JP5660159B2 - 金属箔シートの製造方法 - Google Patents
金属箔シートの製造方法 Download PDFInfo
- Publication number
- JP5660159B2 JP5660159B2 JP2013100906A JP2013100906A JP5660159B2 JP 5660159 B2 JP5660159 B2 JP 5660159B2 JP 2013100906 A JP2013100906 A JP 2013100906A JP 2013100906 A JP2013100906 A JP 2013100906A JP 5660159 B2 JP5660159 B2 JP 5660159B2
- Authority
- JP
- Japan
- Prior art keywords
- metal foil
- etching
- foil sheet
- pattern
- resist ink
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
金属箔シート原反12として、厚さ35μm、幅500mm、長さ500mのロール状に巻き上げられた銅箔を用いた。
金属箔シート原反12として、厚さ35μm、幅500mm、長さ500mのロール状に巻き上げられたアルミニウム箔を用いた。レジストインキ13をパターン印刷する工程およびエッチングマスク14を設ける工程は、実施例1と同じ方法で行った。
2 エッチング絵柄
3 未加工部分
4 貫通孔
5、16 非エッチング部
12 金属箔シート原反
13 レジストインキ
14 エッチングマスク
15 エッチング部
Claims (1)
- 所定形状の貫通孔が一定間隔で規則的に配列され、継ぎ目のない連続するエッチング絵柄を有する金属箔シートの製造方法であって、
金属箔シート原反表面に、輪転印刷によって所定形状の貫通孔が一定間隔で規則的に配列されるようにレジストインキをパターン印刷する工程と、
前記パターン印刷された金属箔シート原反の表面をエッチング加工する工程と、
前記レジストインキを除去する工程と、
前記レジストインキを除去する工程の後に、前記エッチング加工された金属箔シート原反を巻き取る工程と、
を有し、
前記エッチング加工が、片面エッチング加工であり、前記エッチング加工する工程の前に、前記パターン印刷された面の裏面全体にエッチングマスクを設ける工程と、前記エッチング加工する工程の後に、前記エッチングマスクを除去する工程とをさらに有し、
前記パターン印刷された面の裏面全体に設けられる前記エッチングマスクが、前記パターン印刷された面からアルカリ溶液を用いることなく剥離可能な弱粘着性フィルムを含み、
前記エッチングマスクを除去する工程では、アルカリ溶液を用いることなく、前記弱粘着性フィルムを除去することを特徴とする金属箔シートの製造方法。