JPH02214583A - 下水汚泥溶融スラグの処理法 - Google Patents
下水汚泥溶融スラグの処理法Info
- Publication number
- JPH02214583A JPH02214583A JP1034692A JP3469289A JPH02214583A JP H02214583 A JPH02214583 A JP H02214583A JP 1034692 A JP1034692 A JP 1034692A JP 3469289 A JP3469289 A JP 3469289A JP H02214583 A JPH02214583 A JP H02214583A
- Authority
- JP
- Japan
- Prior art keywords
- ladle
- ash
- fly ash
- sewage sludge
- molten slag
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02W—CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT
- Y02W30/00—Technologies for solid waste management
- Y02W30/50—Reuse, recycling or recovery technologies
- Y02W30/78—Recycling of wood or furniture waste
Landscapes
- Processing Of Solid Wastes (AREA)
- Treatment Of Sludge (AREA)
- Mold Materials And Core Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1034692A JPH02214583A (ja) | 1989-02-14 | 1989-02-14 | 下水汚泥溶融スラグの処理法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1034692A JPH02214583A (ja) | 1989-02-14 | 1989-02-14 | 下水汚泥溶融スラグの処理法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH02214583A true JPH02214583A (ja) | 1990-08-27 |
| JPH0450876B2 JPH0450876B2 (enExample) | 1992-08-17 |
Family
ID=12421430
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1034692A Granted JPH02214583A (ja) | 1989-02-14 | 1989-02-14 | 下水汚泥溶融スラグの処理法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH02214583A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2013202870A (ja) * | 2012-03-28 | 2013-10-07 | Teruo Mori | 乾燥スラッジ固化処理方法 |
| CN104942223A (zh) * | 2015-07-30 | 2015-09-30 | 张燕 | 钒铁渣-低压电陶瓷废料消失模铸造涂料及其制备方法 |
-
1989
- 1989-02-14 JP JP1034692A patent/JPH02214583A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2013202870A (ja) * | 2012-03-28 | 2013-10-07 | Teruo Mori | 乾燥スラッジ固化処理方法 |
| CN104942223A (zh) * | 2015-07-30 | 2015-09-30 | 张燕 | 钒铁渣-低压电陶瓷废料消失模铸造涂料及其制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0450876B2 (enExample) | 1992-08-17 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| AU615015B2 (en) | Method for preparation of moulds and cores used in the casting of metals | |
| JPH02229725A (ja) | ガラス溶解炉運転方法 | |
| US4764216A (en) | Method of converting particles liberated in chemical or physical processes into a harmless form by mixing with a molten silicate-containing material | |
| CA2067067A1 (en) | Metallurgical fluxes | |
| JPH02214583A (ja) | 下水汚泥溶融スラグの処理法 | |
| JP2001519854A (ja) | 製鋼作業における鉄含有スラッジのリサイクル方法 | |
| US3532775A (en) | Method for producing aluminum particles | |
| JPH02175047A (ja) | 高純度マグネシウムによる鋳鉄用溶湯の処理方法 | |
| US6189818B1 (en) | Process for stabilizing and reusing ladle slag | |
| JP4250724B2 (ja) | スラッジのリサイクル方法 | |
| NL9402019A (nl) | Werkwijze en poedermengsel voor het repareren van op oxide gebaseerde vuurvaste lichamen. | |
| JP4237965B2 (ja) | Cr含有スラッジや焼却残渣等の処理方法およびそれにより得られる製鋼用ペレット | |
| EP1366002A1 (en) | Production of products from steel slags | |
| JPH11264011A (ja) | スラグの有効利用方法 | |
| US4066446A (en) | Thermally bloated fireclay (scr verilite) ladle insulation | |
| US4178981A (en) | Copper casting method using titanium dioxide release method | |
| KR100499546B1 (ko) | 알루미늄 합금 용탕의 처리 방법 및 그에 사용하는 플럭스 | |
| JPH08224557A (ja) | 廃棄物粒状物及びその製造方法 | |
| JP2007537882A (ja) | 溶融金属を処理するための方法 | |
| KR100246733B1 (ko) | 산업폐기물의 고용화 처리방법 | |
| JP2004315296A (ja) | Cr含有合金鋼精錬スラグの粉化防止方法 | |
| JPS60244454A (ja) | 連続鋳造用鋳型添加剤及びその製造方法 | |
| JP2807435B2 (ja) | 耐火物表面付着物除去用清浄材料 | |
| JPS60231444A (ja) | 高塩基度製鋼スラグの利用方法 | |
| JP3627951B2 (ja) | 廃棄物溶融スラグの骨材化法 |