JP7239031B2 - toilet roll - Google Patents

toilet roll Download PDF

Info

Publication number
JP7239031B2
JP7239031B2 JP2022015001A JP2022015001A JP7239031B2 JP 7239031 B2 JP7239031 B2 JP 7239031B2 JP 2022015001 A JP2022015001 A JP 2022015001A JP 2022015001 A JP2022015001 A JP 2022015001A JP 7239031 B2 JP7239031 B2 JP 7239031B2
Authority
JP
Japan
Prior art keywords
paper
toilet
tube
paper tube
toilet roll
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2022015001A
Other languages
Japanese (ja)
Other versions
JP2022058845A (en
Inventor
遥絵 清水
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
New Oji Paper Co Ltd
Oji Holdings Corp
Original Assignee
Oji Holdings Corp
Oji Paper Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=87885435&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=JP7239031(B2) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.
Priority claimed from JP2017254772A external-priority patent/JP7020116B2/en
Application filed by Oji Holdings Corp, Oji Paper Co Ltd filed Critical Oji Holdings Corp
Priority to JP2022015001A priority Critical patent/JP7239031B2/en
Publication of JP2022058845A publication Critical patent/JP2022058845A/en
Application granted granted Critical
Publication of JP7239031B2 publication Critical patent/JP7239031B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、2プライのトイレットロールに関する。 The present invention relates to a two-ply toilet roll.

トイレットペーパーやキッチンペーパー等の衛生紙の多くは、紙製の巻芯である紙管の外周面に接着剤を塗工して巻き付けた衛生紙ロールとして市販されている。図1に、トイレットロールの端面を示す。トイレットロール1は、紙管2と、紙管2にトイレットペーパーが巻き付いたペーパー部3とからなる。トイレットロール1に用いられる巻き芯に使用される紙管2にはスパイラル紙管が用いられることが多く、その部材にはボール紙やクラフト紙等の厚紙が用いられる。 Many sanitary papers such as toilet paper and kitchen paper are commercially available as sanitary paper rolls in which an adhesive is applied to the outer peripheral surface of a paper tube, which is a core made of paper, and wound. FIG. 1 shows an end face of a toilet roll. The toilet roll 1 consists of a paper tube 2 and a paper part 3 in which toilet paper is wound around the paper tube 2. - 特許庁A spiral paper tube is often used for the paper tube 2 used for the winding core used for the toilet roll 1, and thick paper such as cardboard or kraft paper is used for the member.

このようなトイレットロール1は、原反ロールから繰り出される原紙を巻き芯に巻き取り、そのロールの外周面に原紙の終端を固定した長尺のペーパーログを形成し、図3に示すようにペーパーログ受けガイド4上を送られてペーパーログからログソー等の切断刃5で所定の幅に切断することで得られる(例えば、特許文献1、2参照)。 Such a toilet roll 1 winds base paper fed out from a raw fabric roll around a winding core, forms a long paper log in which the end of the base paper is fixed to the outer peripheral surface of the roll, and as shown in FIG. It is obtained by cutting a paper log into a predetermined width with a cutting blade 5 such as a log saw while being fed on a log receiving guide 4 (see Patent Documents 1 and 2, for example).

実開平6-86687号公報Japanese Utility Model Laid-Open No. 6-86687 特開2005-87788号公報JP-A-2005-87788 特開2016-16951号公報JP 2016-16951 A 特開2010-119582号公報JP 2010-119582 A 特開2013-256131号公報JP 2013-256131 A

紙管2は、トイレットロールの変形を抑え、ホルダーに装着されて使用される際に滑らかに回転するよう、潰れずに製造時の形状を維持する強度を有することが望ましい。紙管2が潰れる原因の1つとしては、ペーパーログをログソー5で切断する際に受ける圧力がある。 It is desirable that the paper tube 2 has the strength to suppress the deformation of the toilet roll and to maintain the shape at the time of manufacture without being crushed so that it can rotate smoothly when attached to the holder and used. One of the causes of the collapse of the paper tube 2 is the pressure received when cutting the paper log with the log saw 5 .

図3に、ペーパーログの切断時に紙管が変形する様子を示す。トイレットロール1は、製品毎に様々な仕様があり、巻長が長く、高密度に巻いた硬巻長尺品などではペーパー部3が硬くなる。ペーパー部3が通常よりも硬くなると、ログソー5でペーパーログを切断するための切断圧力が大きくなり、通常の紙管2の強度ではペーパーログを切断する際に紙管2が潰れる場合もある。 FIG. 3 shows how the paper tube is deformed when the paper log is cut. The toilet roll 1 has various specifications for each product, and the paper part 3 becomes hard in a long product with a long roll length and a hard roll that is wound at high density. When the paper part 3 becomes harder than normal, the cutting pressure for cutting the paper log with the log saw 5 increases, and the normal strength of the paper tube 2 may crush the paper log when cutting the paper log.

ペーパーログを切断する際に紙管2が潰れないようにするためには、紙管2の強度を、ペーパー部3が最も硬い場合の切断圧力にも耐えうる強度に設計すればよい。しかし、強度を高めるとその分紙管2の部材コストが高くなる等、製造コストの上昇を招く。また、廃棄する際に小さく潰し難くなり、使用感が悪化する要因になり得る。そのため、紙管2の強度は、トイレットロール1の仕様に応じて必要最小限の強度に抑えることが望ましい。 In order to prevent the paper tube 2 from being crushed when cutting the paper log, the strength of the paper tube 2 should be designed to withstand the cutting pressure when the paper portion 3 is the hardest. However, increasing the strength leads to an increase in the manufacturing cost, such as an increase in the cost of the members of the paper tube 2 correspondingly. In addition, it becomes difficult to crush them into small pieces when discarding them, which can be a factor in deteriorating usability. Therefore, it is desirable to keep the strength of the paper tube 2 to the minimum necessary strength according to the specifications of the toilet roll 1 .

しかしながら、トイレットロール1の仕様と切断圧力の関係が明らかでなかったため、トイレットロール1の仕様毎に最適な紙管2の強度を設計することは困難であった。 However, since the relationship between the specifications of the toilet roll 1 and the cutting pressure was not clear, it was difficult to design the optimal strength of the paper tube 2 for each specification of the toilet roll 1 .

本発明は、このような課題に鑑みてなされたもので、その目的とするところは、ペーパーログから所定の幅のトイレットロールを切り出す際、紙管が切断圧力により塑性変形しない2プライのトイレットロールを提供することにある。 The present invention has been made in view of such problems, and its object is to provide a two-ply toilet roll that does not undergo plastic deformation due to cutting pressure when a toilet roll having a predetermined width is cut out from a paper log. is to provide

上記の課題を解決するために、本発明の一態様は、紙管と、前記紙管に2プライのトイレットペーパーを巻き付けたトイレットペーパー部とを備えたトイレットロールであって、前記トイレットペーパー1枚あたりの密度が0.140g/cm3以上0.180g/cm3以下であり、前記トイレットペーパー部の応力は13.0N以上22.0N以下であり、前記紙管の応力が7.0N以上13.0N以下であり、前記トイレットペーパー部の応力と前記紙管の応力との差が12.0N以下であることを特徴とする。 In order to solve the above problems, one aspect of the present invention is a toilet roll including a paper tube and a toilet paper section in which two plies of toilet paper are wound around the paper tube, wherein one sheet of the toilet paper The density per unit is 0.140 g/cm 3 or more and 0.180 g/cm 3 or less, the stress of the toilet paper portion is 13.0 N or more and 22.0 N or less, and the stress of the paper tube is 7.0 N or more and 13 0 N or less, and the difference between the stress of the toilet paper portion and the stress of the paper tube is 12.0 N or less.

本発明の別の態様では、さらに前記トイレットペーパーの長手方向の引張強度が1.60N以上2.20N以下であることを特徴とする。 Another aspect of the present invention is characterized in that the tensile strength in the longitudinal direction of the toilet paper is 1.60N or more and 2.20N or less.

本発明の別の態様では、さらに前記トイレットペーパーの長手方向の長さが45~55mであって、前記トイレットロールの直径が112~120mmあることを特徴とする。 Another aspect of the present invention is characterized in that the length of the toilet paper in the longitudinal direction is 45-55 m, and the diameter of the toilet roll is 112-120 mm.

本発明の別の態様では、さらに前記トイレットペーパーの坪量が14.0~17.0g/m2、紙厚が180~225μmであることを特徴とする。 Another aspect of the present invention is characterized in that the toilet paper has a basis weight of 14.0 to 17.0 g/m 2 and a paper thickness of 180 to 225 μm.

本発明の別の態様では、さらに前記紙管は、複数枚の帯状紙を互いに貼り合わせて貼り合わせたスパイラル紙管であることを特徴とする。 Another aspect of the present invention is characterized in that the paper tube is a spiral paper tube formed by laminating a plurality of strips of paper together.

本発明の別の態様では、さらに前記紙管の直径が36mm以上45mm以下あることを特徴とする。 Another aspect of the present invention is characterized in that the paper tube has a diameter of 36 mm or more and 45 mm or less.

本発明は、ペーパーログから所定の幅のトイレットロールを切り出す際、紙管の切断圧力による塑性変形を低コストで防ぐことができる。 INDUSTRIAL APPLICABILITY The present invention can prevent plastic deformation due to cutting pressure of a paper tube at low cost when a toilet roll having a predetermined width is cut out from a paper log.

トイレットロールの端面を示す図である。It is a figure which shows the end surface of a toilet roll. ペーパーログを切断する様子を示す図である。It is a figure which shows a mode that a paper log is cut. ペーパーログの切断時に紙管が変形する様子を示す図である。FIG. 4 is a diagram showing how a paper tube is deformed when a paper log is cut; 2層構造のスパイラル紙管を示す斜視図である。FIG. 3 is a perspective view showing a two-layered spiral paper tube; (a)~(c)は、2層構造スパイラル紙管を製造する工程を示す図である。(a) to (c) are diagrams showing steps for manufacturing a two-layered spiral paper tube. スパイラル紙管の中心軸を含む断面図である。FIG. 4 is a cross-sectional view including the central axis of the spiral paper tube;

本発明のトイレットロールは、2プライのトイレットロールである。2プライのトイレットペーパーは、1枚のペーパーウェブからなるトイレットペーパーである。 The toilet roll of the present invention is a two-ply toilet roll. Two-ply toilet paper is toilet paper that consists of a single paper web.

トイレットロール1においてペーパー部3の硬さを決定するのは、主に、トイレットペーパーの積層枚数(プライ)、トイレットロールの応力、トイレットペーパー1枚あたりの密度、引張強度、クレープ率、伸び率等の特性である。そのため、切断時に切断刃をペーパーログに押し付ける圧力(切断圧力)は、切断装置の切れ味を一定と仮定すると、上記トイレットペーパーの特性と相関を持つ。 The hardness of the paper part 3 in the toilet roll 1 is mainly determined by the number of layers of toilet paper (ply), the stress of the toilet roll, the density per sheet of toilet paper, the tensile strength, the crepe rate, the elongation rate, etc. is a characteristic of Therefore, assuming that the sharpness of the cutting device is constant, the pressure (cutting pressure) with which the cutting blade is pressed against the paper log at the time of cutting has a correlation with the characteristics of the toilet paper.

特に、トイレットペーパー1枚あたりの密度が高い場合は、圧力(切断圧力)が高くてもトイレットペーパー間の空間がクッションとなり、紙管への圧力は低減されるが、1枚あたりの密度が低くなると、トイレットペーパーの巻きが硬くなり、紙管への圧力(切断圧力)が大きくなるため、紙管2が潰れ易くなるという性質をもつ。 In particular, when the density per sheet of toilet paper is high, even if the pressure (cutting pressure) is high, the space between the toilet paper acts as a cushion, reducing the pressure on the paper tube, but the density per sheet is low. Then, the winding of the toilet paper becomes stiff, and the pressure (cutting pressure) on the paper tube increases, so that the paper tube 2 tends to be easily crushed.

そこでトイレットペーパー1枚あたりの密度が高い場合に、ペーパー部3の切断圧力に対する応力が所定の範囲内に収まるようにペーパー部3の特性を設定することで紙管2への圧力を抑え、紙管2の潰れを低減する。 Therefore, when the density per sheet of toilet paper is high, the pressure on the paper tube 2 is suppressed by setting the characteristics of the paper portion 3 so that the stress to the cutting pressure of the paper portion 3 is within a predetermined range, and the paper To reduce collapse of the tube 2.

本発明のトイレットロールは、ペーパー部3の特性が紙管2の潰れを低減するよう設定された2プライのトイレットロールである。なお、本明細書における紙の密度、引張強度、クレープ率、伸び率は下記の通りである。 The toilet roll of the present invention is a two-ply toilet roll in which the properties of the paper portion 3 are set to reduce the crushing of the paper tube 2 . The density, tensile strength, crepe rate and elongation rate of paper in this specification are as follows.

トイレットペーパーの1枚あたりの密度は、坪量を紙厚で割って求めることができる。坪量とは、トイレットロールから引き出したトイレットペーパーをJIS P8124に準拠して1枚あたりの坪量が測定され、紙厚はJIS P8111に準じて試料を調湿後、トイレットロールから引き出したトイレットペーパーをISO12625-3に準じて測定される。 The density per sheet of toilet paper can be obtained by dividing the basis weight by the paper thickness. The basis weight is the basis weight per sheet of toilet paper pulled out from the toilet roll in accordance with JIS P8124, and the paper thickness is measured according to JIS P8111. After conditioning the sample, the toilet paper pulled out from the toilet roll. is measured according to ISO12625-3.

トイレットペーパーの引張強度とは、乾燥引張強度であり、紙を幅15mm、スパン長100mmにカットしたサンプルを、引張速度50mm/分の条件で測定をし、6回の測定の平均を算出した値である。引張強度の測定には、例えば、横型引張試験機(熊谷理機工業株式会社製)を用いることができる。 The tensile strength of toilet paper is the dry tensile strength, and a sample of paper cut into a width of 15 mm and a span length of 100 mm is measured at a tensile speed of 50 mm / min, and the value obtained by calculating the average of 6 measurements. is. For example, a horizontal tensile tester (manufactured by Kumagai Riki Kogyo Co., Ltd.) can be used to measure the tensile strength.

トイレットペーパーの伸び率は、紙を幅15mm、スパン長100mmにカットしたサンプルを、引張速度50mm/分の条件で測定し、6回の測定の平均を算出した値である。伸び率(%)は、試料の伸び量(mm)×100/スパン長(mm)によって求めるものとする。 The elongation rate of the toilet paper is a value obtained by measuring a sample of paper cut into a width of 15 mm and a span length of 100 mm under conditions of a pulling speed of 50 mm/min and calculating the average of six measurements. Elongation rate (%) shall be obtained by elongation amount (mm) of sample x 100/span length (mm).

クレープ率は(ヤンキードライヤーの速度-リール速度)/リール速度×100で求められる。クレープ率が上がると、縦の引張破断伸びが大きくなり、クレープ率を下げると縦の引張破断伸びは小さくなる。 The crepe rate is obtained by (Yankee dryer speed−reel speed)/reel speed×100. As the crepe rate increases, the longitudinal tensile elongation at break increases, and as the crepe rate decreases, the longitudinal tensile elongation at break decreases.

また、ペーパー部の応力、紙管の応力とは、「潰れ強度」であり、トイレットロール、または紙管を定盤の上に中心軸が水平となるように置き、1cm2の円形平型圧縮冶具を取り付けたプッシュプルゲージにより、トイレットロール、または紙管を長さ方向中心位置において垂直に押し潰し、プッシュプルゲージの先端を5mm押し込んだ時の圧力として測定される値である。紙管の強度の調整は、紙管径や、基紙のクラフトパルプの含有量、坪量、密度、基紙の接着面の平滑度、接着剤の塗工量等を調整することで可能である(例えば、特許文献3参照)。 In addition, the stress of the paper part and the stress of the paper tube are "collapse strength". It is a value measured as pressure when a toilet roll or paper tube is vertically compressed at the center position in the longitudinal direction by a push-pull gauge attached with a jig, and the tip of the push-pull gauge is pushed in by 5 mm. The strength of the paper tube can be adjusted by adjusting the paper tube diameter, the kraft pulp content of the base paper, basis weight, density, smoothness of the adhesive surface of the base paper, and the amount of adhesive applied. (See, for example, Patent Document 3).

トイレットロールの巻き芯に使用される紙管2は、複数の基紙を螺旋状に巻き付けて形成したスパイラル紙管とすることができる。 The paper tube 2 used for the winding core of the toilet roll can be a spiral paper tube formed by spirally winding a plurality of base papers.

図4に、2層構造のスパイラル紙管の斜視図を示す。図4に示すように、紙管2は、例えば幅60~80mm程度の細長い形状の帯状紙2枚からなる内面基紙21および外面基紙22を接着剤により互いに張り合わせつつ、螺旋状に巻き付けて形成された2層構造のスパイラル紙管としてもよい。 FIG. 4 shows a perspective view of a two-layered spiral paper tube. As shown in FIG. 4, the paper tube 2 has an inner base paper 21 and an outer base paper 22 made of two elongated strips of paper having a width of about 60 to 80 mm, for example, which are adhered to each other with an adhesive and spirally wound. A formed spiral paper tube having a two-layer structure may be used.

図5(a)~(c)に、2層構造のスパイラル紙管を作製する工程を示す。紙管2を作製するために、先ず内面基紙21をマンドレルシャフト6の中心軸に対して斜め方向に送り込み、内面基紙21の側縁部同士が所定の幅重畳するようにマンドレルシャフトに対してスパイラル状に巻き付ける。内面基紙21の側縁部同士の重なりは、例えば0.5~3.0mm程度とする。内面基紙21の巻き付け工程と並行して、外面基紙22の内側になる面に接着剤を塗工して接着層を形成し、外面基紙22をマンドレルシャフト6の中心軸に対して斜め方向に送り込み、外面基紙22の側縁部同士が重畳しないように、接着層により内面基紙21と貼り合わされるようにマンドレルシャフト6に巻き付けられた内面基紙21に対してスパイラル状に巻き付ける。内面基紙21および外面基紙22が貼り合わされた紙管2が送り出されると、マンドレルシャフト6から突出した紙管2を切断刃7で所定の長さで切断する(例えば、特許文献4、5参照)。 FIGS. 5(a) to 5(c) show the steps of manufacturing a two-layered spiral paper tube. In order to manufacture the paper tube 2, first, the inner base paper 21 is fed obliquely with respect to the central axis of the mandrel shaft 6, and the side edges of the inner base paper 21 overlap each other by a predetermined width. spirally. The overlap between the side edges of the inner base paper 21 is, for example, about 0.5 to 3.0 mm. In parallel with the process of winding the inner base paper 21, an adhesive is applied to the inner surface of the outer base paper 22 to form an adhesive layer, and the outer base paper 22 is inclined with respect to the central axis of the mandrel shaft 6. and spirally wound around the inner base paper 21 wound around the mandrel shaft 6 so that the side edges of the outer base paper 22 are not overlapped with each other and are bonded to the inner base paper 21 by the adhesive layer. . When the paper tube 2 to which the inner surface base paper 21 and the outer surface base paper 22 are attached is sent out, the paper tube 2 protruding from the mandrel shaft 6 is cut to a predetermined length by the cutting blade 7 (for example, Patent Documents 4 and 5). reference).

図6に、紙管の中心軸を含む断面を示す。内面基紙21と外面基紙22との間には接着層23が形成され、この接着層23により内面基紙21と外面基紙22とを貼り合わせて紙管2を形成している。外面基紙22の継ぎ目は、内面基紙21の継ぎ目と重ならない位置に配置することが望ましい。 FIG. 6 shows a cross section including the central axis of the paper tube. An adhesive layer 23 is formed between the inner surface base paper 21 and the outer surface base paper 22 , and the inner surface base paper 21 and the outer surface base paper 22 are adhered together by the adhesive layer 23 to form the paper tube 2 . It is desirable that the seams of the outer base paper 22 are arranged at positions that do not overlap the seams of the inner base paper 21 .

本発明における2プライのトイレットロール1は、ペーパーログから切り出される際に、切断圧力によって紙管2が塑性変形しないために必要なトイレットロールの応力を有する。その具体例として、2プライのトイレットロール1の応力、密度、引張強度、伸び率の組み合わせにおいて、ペーパーログをログソー5で切断した時に紙管2が塑性変形しなかったときの実施例を下表に示す。また、比較例として、紙管2の強度が足りず紙管2が潰れたケースも示す。 The two-ply toilet roll 1 in the present invention has the required toilet roll stress so that the paper tube 2 does not plastically deform due to the cutting pressure when cut from the paper log. As a specific example, in the combination of stress, density, tensile strength, and elongation rate of the two-ply toilet roll 1, the table below shows an example in which the paper tube 2 did not undergo plastic deformation when the paper log was cut with the log saw 5. shown. Also, as a comparative example, a case in which the cardboard tube 2 was crushed due to insufficient strength of the cardboard tube 2 is shown.

Figure 0007239031000001
Figure 0007239031000001

ログソーの切断刃は従来公知の切断刃を用いることができ、ログソーのブレード(切断刃)の厚さとしては2~10mmのものが好適に用いられる。 Conventionally known cutting blades can be used as the cutting blade of the log saw, and the thickness of the log saw blade (cutting blade) is preferably 2 to 10 mm.

ペーパー部3の応力は、紙の密度の影響が強く、さらに引張強度、クレープ率および伸び率も影響する。 The stress in the paper portion 3 is strongly influenced by the density of the paper, and is also influenced by the tensile strength, crepe rate and elongation rate.

表1に実験結果の一部を示すが、トイレットペーパー1枚あたりの密度が0.140g/cm3以上0.180g/cm3以下であり、ペーパー部3の応力は13.0N以上22.0N以下であれば、一般的な紙管2の潰れを大幅に低減できる。 Some of the experimental results are shown in Table 1. The density per sheet of toilet paper is 0.140 g/cm 3 or more and 0.180 g/cm 3 or less, and the stress of the paper portion 3 is 13.0 N or more and 22.0 N. If it is below, crushing of the general paper tube 2 can be significantly reduced.

尚、トイレットペーパー1枚あたりの密度は、0.150g/cm3以上0.180g/cm3以下であれば、紙管2はさらに潰れにくくなる。また、ペーパー部3の応力は、13.0N以上20.0N以下であることが好ましい。ペーパー部の応力が20.0N以上になると、潰れることはないが楕円形に変形する場合が生じるためである。 Incidentally, if the density per sheet of toilet paper is 0.150 g/cm 3 or more and 0.180 g/cm 3 or less, the paper tube 2 is even less likely to collapse. Moreover, the stress of the paper portion 3 is preferably 13.0N or more and 20.0N or less. This is because when the stress of the paper portion is 20.0 N or more, the paper portion is not crushed, but may be deformed into an elliptical shape.

これに対し紙管2の応力は、7.0N以上13.0N以下であることが好ましく、ペーパー部3の応力と紙管2の応力との差は、12.0N以下であることが好ましい。 On the other hand, the stress of the paper tube 2 is preferably 7.0N or more and 13.0N or less, and the difference between the stress of the paper portion 3 and the stress of the paper tube 2 is preferably 12.0N or less.

また、トイレットペーパーの長手方向の引張強度は、1.60N以上2.20N以下であることが好ましく、トイレットペーパー1枚あたりの坪量は14.0~17.0g/m2、紙厚は180~225μmであることが好ましい。 In addition, the tensile strength in the longitudinal direction of the toilet paper is preferably 1.60 N or more and 2.20 N or less, and the basis weight per sheet of toilet paper is 14.0 to 17.0 g/m 2 and the paper thickness is 180. It is preferably ˜225 μm.

紙管2の坪量は130~180g/m2、厚みは180~300μmであることが好ましい。紙管2の直径は36mm以上45mm以下であることが好ましい。 The paper tube 2 preferably has a basis weight of 130 to 180 g/m 2 and a thickness of 180 to 300 μm. The diameter of the paper tube 2 is preferably 36 mm or more and 45 mm or less.

表1ではトイレットロールの巻長を50m、巻径を114mmとしているが、トイレットペーパー1枚あたりの密度、ペーパー部3の応力、紙管2の応力、トイレットペーパーの長手方向の引張強度が上記要件を満たしていれば、トイレットロールの巻長は45~55m、巻径は112~120mmとすることができる。 In Table 1, the roll length of the toilet roll is 50 m, and the roll diameter is 114 mm. is satisfied, the roll length of the toilet roll can be 45 to 55 m, and the roll diameter can be 112 to 120 mm.

1 トイレットロール
2 紙管
3 衛生紙部
4 ペーパーログ受けガイド
5、7 切断刃
6 マンドレルシャフト
21 内面基紙
22 外面基紙
23 接着層
REFERENCE SIGNS LIST 1 toilet roll 2 paper tube 3 sanitary paper section 4 paper log receiving guide 5, 7 cutting blade 6 mandrel shaft 21 inner base paper 22 outer base paper 23 adhesive layer

Claims (6)

紙管と、前記紙管に2プライのトイレットペーパーを巻き付けたトイレットペーパー部とを備えたトイレットロールであって、
前記トイレットペーパー1枚あたりの密度が0.140g/cm3以上0.180g/cm3以下であり、前記トイレットペーパー部の応力は13.0N以上22.0N以下であり、前記紙管の応力が7.0N以上13.0N以下であり、前記トイレットペーパー部の応力と前記紙管の応力との差が12.0N以下であることを特徴とするトイレットロール。
A toilet roll comprising a paper tube and a toilet paper section in which two plies of toilet paper are wound around the paper tube,
The density per sheet of toilet paper is 0.140 g/cm 3 or more and 0.180 g/cm 3 or less, the stress of the toilet paper portion is 13.0 N or more and 22.0 N or less, and the stress of the paper tube is 7.0 N or more and 13.0 N or less, and a difference between the stress of the toilet paper portion and the paper tube is 12.0 N or less.
前記トイレットペーパーの長手方向の長さが45~55mであって、前記トイレットロールの直径が112~120mmであることを特徴とする請求項1に記載のトイレットロール。 2. The toilet roll according to claim 1, wherein the length of the toilet paper in the longitudinal direction is 45-55 m, and the diameter of the toilet roll is 112-120 mm. 前記トイレットペーパーの坪量が14.0~17.0g/m2、紙厚が180~225μmであることを特徴とする請求項1または2に記載のトイレットロール。 3. The toilet roll according to claim 1, wherein the toilet paper has a basis weight of 14.0 to 17.0 g/m 2 and a paper thickness of 180 to 225 μm. 前記トイレットペーパーの長手方向の引張強度が1.60N以上2.20N以下であることを特徴とする請求項1~3のいずれかに記載のトイレットロール。 The toilet roll according to any one of claims 1 to 3, wherein the tensile strength in the longitudinal direction of the toilet paper is 1.60N or more and 2.20N or less. 前記紙管は、複数枚の帯状紙を互いに貼り合わせて貼り合わせたスパイラル紙管であることを特徴とする請求項1~4のいずれかに記載のトイレットロール。 5. The toilet roll according to any one of claims 1 to 4, wherein the paper tube is a spiral paper tube formed by laminating a plurality of strips of paper together. 前記紙管の直径が36mm以上45mm以下であることを特徴とする請求項1~5のいずれかに記載のトイレットロール。 The toilet roll according to any one of claims 1 to 5, wherein the paper tube has a diameter of 36 mm or more and 45 mm or less.
JP2022015001A 2017-12-28 2022-02-02 toilet roll Active JP7239031B2 (en)