
ル構造となつて、炉壁に吸蔵作用がないため、メ
ツキ浴の交換にあたつての露点調整を、従来のも
のの1/5〜1/6に短縮でき、炉内雰囲気の早期安定
を図ることができた。
(Effects) As is clear from the above explanation, according to the present invention, the low-temperature holding zone connected to the snout has a pine-full structure and has no occlusion function on the furnace wall, so it is effective when replacing the plating bath. The time required for dew point adjustment was reduced to 1/5 to 1/6 of the conventional method, and the atmosphere inside the furnace could be stabilized quickly.

なお、低温保持帯を、マツフル構造を形成する
鋼板に繊維質系断熱材を設ける構成とし、軽量化
を図るとともに、ユニツト化することにより、据
え付けコストは勿論のこと、溶融メツキ用連続焼
鈍炉そのものを安価なものとすることができる。
In addition, the low-temperature holding zone is constructed by providing a fibrous insulation material on the steel plate that forms the pine-full structure to reduce the weight and by making it into a unit, not only the installation cost but also the continuous annealing furnace itself for molten plating is reduced. can be made inexpensive.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は、本考案にかかる溶融メツキ用連続焼
鈍炉の低温保持帯の断面図で、第2図は従来の溶
融メツキ用連続焼鈍炉を示す説明図である。 T〜溶融メツキ用連続焼鈍炉、5〜低温保持
帯、9〜マツフル構造。
FIG. 1 is a cross-sectional view of a low-temperature holding zone of a continuous annealing furnace for fusion plating according to the present invention, and FIG. 2 is an explanatory diagram showing a conventional continuous annealing furnace for fusion plating. T - Continuous annealing furnace for melt plating, 5 - Low temperature holding zone, 9 - Pine full structure.

Claims (1)

【実用新案登録請求の範囲】 (1) 予熱帯、加熱帯、還元帯、冷却帯、低温保持
帯等よりなる溶融メツキ用連続焼鈍炉の低温保
持帯を、マツフル構造としたことを特徴とする
溶融メツキ用連続焼鈍炉。 (2) 前記マツフル構造が、繊維質系断熱材とその
内側表面に鋼板を取り付けたものであることを
特徴とする前記実用新案登録請求の範囲第1項
に記載の溶融メツキ用連続焼鈍炉。
[Claims for Utility Model Registration] (1) The low-temperature holding zone of a continuous annealing furnace for molten plating, which consists of a pre-heating zone, a heating zone, a reduction zone, a cooling zone, a low-temperature holding zone, etc., has a pine-full structure. Continuous annealing furnace for molten plating. (2) The continuous annealing furnace for molten plating according to claim 1, wherein the pine-full structure includes a fibrous heat insulating material and a steel plate attached to the inner surface of the fibrous heat insulating material.
JP742986U 1986-01-21 1986-01-21 Expired JPH031472Y2 (en)